Search NASA⌕ Search

SEARCH · Search NASA

Results for “parasitics”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Modeling of transverse stimulated Raman scattering in KDP/DKDP in large-aperture plates suitable for polarization control

Transverse stimulated Raman scattering (TSRS) in potassium dihydrogen phosphate (KDP) and deuterated potassium dihydrogen phosphate (DKDP) plates for large-aperture, inertial confinement fusion (ICF)-class laser systems is a well-recognized limitation giving rise to parasitic energy conversion and laser-induced damage. The onset of TSRS is manifested in plates exposed to the ultraviolet section of the beam. TSRS amplification is a coherent process that grows exponentially and is distributed nonuniformly in the crystal and at the crystal surfaces. To understand the growth and spatial distribution of TSRS energy in various configurations, a modeling approach has been developed to simulate the operational conditions relevant to ICF-class laser systems. Specific aspects explored in this work include (i) the behavior of TSRS in large-aperture crystal plates suitable for third-harmonic generation and use as wave plates for polarization control in current-generation ICF-class laser system configurations; (ii) methods, and their limitations, of TSRS suppression and (iii) optimal geometries to guide future designs.

47 OTHER INSTRUMENTATION↗

Improved accuracy in degenerate variational integrators for guiding centre and magnetic field line flow

First-order-accurate degenerate variational integration (DVI) was introduced in Ellison et al. ( Phys. Plasmas , vol. 25, 2018, 052502) for systems with a degenerate Lagrangian, i.e. one in which the velocity-space Hessian is singular. In this paper we introduce second-order-accurate DVI schemes, both with and without non-uniform time stepping. We show that it is not in general possible to construct a second-order scheme with a preserved two-form by composing a first-order scheme with its adjoint, and discuss the conditions under which such a composition is possible. We build two classes of second-order-accurate DVI schemes. We test these second-order schemes numerically on two systems having non-canonical variables, namely the magnetic field line and guiding centre systems. Variational integration for Hamiltonian systems with non-uniform time steps, in terms of an extended phase space Hamiltonian, is generalized to non-canonical variables. It is shown that preservation of proper degeneracy leads to single-step (one-step) methods without parasitic modes, i.e. to non-uniform time step DVIs. This extension applies to second-order-accurate as well as first-order schemes, and can be applied to adapt the time stepping to an error estimate.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Long-Term Cyclability of NCM-811 at High Voltages in Lithium-Ion Batteries: an In-Depth Diagnostic Study

High-nickel layered oxides, such as LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NCM-811), offer higher energy density than their low-nickel counterparts at a given voltage and are gaining major traction in automotive lithium-ion batteries for electric vehicles. Besides high-Ni content, higher charging voltages above 4.3 V vs Li + /Li boost the energy and represent another focus in battery development. Here, we investigate the long-term cyclability of NCM-811 in graphite pouch cells over 1000 deep cycles between 2.5–4.2, 2.5–4.4, and 2.5–4.5 V through a suite of sensitive characterization techniques. The NCM-811 full cells show severely deteriorated cyclability with higher charging voltages, from 78% at 4.2 V to 52 and 32% at 4.4 and 4.5 V, respectively. At 4.2 V, minor parasitic electrolyte oxidation as well as cathode Li/Ni mixing and cracking are revealed after cycling, while transition-metal dissolution and surface reconstruction into rock-salt NiO are virtually undetectable. At 4.4 and 4.5 V, transition-metal dissolution and crossover to the anode become much more pronounced and a primary contributor to the capacity fade, while significant surface NiO formation causes substantial voltage polarization, which is less noticeable at 4.2 V. Meanwhile, more severe electrolyte oxidation, Li/Ni mixing, and particle pulverization exacerbate the voltage and capacity fade. Finally, these results outline distinct challenges for stable high-Ni layered oxide cathodes in high-voltage Li-ion batteries.

