Search NASA⌕ Search

SEARCH · Search NASA

Results for “ion conductivity”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Exploring sodium dynamics in the dilute oxygen regime of mixed oxy-sulfide NaPSiSO glasses

All-solid-state‑sodium batteries have great potential to lower the cost of grid-scale energy storage systems. However, they require a low cost, high conductivity solid electrolyte to become a reality. The electrochemical properties of mixed oxy-sulfide glasses NaPSiSO exceed those of either the pure sulfide or the pure oxide glass alone. In this work, we have tested models of sodium ion dynamics in the NaPSiSO series: zNa 2 S+(1-z)[(1-y)[(1-x)SiS 2 + xPS 5/2 ] + yNaPO 3 ] where 0.57 ≤ z ≤ 0.588, 0 ≤ x ≤ 0.35, and 0.15 ≤ y ≤ 0.35 using 23 Na nuclear magnetic resonance to directly probe the local fields and their fluctuations at the nuclear sites. We determined the distribution of activation energies in these materials arising from distributions of local environments and provided quantitative information about the connectivity of the ionic pathways through which the sodium ions move. We found that the sodium ion conduction dynamics were described as an ionic percolation through a Gaussian distribution of energy barriers and that the composition dependence of the ionic conductivity in the dilute oxygen regime is well-described by the Nernst-Einstein relation modified for percolation.

25 ENERGY STORAGE↗

Local electrical degradations of solid-state electrolyte by nm-scale operando imaging of ionic and electronic transports

We report on degradation mechanisms of solid-state electrolyte (SSE) based on insights from nm-scale ionic conduction and electronic leakage for solid-state batteries. The significantly different local degradations revealed by nm-scale ionic and electronic transport imaging demonstrate the need for this nm-scale investigation. State-of-the-art lithium-ion conductive glass ceramic (Li 2 O–Al 2 O 3 –SiO 2 –P 2 O5–TiO2-GeO2) SSE shows at least two types of degradations spatially separated within the SSE, namely: (1) ionic conduction blocking and slight electronic leaking and (2) highly electronic shunting. Degradation was significantly suppressed by application of a Li-containing polyacrylonitrile thin coating on both sides of the ceramic SSE. With this coating, the ionic conduction was not reduced by the extensive cycling; instead, it improved slightly, although accompanied by a slight increase in electronic leaking. Our nm-scale transport imaging was achieved using an atomic force microscopy (AFM)-based half-cell setup and a logarithmic-scale amplifier with current sensitivity down to the fA (10-15 A) range. This half-cell setup consisting of an AFM-probe/SSE/Li structure can distinguish the ionic from the electronic current by flipping the bias-voltage polarity. This nm-scale operando imaging opens up novel characterization of ionic and electronic transport in the field of solid-state batteries.

42 ENGINEERING↗

Mechanistic insight into the effects of A-site doping in perovskite nanorods on interfacial Li-ion and Na-ion transport in polymer–perovskite composite electrolytes

Composite polymer electrolytes (CPEs) offer a promising pathway to safer and higher energy density electrochemical energy storage yet optimizing interfacial ion transport remains a critical challenge due to high resistances and a lack of understanding of the complex interfacial electrostatic interactions. This work investigates the mechanistic origins of the interfacial ion transport enhancement in single-ion conducting (SIC) polymer electrolytes filled with A-site disordered perovskite LaxMyTiOz (LMTO) (M = Li, Na, K) nanorods. By integrating Density Functional Theory (DFT) with broadband dielectric spectroscopy (BDS) and pulsed-field-gradient NMR (PFG-NMR), we analyze the ion transport behavior in Li-based and Na-based SIC systems containing compositionally distinct LMTO fillers (LMTO800 and LMTO900). Specifically, we introduce the site-to-site energy difference (ΔE) descriptor, which extends beyond single-site descriptors such as adsorption energy and ion binding energies. We demonstrate that ΔE together with ion binding energies provide a more comprehensive picture of the energy landscape at the polymer–ceramic interface. The combined DFT and experimental results show that A-site doping in the ceramic filler can effectively modulate ΔE and ion binding energies, creating a favorable potential energy landscape that promotes enhanced ion transport along the interface. This comprehensive study illustrates the impact of ceramic compositional tuning on interfacial ion transport and provides materials design rules towards real-world applications.

