Search NASA⌕ Search

SEARCH · Search NASA

Results for “FCC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Propagation considerations in land mobile satellite transmission

It appears likely that the Land Mobile Satellite Services (LMSS) will be authorized by the FCC for operation in the 800 to 900 MHz (UHF) and possibly near 1500 MHz (L-band). Propagation problems are clearly an important factor in the effectiveness of this service, but useful measurements are few, and produced contradictory interpretations. A first order overview of existing measurements is presented with particular attention to the first two NASA balloon to mobile vehicle propagation experiments. Some physical insight into the interpretation of propagation effects in LMSS transmissions is provided.

Vogel, W. J.↗

Deformation and erosion of f.c.c. metals and alloys under cavitation attack

Experimental investigations have been conducted to determine the early stages of cavitation attack on 6061-T6 aluminum alloy, electrolytic tough pitch copper, brass, and bronze, all having polycrystalline fcc matrices. The surface profiles and scanning electron micrographs show that the pits are initially formed at the grain boundaries, while the grain surfaces are progressively roughened by multiple slip and twinning. The initial erosion is noted to have occurred from the material in the grain boundaries, as well as by fragmentation of part of the grains. Further erosion occurred by shearing and necking of the surface undulations caused by plastic deformation. The mean penetration depth, computed on the basis of mass loss, was lowest on the bronze and greatest on the copper. Attention is given to the relation of cavitation attack to grain size, glide stress and stacking fault energy.

Rao, B. C. S.↗

An integrated voice and data multiple-access scheme for a land-mobile satellite system

An analytical study is performed of the satellite requirements for a land mobile satellite system (LMSS). The spacecraft (MSAT-X) would be in GEO and would be compatible with multiple access by mobile radios and antennas and fixed stations. The FCC has received a petition from NASA to reserve the 821-825 and 866-870 MHz frequencies for the LMSS, while communications with fixed earth stations would be in the Ku band. MSAT-X transponders would alter the frequencies of signal and do no processing in the original configuration considered. Channel use would be governed by an integrated demand-assigned, multiple access protocol, which would divide channels into reservation and information channels, governed by a network management center. Further analyses will cover tradeoffs between data and voice users, probability of blocking, and the performance impacts of on-board switching and variable bandwidth assignment. Initial calculations indicate that a large traffic volume can be handled with acceptable delays and voice blocking probabilities.

Li, V. O. K.↗

Undercooled and rapidly quenched Ni-Mo alloys

Hypoeutectic, eutectic, and hypereutectic nickel-molybdenum alloys were rapidly solidified by both bulk undercooling and melt spinning techniques. Alloys were undercooled in both electromagnetic levitation and differential thermal analysis equipment. The rate of recalescence depended upon the degree of initial undercooling and the nature (faceted or nonfaceted) of the primary nucleating phase. Alloy melts were observed to undercool more in the presence of primary Beta (NiMo intermetallic) phase than in gamma (fcc solid solution) phase. Melt spinning resulted in an extension of molybdenum solid solubility in gamma nickel, from 28 to 37.5 at % Mo. Although the microstructures observed by undercooling and melt spinning were similar the microsegregation pattern across the gamma dendries was different. The range of microstructures evolved was analyzed in terms of the nature of the primary phase to nucleate, its subsequent dendritic growth, coarsening and fragmentation, and final solidification of interfenderitic liquid.

Tewari, S. N.↗

The northern Utah satellite (NUSAT) communications link

During the planning Stages of the NUSAT satellite, an obvious issue to be discussed was the method of communications to be used. The frequencies would have to be high enough to pass through the atmosphere relatively unattenuated but low enough that antennas and transmission lines would not be so critical in length and properties that unexperienced students would have difficulty with handling them. In conversations with the Federal Communications Commission (FCC) in Washington D.C., the frequencies of 450.000 MHz and 137.900 MHz were decided upon and applied for licensing. The 450.000 MHt up-link is used on a "non-interference" basis to control the satellite while the 137.900 MHz frequency down-links data from the satellite. A reasonable amount of time was spent discussing the mods of transmission to be used in communication with the satellite. Representatives of the amateur radio satellite organization, AMSAT, were contacted for ides. This organization seems to favor AM types of emissions such as CW to control their OSCAR series of satellites and also the current Phase 111 unit. NUSAT personnel felt, however, that there would be merit in the improved signal to noise ratio usually obtained in an FM mode. Doppler shift of the transmitted information on the NUSAT also had to be considered. The final decision WBS to use Audio Frequency Shift Keying (AFSK) modulated on an FM carrier. In this mode the audio tones used would not shift frequency with Doppler - only the carrier would shift in frequency. If necessary, the receivers could be fitted with a form of AFC control or simply have enough bandwidth to handle the Doppler shift with an acceptable increase in noise.