25 ENERGY STORAGE↗

Mitigating Calendar Aging in Si-NMC Batteries with Advanced Dual-Salt Glyme Electrolytes

In addressing the critical challenge of calendar aging in silicon (Si)-based lithium-ion batteries, this study introduces a groundbreaking strategy utilizing glyme-type dual-salt electrolytes (lithium bis(trifluoromethanesulfonyl)imide [LiTFSI] and lithium difluoro(oxalato)borate [LiDFOB]). These electrolytes are demonstrated to significantly mitigate parasitic reactions and capacity loss in Si-NMC (lithium nickel manganese cobalt oxide) full cells, especially when compared with traditional carbonate-based electrolytes. Further, our exhaustive mechanistic analysis reveals that such electrolytes not only preserve the integrity of the Si anode but also improve the cathode/electrolyte interphases (CEI) through the formation of a conformal coating on the high-voltage cathode surface. This dual-salt approach, enhanced by the addition of a phosphate additive, effectively decelerates calendar aging, marking a substantial advance in the quest for durable and reliable Si-based energy storage technologies. The findings underscore the vital role of electrolyte composition in extending the calendar life of Si batteries, offering an alternative avenue toward maximizing the performance and longevity of next-generation Li-Si batteries.

36 MATERIALS SCIENCE↗

Quantitative DNA Stable Isotope Probing Identifies Active Microorganisms Assimilating Volatile Fatty Acids in Full-Scale Enhanced Biological Phosphorus Removal Processes

Enhanced biological phosphorus removal (EBPR) systems often rely on exogenous carbon sources, such as volatile fatty acids (VFAs), to achieve higher P removal. Here, we employed DNA quantitative stable isotope probing (qSIP) using two VFAs, acetate and propionate, in cyclic anaerobic/aerobic incubations to assess their effects on P cycling and microbial activity with biomass from two full-scale EBPR water resource-recovery facilities that utilize VFA addition. We found that anaerobic VFA uptake preferences differed within known groups of PAOs, such as Candidatus Accumulibacter and Tetrasphaera-affiliated members (e.g., Ca. Phosphoribacter), between the two biomasses. The combination of qSIP with metagenomics identified isotopically labeled phages that were linked to active PAOs, highlighting their potential roles in modulating EBPR community composition and activity. The highest levels of anaerobic labeling from acetate were in genomes belonging to Saccharimonadales and Rickettsiales, which are generally host-associated with bacteria and eukaryotes, respectively. Furthermore, this finding highlights the possibility of cross-feeding between PAO hosts and their parasites or predators, as well as the role of so-far uncharacterized organisms participating in carbon cycling under EBPR conditions. Collectively, these results expand our understanding of the ecological interactions involved in communities anaerobically uptaking VFAs and cycling P that are central to EBPR.

Polyphosphate accumulating organisms↗

Rate-Based Absorption Modeling for Postcombustion CO 2 Capture with Additively Manufactured Structured Packing

Carbon capture using amine-based solvents in an absorption process is a leading candidate for reducing greenhouse gas emissions in industrial flue gas streams. To reduce operating costs and associated parasitic energy of these processes, process intensification utilizing additively manufactured structured packing has emerged as a new technology to manage exothermic reactions during absorption while improving CO 2 capture. A rate-based model framework has been developed for these novel packings that incorporates the mass and heat transfer phenomena for amine-based absorption of CO 2 . The rate-based model framework is first benchmarked using available solubility data and pilot plant data for aqueous monoethanolamine. The model validation shows accurate prediction of both CO 2 equilibrium partial pressures and ion speciation for solubility data as well as CO 2 capture, temperature profile, and solvent composition for pilot plant data in the absorption column. The model framework is then applied toward predicting the CO 2 capture performance of additively manufactured structured packing. Simulations agree with experimental data in predicting the CO 2 capture and the capture performance increase due to cooling within the structured packing device. Finally, advantages of this rate-based model framework are the utilization of correlations that may predict mass transfer and heat transfer coefficients of the packing based on the geometric properties of the device and the implementation of the model framework in open-source programming.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Liquid Phase Exfoliation of Chemically Prelithiated Bilayered Vanadium Oxide in Aqueous Media for Li-Ion Batteries

