Search NASA⌕ Search

SEARCH · Search NASA

Results for “dislocation densities”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Flow of the current along metallic shunts in ohmic contacts to wide-gap III-V semiconductors

It is established experimentally that the contact metal-wide-gap semiconductor (GaAs, GaP, GaN) with the Schottky barrier transforms into the ohmic contact either in the process of continuous heating or in the process of holding at an elevated temperature before the formation of any recrystallized layers. In this case, resistance of the contact reduced to the unit area increases as the temperature increases for semiconductors with a high dislocation density (GaP, GaN). It is assumed that in such contacts, the current flows along the metallic shunts, which shorten the layer of space charge and are formed by metal atoms diffused along the dislocation lines or other imperfections of the semiconductor. In semiconductors with a low dislocation density (GaAs), resistance of the ohmic contact per unit area decreases with increasing the temperature as it was expected for the thermionic mechanism of current flowing.

36 MATERIALS SCIENCE↗

Strategies for Thinning Graded Buffer Regions in Metamorphic Solar Cells and Performance Tradeoffs

Compositionally graded buffers (CGBs) have enabled the development of inverted metamorphic (IMM) multijunction solar cells that contain three or more junctions and exhibit record efficiencies. Typically, the CGB is grown thick with a constant grading rate, because this is the most straightforward way to minimize the threading dislocation density (TDD) in device active regions. The CGB growth represents a significant expense, in terms of materials consumption and capital cost, however, hampering the economic viability of metamorphic devices. This work explores strategies for thinning Ga1-xInxP CGBs from GaAs to InP while minimizing performance loss, as evaluated by the open-circuit voltage (VOC) of ~0.74 eV Ga0.47In0.53As solar cells. Using the Ga1-xInxP CGB as a model, we demonstrate that slower grading is necessary in certain regions of the grade where dislocation nucleation rates are higher. Grading must be more gradual in these regions to suppress threading dislocation density. Grading rates can be increased in non-critical areas where dislocation nucleation is lower, permitting a thinner buffer. We demonstrate the relationship between VOC and TDD, establishing tradeoffs between thickness and performance. Through careful design, we demonstrate a CGB with a 40% thickness reduction (2 im) achieved with a VOC decrease of only 6.3% (21 mV).

14 SOLAR ENERGY↗

Hardness and microstructural inhomogeneity at the epitaxial interface of laser 3D-printed Ni-based superalloy

Here in this letter, microstructural and mechanical inhomogeneities, a great concern for single crystal Ni-based superalloys repaired by laser assisted 3D printing, have been probed near the epitaxial interface. Nanoindentation tests show the hardness to be uniformly lower in the bulk of the substrate and constantly higher in the epitaxial cladding layer. A gradient of hardness through the heat affected zone is also observed, resulting from an increase in dislocation density, as indicated by the broadening of the synchrotron X-ray Laue microdiffraction reflections. Lastly, the hardening mechanism of the claddin g region, on the other hand, is shown to originate not only from high dislocation density but also and more importantly from the fine γ/γ' microstructure.

36 MATERIALS SCIENCE↗

Diffusion and Deformation Mechanism Maps in Li Metal from Atomistic Simulations

The rate of Li transport in the Li metal anode is important for the operation of Li metal-solid state batteries. Here, transport rates due to diffusion and creep are predicted in Li using atomistic simulations. First, molecular dynamics is used to estimate the rate of Li diffusion along dislocations and in grain boundary triple junctions. By combining this data with that from a prior study of grain boundary diffusion the dominant mechanisms and rates of self-diffusion in Li polycrystals are predicted as a function of grain size, grain shape, dislocation density, and temperature. Second, the dominant creep mechanisms are predicted and used to estimate critical current densities and void annihilation times. Grain boundary sliding and coble creep are the dominant mechanisms for micron-sized grains. Lastly, a continuum model for interfacial contact loss reveals that high dislocation densities of ∼10 12 /cm 2 enable achieving battery performance targets for Li grain sizes of ∼10 μm.

