Search NASA⌕ Search

SEARCH · Search NASA

Results for “coating durability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Composition and method embodiments for plating metal coatings

Disclosed herein are embodiments of a coating composition and a method of using the same for forming metal coatings on substrates. In particular embodiments, the coating composition comprises a deep eutectic solvent and/or an ionic liquid; a metal precursor; an alkali metal salt; and an optional additive component. The coating composition and method embodiments disclosed herein provide durable, even, high-surface area coatings on various types of substrates and also can be used at low temperatures.

Hubbard, Lance R.↗

High Throughput In-Line Coating Metrology Development for Solid Oxide Fuel Cell Manufacturing

Coatings play key roles in solid oxide fuel cell (SOFC) stack durability. For example, diffusion barrier coatings on Cr-containing interconnect and balance of plant (BOP) components protect electrodes from Cr poisoning over the long operational lifetimes (>10,000 hours) of the fuel cell stack. Common defects in coatings, such as cracks, pinholes, and porosity, result in a failure to protect the electrodes, resulting in shorter operational lifetime and thus higher cost. It is very unlikely, even in the best coating process, that all these defects can be mitigated, hence identifying critical defects in parts, and removing defective parts from production before they can damage the stack, becomes paramount. Furthermore, these quality control techniques must be operational in the production/assembly line (in-line), i.e., high throughput and non-destructive, and cost effective. Redox Power Systems, LLC (Redox) together with the National Renewable Energy Laboratory (NREL) developed much needed high throughput, in-line metrology techniques for protective coatings. The overall goal of the project is to lower cost while increasing robustness, reliability, and endurance of SOFC stacks. To accomplish this, we had several objectives, including: to identify key coating and substrate defects that lead to coating failure through the use of detailed characterization methods (e.g., microscopy, XRD, EDS, electrochemistry); to assess capabilities of in-line metrology techniques, e.g., optical profilometry (Redox) and thermography (NREL), to probe these defects, or evidence thereof; demonstrate long-term performance of “defect-free” protective coatings, as identified by in-line metrology, in solid oxide fuel cell (SOFC) stack operation. In the first part of this project, the ability to identify key defects expected to lead to coating and SOFC degradation using in-line metrology tools were evaluated. Coated interconnect samples with controlled defect types and populations were tested under conditions similar to SOFC operation, followed by detailed post-test analysis to reveal the defects responsible for observed degradation. In the second part of the project, the optimal in-line metrology techniques and methodologies were used to map the defect distribution in full-size interconnects with critical defects intentionally allowed to exist in some cases. These interconnects underwent SOFC testing for extended periods (up to ~3,000 hours) followed by post-test analysis to evaluate the effectiveness of in-line metrology techniques in mitigating MCO coating related degradation. Key accomplishments in this project included the following: Demonstrated ASR of < 0.05 ohm-cm 2 at 650 °C for 1,000 hours with low defect (determined by in-line metrology) interconnect samples (average ASR=37 milliohms-cm 2 after over 1,000 hours). Demonstrated that low defect coatings on interconnects (as screened using in-line metrology) have low volatilization of chromium at ~650 °C for 1,000 hours as detected using Cr-getter material (< 5 at% increase above baseline); 1022 hour duration tests under humidified, elevated temperature (750 °C rather than 650 °C) compared a base case against different coating thicknesses. Demonstrated capability to identify initial key defects of interest with in-line metrology techniques using up to 8 cm by 10 cm having coatings with and without intentional defects of interest using thermal imaging and optical profilometry. Correlated key defects identified using metrology techniques with observed coating performance (e.g., ASR and Cr volatility). Conducted several 4 cm by 4 cm cell tests using MCO-interconnects that were pre-screened using some of the metrology techniques developed in the project (e.g., optical profilometry). An analysis of ASR measurements were able to show that defect-free coatings resulted in the anticipated performance in the cell tests.