Bilayered vanadium oxides are attractive for energy storage due to their high initial specific capacities, which could be stabilized by integrating the bilayers with conductive nanoflakes often produced in a form of aqueous dispersions. Therefore, exfoliation of the bilayered vanadium oxides in water with high yield is desirable. Here, this work introduces the first aqueous exfoliation of chemically prelithiated bilayered vanadium oxide (i.e., δ-Li x V 2 O 5 ·nH 2 O or LVO) followed by vacuum filtration to produce a free-standing film, exhibiting a lamellar stacking of the bilayered vanadium oxide nanoflakes as evidenced by scanning electron microscopy. Due to the hydrated nature of bilayered vanadium oxides, the relationship between interlayer water content and the vacuum drying temperature (105 °C vs 200 °C) was studied using X-ray diffraction, thermogravimetric analysis, and Raman spectroscopy. It was found that vacuum drying the LVO nanoflakes at 200 °C enabled more efficient removal of crystallographic water than drying at 105 °C, and did not induce a phase transformation. Scanning transmission electron microscopy confirmed the layered structure of the samples, which was more well-ordered in the 200 °C case and had no clear boundaries between flakes at the atomic scale. Furthermore, electrochemical testing in nonaqueous Li-ion cells revealed that vacuum drying at 200 °C led to improvements in ion storage capacity and electrochemical stability. Improvements in electrochemical charge storage properties of the electrodes obtained via LVO exfoliation and free-standing film assembly in water dried at 200 °C reveal that conventional battery electrode drying protocols need to be revised as new electrochemically active materials are synthesized, such as hydrated layered oxides with expanded interlayer regions. The remaining capacity fading can be attributed to the structural LVO degradation, dissolution of vanadium oxide in electrolyte, and parasitic effects of the remaining interlayer water molecules. Our results establish an environmentally friendly and safe approach to obtain two-dimensional (2D) bilayered vanadium oxide nanoflakes and create a pathway to constructing novel 2D heterostructures for improved performance in energy storage applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Calcium Cosalt Addition to Alter the Cation Solvation Structure and Enhance the Ca Metal Anode Performance

Accessing the energy density and sustainability of calcium metal batteries requires mastering reversible calcium electrodeposition through electrolyte design. Several electrolytes support reversible, ambient temperature deposition but at utilization and rate too low for practical applications. These challenges stem from solvation structures characterized by either high barriers for cation desolvation or thermodynamic instability, leading to parasitic decomposition of the salt and solvent. The optimal solvation structure for the effective delivery of calcium to the electrode interface is not known. In this work, we show that adding a relatively small amount of a weakly associating calcium salt (calcium carba-closo-dodecaborate) to an otherwise strongly associated solution (calcium borohydride in tetrahydrofuran) produces a surprising population of fully solvent-coordinated Ca2+ cations in the form of solvent-separated ion pairs (SSIPs). We further demonstrate that the formation of these SSIPs beneficially impacts the kinetics and thermodynamics of calcium electrodeposition, revealing the unexpected finding that direct coordination of Ca2+ by the BH4– anion limits the electrodeposition process. These findings reveal how the competition between solvent and anion coordination to Ca2+ affects calcium deposition kinetics and cycling stability, setting the stage for a new calcium electrolyte design based on mixed anion electrolytes.

Landers, Alan T.↗

Operando XPS for Plasma Process Monitoring: A Case Study on the Hydrogenation of Copper Oxide Confined under h-BN

Here, we demonstrate that ambient pressure x-ray photoelectron spectroscopy (APXPS) can be used for in situ studies of dynamic changes in surface chemistry in a plasma environment. This opens a new and vast application space for XPS and greatly complements modern spectroscopy techniques to probe plasma-solid/liquid interactions relevant to process monitoring in the semiconductor industry, bio-medical plasma applications and plasma remediation technologies. Hexagonal boron nitride (h-BN) grown on Cu was used in this study as a well-defined model system for plasma process monitoring and because of its unique chemical, optical and electrical properties that make it a prospective material for advanced electronics. To better understand the stability and surface chemistry of h-BN during plasma assisted processing, we track in real time the plasma-induced chemical state changes of B, N and the underlying Cu substrate using APXPS equipped with an AC discharge plasma source operating at 13 Pa. Residual gas analysis (RGA) mass-spectra were concurrently collected during plasma-XPS to track reaction products formed during plasma exposure. A clear reduction of Cu x O is seen, while an h-BN layer remains intact, suggesting hydrogen radical (H • ) species can attack the exposed and h-BN covered Cu oxide patches and partially reduce the underlying substrate without significantly damaging the overlaying h-BN, which is of practical importance for development of h-BN encapsulated devices and interfaces. In addition to demonstration of plasma-XPS capabilities we discuss the observed challenges (e.g., parasitic plasma-chamber walls reactions and charging effects) and propose potential solutions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Amine Structure Governs Corrosion Rates of Copper Catalysts in Electrochemical Reactive Capture of CO 2