Batteries↗

Features of the Temperature Dependence of the Specific Contact Resistance of Au–Ti–Pd–n{sup +}–n-Si Diffusion Silicon Structures

The temperature dependences of the specific contact resistance of silicon ρ{sub c} with a doping step are measured experimentally and described theoretically. The measurements are performed in the temperature range from 4.2 to 380 K. It is established that the contacts of the studied Au–Ti–Pd–n{sup +}–n-Si structures are ohmic. It is shown that minimal ρ{sub c} is implemented at T = 75 K. Its value rises both with a decrease in temperature (due to the freezing effect) and with an increase in temperature (due to the electron-enriched layer at the boundary with the bulk material). It is established that the bulk electron concentration strongly decreases in the near-contact region in a layer with a thickness on the order of one micron due to the compensation of silicon by deep acceptors appearing because of the formation of a rather high vacancy concentration during stress relaxation and the appearance of a high dislocation density, as well as due to their diffusion from the contact after heating to 450°C. The data on the occurrence of vacancy-type defects are confirmed by X-ray measurements. The dislocation density in the studied structures is also estimated from X-ray measurements.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

MULTI-SCALE DIFFRACTION STUDY OF REVERSIBLE/IRREVERSIBLE DEFORMATION MECHANISMS IN THE NI-BASED SUPERALLOYS DURING FATIGUE

In this study, a nickel-based polycrystalline is subjected to cyclic loading. The subsequent fatigue damage has been investigated with in-situ neutron-diffraction, thermal characterization for a single-phase, transmission-electron microscopy (TEM) and polychromatic X-ray microdiffraction (PXM). Different stages of fatigue damage are observed including bulk hardening, softening, and eventual saturation evident in the diffraction patterns and the thermal-evolution features. An increase in dislocation density is responsible for hardening within the early cycles. The transition to saturation cycles is characterized by the anisotropy of the lattice-strain evolution. Inhomogeneity of the thermal response and irreversible compression of the lattice planes and statistical dislocation structures are observed in the final saturation fatigue cycles. Analysis of the PXM-Laue patterns reveals cyclically-deformed microstructure near the grain boundaries, which are composed of the lattice rotations and grain subdivisions. The PXM results are in good agreement with the TEM results. Combined simulation/experimental analysis allows determination of slip-system dependent dislocation density in individual grains.

36 MATERIALS SCIENCE↗

Effect of dislocations on electron mobility in AlGaN/GaN and AlGaN/AlN/GaN heterostructures

Al{sub x}Ga{sub 1-x}N/GaN (x = 0.06, 0.12, 0.24) and AlGaN/AlN/GaN heterostructures were grown on 6 H-SiC, GaN-on-sapphire, and free-standing GaN, resulting in heterostructures with threading dislocation densities of {approx}2 Multiplication-Sign 10{sup 10}, {approx}5 Multiplication-Sign 10{sup 8}, and {approx}5 Multiplication-Sign 10{sup 7} cm{sup -2}, respectively. All growths were performed under Ga-rich conditions by plasma-assisted molecular beam epitaxy. Dominant scattering mechanisms with variations in threading dislocation density and sheet concentration were indicated through temperature-dependent Hall measurements. The inclusion of an AlN interlayer was also considered. Dislocation scattering contributed to reduced mobility in these heterostructures, especially when sheet concentration was low or when an AlN interlayer was present.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure, Hardness, and Residual Stress of the Dissimilar Metal Weldments of SA508-309L/308L-304L

A dissimilar metal weldment consisting of SA508-309L-308L-304L is widely used in light-water nuclear reactors. These weldments demonstrate dissimilar susceptibility to stress corrosion cracking that are related to the microstructure, properties, and residual stress. In this work, microstructures, hardness, and the residual stress distribution of the dissimilar metal weldments were investigated, with the correlation of increased hardness in the heat-affected zone (HAZ) to the microstructure. 304L HAZ demonstrated similar grain morphology as the base material, and the increase in hardness was primarily attributed to the increased dislocation density. SA508 HAZ demonstrated a change of grain morphology resulting from the different peak temperatures and cooling rates. The increased hardness in the SA508 HAZ was attributed to the refined grain morphology, higher dislocation density, and higher number density of precipitates. A ~ 20–30-μm-wide martensitic zone formed at the fusion boundary of SA508-309L, where Cr-rich carbide precipitates were observed, with the average size and the number density of 44.1 ± 16.9 nm and 1.5 × 10 21 m ₋3 , respectively. In conclusion, residual stress results demonstrated the largest tensile stress at 309L butter, indicating its high cracking susceptibility.

