Laser Sintering of Thermoset Polyimide Composites

Selective Laser Sintering (SLS) is an additive manufacturing technique that builds 3D models layer by layer using a laser to selectively melt cross sections in powdered polymeric materials, following sequential slices of the CAD model. SLS generally uses thermoplastic polymeric powders, such as polyamides (i.e. Nylon), and the resultant 3D objects are often weaker in their strength compared to traditionally processed materials, due to the lack of polymer inter-chain connection in the z-direction. Our previous effort showed the challenges of printing a melt-processable RTM370 imide resin powder terminated with reactive 4-phenylethynylphthalic anhydride by LS, due to its inherently low viscosity of these oligomers. This paper presented the first successful 3D printing of high temperature carbon fiber filled thermoset polyimide composites, followed by post cure cycles to promote additional crosslinking for achieving higher temperature (Tg = 370 °C) capability. The processes to build tensile specimens and a component by LS, and the characterization of RTM370 imide resin by DSC and rheology as well as evaluation of the LS printed polyimide composite specimens by SEM and mechanical tests will be discussed.

Polyimide Composites↗

6FDA-DETDA: DABE polyimide-derived carbon molecular sieve hollow fiber membranes: Circumventing unusual aging phenomena

Transport properties are discussed for asymmetric carbon molecular sieve (CMS) hollow fiber membranes based on polyimide precursors derived from a butanol esterified diamino benzoic acid (DABA) based polyimide, 6FDA-DETDA:DABE. Precursor fiber pretreatment with 10% Ethenyl(trimethoxy)silane [vinyltrimethoxysilane (VTMS)] solution in hexane followed by pyrolysis at 550 °C in ultra-high purity argon created asymmetric CMS fibers with CO 2 permeance above 1000 GPU and CO 2 /CH 4 selectivities > 25. Storage of the as-made modules for 72 days in 7 bar CO 2 suppressed undesirable aging typically seen under vacuum or atmospheric pressure air and provided CO 2 permeance and CO 2 /CH 4 selectivity of 780 GPU and 48 respectively. These results are in contrast to significant losses in CO 2 permeance and CO 2 /CH 4 selectivity for CMS created under equivalent pyrolysis conditions from non-esterified 6FDA-DETDA: DABA variant, even under CO 2 storage. The 6FDA-DETDA: DABA-derived CMS results were surprising, since dense film CMS samples from the same precursors did not show the undesirable permeance and selectivity changes. Moreover, other non-DABA containing precursors in dense film and asymmetric fiber forms can be effectively stabilized under CO 2 storage. Such findings suggest that high residual stress in the freshly formed thin selective layers of asymmetric structures in DABA-derived CMS causes undesirable micro-scale rearrangements. In dense films and even asymmetric skins of non-DABA derived CMS membranes, evidence of such undesirable rearrangements are not apparent. DABA-derived cross-links are presumably the cause of these effects. Mono-esterification of 6FDA-DETDA: DABA to form 6FDA-DETDA: DABE controls such crosslinking-derived stresses and resultant instabilities in the CMS fibers, thereby providing stable high performance gas separation properties under CO 2 storage or use in mixed gas feeds.

03 NATURAL GAS↗

Polyimide aerogels for ballistic impact protection

The ballistic performance of edge-clamped monolithic polyimide aerogel blocks (12 mm thickness) has been studied through a series of impact tests using a helium-filled gas gun connected to a vacuum chamber and a spherical steel projectile (approximately 3 mm diameter) with an impact velocity range of 150–1300 m s -1 . The aerogels had an average bulk density of 0.17 g cm -3 with high porosity of approximately 88%. The ballistic limit velocity of the aerogels was estimated to be in the range of 175–179 m s -1 . Moreover, the aerogels showed a robust ballistic energy absorption performance (e.g., at the impact velocity of 1283 m s -1 at least 18% of the impact energy was absorbed). At low impact velocities, the aerogels failed by ductile hole enlargement followed by a tensile failure. By contrast, at high impact velocities, the aerogels failed through an adiabatic shearing process. Given the substantially robust ballistic performance, the polyimide aerogels have a potential to combat multiple constraints such as cost, weight, and volume restrictions in aeronautical and aerospace applications with high blast resistance and ballistic performance requirements such as in stuffed Whipple shields for orbital debris containment application.