B shepard, Lauren [Pennsylvania State University]↗

Electrical, thermal, and H 2 O and CO 2 poisoning behaviors of PrNi 0.5 Co 0.5 O 3-δ electrode for intermediate temperature protonic ceramic electrochemical cells

PrNi 0.5 Co 0.5 O 3-δ (PNC) exhibits adequate total electrical conductivity (~300 S/cm at 400–600 °C) and moisture has no significant effect on it. The thermal expansion coefficient of PNC is 17.6 × 10 –6 /K by dilatometry and 18.43 × 10 –6 /K by in situ XRD. PNC also demonstrates chemical stability against H 2 O and CO 2 . However, PNC symmetrical cell over proton-conducting BaZr 0.4 Ce 0.4 Y 0.1 Yb 0.1 O 3-δ (BZCYYb4411) electrolyte shows significant H 2 O and CO 2 poisoning when those are introduced into O 2 –N 2 mixture. In comparison, symmetrical cells with PNC electrode over the oxygen ion conducting Ce 0.9 Gd 0.1 O 2-δ (GDC) electrolyte show no H 2 O and CO 2 poisoning under similar conditions. Here, it is hypothesized that poisoning from H 2 O and CO 2 of the PNC proton conducting symmetrical cell is caused by their adsorption on the BZCYYb4411 electrolyte instead of PNC electrode. Such a hypothesis is supported by the H 2 O and CO 2 adsorption behaviors on PNC and BZCYYb4411 powder surfaces, as measured by temperature programmed desorption (TPD).

08 HYDROGEN↗

Identifying Spectral Descriptors for Protonation in BaZr 0.8 Y 0.2 O 3-x with Electron Energy Loss Spectroscopy

Hydrogen economy is of paramount importance in the global transition to a sustainable, clean energy source that contributes to decarbonization efforts. In particular, the proton conducting proton ceramic fuel cells (PCFCs) play a crucial role in promoting hydrogen energy technology [1-5]. In a PCFC, the electrolyte is typically a solid oxide material that enables proton transport and can operate at temperatures lower than those of traditional oxygen ion conducting fuel cells [6]. The reduced operating temperature of PCFCs contributes to their durability, scalability, and efficiency [7,8]. BaZr 0.8 Y 0.2 O 3-x (BZY) is a promising proton conducting solid oxide electrolyte [9,10]. The emphasis on proton conductivity entails the importance of understanding proton content in the system. However, previous studies have largely relied on bulk techniques such as electrochemical impedance spectroscopy [7,11], Karl-Fischer titration [12,13], and thermogravimetric analysis [14] to obtain proton concentration. This is due to the small atomic size and light mass of hydrogen species making direct detection challenging. Bulk methods may be useful in estimating the proton content; however, it overlooks possible proton concentration gradient or segregation that may occur across or within a nanoparticle, especially when proton incorporation occurs nonuniformly through steam exposure on powder samples. In this paper, BZY is protonated at an estimated 0.15 mol of protons via steam exposure. Electron energy loss spectroscopy (EELS) with nanoscale spatial resolution is explored to identify proxy signals for proton detection using a JEOL ARM300 microscope operated at 300 kV with a Gatan GIF Continuum detector.

08 HYDROGEN↗

Degradation of Anion Exchange Membranes by Cation Elimination: Impact on Water Uptake, Nanostructure, and Ionic Mobility

Anion exchange membranes (AEMs) are an attractive platform for fuel cell and electrolysis technologies since they enable the use of cheaper, nonplatinum group metal electrodes and components. However, the widespread adoption of AEM-based devices is limited by chemical degradation of the AEM in the highly alkaline medium of operation. Experimental studies report three major pathways of degradation, including substitution (S N 2), elimination (E2), and backbone cleavage. The decline in membrane performance is likely due to a cumulative effect of several pathways, which has proven to be difficult to disentangle through experiments. Here we use coarse-grained molecular simulations to isolate the impact of E2 degradation, where cationic sites are replaced by an alkene group, on AEM water uptake, nanoscale morphology, structure of the ion-conducting channels, water mobility, and ionic conductivity. Our studies focus on the well-studied model AEM polyphenylene oxide with tetraalkylammonium cationic sites (PPO-TMA). We find that about half of the hydrophobic groups resulting from the degradation retract into the hydrophobic domains of the membrane. The reduction in ion exchange capacity (IEC) and the hydrophobicity of the alkene groups decrease both the equilibrium water uptake (%WU) and the number of water molecules per cation (λ) of the membrane. Interestingly, the evolution of λ with the IEC seems to follow that of undegraded PPO-TMA membranes. Additionally, we ascribe this to the similarity between the structure of the degraded monomer and the neutral one in the polymer. We conclude that most of the performance losses originate in the lower hydration of the degraded membrane.

