Search NASA⌕ Search

SEARCH · Search NASA

Results for “Graphite specimens”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

The effects of crushing surface roughness on the crushing characteristics of composite tubes

The effects of crushing-surface roughness on the energy-absorption capability of graphite and glass-epoxy composite tubes were investigated. Fifty different combinations of fiber, matrix, and specimen ply orientation were evaluated. Two different crushing surface roughnesses were used in this investigation. Crushing surface significantly influences the energy-absorption capability only of tubes that crush in the lamina bending crushing mode; tubes that crush in other modes are not influenced because their lamina bundles do not slide against the crushing surface. Those tubes that crush in the lamina bending mode can achieve higher, lower, or no change in energy-absorption capability as crushing surface roughness increases. If the fiber failure strain of tubes that crush in the lamina bending crushing mode exceeds the matrix failure strain then the energy-absorption capability increases as crushing surface roughness increases. However, if the matrix failure strain exceeds the fiber failure strain then the energy-absorption capability increases as crushing surface roughness decreases. Energy-absorption capability is uninfluenced by crushing surface roughness for tubes that have equal fiber and matrix failure strains.

Farley, Gary L.↗

TREAT reactor LEU fuel-clad chemical interaction empirical modeling analysis

DOE is converting TREAT (Transient Reactor Test) facility from its existing highly enriched uranium (HEU) core to a low-enriched uranium (LEU) core. In order to assess the magnitude of chemical interaction between fuel and cladding materials during physical contact under expected TREAT operational limits, planned transients tests, and reactivity accident scenarios, a combination of experimental testing and thermodynamic modeling was performed to predict the expected chemical interactions among fuel and cladding chemical constituents. Thermodynamic calculations were then validated with empirical data from experiments that emulate TREAT's expected upper operational limits. Pellet samples composed of LEU oxide powder dispersed in a graphite matrix had intimate contact with zirconium-based alloy cladding. The samples were subjected to long-term isothermal heating under high vacuum. Specimen characterization consisted of scanning electron microscopy, x-ray diffraction analysis, and x-ray tomography. ThermoCalc software and Ellingham's diagrams were used for thermodynamic calculations. The X-ray tomography and SEM analysis of the pellets showed a homogeneous distribution of UO{sub 2} particles within the graphite matrix with isolated larger UO{sub 2} agglomerates. The SEM analysis showed the formation of a lamellar structure between the large UO{sub 2} agglomerate and the graphite matrix. This is an indication that diffusion is taking place at a rather moderate temperature and reaction time during the pellet fabrication. Secondary phases, with high Al and Mg content, were detected inside a UO{sub 2} agglomerate using SEM in SE/EBSD mode and chemical analysis with EDS. LEU feedstock impurities, as Al and Mg, seem to promote the chemical reactivity between UO{sub 2} particles and graphite matrix. XRD analysis of a pellet sample showed the presence of UO{sub 2} and graphite, but no other crystalline phases were detected with this technique. Thermodynamic analysis through the use of Ellingham diagrams showed that within TREAT's operational to reactivity accident temperature (278-820 Celsius degrees), UO{sub 2} can be reduced to U metal by Zr due to a more favorable ΔG for the oxidation of Zr.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An Innovative Technique for Evaluating Fracture Toughness of Graphite Materials

Spiral Notch Torsion Fracture Toughness Test (SNTT) was developed recently to measure the intrinsic fracture toughness (KIC) of structural materials. The SNTT system operates by applying pure torsion to uniform cylindrical specimens with a notch line that spirals around the specimen at a 45 a pitch. The KIC values are obtained with the aid of a three-dimensional finite-element computer code, TOR3D-KIC. The SNTT method is uniquely suitable for testing a wide variety of materials used extensively in pressure vessel and piping structural components and weldments, including others such as ceramics, their composites, graphite and concrete.

36 MATERIALS SCIENCE↗

Interfacial strength development in thermoplastic resins and fiber-reinforced thermoplastic composites

An experimental program to develop test methods to be used to characterize interfacial (autohesive) strength development in polysulfone thermoplastic resin and graphite-polysulfone prepreg during processing is reported. Two test methods were used to examine interfacial strength development in neat resin samples. These included an interfacial tension test and a compact tension (CT) fracture toughness test. The interfacial tensile test proved to be very difficult to perform with a considerable amount of data scatter. Thus, the interfacial test was discarded in favor of the fracture toughness test. Interfacial strength development was observed by measuring the refracture toughness of precracked compact tension specimens that were rehealed at a given temperature and contact time. The measured refracture toughness was correlated with temperature and contact time. Interfacial strength development in graphite-polysulfone unidirectional composites was measured using a double cantilever beam (DCB) interlaminar fracture toughness test. The critical strain energy release rate of refractured composite specimens was measured as a function of healing temperature and contact time.