Lee Barrett↗

Computer simulation of surface and film processes

All the investigations which were performed employed in one way or another a computer simulation technique based on atomistic level considerations. In general, three types of simulation methods were used for modeling systems with discrete particles that interact via well defined potential functions: molecular dynamics (a general method for solving the classical equations of motion of a model system); Monte Carlo (the use of Markov chain ensemble averaging technique to model equilibrium properties of a system); and molecular statics (provides properties of a system at T = 0 K). The effects of three-body forces on the vibrational frequencies of triatomic cluster were investigated. The multilayer relaxation phenomena for low index planes of an fcc crystal was analyzed also as a function of the three-body interactions. Various surface properties for Si and SiC system were calculated. Results obtained from static simulation calculations for slip formation were presented. The more elaborate molecular dynamics calculations on the propagation of cracks in two-dimensional systems were outlined.

Tiller, W. A.↗

Propagation considerations in land mobile satellite transmission

It appears likely that the Land Mobile Satellite Services (LMSS) will be authorized by the FCC for operation in the 800 to 900 MHz (UHF) and possibly near 1500 MHz (L-band). Propagation problems are clearly an important factor in the effectiveness of this service, but useful measurements are few, and produced contradictory interpretations. A first order overview of existing measurements is presented with particular attention to the first two NASA balloon to mobile vehicle propagation experiments. Some physical insight into the interpretation of propagation effects in LMSS transmissions is provided.

Vogel, W. J.↗

High T(c) superconducting NbN films deposited at room temperature

The dc reactive magnetron sputtering process yields stoichiometric NbN films with superconducting transition temperature T(c) as high as 15.7 K on substrates as varied as glass, glazed ceramic, fused quartz, and sapphire. These films posses fcc (B1) structure and (111) texture. The most dominant factors governing the formation of the transition metal nitrides are the relative metal and nitrogen fluxes incident on the substrate and the background argon pressure (which dictates the overall reactive sites and residence times for nitrogen).

Thakoor, S.↗

The structure of small metal clusters

One metal atom surrounded by its 12 nearest neighbors is considered for both D(3d) (face-centered cubic-like) and D(3h) (hexagonal close-packed-like) geometries. For Al and Be, the neutral cluster and the positive and negative ions are considered for idealized (all bonds equal) and distorted geometries. The D(3d) geometry is found to be the lowest for Be13, while the D(3h) geometry is lower for Al13. This is the reverse of what is expected based upon the bulk metal structures, Be(hcp) and Al(fcc). Al13 is found to have only small distortions, while Be13 shows large distortions for both the D(3d) and D(3h) geometries. The ions have geometries which are similar to those found for the neutral systems. Both all-electron and effective core potential calculations were carried out on the X13 clusters; the agreement is very good.

Bauschlicher, C. W., Jr.↗

A review of rapid solidification studies of intermetallic compounds

A review of rapid solidification studies of high-temperature ordered intermetallic compounds is presented. Emphasis is on the nickel - and iron- aluminides which are of potential interest as structural materials. The nickel-base aluminides which have been rapidly solidified exhibit changes in grain size, compositional segregation, and degree of long range order (as reflected in APB size and distribution) which markedly affect mechanical properties. Some experiments indicate the formation of a metastable L1(2) phase in rapidly solidified Fe-(Ni,Mn)-Al-C alloys, while other work observes only a metastable fcc phase in the same composition range. The metastable phases and/or microstructures in both nickel and iron aluminides are destroyed by annealing at temperatures above 750 K, with subsequent degradation of mechanical properties. Rapid solidification studies of several other intermetallic compounds are briefly noted.

Koch, C. C.↗

Analysis of interference to remote passive microwave sensors

The final acts of the 1979 World Administrative Radio Conference (WARC) were analyzed to determine potential interference to remote passive microwave sensors. Using interferer populations determined from the U.S. Government and FCC Master File Lists and assuming uniform geographical distribution of interferers, the level of interference from shared services and active services in adjacent and subharmonic bands was calculated for each of the 22 passive sensing bands. In addition, due to the theoretically large antennas required for passive sensing, an analysis was performed to determine if smaller antennas, i.e., relaxed resolution requirements, would have an effect on interference and to what extent.

Boyd, Douglas↗

Transmission of order in some unusual dilute systems

As a system is diluted, the critical temperature T may fall to zero at a concentration X sub c greater than the percolation concentration, because mere connectivity does not guarantee the transmission of order even at T = 0. Detailed results, including bounds on X sub c, are presented for the three-state Potts antiferromagnet on a triangular lattice and for quadrupolar models of (o-H2)x(p-H2)1-x mixtures on fcc and triangular lattices.