36 MATERIALS SCIENCE↗

Microstructural impacts on ionic conductivity of oxide solid electrolytes from a combined atomistic-mesoscale approach

Abstract Although multiple oxide-based solid electrolyte materials with intrinsically high ionic conductivities have emerged, practical processing and synthesis routes introduce grain boundaries and other interfaces that can perturb primary conduction channels. To directly probe these effects, we demonstrate an efficient and general mesoscopic computational method capable of predicting effective ionic conductivity through a complex polycrystalline oxide-based solid electrolyte microstructure without relying on simplified equivalent circuit description. We parameterize the framework for Li 7- x La 3 Zr 2 O 12 (LLZO) garnet solid electrolyte by combining synthetic microstructures from phase-field simulations with diffusivities from molecular dynamics simulations of ordered and disordered systems. Systematically designed simulations reveal an interdependence between atomistic and mesoscopic microstructural impacts on the effective ionic conductivity of polycrystalline LLZO, quantified by newly defined metrics that characterize the complex ionic transport mechanism. Our results provide fundamental understanding of the physical origins of the reported variability in ionic conductivities based on an extensive analysis of literature data, while simultaneously outlining practical design guidance for achieving desired ionic transport properties based on conditions for which sensitivity to microstructural features is highest. Additional implications of our results are discussed, including a possible connection between ion conduction behavior and dendrite formation.

25 ENERGY STORAGE↗

Solution-assisted densification of NaSICON ceramics

A sodium-ion conducting NaSICON ceramic can be densified via the addition of a solvent to a NaSICON powder and subsequent pressing under high pressure and mild heat. Densification to ˜90% relative density can be achieved, providing a path toward low-temperature fabrication of Na-ion conductors.

Bock, Jonathan Anton↗

A New Class of Oxyhalide Solid Electrolytes NaNbCl 6‐2x O x for Solid‐state Sodium Batteries

Abstract Sodium‐based batteries are gaining momentum due to the abundance and lower cost of sodium compared to lithium. Solid‐state sodium batteries can also provide further safety advantages. However, sodium‐based solid‐state electrolytes (SSEs) that meet all the rigorous requirements, such as high ionic conductivity, oxidative stability with the cathode, and ease of processability, are lacking. We present here a new class of sodium‐based oxyhalide electrolytes NaNbCl 6‐2x O x with a facile mechanochemical synthesis. The oxyhalide NaNbCl 4 O exhibits close to two orders of magnitude higher ambient‐temperature sodium‐ion conductivity (1.03×10 −4 S cm −1 ) compared to the halide counterpart NaNbCl 6 (3×10 −6 S cm −1 ). Structural motifs unique to the oxygen content in NaNbCl 6‐2x O x are identified with 23 Na and 93 Nb magic angle spinning nuclear magnetic resonance (MAS NMR) spectroscopy and x‐ray diffraction (XRD). Solid‐state sodium batteries assembled with NaNbCl 4 O electrolyte and the cobalt‐ and nickel‐free layered Na 0.70 Fe 0.3 Mn 0.65 Al 0.05 O 2 cathode exhibit a maximum discharge capacity of 155 mAh g −1 with good cycle life at ambient temperature.

Kmiec, Steven↗

A New Class of Oxyhalide Solid Electrolytes NaNbCl 6‐2x O x for Solid‐state Sodium Batteries

Abstract Sodium‐based batteries are gaining momentum due to the abundance and lower cost of sodium compared to lithium. Solid‐state sodium batteries can also provide further safety advantages. However, sodium‐based solid‐state electrolytes (SSEs) that meet all the rigorous requirements, such as high ionic conductivity, oxidative stability with the cathode, and ease of processability, are lacking. We present here a new class of sodium‐based oxyhalide electrolytes NaNbCl 6‐2x O x with a facile mechanochemical synthesis. The oxyhalide NaNbCl 4 O exhibits close to two orders of magnitude higher ambient‐temperature sodium‐ion conductivity (1.03×10 −4 S cm −1 ) compared to the halide counterpart NaNbCl 6 (3×10 −6 S cm −1 ). Structural motifs unique to the oxygen content in NaNbCl 6‐2x O x are identified with 23 Na and 93 Nb magic angle spinning nuclear magnetic resonance (MAS NMR) spectroscopy and x‐ray diffraction (XRD). Solid‐state sodium batteries assembled with NaNbCl 4 O electrolyte and the cobalt‐ and nickel‐free layered Na 0.70 Fe 0.3 Mn 0.65 Al 0.05 O 2 cathode exhibit a maximum discharge capacity of 155 mAh g −1 with good cycle life at ambient temperature.