Howes, Jeremy C.↗

Electron microscopy data on irradiation effects in glassy carbon, nuclear graphite, pyrolytic carbon, and carbon fibers

Glassy carbon, a monoatomic allotrope of carbon, is a candidate material for components in fission nuclear power systems due to its radiation tolerance. This article presents comprehensive electron microscopy data revealing the effects of neutron and electron irradiation on glassy carbon. For comparison, additional data are provided for pyrolytic graphite and carbon fibers, materials that exhibit similar structural behavior under irradiation. In situ electron irradiation experiments further illustrate the real-time microstructural evolution of glassy carbon during exposure. The dataset is organized into five parts: (1) transmission electron microscopy (TEM) micrographs of as-received and neutron-irradiated glassy carbon; (2) TEM micrographs of neutron-irradiated graphite; (3) TEM micrographs of unirradiated and irradiated carbon–carbon composites; (4) TEM micrographs of pyrolytic carbon specimens in both conditions; (5) scanning transmission electron microscopy (STEM) micrographs of as-received and neutron-irradiated glassy carbon and (6) in situ electron irradiation data of a glassy carbon particle. These datasets provide valuable insights into radiation-induced structural changes in carbon-based materials relevant to nuclear applications.

36 MATERIALS SCIENCE↗

An experimental and analytical investigation of the rail shear-test method as applied to composite materials

This report presents the results from an experimental and analytical investigation of the stress distributions occurring in a rail shear test. The effects of non-uniform stresses induced by differential thermal expansion, rail flexibility and specimen aspect ratio on measured shear modulus and ultimate strength of composite laminates are shown. A two-dimensional linearly elastic finite element model was used to analytically determine how various geometric parameters influenced the magnitude and distribution of inplane normal and shear stresses in a tensile rail shear specimen. Rail shear tests were conducted at room temperature and 589 K (600 F) on selected graphite-polyimide composite laminates using two titanium rail configurations. The analysis and test methods are discussed, and the results of the effects of the various parameters on shear modulus and ultimate strength are presented.

Garcia, R.↗

Mechanical property characterization of intraply hybrid composites

An investigation of the mechanical properties of intraply hybrids made from graphite fiber/epoxy matrix hybridized with secondary S-glass or Kevlar 49 fiber composites is presented. The specimen stress-strain behavior was determined, showing that mechanical properties of intraply hybrid composites can be measured with available methods such as the ten-degree off-axis test for intralaminar shear, and conventional tests for tensile, flexure, and Izod impact properties. The results also showed that combinations of high modulus graphite/S-glass/epoxy matrix composites exist which yield intraply hybrid laminates with the best 'balanced' properties, and that the translation efficiency of mechanical properties from the constituent composites to intraply hybrids may be assessed with a simple equation.

Chamis, C. C.↗

Physical aging in graphite epoxy composites

The matrix dominated mechanical behavior of a graphite epoxy composite was found to be affected by sub Tg annealing. Postcured + or - 45 deg 4S specimens of Thornel 300 graphite/Narmco 5208 epoxy were quenched from above Tg and given a sub Tg annealing at 140 C for times up to 10 to the 5th power min. The ultimate tensile strength, strain to break, and toughness of the composite material were found to decrease as functions of sub Tg annealing time. No weight loss was observed during the sub Tg annealing. The time dependent change in mechanical behavior is explained on the basis of free volume changes that are related to the physical aging of the nonequilibrium glassy network epoxy. The results imply possible changes in composite properties with service time.

Kong, E. S. W.↗

Modal response and noise transmission of composite panels

Noise transmission through flat, angular, fiber-reinforced composite panels is investigated experimentally and analytically. A modal decomposition technique was used to obtain solutions to the governing differential equation of motion. Experimental modal analysis was performed in order to confirm the theoretical results. The test specimens were cross-ply and angle-ply composite panels made of various concentrations of fiberglass, graphite, or aramid fibers embedded in epoxy resion. The experimental results showed good agreement with the theoretical calculations. Graphs of the transmission loss characteristics of the different composite panels are provided.

Grosveld, F. W.↗

Crosslinking-property relationships in PMR polyimide composites. I

The thermooxidatively-induced crosslinking/ physical and mechanical property relationships of graphite fiber-reinforced PMR polyimide-matrix composites were studied during isothermal exposure of the composite specimens at 288 C in air for periods of up to 5000 hr. The crosslinking densities due to this treatment were estimated on the basis of the kinetic theory of rubber elasticity and shifts in the glass transition temperature T(g). Several linear relationships are noted between crosslink density and physical and mechanical properties: T(g), initial weight loss, and elevated temperature interlaminar shear strength increase with crosslink density, while initial moisture absorption decreases. After achieving the highest crosslink density, several of the composite properties begin to decrease from their maximum values.

