Effects of Sb and Ag Addition on the Mechanical Behavior of Near-eutectic Sn-Bi Solder Alloys
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Oral presentation for ecs PRIME 2024
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Solidification structure and properties of eutetic alloys
Alloy contact layer is made at relatively low temperature and has good wetting characteristics. Contacts adhere well to silicon carbide surface, penetrating about 300 to 500 angstroms into it. Contacts are ohmic on p-type silicon carbide and blocking on n-type.
Technique joins titanium or one of its alloys to materials, such as iron, nickel or cobalt base material, or to refractory metals. To ensure formation of a satisfactory bond, the temperature, time, environment and pressure must be controlled.
By means of a screening and solidification optimization study of certain alloys located on the gamma-sigma liquidus surface within the Ni-Cb-Cr-Al system, alloys with high temperature properties superior to those of all known superalloys were defined. One alloy, Ni - 19.7w/o Cb - 6.0w/o Cr - 2.5w/o Al, directionally solidified at 3 cm/hr met or exceeded each program goal. A second alloy, Ni-21.75 w/o Cb-2.55 w/o Al, although deficient in its inherent oxidation resistance, met the other program goals and combined a remarkable insensitivity of composite microstructure to solidification parameters with excellent low temperature toughness. This investigation demonstrated that useful properties for gas turbine airfoil application have been achieved by reinforcing a strong and tough gamma solid solution matrix containing precipitated gamma prime by a lamellar intermetallic compound Ni3 Cb having greater strength at elevated temperature.
Coating compositions were evaluated for oxidation protection of directionally solidified composite alloy NiTaC-13. These coatings included three NiCrAlY compositions (30-5-1, 25-10-1 and 20-15-1), two FeCrAlY compositions (30-5-1 and 25-10-1), a CoCrAlY composition (25-10-1), and one duplex coating, Ni-35Cr + Al. Duplicate pin samples of each composition were evaluated using two cyclic furnace oxidation tests of 100 hours at 871 C and 500 hours at 1093 C. The two best coatings were Ni-20Cr-15Al-lY and Ni-35Cr + Al. The two preferred coatings were deposited on pins and were evaluated in detail in .05 Mach cyclic burner rig oxidation to 1093 C. The NiCrAlY coating was protective after 830 hours of cycling, while the duplex coating withstood 630 hours. Test bars were coated and cycled for up to 500 hours. Tensile tests indicated no effect of coatings on strength. In 871 C air stress rupture, a degradation was observed for coated relative to bare material. The cycled NiCrAlY coating offered excellent protection with properties superior to the bare cycled NiTaC-13 in 1093 C air stress rupture.
Results are presented of extensive testing recently completed on boron-aluminum composites to determine mechanical property data for structural design and analysis. Average property data and associated test methods are given for unidirectional and cross plied laminates at room temperature and 600 F. Results from crippling tests of hat-shaped stringers and mechanical fastener joint tests of laminates containing titanium interleaves are also presented. Compared to aluminum which has approximately same density, tests show that boron-aluminum loaded in compression is 4 1/2 times stronger and 3 1/2 times stiffer. When loaded in tension it is 2 times stronger and 3 times stiffer.
Explore the source record for details and available documents.
Alloy has high temperature properties exceeding strength of all known superalloys. It exhibits inherent resistance to oxidation and high temperature hot corrosion.
Method enables use of crystal or semiconductor materials with selective spectral-response characteristics (ultraviolet, visible, or infrared wavelengths) in fabrication of contact lenses, reading glasses, and photographic processing equipment.
By means of a compositional and heat treatment optimization program based on the quaternary gamma/gamma prime-delta, a tantalum modified gamma/gamma prime-delta alloy with improved shear and creep strength combined with better cyclic oxidation resistance was identified. Quinary additions, quaternary adjustments, and heat treatment were investigated. The tantalum modified gamma/gamma prime-delta alloy possessed a slightly higher liquidus temperature and exhibited rupture strength exceeding NASA VIA by approximately three and one-half Larson-Miller parameters (C = 20) above 1000 C. Although improvements in longitudinal mechanical properties were achieved, the shear and transverse strength property goals of the program were not met and present a continuing challenge to the alloy metallurgist.
A nominal composition of Co-15Cr-2ONi-10.5 Hf-0.7 C (NASA-HAFCO-11) was directionally solidified at 0.8 cm/hr growth rate to produce aligned HfC in a cobalt matrix alloy. The aligned HfC fibers were present as rod and plate types. The diameter of the aligned fibers was about 1 micron, with volume fraction in the range of 11 to 15 percent. The growth direction of the fibers was parallel to the 100. The NASA-HAFCO-11 alloy was subjected to thermal cycling between 425 deg and 1100 C, using a 2.5 minute cycle. No microstructural degradation of the HfC fibers in the alloy was observed after 2500 cycles.
The experimental procedures used in the investigation are considered, taking into account solidification and heat treatment, fatigue testing, questions of test specimen and loading fixture design verification, metallographic techniques, and electron microscopy techniques. Attention is given to the characteristics of the microstructure, aspects of fatigue crack propagation (FCP) in the Ni-Ni3Nb composite, the effect of test variables on FCP, the effect of metallurgical variables on FCP, and fatigue fracture mechanisms. Fractographic and metallographic observations are discussed.
Inverted Bridgman Method yields crystals of higher homogeneity and better structure than those grown by ordinary Bridgman method. Process controls thermotransport by holding molten alloy in known temperature for known period of time. Rapid cooling quenches in state of segregation. Method is applicable to other eutectiferous systems where thermotransport is appreciable.
A nominal composition of Co-15Cr-20Ni-10.5Hf-0.7C was directionally solidified at 0.8 cm/hr growth rate to produce aligned HfC in a cobalt matrix alloy. The aligned HfC fibers were present as rod and plate types. The diameter of the aligned fibers was about 1 micron, with volume fraction in the range of 11 to 15 per cent. The growth direction of the fibers was parallel to the 100 direction. The alloy was subjected to thermal cycling between 425 and 1100 C, using a 2.5 minute cycle. No microstructural degradation of the HfC fibers in the alloy was observed after 2500 cycles.