01 COAL, LIGNITE, AND PEAT↗

Thermal barrier coating evaluation needs

A 0.025 cm (0.010 in) thick thermal barrier coating (TBC) applied to turbine airfoils in a research gas turbine engine provided component temperature reductions of up to 190 C. These impressive temperature reductions can allow increased engine operating temperatures and reduced component cooling to achieve greater engine performance without sacrificing component durability. The significant benefits of TBCs are well established in aircraft gas turbine engine applications and their use is increasing. TBCs are also under intense development for use in the Low Heat Rejection (LHR) diesel engine currently being developed and are under consideration for use in utility and marine gas turbines. However, to fully utilize the benefits of TBCs it is necessary to accurately characterize coating attributes that affect the insulation and coating durability. The purpose there is to discuss areas in which nondestructive evaluation can make significant contributions to the further development and full utilization of TBCs for aircraft gas turbine engines and low heat rejection diesel engines.

Brindley, William J.↗

Thermal Conductivity and Erosion Durability of Composite Two-Phase Air Plasma Sprayed Thermal Barrier Coatings

To enhance efficiency of gas turbines, new thermal barrier coatings (TBCs) must be designed which improve upon the thermal stability limit of 7 wt% yttria stabilized zirconia (7YSZ), approximately 1200 C. This tenant has led to the development of new TBC materials and microstructures capable of improved high temperature performance. This study focused on increasing the erosion durability of cubic zirconia based TBCs, traditionally less durable than the metastable t' zirconia based TBCs. Composite TBC microstructures composed of a low thermal conductivity/high temperature stable cubic Low-k matrix phase and a durable t' Low-k secondary phase were deposited via APS. Monolithic coatings composed of cubic Low-k and t' Low-k were also deposited, in addition to a 7YSZ benchmark. The thermal conductivity and erosion durability were then measured and it was found that both of the Low-k materials have significantly reduced thermal conductivities, with monolithic t' Low-k and cubic Low-k improving upon 7YSZ by approximately 13 and approximately 25%, respectively. The 40 wt% t' Low-k composite (40 wt% t' Low-k - 60 wt% cubic Low-k) showed a approximately 22% reduction in thermal conductivity over 7YSZ, indicating even at high levels, the t' Low-k secondary phase had a minimal impact on thermal in the composite coating. It was observed that a mere 20 wt% t' Low-k phase addition can reduce the erosion of a cubic Low-k matrix phase composite coating by over 37%. Various mixing rules were then investigated to assess this non-linear composite behavior and suggestions were made to further improve erosion durability.

Rare earth zirconia↗

Multilayer, Multimaterial Thermal Barrier Coating Systems: Design, Synthesis, and Performance Assessment

Thermal barrier coatings ( TBC s) are increasingly playing a vital role in enhancing efficiency and performance of gas turbine engines. As engine operating temperatures rise, yttria‐stabilized zirconia ( YSZ ), the currently principal TBC material, reaches its operational limits. Gadolinium Zirconate ( GDZ )‐based pyrochlore oxides are now emerging contenders, not only due to their lower thermal conductivity, but also their ability to resist attack by silicate deposits. However, GDZ cannot be directly substituted for YSZ due to its incompatibility with the thermally grown alumina layer, therefore requiring to be a component of multilayer system. Although industry has already adopted these materials in various applications, a number of fundamental issues arise with respect to layered‐coating design, their properties and processing dependence. In this study several multilayer architectures, based on the YSZ – GDZ system, have been developed and tested for durability under furnace thermal cycling conditions. Coating designs considered optimization of microstructure and properties of individual layers based on their location within the top‐coat thickness to address competing interests of thermal conductivity, compliance, and resistance to silicates. A large variance in durability was observed in coatings made with different multilayer designs. The results and the associated failure mechanisms are rationalized through preliminary evaluation of elastic energies at the failure locations and corresponding energy release rates. The results point to new strategies in the design and manufacturing of optimal multilayer coatings.

Viswanathan, Vaishak↗

Property Evaluation and Damage Evolution of Environmental Barrier Coatings and Environmental Barrier Coated SiC/SiC Ceramic Matrix Composite Sub-Elements

This paper describes recent development of environmental barrier coatings on SiC/SiC ceramic matrix composites. The creep and fatigue behavior at aggressive long-term high temperature conditions have been evaluated and highlighted. Thermal conductivity and high thermal gradient cyclic durability of environmental barrier coatings have been evaluated. The damage accumulation and complex stress-strain behavior environmental barrier coatings on SiCSiC ceramic matrix composite turbine airfoil subelements during the thermal cyclic and fatigue testing of have been also reported.