42 ENGINEERING↗

Mechanical and electrical changes in electrochemically active polyimide binders for Li-ion batteries

Polyimide binders are often used in electrodes made with silicon for lithium-ion batteries for their mechanical strength and adhesion, which help mitigate mechanical issues associated with large volumetric expansion. These binders can be electrochemically active, but it is difficult to characterize what physical and chemical changes occur due to a composite electrode with multiple components and processes at play. Here, in this work, we study electrodes consisting only of polyimide binder and conductive carbon, using scanning probe-based techniques—contact resonance, force volume, and scanning spreading resistance microscopy—along with cryo-scanning transmission electron microscopy, electron energy loss spectroscopy, and energy dispersive X-ray spectroscopy. We show that lithium becomes trapped in the binder during cycling and results in large initial capacity losses, the formation of dendrite-like features, column-like domains of significantly increased mechanical modulus, and a slight increase in electronic resistivity.

25 ENERGY STORAGE↗

Mechanical Failure of Thin Ta and Cu/Ta Layers on Polyimide Substrates: A Synchrotron-Based Technique for In Situ Characterization

In situ synchrotron radiation diffraction and confocal light microscopy is used to study fragmentation and buckling of thin brittle Ta layers with thicknesses of 50 nm, 100 nm and 200 nm on polyimide substrates. Synchrotron-based stress measurements confirm that cracking leads to relaxation of tensile stress. Simultaneously, compressive stress arises in transverse direction, which finally leads to buckling. This behavior can be explained quantitatively by a two-dimensional shear lag model. It is well established that the properties of the coating-substrate interface determine the processes of coating fragmentation and delamination. A possible approach for influencing and controlling these processes is given by the incorporation of a ductile interlayer. It can be observed that the presence of Cu interlayers with thicknesses of 5 nm, 20 nm and 50 nm reduces the fracture strength of brittle Ta coatings on polyimide substrates, whereas the resistance to buckling is increased significantly.

36 MATERIALS SCIENCE↗

Outgassing and degradation of polyimide induced by swift heavy ion irradiation at cryogenic temperature

Polyimide foils were irradiated with energetic Kr (740 MeV) and Pb (890 MeV) ions at cryogenic temperature (12 K). Beam-induced degradation processes were monitored by residual gas analysis and online infrared spectroscopy. The outgassing components observed at low irradiation temperatures differ in quantity but are similar in mass distribution to those identified at room temperature exposure. Besides CO as major volatile fragment, a significant contribution of short hydrocarbons like C{sub 2}H{sub x} is released. In situ infrared spectroscopy indicates accumulation of CO and CO{sub 2} molecules at 12 K in the foils. During heat-up cycles, most of these frozen gases become mobile and outgas at a temperature between 35 and 55 K. The study is motivated by the application of polyimide foils as insulating material in high radiation environment of the future accelerator facility for antiproton and ion research (FAIR).

36 MATERIALS SCIENCE↗

Pyrolytic carbon free-radical evolution and irradiation damage of polyimide under low-energy proton irradiation

Ionization and displacement effects are basic phenomena in damage processes of materials under space-particle irradiation. In this paper, the damage behaviors were investigated on the polyimide under proton irradiation using electron paramagnetic resonance (EPR) spectra analysis and optical absorbance valuation. The results indicate that the proton irradiation induces the formation of pyrolytic carbon free-radical with a g value of 2.0025, and the population of free radicals increases with the irradiation fluence. The most important finding is that the irradiation-induced free-radical population increases linearly with the displacement damage dose, as does the optical degradation, whereas the ionization effect alone, during the irradiation, cannot induce the formation of pyrolytic carbon free radical. Furthermore, during the post storage, after irradiation, the free-radical population decreases following a sum of an exponential and a linear mode with the storage time. It is interesting that, during the post storage, the recovery of the degraded optical absorbance of the polyimide follows a similar mode to that of free radicals, and the characteristic time constant changes with the wavelength of the optical spectra.