36 MATERIALS SCIENCE↗

Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP)

Thermal stability of the ultra-fine grained (UFG) microstructure of magnesium AZ31 alloy was investigated. UFG microstructure was achieved by a combined two-step severe plastic deformation process: the extrusion (EX) and subsequent equal-channel angular pressing (ECAP). This combined process leads to refined microstructure and enhanced microhardness. Specimens with UFG microstructure were annealed isochronally at temperatures 150–500 °C for 1 h. The evolution of microstructure, mechanical properties and dislocation density was studied by electron backscatter diffraction (EBSD), microhardness measurements and positron annihilation spectroscopy (PAS). The coarsening of the fine-grained structure at higher temperatures was accompanied by a gradual decrease of the microhardness and decrease of dislocation density. Mechanism of grain growth was studied by general equation for grain growth and Arrhenius equation. Activation energies for grain growth were calculated to be 115, 33 and 164 kJ/mol in temperature ranges of 170–210 °C, 210–400 °C and 400–500 °C (443–483 K, 483–673 K and 673–773 K), respectively. - Highlights: • Microhardness of UFG AZ31 alloy decreases with increasing annealing temperature. • This fact has two reasons: dislocation annihilations and/or grain growth. • The activation energies for grain growth were calculated for all temperature ranges.

36 MATERIALS SCIENCE↗

The comparison of microstructures and mechanical properties between 14Cr-Al and 14Cr-Ti ferritic ODS alloys

In this study, two kinds of 14Cr ODS alloys (14Cr-Al and 14Cr-Ti) were investigated to reveal the different effects between Al and Ti on the microstructures and mechanical properties of 14Cr ferritic ODS alloys. The microstructure information such as grains, minor phases of these two alloys has been investigated by high-energy X-ray diffraction and transmission electron microscopy (TEM). The in situ synchrotron X-ray diffraction tensile test was applied to investigate the mechanical properties of these two alloys. The lattice strains of different phases through the entire tensile deformation process in these two alloys were analyzed to calculate their elastic stresses. From the comparison of elastic stress, the strengthening capability of Y 2 Ti 2 O 7 is better than TiN in 14Cr-Ti, and the strengthening capability of YAH is much better than YAM and AlN in 14Cr-Al ODS. The dislocation densities of 14Cr-Ti and 14Cr-Al ODS alloys during tensile deformation were also examined by modified Williamson-Hall analyses of peak broadening, respectively. In conclusion, the different increasing speed of dislocation density with plastic deformation reveals the better strengthening effect of Y-Ti-O particles in 14Cr-Ti ODS than that of Y-Al-O particles in 14Cr-Al ODS alloy.

36 MATERIALS SCIENCE↗

Strain relaxation properties of InAs{sub y}P{sub 1-y} metamorphic materials grown on InP substrates

The strain relaxation mechanism and defect properties of compositionally step-graded InAs{sub y}P{sub 1-y} buffers grown by molecular beam epitaxy on InP have been investigated. InAsP layers having lattice misfits ranging from 1% to 1.4% with respect to InP, as well as subsequently grown lattice matched In{sub 0.69}Ga{sub 0.31}As overlayers on the metamorphic buffers were explored on both (100) and 2 deg. offcut (100) InP substrates. The metamorphic graded buffers revealed very efficient relaxation coupled with low threading dislocation densities on the order of (1-2)x10{sup 6} cm{sup -2} for the range of misfit values explored here. A detailed analysis via high resolution x-ray diffraction revealed that the strain relaxed symmetrically, with equivalent numbers of {alpha} and {beta} dislocations, and to greater than 90% for all cases, regardless of substrate offcut. Further analysis showed the relaxation to always be glide limited in these materials when grown on a graded buffer compared to a single step layer. The threading dislocation density was observed by plan-view transmission electron microscopy to be constant for the range of misfit values studied here in the top layer of the graded structures, which is attributed to the very efficient use of residual dislocations and the dominance of dislocation glide over nucleation in these graded anion metamorphic buffers, suggesting great promise for metamorphic devices with lattice constants greater than that of InP to be enabled by InAsP metamorphic structures on InP.