Creep and fatigue↗

Transparent superhydrophobic surfaces using a spray coating process

One significant maintenance problem and cost associated with solar energy conversion systems is the soiling due to the accumulation of dust and other pollutants. Here in this work, we describe a scalable approach for applying antisoiling coatings based on superhydrophobic (SH) silica particles using a spray coating process. A large water contact angle (WCA) is one of the characteristics of excellent SH surfaces and because of the low surface energy and low adhesion forces the soiling rate is reduced. Our findings indicate that the WCA depends strongly on the ratio of the polymer binder and the nanoparticles. The nanoparticle surface coverage of the spray coated samples was substantially improved after rinsing with solvent. This process tended to remove large aggregates and excess polymer binder and further increased the WCA by allowing exposure of the functionalized nanoparticles. The durability of the SH coatings was enhanced when the substrate was pretreated with polymer binder and an optimal curing time between 30 and 60 min. The abrasion tests of the SH coatings we report in this study showed that the WCA decreased from ~ 166° to ~ 157° after exposure to 2.6 g of sand. Such coatings will help reduce costs of periodic cleaning of solar energy conversion systems (photovoltaic panels and concentrated solar mirrors).

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Environmental Barrier Coatings Having a YSZ Top Coat

Environmental barrier coatings (EBCs) with a Si bond coat, a yttria-stabilized zirconia (YSZ) top coat, and various intermediate coats were investigated. EBCs were processed by atmospheric pressure plasma spraying. The EBC durability was determined by thermal cycling tests in water vapor at 1300 C and 1400 C, and in air at 1400 C and 1500 C. EBCs with a mullite (3Al2O3 (dot) 2SiO2) + BSAS (1 - xBaO (dot) xSrO (dot) Al2O3 (dot) 2SiO2) intermediate coat were more durable than EBCs with a mullite intermediate coat, while EBCs with a mullite/BSAS duplex intermediate coat resulted in inferior durability. The improvement with a mullite + BSAS intermediate coat was attributed to enhanced compliance of the intermediate coat due to the addition of a low modulus BSAS second phase. Mullite + BSAS/YSZ and BSAS/YSZ interfaces produced a low melting (less than 1400 C) reaction product, which is expected to degrade the EBC performance by increasing the thermal conductivity. EBCs with a mullite + BSAS / graded mullite + YSZ intermediate coat showed the best durability among the EBCs investigated in this study. This improvement was attributed to diffused CTE (Coefficient of Thermal Expansion) mismatch stress and improved chemical stability due to the compositionally graded mullite+YSZ layer.

Lee, Kang N.↗

Coatings and Process Development for Reduced Energy Automotive OEM Manufacturing Final Technical Report

The project team successfully developed a new low-temperature coating system that achieves performance, durability, and appearance requirements for an Automotive Original Equipment Manufacturer paint system. This coating system is compatible with current OEM manufacturing paint lines, allowing application to existing manufacturing locations. The new coating system can also save capital expenses for new lines or renovations of existing lines. The new paint system enable energy savings and operational expense savings. DURR has designed a reference system that can serve as the starting point for new or retrofit paint line upgrades to this low temperature coating system. NDSU has developed and demonstrated the value of high-throughput screening for polymers and cure performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improved adhesion of polyurethane-based nanocomposite coatings to tin surface through silane coupling agents

Conformal coatings with higher adhesion strength is critical for mitigating the growth of whiskers from the pure tin (Sn) or Sn-rich surfaces of the Pb-free electronics. Silane coupling agents have the ability to form a durable bond between polymeric coatings and metallic materials. The main goal of this paper is to investigate the effect of silane agents on the adhesion behavior of polyurethane (PU), polyurethane acrylate (PUA) and both coatings filled with silicone rubber (SR) nanoparticles on the tin solder pads. It was found that an isocyanate-based silane provided excellent adhesion for PU and PU + SR coatings and an acrylic-based silane for PUA and PUA + SR coatings on the tin surface. This was due to the reaction bond formation between the silane coupling agent and the coating. Hence, the selection of silane coupling agents with the organofunctional group similar to the coating material is crucial to improve the adhesion properties of the coating.