Reactive capture of CO 2 (RCC) offers an integrated approach that combines CO 2 capture with its direct electrochemical conversion, eliminating the need for CO 2 release from the capture agent. By avoiding the pH, pressure, and temperature swings required for the release step, RCC has the potential to reduce both energy consumption and capital costs compared to the conventional sequential process of CO 2 capture, release, concentration, and conversion. Amines, widely used in industrial CO 2 capture, face challenges in RCC systems due to their incompatibility with transition metal catalysts as well as their tendency to promote electrode corrosion and parasitic hydrogen evolution. Identifying suitable combinations of amines and catalysts is therefore critical to enabling integrated CO 2 capture and conversion. Here, this work systematically investigates the performance of four primary and four secondary amines for RCC on polycrystalline Cu catalysts. Among the eight tested amines, only dimethylamine showed no measurable Cu corrosion near the open circuit potential. In contrast, ammonia, methylamine, ethylamine, monoethanolamine, diethylamine, diethanolamine, and piperazine all induced Cu corrosion. Corrosion rates correlate with the pK a and steric hindrance of the amines, highlighting key parameters for catalyst–amine codesign. Grand canonical DFT calculations indicate a correlation between the adsorption strength of protonated amines, their pK a , and the extent of Cu corrosion, suggesting that both the surface binding of protonated amines and the lability of their protons play critical roles in corrosion acceleration near open circuit potentials. These finding suggest that amines with high pK a values and weak binding of their protonated forms to Cu surfaces are preferred, as they offer better corrosion resistance.

Choi, Jounghwan [Univ. of California, Los Angeles,↗

Cations Enhance Hydride Transfer to Noncatalytic Metals in Concentrated Alkaline Electrolytes

Alkali metal cations are known to influence the kinetics of the hydrogen evolution reaction (HER), acting as either promoters or inhibitors to the rate-determining step depending on the metal surface, local pH, and cation concentration. Despite the importance of concentrated electrolytes for commercial electrochemical cells, the impact of cations on the HER in concentrated alkaline environments (>1 M) and in mixed cation systems remains poorly understood. Here, this study quantifies the HER kinetics at polycrystalline metal surfaces (Pt, Au, Cu, and Fe) and the equilibrium solvation environment in pure and mixed alkali metal hydroxide electrolytes at concentrations up to 3.0 M. Kinetic analyses of Au, Cu, and Fe revealed a positive cation-concentration-effect that was primarily driven by changes to the charge transfer coefficient. Multinuclear NMR spectroscopy examined the solvation of H 2 O/OH – species and the alkali cations as a function of (mixed) alkali cation concentration(s), and demonstrated rapid exchange between solvent, hydroxide, and solvated cations. Together, these findings support models where HER kinetics on noncatalytic metal surfaces in strongly alkaline conditions are primarily governed by the average polarization and polarizability of the metal/solution interface and that increasing cation activity continues to increase the transfer coefficient at metal-hydroxide concentrations up to 3.0 M. Electrolytes and additives which can outcompete weakly hydrated cations and disrupt the interfacial water structure are expected to suppress parasitic HER at electrodes for energy storage and electroplating.

Cations↗

Role of Polysulfide Anions in Solid-Electrolyte Interphase Formation at the Lithium Metal Surface in Li–S Batteries

Delineating intricate interactions between highly reactive Li-metal electrodes and the diverse constituents of battery electrolytes has been a long-standing scientific challenge in materials design for advanced energy storage devices. Here, we isolated lithium polysulfide anions (LiS 4 - ) from an electrolyte solution based on their mass-to-charge ratio and deposited them on Li-metal electrodes under clean vacuum conditions using ion soft landing (ISL), a highly controlled interface preparation technique. The molecular level precision in the construction of these model interfaces with ISL, coupled with in situ x-ray photoelectron spectroscopy and ab initio theoretical calculations, allowed us to obtain unprecedented insight into the parasitic reactions of well-defined polysulfides on Li-metal electrodes. Our study reveals that the oxide-rich surface layer, which is amenable to direct electron exchange, drives multielectron sulfur oxidation (S o → S 6+ ) processes. Furthermore, our results have substantial implications for the rational design of future Li-S batteries with improved efficiency and durability.