Adler, Joan↗

Chill block melt spinning of nickel-molybdenum alloys

Samples of Ni-Mo alloys ranging in composition from pure nickel to Ni-40 at. pct molybdenum were cast by the chill block melt-spinning rapid solidification technique and examined by optical metallography, X-ray diffraction, and microhardness testing. Casting difficulties were encountered with lean alloys, but richer alloys spread more readily on the casting wheel. Alloy microstructures for 5 to 37.5 at. pct molybdenum ribbons were primarily cellular/dendritic; microstructure feature size decreased with increasing molybdenum content. Extended solubility of molybdenum in gamma-nickel, with fcc lattice parameter increasing with composition to the 1.05 power, was observed up to 37/5 at. pct molybdenum. Substoichiometric Ni-Mo (delta) nucleated on the wheel side of the ribbons of compositions 35, 37.5, and 40 at. pct molybdenum. The amount of partitionless delta-phase thus formed increased with increasing molybdenum content and quench rate. This substoichiometric delta transformed readily to a fine structure gamma-delta mixture.

Hemker, Kevin J.↗

Small Al clusters. II - Structure and binding in Al(n) (n = 2-6, 13)

The structure and stability of aluminum clusters containing up to six atoms have been studied using correlated wave functions and extended basis sets. The lowest energy structure is planar for Al4 and Al5, but three dimensional for Al6. The icosahedral, hcp, fcc, and two planar structures of Al13 were considered at the SCF level. The lowest energy structure is the icosahedron, but the planar structures are fairly low lying even in this case. A simplified description using two- and three-body interaction potentials is found to agree well with the ab initio structures and binding energies.

Pettersson, Lars G. M.↗

Undercooled and rapidly quenched Ni-Mo alloys

Hypoeutectic, eutectic, and hypereutectic nickel-molybdenum alloys were rapidly solidified by both bulk undercooling and melt spinning techniques. Alloys were undercooled in both electromagnetic levitation and differential thermal analysis equipment. The rate of recalescence depended upon the degree of initial undercooling and the nature (faceted or nonfaceted) of the primary nucleating phase. Alloy melts were observed to undercool more in the presence of primary Beta (NiMo intermetallic) phase than in gamma (fcc solid solution) phase. Melt spinning resulted in an extension of molybdenum solid solubility in gamma nickel, from 28 to 37.5 at. pct Mo. Although the microstructures observed by undercooling and melt spinning were similar, the microsegregation pattern across the gamma dendries was different. The range of microstructures evolved was analyzed in terms of the nature of the primary phase to nucleate, its subsequent dendritic growth, coarsening and fragmentation, and final solidification of interfenderitic liquid.

Tewari, S. N.↗

Predicting diffusion paths and interface motion in gamma/gamma + beta, Ni-Cr-Al diffusion couples

A simplified model has been developed to predict Beta recession and diffusion paths in ternary gamma/gamma + beta diffusion couples (gamma:fcc, beta: NiAl structure). The model was tested by predicting beta recession and diffusion paths for four gamma/gamma + beta, Ni-Cr-Al couples annealed for 100 hours at 1200 C. The model predicted beta recession within 20 percent of that measured for each of the couples. The model also predicted shifts in the concentration of the gamma phase at the gamma/gamma + beta interface within 2 at. pct Al and 6 at. pct Cr of that measured in each of the couples. A qualitative explanation based on simple kinetic and mass balance arguments has been given which demonstrates the necessity for diffusion in the two-phase region of certain gamma/gamma + beta, Ni-Cr-Al couples.

Nesbitt, J. A.↗

The effect of composition and cooling rate on the structure of rapidly solidified (Fe, Ni)3Al-C alloy

The quench rate-metastable structure dependence in the Fe-20Ni-8Al-2C wt pct alloy has been experimentally studied. The nonequilibrium gamma-prime and gamma phases were noted in foils 65-100 microns thick, while at higher quench rates (thinner samples) the matrix was found to be in a disordered fcc gamma phase with kappa carbide precipitates. With the addition of silicon to the alloys, the nonequilibrium gamma-prime and gamma structures are observed at higher cooling rates.

Myers, S. A.↗

Effects of crystal-melt interfacial energy anisotropy on dendritic morphology and growth kinetics

Morphological and kinetic studies of succinonitrile, a BCC crystal with a low (0.5 percent) anisotropy and pivalic acid, and FCC crystal with relatively large (5 percent) anisotropy in solid-liquid interfacial energy, show clearly that anisotropy in the solid-liquid interfacial energy does not affect the tip radius-velocity relationship, but has a profound influence on the tip region and the rate of amplification of branching waves. Anisotropy of the solid-liquid interfacial energy may be one of the key factors by which the microstructural characteristics of cast structures reflect individual material behavior, especially crystal symmetry.

Glicksman, M. E.↗