36 MATERIALS SCIENCE↗

Polarization-induced 2D hole gases in pseudomorphic undoped GaN/AlN heterostructures on single-crystal AlN substrates

A high-conductivity two-dimensional (2D) hole gas is the enabler of wide-bandgap p-channel transistors. Compared to commonly used AlN template substrates with high dislocation densities, the recently available single-crystal AlN substrates are promising to boost the speed and power handling capability of p-channel transistors based on GaN/AlN 2D hole gases (2DHGs) thanks to the much lower dislocation densities and the absence of thermal boundary resistance. Using plasma-assisted molecular beam epitaxy, we report the observation of polarization-induced high-density 2DHGs in undoped pseudomorphic GaN/AlN heterostructures on the single-crystal AlN substrates with high structural quality and atomic steps on the surface. The high-density 2DHG persists down to cryogenic temperatures with a record high mobility exceeding 280 cm 2 /V s and a density of 2.2 × 10 13 /cm 2 at 10 K. These results shed light on aspects of improving 2D hole mobilities and indicate significant potential of GaN/AlN 2DHG grown on bulk AlN substrates for future high performance wide-bandgap p-channel transistors.

36 MATERIALS SCIENCE↗

Role of dislocations on martensitic transformation temperatures and microstructure: A molecular dynamics study

Microstructure and defects strongly affect martensitic transformations in metallic alloys. Significant progress has been made in understanding the atomic-level processes that control the role of grain boundaries and precipitates in these solid-to-solid phase transformations. Yet, the role of dislocations and their structures on martensitic transformation temperature and the resulting microstructure remains unclear. Therefore, we used large-scale molecular dynamics simulations to study the forward and reverse transformation of a martensitic material modeled after Ni63Al37 under cyclic thermal loading. The simulations reveal that dislocations in the austenite phase act as one-dimensional seeds for the martensite phase, which is present at temperatures significantly above the martensite start value. We find a reduction in the dislocation density during cyclic thermal loading, which results in the increase in martensite and austenite transition temperatures, in agreement with experiments. Importantly, we extracted a critical martensitic nuclei size for developing stable domains and found that relatively low dislocation densities are needed to grow independent martensitic variants resulting in a multi-domain structure.

Physics↗

The role of AlGaN buffers and channel thickness in the electronic transport properties of Al{sub x}In{sub 1–x}N/AlN/GaN heterostructures

We try to theoretically analyze the reported experimental data of the Al{sub x}In{sub 1–x}N/AlN/GaN heterostructures grown by MOCVD and quantitatively investigate the effects of AlGaN buffers and the GaNchannel thickness on the electrical transport properties of these systems. Also, we obtain the most important effective parameters of the temperature-dependent mobility in the range 35–300 K. Our results show that inserting a 1.1 μm thick Al{sub 0.04}Ga{sub 0.96}N buffer enhances electron mobility by decreasing the effect of phonons, the interface roughness, and dislocation and crystal defect scattering mechanisms. Also, as the channel thickness increases from 20 nm to 40 nm, the electron mobility increases from 2200 to 2540 cm{sup 2}/(V s) and from 870 to 1000 cm{sup 2}/(V s) at 35 and 300 K respectively, which is attributed to the reduction in the dislocation density and the strain-induced field. Finally, the reported experimental data show that inserting a 450 nm graded AlGaN layer before an Al{sub 0.04}Ga{sub 0.96}N buffer causes a decrease in the electron mobility, which is attributed to the enhancement of the lateral size of roughness, the dislocation density, and the strain-induced field in this sample.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High-efficiency inverted metamorphic 1.7/1.1 eV GaInAsP/GaInAs dual-junction solar cells