36 MATERIALS SCIENCE↗

Temperature dependence and the dispersion of nonlinear optical properties of chromophore-containing polyimide thin films

Detailed investigations of the quadratic nonlinear response of a series of new polyimides with covalently attached chromophore DR13 are performed by the Maker fringes method in the range of fundamental wavelength from 850 to 1450 nm. Polymer films with thickness of 100–400 nm were spin-coated on glass substrates and corona poled. For these materials, the maximum values of the second harmonic generation coefficients d{sub 33} are 80–120 pm/V. A red shift of the nonlinear response dispersion with respect to the linear absorption spectrum was observed for the DR13 chromophore. The temperature dependences of linear absorption and nonlinear coefficients d{sub 33} for studied structures are observed. It was found that the temperature changes of the absorption spectra lead to appreciable contribution to the value of the nonlinear coefficient d{sub 33}. The demonstrated high temperature stability (up to 120 °C) of chromophore-containing polyimide thin films makes it possible to eliminate the degradation of their nonlinear optical properties in the future applications of such structures.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High-temperature polyimide coating for optical fibres

We present our first results on the fabrication of new, high-performance polyimide coatings. The key components of the coatings are polyimides containing various cardo and/or fluoroalkylene groups, which allows the coatings to retain their high-temperature stability and facilitates the storage of the starting polymer and the optical fibre coating process owing to the good solubility of such copolymers in many organic solvents. Annealing for 30 s, 1 h and 24 h at temperatures of 430, 350 and 300 °C, respectively, reduces the strength of optical fibres having such coating by no more than 10%. (optical fibres)

36 MATERIALS SCIENCE↗

The Effect of γ Irradiation on Phase Transitions in the Polyimide–YBa{sub 2}Cu{sub 3}O{sub 6+} {sub x} System

The effect of γ irradiation on optical properties of films of the polyimide–YBa{sub 2}Cu{sub 3}O{sub 6.7} system with different concentrations of the filler in the form of the finely crystalline compound YBa{sub 2}Cu{sub 3}O{sub 6.7} (0.05 wt %, 0.10 wt %, and 0.50 wt %) has been investigated. The properties were studied on an IKS-29 infrared spectrophotometer in a spectral range of 400–4200 cm{sup –1} at room temperature. The samples were irradiated in air under room conditions on an RKhM-γ-20 by doses of 150, 250, and 600 kGy. The power of the exposure dose of the {sup 60}Co source was 0.16 rad/s. It has been established that irradiation with a dose of up to 600 kGy of the abovementioned system slightly affects the structure of the polyimide matrix but decreases the number of free radical groups in the film structure with the formation of hydrogen bonds. In the range of 400–4200 cm{sup –1} at D = 150 kGy, the most intense changes in spectra of polymeric composite samples have been revealed. In the range of 2850–3350 cm{sup –1}, the wide absorption spectrum band is preserved, which is caused by the presence of Cu, Y, and Ba crystallohydrates. The band is related to deformation vibrations of the Cu–O bond in YBa{sub 2}- Cu{sub 3}O{sub 6.7} (YBCO) chains due to properties of barium carbonate, formation of oxygen vacancies in the filler, and vibrations of the Cu(I)–O(I) bonds near one or several O(4) vacancies. Irradiation by doses of 250 and 600 kGy for different concentrations of the filler leads to a decrease in the signal intensity in the range of 1800–3600 cm{sup –1} by 20–35% on average. Peaks related to interband transitions (transitions of the Cu(I)–Cu(IY)–Cu(II) system) and bending vibrations O(I)–Cu(I) are not changed by strains of O(IY)–Cu(I) bonds. This testifies to the radiation-stimulated diffusion of oxygen atoms to O(IY) sites determining the orthorhombic phase of YBa{sub 2}Cu{sub 3}O{sub 6.7} from the occupied positions in the Cu–O sublattice.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Soluble high molecular weight polyimide resins

High molecular weight polyimide resins have greater than 20 percent /by weight/ solubility in polar organic solvents. They permit fabrication into films, fibers, coatings, reinforced composite, and adhesive product forms. Characterization properties for one typical polyimide resin are given.