Kmiec, Steven↗

Optimization of anionic conductivity through the coexistence of ionomer cluster and backbone-backbone morphologies in anion exchange membranes

Random copolymers of poly(4-vinylpyridine) and polyisoprene were synthesized, and subsequently quaternized with 1-alkylbromides. The number of carbons on the pendant side-chain of the resultant comb-shaped polymer, n, ranged from 2-8. The comb-shaped polymers were crosslinked employing thiol-ene chemistry to give mechanically robust ion conducting membranes. Analysis by wide and medium-angle X-ray scattering show three morphology regimes that are dependent on the number of carbons on the pendant side-chains. When n = 2, ionomer cluster morphology was dominant, when n = 8 backbone-backbone morphology was dominant, and when n = 3-6, the membrane showed a coexistence of both ionomer cluster and backbone-backbone morphologies. Evaluation of the water uptake of the membranes showed a maximum water uptake per cation of 9.5 when n = 5 at 95% relative humidity (RH) and 60 degrees C. Finally, conductivity of the samples characterized by electrochemical impedance spectroscopy showed bromide conductivity as high as 110 mS/cm when n = 3 at 95% RH and 90 degrees C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In-situ re-crystallization of heavily-irradiated Gd 2 Ti 2 O 7

Gadolinium titanate (Gd 2 Ti 2 O 7 , or GTO) and other lanthanide pyrochlores are interesting candidates for actinide waste disposal and fast ion conduction because the relevant material properties are intimately dependent on local cation structure. Therefore, a deep understanding of the kinetics associated with cation ordering and disordering is required if such material properties are to be tuned for specific device designs. To this end, single crystals of GTO were irradiated with 190 keV helium ions to a total fluence of 1 × 10 17 ions/cm 2 , amorphizing the sample surface to a depth of ~1 μm and resulting in significant He bubble accumulation. FIB lamellae lifted out from the irradiated sections were examined during heat treatment in the (scanning) transmission electron microscope. Two distinct stages of the re-crystallization of the amorphized material were observed. The material near the end of the ions’ range transformed first and with the same orientation as the pristine material. This was due to the close proximity of the pristine material and the presence of small defect fluorite seeds, but the propagation of this growth front was frustrated by the large pores (formerly bubbles) in the He accumulation layer. This was followed by heterogeneous nucleation of new crystallites at random orientations at the top of the He accumulation layer, which is attributed to the high surface area associated with the many small He bubbles in that region. Finally, it is inferred that the kinetics of grain growth in this material are significantly faster than the kinetics of grain nucleation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Probing degradation at solid-state battery interfaces using machine-learning interatomic potential

Solid-state batteries featuring fast ion-conducting solid electrolytes are promising next-generation energy storage technologies, yet challenges remain for practical deployment due to electro-chemo-mechanical instabilities at solid-solid interfaces. These interfaces, which include homogeneous/internal interfaces such as grain boundaries (GBs) and heterogeneous/external interfaces between solid-electrolyte and electrode materials, can impede Li-ion transport, deteriorate performance, and eventually lead to cell failure. Here, in this study, we leverage large-scale molecular simulations, enabled by validated machine-learning interatomic potentials, to directly probe the onset of interfacial degradation at the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid-electrolyte/LiCoO 2 (LCO) cathode interface. By surveying different interfacial geometries and compositions, it is found that Li-deficient interfaces can lead to severe interfacial disordering with cation mixing and Co interdiffusion from LCO into LLZO. By contrast, Li-sufficient interfaces are less disordered, although elemental segregation with local ordering is observed. As a consequence of Co interdiffusion, Co-rich regions are formed at the GBs of LLZO due to cation segregation and trapping effects. This behavior is independent of the GB tilting axis, degree of disorder at the GBs, and Co concentration, which implies Co clustering at GBs is a general phenomenon in polycrystalline LLZO and can dictate its overall transport and mechanical properties. Our findings elucidate the underlying fundamental mechanisms that give rise to experimentally observed physicochemical properties and provide guidelines for interface design that can mitigate interfacial degradation and improve cycling performance.