Photovoltaic conversion efficiencies of 32.6 +/- 1.4% under the AM1.5 G173 global spectrum, and 35.5 +/- 1.2% at 38-suns concentration under the direct spectrum, are demonstrated for a monolithic, dual-junction 1.7/1.1 eV solar cell. The tandem cell consists of a 1.7 eV GaInAsP top-junction grown lattice-matched to a GaAs substrate, followed by a metamorphic 1.1 eV GaInAs junction grown on a transparent, compositionally graded metamorphic AlGaInAs buffer. This bandgap combination is much closer to the dual-junction optimum and offers headroom for absolute 3% improvement in efficiency, in comparison to the incumbent lattice-matched GaInP/GaAs (~1.86/1.41 eV) solar cells. The challenge of growing a high-quality 1.7 eV GaInAsP solar cell is the propensity for phase separation in the GaInAsP alloy. The challenge of lattice-mismatched GaInAs solar cell growth is that it requires minimizing the residual dislocation density during the growth of a transparent compositionally graded buffer to enable efficient metamorphic tandem cell integration. Transmission electron microscopy reveals relatively weak composition fluctuation present in the 1.7 eV GaInAsP alloy, attained through growth control. The threading dislocation density of the GaInAs junction is ~1 x 10^6 cm-2, as determined from cathodoluminescence measurements, highlighting the quality of the graded buffer. These material advances have enabled the performance of both junctions to reach over 80% of their Shockley-Queisser limiting efficiencies, with both the subcells demonstrating a bandgap-voltage offset, WOC (=Eg/q-VOC), of ~0.39 V.

14 SOLAR ENERGY↗

The compressive deformation mechanisms of a coarse-grained AgInCd alloy

Highlights: • The compressive deformation mechanisms of a coarse-grained AgInCd alloy are investigated. • The deformation mechanisms are full dislocation slip and multiplication when strain is small. • Dominant deformation mechanisms convert into deformation twinning when strain reaches 50%. • Dislocation densities and twin thicknesses reduce in twinned grains with strain increasing. - Abstract: The compressive deformation mechanisms of a coarse-grained AgInCd alloy have been investigated in the present study. When compressive strain is not higher than 30%, the deformation mechanisms transform from full dislocation slip and multiplication into the two coefficient mechanisms of full dislocation slip and partial dislocation emission with increasing compressive strain. When compressive strain reaches 50%, the dominant deformation mechanisms convert into deformation twinning. With further increasing strain, the dislocation densities decrease and the twin thicknesses reduce in the nano-twinned grains. Twin boundary possesses a weaker strengthening effect comparing with grain boundary for the AgInCd alloys.

36 MATERIALS SCIENCE↗

Understanding the Effect of Na in Improving the Performance of CuInSe 2 Based Photovoltaics