36 MATERIALS SCIENCE↗

Demonstration of a 600 Watt Hybrid Iodine-Xenon Electric Propulsion System

This paper reviews recent iodine compatible electric propulsion technologies evaluated at the NASA Glenn Research Center. The work culminated in a 1,174-hour hybrid iodine-xenon propulsion system durability demonstration (iodine fed thruster with xenon fed cathode). The test demonstrated that (i) a Hall-effect thruster operates with nearly identical performance whether employing iodine or xenon propellant, (ii) careful selection of propulsion system materials and coatings can result in durable iodine-compatible hardware, and (iii) implementation of appropriate facility improvements and procedures can limit negative impacts of iodine on test hardware and ground support equipment. The work was motivated by advancements in capability of very dense small-spacecraft (<500 kg), but spacecraft still lacking very dense in-space propulsion to provide the large delta-v capabilities (3 to 10 km/s) required for many high-value NASA exploration and science missions. Volume limitations of small-spacecraft not only require dense propulsion systems, but more so dense propellants. NASA identifies xenon and iodine as having both favorable storage densities and propulsive properties to enable many NASA small-spacecraft mission scenarios. While xenon is inert and well-proven in spaceflight applications, iodine has triple the storage density of xenon and stores at low pressures, permitting use of conformal tank designs. Unlike xenon, iodine does raise concerns related to its reactivity with most materials, potential spacecraft-propellant interactions, impact on ground test facilities, and challenges to acceptance test iodine propulsion systems prior to flight. This work begins to address these challenges. This work was conducted under the Advanced In-Space Propulsion (AISP) project funded through the Game Changing Development (GCD) program within NASA's Science Technology Mission Directorate (STMD).

Benavides, G. F.↗

Plasma sprayed ceramic thermal barrier coating for NiAl-based intermetallic alloys

A thermal barrier coating system consists of two layers of a zirconia-yttria ceramic. The first layer is applied by low pressure plasma spraying. The second layer is applied by conventional atmospheric pressure plasma spraying. This facilitates the attachment of a durable thermally insulating ceramic coating directly to the surface of a highly oxidation resistant NiAl-based intermetallic alloy after the alloy has been preoxidized to promote the formation of a desirable Al2O3 scale.

Miller, Robert A.↗

Rapid and Efficient Deposition of Metal Oxide Coatings for Bearings and Gears in Harsh Environments

The objective of this project is to develop Tribocoating; an innovative, rapid, low-cost, energy-efficient, and environmentally friendly coating technology designed to enhance the performance and durability of bearings and gears operating under harsh conditions. Tribocoating creates protective metal-oxide tribofilms through in-situ tribosintering of nanocrystals (NCs). Components are simply run in a nano-enabled Tribocoating fluid prior to deployment; no surface pretreatment, coating equipment, or external energy input is required.

17 WIND ENERGY↗

The Development of Erosion and Impact Resistant Turbine Airfoil Thermal Barrier Coatings

Thermal barrier coatings are used in gas turbine engines to protect engine hot-section components in the harsh combustion environments and extend component lifetimes. For thermal barrier coatings designed for turbine airfoil applications, further improved erosion and impact resistance are crucial for engine performance and durability. Advanced erosion resistant thermal barrier coatings are being developed, with a current emphasis on the toughness improvements using a combined rare earth- and transition metal-oxide doping approach. The performance of the doped thermal barrier coatings has been evaluated in burner rig and laser heat-flux rig simulated engine erosion and thermal gradient environments. The results have shown that the coating composition optimizations can effectively improve the erosion and impact resistance of the coating systems, while maintaining low thermal conductivity and cyclic durability. The erosion and impact damage mechanisms of the thermal barrier coatings will also be discussed.