Pater, R. H.↗

Effect of dropped plies on the strength of graphite-epoxy laminates

The reduction in the compressive and tensile strengths of graphite-epoxy laminates with thickness discontinuities due to dropped plies was studied by experiment and analysis. The specimens were fabricated with all the dropped plies lumped together in the center of a sixteen-ply quasi-isotropic layup, such that one surface was flat and the slope of the opposite surface changed abruptly at the dropped ply location to accommodate the thickness change. Even though the thick and thin sections are symmetrically laminated, there exists bending-extension coupling due to the geometric eccentricity of the middle planes of the thick and thin sections. Experiments were conducted on fifty-four specimens that differed in the configuration of the dropped plies only. The strength of a laminate with dropped plies is less than the strength of its thin section, and the compressive strength of a laminate with dropped plies is less than its tensile strength. The reduction in strength is directly related to the axial stiffness change between the thick and thin sections. To examine the mechanism of failure, the three-dimensional state of stress in the dropped ply region was evaluated by the finite element method. A tensile interlaminar criterion predicted the correct location of failure, but underestimated the failure load.

Curry, James M.↗

A study of graphite-epoxy laminate failures due to high transverse shear strains using the multi-span-beam shear test procedure

The multi-span-beam shear test procedure is used to study failure mechanisms in graphite-epoxy laminates due to high transverse shear strains induced by severe local bending deformations in test specimens. Results of a series of tests on specimens with a variety of stacking sequences, including some with adhesive interleaving, are presented. These results indicate that laminates with stacking sequences with several + or - 45 and 90 deg plies next to each other are more susceptible to failures due to high transverse shear strains than laminates with + or - 45 and 0 deg plies next to each other or with + or - 45 deg plies next to layers of adhesive interleaving. Results of these tests are compared with analytical results based on finite elements.

Jegley, Dawn C.↗

Post impact compressive strength in composites

Presented in this paper are the plan, equipment, procedures, and findings of an experimental investigation of the tolerance to low velocity impact of a graphite epoxy (AS4/3501-6) and graphite bismaleimide (M6/CYCOM3100) advanced composites. The applied impacts were governed by the Air Force Guide Specification 87221. Specimens of each material system having a common nominal layup (10% 0 deg; 80% +/-45 deg; 10% 90 deg), a common 7 inch (17.78 cm) by 10 inch (25.40 cm) size, five different thicknesses (9, 26, 48, 74, and 96 plies), and ambient moisture content were impacted and strength tested at room temperature. Damaged areas and post impact compression strengths (PICS) were among the most significant findings obtained. While the undamaged per ply compression strength of both materials is a strong function of laminate thickness, the per ply PICS is not. The average difference in per ply PICS between the two material systems is about seven percent. Although a smaller percentage of the applied kinetic energy was absorbed by the Gr/BMI than by the Gr/Epoxy composites, larger damaged areas were produced in the Gr/BMI than in Gr/Epoxy. Within the limitations of this investigation, the Gr/BMI system seems to offer no advantage in damage tolerance over the Gr/Epoxy system examined.

Demuts, Edvins↗

Characterization of Two-Dimensionally Braided Composites Subject to Static and Fatigue Loading

This paper presents a characterization of damage processes in four different two-dimensionally braided architectures consisting of graphite fibers in an epoxy matrix, subjected to both static and fatigue loading. Both notched and unnotched specimens were tested from each architecture. Damage mechanisms in static compression testing were found to range from matrix cracking in an architecture controlled by shearing characteristics of the matrix to axial fiber bundle kinking and splitting in architectures controlled by unidirectional fiber bundles. In both static tension and tension-tension fatigue testing, it was found that all architectures sustained the same basic damage types and progression sequences. The first types of damage to occur were splits in the braider bundles and cracks in the resin rich areas. Once a sufficient density of this type of damage had occurred, the axial bundles began to disbond from the surrounding constituents, and continued to do so until ultimate failure. One architecture sustained an additional mode of failure, which involved splitting of the axial bundles along their length. Varied degrees of notch sensitivity were found among the different architectures. In one architecture, this was attributed to differences found in the stacking of the individual plys of the braided architecture. As the density of axial bundles adjacent to the notch increased, the rate of stiffness loss increased and the life decreased.