25 ENERGY STORAGE↗

Single-phase local-high-concentration solid polymer electrolytes for lithium-metal batteries

Solid polymers are promising electrolytes for Li-metal batteries, but they have limitations: they cannot simultaneously achieve high ionic conductivity, good mechanical strength and compatibility with high-voltage cathodes while suppressing Li dendrites. Here, we design a class of locally high-concentration solid polymer electrolytes based on polymer blends, which are termed Li-polymer in F diluter (LPIFD). The Li-polymer (polymer-in-salt) ensures continuous Li-ion conduction channels and contributes to the solid electrolyte interphase (SEI), and the F diluter (inert fluorinated polymer) adds mechanical strength. Studies reveal that a single-phase LPIFD, which is based on a miscible polymer blend, lacks phase boundaries and forms an organic-less and LiF-rich SEI, effectively suppressing lithium dendrites. The single-phase LPIFD delivers ionic conductivity of 3.0 x 10 -4 S cm -1 and enables the Li anode to reach a high coulombic efficiency of 99.1% and a critical current density of 3.7 mA cm -2 . Furthermore, the ability to form an F-rich cathode electrolyte interphase allows LiNi 0.8 Co 0.1 Mn 0.1 O 2 ||Li cells to achieve a cycle life of 450 cycles at a high operating voltage of 4.5 V. In conclusion, this design will inspire efforts to commercialize polymer electrolytes for high-energy Li-metal batteries.

25 ENERGY STORAGE↗

Sodium-halogen secondary cell

An intermediate temperature sodium-halogen secondary cell that includes a negative electrode compartment housing a negative, molten sodium-based electrode and a positive electrode compartment housing a current collector disposed in a highly conductive molten positive electrolyte. A sodium halide (NaX) positive electrode is disposed in a molten positive electrolyte comprising one or more AlX3 salts, wherein X may be the same or different halogen selected from Cl, Br, and I, wherein the ratio of NaX to AlX3 is greater than or equal to one. A sodium ion conductive solid electrolyte membrane separates the molten sodium negative electrode from the molten positive electrolyte. The secondary cell operates at a temperature in the range from about 80° C. to 210° C.

Bhavaraju, Sai↗

Suppressing Atmospheric Degradation of Sulfide-Based Solid Electrolytes via Ultrathin Metal Oxide Layers

Sulfide-based solid-state electrolytes (SSEs) are promising materials with superior Li-ion conductivity; however, their poor atmospheric stability limits commercial manufacturing at scale. Here, we investigate the impact of ultrathin metal oxide layers deposited via atomic layer deposition (ALD) on the stability of Li 6 PS 5 Cl (LPSCl). Al 2 O 3 layers grown directly on LPSCl particles significantly stabilize the surface chemistry and Li-ion transport properties relative to uncoated material upon exposure to both an ambient atmosphere (22% relative humidity, RH) and humidified O 2 (100% RH). Detailed investigations indicate that coatings impede the surface and bulk degradation kinetics of exposed materials, even for coatings as thin as ∼1 Å. Furthermore, this suggests that stabilization is due to more than just a physical barrier. Shifts in valence band edge positions of coated LPSCl indicate that ALD coatings alter the surface electronic structure and resulting oxidation tendency of underlying LPSCl, suggesting new avenues to improving the environmental stability of sulfide SSEs.

Atmospheric chemistry↗

Unlocking Li superionic conductivity in face-centred cubic oxides via face-sharing configurations

Oxides with a face-centred cubic (fcc) anion sublattice are generally not considered as solid-state electrolytes as the structural framework is thought to be unfavourable for lithium (Li) superionic conduction. Here we demonstrate Li superionic conductivity in fcc-type oxides in which face-sharing Li configurations have been created through cation over-stoichiometry in rocksalt-type lattices via excess Li. We find that the face-sharing Li configurations create a novel spinel with unconventional stoichiometry and raise the energy of Li, thereby promoting fast Li-ion conduction. The over-stoichiometric Li–In–Sn–O compound exhibits a total Li superionic conductivity of 3.38 × 10 -4 S cm -1 at room temperature with a low migration barrier of 255 meV. Our work unlocks the potential of designing Li superionic conductors in a prototypical structural framework with vast chemical flexibility, providing fertile ground for discovering new solid-state electrolytes.

36 MATERIALS SCIENCE↗