Zhu, Dongming↗

Nanostructured CVD Tungsten Carbide Coating on Aircraft Actuators and Gearbox Shafts Reduces Oil Leakage and Improves Durability

Wear and corrosion of aircraft actuator parts, helicopter gearbox rotating shafts and wear of seals working against these parts can lead to oil leaks which require expensive maintenance and increase the risk of failure. The Hardide® nanostructured chemical vapor deposition (CVD) Tungsten Carbide coating was tested on metal parts working against seals as an approach to reduce oil leakage from gearboxes and actuators and increase maintenance intervals. The coating protects metal pistons and shafts from abrasion and corrosion, keeping their surface roughness parameters within optimum ranges for longer; this reduces seal wear and makes the whole unit more durable and reliable. The 50-100 micron-thick CVD Hardide coating can be applied uniformly on internal and external surfaces and has enhanced fatigue and anti-galling properties. The coating has high wear resistance outperforming Hard Chrome by 14 times and Thermal Spray WC-Co (12%) by three times. The fine-grain coating nanostructure wears uniformly so even worn Hardide coating shows no hard micro-grain asperities which are abrasive for seals. The coating is free from porosity and from Cobalt binder and is an effective barrier against corrosion. As a result the coating keeps the optimal seal-friendly surface finish for longer even in abrasive and corrosive environments. The coating was qualified by Airbus as an environmentally friendly replacement for Hard Chrome plating.

36 MATERIALS SCIENCE↗

Effects of Strain Gauge Coatings on Water Intrusion in Submerged Composite Coupon Testing

Marine energy structures are typically made using composite materials and are repeatedly loaded by currents and waves. Submersion and repeated loading lead to two environmental effects: moisture intrusion and mechanical fatigue. To understand their combined effects, submerged fatigue testing can be used. Submerged fatigue testing often requires submerged instrumentation to validate component manufacturing methods and models. Strain measurements are critical for understanding marine energy component loads. One common method for measuring strain is by using foil strain gauges, but the durability of strain gauges in submerged fatigue conditions is not well-understood. To increase strain gauge durability and protection from contamination, delamination, and water intrusion, strain gauge coatings may be applied over strain gauges and wire connections. In this study, strain gauges were adhered to composite coupons, coated, and mechanically tested in a water tank. Cycles to composite failure, cycles to strain gauge failure (SGF), strains, and SGF modes were used to measure the effects of strain gauge coatings on composite fatigue life and strain gauge durability. The coatings did not have significant effects on composite fatigue life or strain gauge durability. The methods developed and measurements taken at the coupon scale in this study will be used to inform methods and designs for subsequent submerged subcomponent testing, full-scale testing, and standards development. The benefits of designing marine energy structures to informed standards and designs are decreased lifetime costs and increased reliability and energy production, ultimately leading to a sustainable and low-carbon energy system.

composite materials↗

Aerogel Development

Aerogel is one of the most promising materials of the future. It's unique properties, including high porosity, transparency, very high thermal tolerance, and environmental friendliness give it the potential of replacing many different products used in society today. However, the market for aerogel is still very limited because of the cost of producing the material and its fragility. The principle objective of my project has been to find new ways to apply aerogel in order to increase its practicality and appeal to different aspects of society. More specifically, I have focused on finding different chemicals that will coat aerogel and increase its durability. Because aerogel is so fragile and will crumble under the pressure of most coatings this has been no easy task. However, by experimenting with many different coatings and combinations of aerogel properties, I have made several significant discoveries. Aerogel (ideally, high density and hydrophobic) can be coated with several acrylic polymers, including artist's gel and nail polish. These materials provide a protective layering around the aerogel and keep it from breaking as easily. Because fragility is one of the main reasons applications of aerogel are limited, these discoveries will hopefully aid in finding future applications for this extraordinary material.

Sahai, Rashmi K.↗

Issues and Consequences of Atomic Oxygen Undercutting of Protected Polymers in Low Earth Orbit

Hydrocarbon based polymers that are exposed to atomic oxygen in low Earth orbit are slowly oxidized which results in recession of their surface. Atomic oxygen protective coatings have been developed which are both durable to atomic oxygen and effective in protecting underlying polymers. However, scratches, pin window defects, polymer surface roughness and protective coating layer configuration can result in erosion and potential failure of protected thin polymer films even though the coatings are themselves atomic oxygen durable. This paper will present issues that cause protective coatings to become ineffective in some cases yet effective in others due to the details of their specific application. Observed in-space examples of failed and successfully protected materials using identical protective thin films will be discussed and analyzed. Proposed approaches to prevent the failures that have been observed will also be presented.

Banks, Bruce A.↗