Jones, R. J.↗

Polyimide foams provide thermal insulation and fire protection

Chemical reactions to produce polyimide foams for application as thermal insulation and fire prevention materials are discussed. Thermal and physical properties of the polyimides are described. Methods for improving basic formulations to produce desired qualitites are included.

Rosser, R. W.↗

Development of a low void polyimide resin for autoclave processing of glass and graphite reinforced composites.

Experimental studies are described in which new A-type polyimide prepolymer chemical modifications were investigated with the aim of increasing the melt phase duration and temperature range permitting autoclave processing, yet retaining the addition-type cure mechanism required for low-void content composites. Several modification candidates were examined, and one specific formulation was selected for detailed investigation. This A-type polyimide prepolymer formulation is shown to possess the desired characteristics.

Vaughan, R. W.↗

Preparation of polyimides from mixtures of monomeric diamines and esters of polycarboxylic acids

Polyimides having high thermal and oxidative stability are prepared by the reaction of a mixture of monomers comprising (1) a dialkyl or tetraalkyl ester of an aromatic tetracarboxylic acid; (2) an aromatic diamine; and (3) a monoalkyl or dialkyl ester of a dicarboxylic acid where in the ratio of a:b:c is n:(n+1):2, wherein n has a value from 1 to 20. The mixture of monomers is prepared in a 30 to 70 percent by weight solution of an organic solvent, a substrate impregnated with the solution and heated at 50 to 205 C to remove said solvent and form a low molecular weight prepolymer, and thereafter heated at 275 to 350 C to cure to a high molecular weight polyimide.

Serafini, T. T.↗

Development and evaluation of graphite and boron polyimide composites.

This paper covers the development and evaluation of the HT-S/710 graphite/polyimide system and initial evaluations of high modulus graphite and boron reinforced polyimide systems. Detail design properties of the HT-S/710 graphite/polyimide systems, test results of test sheet stringer components, and initial test evaluations of high modulus graphite and boron reinforced polyimide composites are presented. Preliminary design applications utilizing the basic processing and design data from this development program are presented as to their utilization in aircraft and space applications.

Scheck, W. G.↗

Polyimide foam for the thermal insulation and fire protection

The preparation of chemically resistant and flame retardant foams from polyfunctional aromatic carboxylic acid derivatives and organic polyisocyanates is outlined. It was found that polyimide foams of reproducible density above 1 lb./ft. and below 6 lbs./cu ft. can be obtained by employing in the reaction of least 2% by weight of siloxane-glycol copolymer as a surfactant which acts as a specific density control agent. Polyimide foams into which reinforcing fibers such as silicon dioxide and carbon fibers may be incorporated were also produced.

Rosser, R. W.↗

Dynamic load capacities of graphite fiber: Polyimide composites in oscillating plain bearings to 340 C (650 F)

Load capacities were determined for plain spherical bearings with self-lubricating spherical elements of graphite-fiber-reinforced-polyimide, and for plain cylindrical bearings with thin-wall liners of the composite in the bearing bores. Composites consisted of a 1-to-1 weight ratio of graphite fibers and polyimide. Oscillation was at an amplitude of + or - 15 deg at a frequency of 1 hertz. Bearings with composite ball material had a load capacity of approximately 69 MN/sq m (10 000 psi) at room temperature 25 MN/sq m (3600 psi) at 340 C (650 F). Bearings with thin-wall composite liners had much higher load capacities of 280 MN/sq m (40 000 psi) at room temperature amd 240 MN/sq m (35 000 psi) at 320 C (600 F). Friction coefficients were in the range of 0.12 to 0.19. The addition of 10 wt.% graphite fluoride solid lubricant to the composition of the thin-wall liners reduced friction coefficients into the range of 0.10 to 0.12.

Sliney, H. E.↗