Cu(In,Ga)Se 2 (CIGS) thin film photovoltaic technology is in the early stages of commercialization with an annual manufacturing capacity over 1 GW and has demonstrated the highest module efficiency of any of the thin film technologies. However there still is a lack of fundamental understanding of the relationship between the material properties and solar cell device operation. It is well known that the incorporation of a small amount of Na into the CIGS film during processing is essential for high efficiency devices. However, there are conflicting explanations for how Na behaves at the atomic scale. This report investigates how Na is incorporated into the CIGS device structure and evaluates the diffusion of Na into CIGS grain boundaries (GBs) and bulk crystallites. Participants: This project was carried out at the Institute of Energy Conversion at the University of Delaware, collaborating with the Rockett group at the University of Illinois Urbana-Champagne. Significant Findings: The significant outcomes of this project for each task include; Task 1.0: Effect of Na in Devices Fabricated on PVD Deposited CIGS; Na diffusion occurs through the Mo back contact via GBs driven by the presence of oxygen; Na reversibly compensates donor defects in CIGS GBs,Task 2.0: Na Incorporation in Single Crystal CIGS; and bulk Na diffusion proceeds rapidly such that grains are Na-saturated immediately following CIGS thin film manufacture. Industry Guidance: The presented results offer interesting concepts for modification of manufacturing processes of CIGS-based PV modules. Possible approaches to improve control of Na uptake and uniformly increase levels in CIGS films are highlighted for processes that employ either soda-lime glass or NaF as the Na source. Concepts include the potential of O 2 or oxidative based treatments of Mo back contacts to improve Na diffusion through the metal film and increase Na uptake into the growing CIGS. This project has also offered fundamental understanding of the behavior of Na in CIGS grains and GBs, particularly the confirmation that CIGS grains will be saturated with Na immediately following manufacture Summary of Results: Most commercially available CIGS modules are fabricated on soda-lime glass coated with Mo as the back electric contact, and Na in the glass diffuses through the Mo layer into the CIGS during film growth. In Task 1 the transport of Na through Mo was evaluated using x-ray photoelectron surface spectroscopy along with diffusion modeling to obtain diffusion coefficients at several temperatures. It was determined that Na diffusion in Mo only occurs along GBs and that oxygen provides an additional driving force to enhance Na transport. Device data revealed that older Mo substrates with a greater amount of surface oxide resulted in slightly higher efficiencies due to enhanced Na incorporation caused by the oxide. This finding shows that Mo substrates could potentially undergo an oxidation treatment prior to CIGS deposition to further improve and control the incorporation of Na. To determine if in-grain Na affects device performance, in Task 1 Na was selectively removed from GBs using heat/rinse cycles. Due to the low temperature of this treatment, Na at GBS remained mobile while diffusion within the bulk was too slow for Na removal from the grain interiors. Changes in electrical properties were evaluated using conductivity and Seebeck coefficient measurements, with both decreasing as Na was removed to reach values similar to Na-free controls samples. This can be explained by the compensation of donor defects by Na, causing an increase in the free carrier concentration. Devices showed a decrease in open-circuit voltage after Na removal confirming that the beneficial effects of GB Na. The findings of this project will provide guidance for rational optimization of Na incorporation procedures in the manufacturing of CIGS solar cells. While it is known that Na segregates at CIGS GBs, the nature and role of Na diffusion into grain interiors was less clear. In Task 2, single crystal CuInSe 2 was used as a model system to represent the grain interiors of CIGS. Crystals processed by two different methods of different compositions and dislocation densities, were evaluated. Diffusion coefficients were obtained at two temperatures after Na diffusion, giving near identical values, ~2x10 11 cm 2 /s and ~6x10 11 cm2/s at 420°C and 480°C, respectively, for each crystal. Characterization confirmed that dislocation densities were too low to significantly impact the effective diffusion coefficient. The Cu-poor crystal had a higher solubility suggesting that Na diffusion is mediated by Cu-vacancies, but was not accompanied by an expected increase in diffusion coefficient. The activation energy for diffusion was similar to values expected for interstitial diffusion, but the large size of Na + ions should result in a solubility that is much lower than what was experimentally measured. A hybrid interstitial-substitutional mechanism is proposed that combines the fast diffusion of interstitial atoms with the high solubility common for substitutional impurities. Lattice diffusion of Na proceeds fast enough that CIGS grain interiors will have Na concentrations near the solubility limit of 1018 cm -3 when manufactured under standard conditions. Na and K treated epitaxial CIS films showed a significant increase in cathodoluminescence emission intensity, indicating a reduction of non-radiative recombination pathways, which is consistent with improvements in CIGS device performance, though the mechanism is not clear. Pathways forward: Despite the success of this project, there are a number of questions remaining related to further the understanding of the chemistry of Na in CIGS films and devices. These include further elucidation of the mechanisms of Na passivation in CIGS GBs, with identification of which defects are involved and confirmation of the possible effects of in-grain Na on device performance. To complete analysis of the cell structure, conformation of the presence and possible chemistries of Na at the CIGS/CdS junction and/or in the front transparent contacts, and its effects on device performance, is needed.

14 SOLAR ENERGY↗

Reduction in the Number of Mg Acceptors with Al Concentration in Al x Ga 1-x N

High hole concentrations in Al x Ga 1-x N become increasingly difficult to obtain as the Al mole fraction increases. The problem is believed to be related to compensation, extended defects, and the band gap of the alloy. Whereas electrical measurements are commonly used to measure hole density, we used electron paramagnetic resonance (EPR) spectroscopy to investigate a defect related to the neutral Mg acceptor. The amount and symmetry of neutral Mg in MOCVD-grown Al x Ga 1-x N with x = 0 to 0.28 was monitored for films with different dislocation densities and surface conditions. EPR measurements indicated that the amount of neutral Mg decreased by 60% in 900°C-annealed Al x Ga 1-x N films for x = 0.18 and 0.28 as compared with x = 0.00 and 0.08. A decrease in the angular dependence of the EPR signal accompanied the increased x, suggesting a change in the local environment of the Mg. Neither dislocation density nor annealing conditions contribute to the reduced amount of neutral Mg in samples with the higher Al concentration. Rather, compensation is the simplest explanation of the observations, because a donor could both reduce the number of neutral acceptors and cause the variation in the angular dependence.

36 MATERIALS SCIENCE↗