Burr, Scott T.↗

Specimens Prepared for Materials International Space Station Experiment

The Materials International Space Station Experiment (MISSE) is a materials flight experiment sponsored by the Materials and Manufacturing Directorate of the Air Force Research Laboratory at Wright-Patterson Air Force Base and the NASA Space Environmental Effects Program at the NASA Marshall Space Flight Center. MISSE is a cooperative effort among the Air Force, several NASA field centers, and industry. The experiment package will be placed on the exterior of the International Space Station in the summer of 2001. Approximately half of the specimens will be exposed to the space environment for 1 year, and the other half will be exposed for 3 years. The Electro-Physics Branch at the NASA Glenn Research Center has prepared and delivered over 150 specimens to be included in MISSE. Specimens include: 1) Double-coated polyimide Kapton to compare mass loss from in-space atomic oxygen undercutting erosion to ground-laboratory atomic oxygen undercutting erosion for predicting in-space durability; 2) Silicones to study changes in surface hardness and optical properties after combined atomic oxygen--ultraviolet radiation exposure for predicting in-space durability; 3) Forty-one different polymers to accurately measure their atomic oxygen erosion yields; 4) Scattering chambers to study atomic oxygen scattering characteristics that are relevant to the degradation found in spacecraft with exterior openings; 5) Thin polymer film disks and tensile specimens to study the effects of radiation on their optical properties and mechanical properties; 6) Lightweight intercalated graphite epoxy composites to study electromagnetic interference shielding performance; and 7) Polymer-based materials utilizing new atomic oxygen protection concepts to study their durability.

Banks, Bruce A.↗

Optical Fiber Distributed Sensing Structural Health Monitoring (SHM) Strain Measurements Taken During Cryotank Y-Joint Test Article Load Cycling at Liquid Helium Temperatures

This paper outlines cryogenic Y-joint testing at Langley Research Center (LaRC) to validate the performance of optical fiber Bragg grating strain sensors for measuring strain at liquid helium temperature (-240 C). This testing also verified survivability of fiber sensors after experiencing 10 thermal cool-down, warm-up cycles and 400 limit load cycles. Graphite composite skins bonded to a honeycomb substrate in a sandwich configuration comprised the Y-joint specimens. To enable SHM of composite cryotanks for consideration to future spacecraft, a light-weight, durable monitoring technology is needed. The fiber optic distributed Bragg grating strain sensing system developed at LaRC is a viable substitute for conventional strain gauges which are not practical for SHM. This distributed sensing technology uses an Optical Frequency Domain Reflectometer (OFDR). This measurement approach has the advantage that it can measure hundreds of Bragg grating sensors per fiber and the sensors are all written at one frequency, greatly simplifying fiber manufacturing. Fiber optic strain measurements compared well to conventional strain gauge measurements obtained during these tests. These results demonstrated a high potential for a successful implementation of a SHM system incorporating LaRC's fiber optic sensing system on the composite cryotank and other future cryogenic applications.

Allison, Sidney G.↗

Ultrasonic Monitoring of Ply Crack and Delamination Formation in Composite Tube Under Torsion Load

As a simple model of a rotor spar, a circular graphite-epoxy composite laminate cylinder was subjected to cyclic torsional load. The test section of the cylindrical specimen varied from four to six plies of plus or minus 45 degree fibers, due to intentional ply overlaps and gaps. A layer of 13-micrometer Teflon film was inserted between plies at three locations to serve as delamination initiators. A commercial X-Y scanner was mounted to the load frame to enable ultrasonic inspection without removing the specimen. A focused immersion probe was mounted in a captive water column with a rugged Nitrile membrane tip, which was coupled to the cylinder using a mist of soapy water. The transducer was aligned normal to the cylinder surface using the X-axis. Scanning was performed along the length of the specimen with the Y-axis and the specimen was incrementally rotated by the torsion head of the load frame. After 350k cycles of torsion, several linear 45 degree diagonal indications appeared as 5-40% attenuation of the back wall echo, with no apparent echoes from the interior of the composite, suggesting through-ply cracks in the innermost ply. Crack indications grew and new cracks appeared as torsion cycling continued. Internal reflections from delaminations associated with the growing ply cracks appeared after 500k cycles. Three areas of extensive multi-layer delaminations appeared after 1150k cycles. Failure of the specimen occurred at 1600k cycles. The observed progressive damage was not associated with the Teflon inclusions. Concurrent thermographic measurements provided lower resolution confirmation of the damage observed.

Johnston, P. H.↗

Properties of autoclaved Gr/PI composites made from improved tack PMR-15 prepreg

Autoclave processing studies were conducted, using improved tack PMR-15 prepreg, to determine the effect of tack enhancing PMR resin modifications on composite processability and mechanical properties. Improved tack graphite fiber reinforced PMR-15 prepregs were prepared and exposed to ambient conditions for various times and then autoclave molded into composites. Composite specimens were prepared and tested for flexural and interlaminar shear strengths at room temperature and 316 C. The retention of flexural and interlaminar shear strength as a function of exposure in air at 316 C was also determined. The results show that the modified PMR resin solutions provide prepreg with improved tack and drape retention characteristics without adversely affecting processability or mechanical properties of autoclave molded graphite fiber reinforced PMR-15 composites.

Vannucci, R. D.↗