25 ENERGY STORAGE↗

Atomic Layer Deposition of Cu Electrocatalysts on Gas Diffusion Electrodes for CO 2 Reduction

Electrochemical reduction of CO 2 using Cu catalysts enables the synthesis of C 2+ products including C 2 H 4 and C 2 H 5 OH. Here, in this study, Cu catalysts were fabricated using plasma-enhanced atomic layer deposition (PEALD), achieving conformal deposition of catalysts throughout 3-D gas diffusion electrode (GDE) substrates while maintaining tunable control of Cu nanoparticle size and areal loading. The electrochemical CO 2 reduction at the Cu surface yielded a total Faradaic efficiency (FE) > 75% for C 2+ products. Parasitic hydrogen evolution was minimized to a FE of ~10%, and a selectivity of 42.2% FE for C 2 H 4 was demonstrated. Compared to a line-of-sight physical vapor deposition method, PEALD Cu catalysts show significant suppression of C 1 products compared to C 2+ , which is associated with improved control of catalyst morphology and conformality within the porous GDE substrate. Finally, PEALD Cu catalysts demonstrated a stable performance for 15 h with minimal reduction in the C 2 H 4 production rate.

42 ENGINEERING↗

Uncovering the Relationship between Aging and Cycling on Lithium Metal Battery Self-Discharge

Lithium metal is considered the “holy grail” material to replace typical Li-ion anodes due to the absence of a host structure coupled with a high theoretical capacity. The absence of a host structure results in large volumetric changes when lithium is electrodeposited/dissolved, making the lithium prone to stranding and parasitic reactions with the electrolyte. Lithium research is focused on enabling highly reversible lithium electrodeposition/dissolution, which is important to achieving long cycle life. Understanding the various mechanisms of self-discharge is also critical for realizing practical lithium metal batteries but is often overlooked. In contrast to previous work, it is shown here that self-discharge via galvanic corrosion is negligible, particularly when lithium is cycled to relevant capacities. Rather, the continued electrochemical cycling of lithium metal results in self-discharge when periodic rest is applied during cycling. The extent of self-discharge can be controlled by increasing the capacity of plated lithium, tuning electrolyte chemistry, incorporating regular rest, or introducing lithiophilic materials. Finally, the Coulombic losses that occur during periodic rest are largely reversible, suggesting that the dominant self-discharge mechanism in this work is not an irreversible chemical process but rather a morphological process.

25 ENERGY STORAGE↗

Stability Enhancement in Na 0.67 Fe 0.2 Mn 0.8 O 2 Positive Electrodes via Spherical Coprecipitated Hydroxide Precursor Synthesis for Na-Ion Batteries

Mn/Fe-based layered transition metal oxides (LTMOs) are promising positive electrode materials for sodium-ion batteries (SIBs) due to their high abundance, low cost, and stable price fluctuations. At commercial scale, the fabrication of these materials commonly employs coprecipitation of hydroxide precursors, which allows for the scalable synthesis of uniform, dense particles with a tunable morphology. However, the common chelating agent (ammonia) forms unstable complexes with Fe 2+ ions, resulting in uncontrollable particle morphology and poor electrochemical properties. Here, in this study, three chelation strategies (no chelation, ammonia, oxalate) for Fe/Mn-based hydroxides are evaluated. It was found that oxalate chelation produced uniform, dense spherical hydroxide particles while particles via ammonia / no chelate routes exhibited no morphological control. The LTMOs synthesized from the oxalate-chelated hydroxide precursor formed uniform spherical particles, while the other two LTMOs showed greater variation in particle morphology. The oxalate-chelated LTMO electrode exhibited increased cycling stability due to reduced parasitic reactions with the electrolyte, as characterized by static leakage current measurements and electrochemical impedance spectroscopy.

25 ENERGY STORAGE↗

Calcium Gradient-Doped LiNi 0.5 Mn 1.5 O 4 Cathode for Long Cycle Life Lithium-Ion Batteries

High-voltage spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) has attracted considerable attention as a cathode material for next-generation lithium-ion batteries due to its high operating voltage and intrinsically fast lithium-ion diffusion kinetics. However, the practical implementation of LNMO remains limited by its rapid capacity decay, primarily associated with bulk structural instability and parasitic interfacial reactions. To address these issues, we innovatively introduced calcium (Ca) as a dopant to enhance both the oxygen framework and surface stabilities of the LNMO crystal through gradient doping. Observations from the electronic microscopies, X-ray diffraction, and the elemental analysis confirmed that Ca is preferentially enriched at the particle surface, and a disordered crystal phase is preserved in the bulk in the gradient-doped LNMO cathodes. As cathodes in LIBs, the Ca gradient-doped (Ca gr) LNMO materials delivered formation capacities of ∼126−130 mAh/g and exhibited Coulombic efficiencies of 88−95%, which are consistently higher than those of the uniform-doped samples at the same doping level and undoped sample. Especially, the Ca gr 0.05 LNMO cathode demonstrated significantly improved rate capability with ∼113 mAh/g preserved at 10 C, while ∼92 mAh/g and ∼110 mAh/g for undoped and Ca uniform 0.05 LNMO, respectively, and excellent cycling stability, retaining ∼124.1 mAh/g (∼96.3% capacity retention) after 500 cycles. The analysis of cyclic voltammetry, differential capacity, and electrochemical impedance revealed that the excellent electrochemical performance is attributed to the structural and morphological advantages of gradient-doped LNMO cathodes with a disordered bulk structure for fast Li + diffusion and a Ca-enriched surface for minimizing the Mn dissolution.

25 ENERGY STORAGE↗

Effect of Water Concentration in LiPF 6 -Based Electrolytes on the Formation, Evolution, and Properties of the Solid Electrolyte Interphase on Si Anodes

A trace amount of water in an electrolyte is one of the factors detrimental to the electrochemical performance of silicon (Si)-based lithium-ion batteries that adversely affect the formation and evolution of the solid electrolyte interphase (SEI) on Si-based anodes and change its properties. Thus far, a lack of fundamental and mechanistic understanding of SEI formation, evolution, and properties in the presence of water has inhibited efforts to stabilize the SEI for improved electrochemical performance. As such, we investigated the SEI formed in a Gen2 electrolyte (1.2 M LiPF6 in ethylene carbonate/ethyl methyl carbonate, 3:7 wt %, water content: <10 ppm) with and without additional water (50 ppm) at varying potentials (1.0, 0.5, 0.2, and 0.01 V vs Li/Li + ). The impact of additional water on the morphological, (electro)chemical, and structural properties of SEI was studied using microscopic (atomic force microscopy and scanning spreading resistance microscopy) and spectroscopic (X-ray photoelectron spectroscopy, attenuated total reflection Fourier-transform infrared spectroscopy, and time-of-flight secondary ion mass spectrometry) techniques. The SEI exhibits both potential- and water concentration-dependent trends in its morphology and chemical composition. The presence of additional water in the electrolyte causes parasitic reactions, which onset at ~1.0 V, resulting in a reduction of electrolyte components and result in the formation of an insulating, fluorophosphate-rich SEI. In addition, hydrolysis of LiPF 6 creates hydrofluoric acid, which reacts with the surface oxide layer on the Si electrode, leading to a pitted and inhomogeneous SEI structure.

36 MATERIALS SCIENCE↗

Probing Depth-Dependent Transition-Metal Redox of Lithium Nickel, Manganese, and Cobalt Oxides in Li-Ion Batteries

Layered lithium nickel, manganese, and cobalt oxides (NMC) are among the most promising commercial positive electrodes in the past decades. Understanding the detailed surface and bulk redox processes of Ni-rich NMC can provide useful insights into material design options to boost reversible capacity and cycle life. Both hard X-ray absorption (XAS) of metal K-edges and soft XAS of metal L-edges collected from charged LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) showed that the charge capacity up to removing ~0.7 Li/f.u. was accompanied with Ni oxidation in bulk and near the surface (up to 100 nm). Of significance to note is that nickel oxidation is primarily responsible for the charge capacity of NMC622 and 811 up to similar lithium removal (~0.7 Li/f.u.) albeit charged to different potentials, beyond which was followed by Ni reduction near the surface (up to 100 nm) due to oxygen release and electrolyte parasitic reactions. Overall, this observation points toward several new strategies to enhance reversible redox capacities of Ni-rich and/or Co-free electrodes for high-energy Li-ion batteries.

25 ENERGY STORAGE↗