At least 325 records · Page 18

Adhesion, friction, and wear behavior of clean metal-ceramic couples

When a clean metal is brought into contact with a clean, harder ceramic in ultrahigh vacuum, strong bonds form between the two materials. The interfacial bond strength between the metal and ceramic surfaces in sliding contact is generally greater than the cohesive bond strength in the metal. Thus, fracture of the cohesive bonds in the metal results when shearing occurs. These strong interfacial bonds and the shearing fracture in the metal are the main causes of the observed wear behavior and the transfer of the metal to the ceramic. In the literature, the surface energy (bond energy) per unit area of the metal is shown to be related to the degree of interfacial bond strength per unit area. Because the two materials of a metal-ceramic couple have markedly different ductilities, contact can cause considerable plastic deformation of the softer metal. It is the ductility of the metal, then, that determines the real area of contact. In general, the less ductile the metal, the smaller the real area of contact. The coefficient of friction for clean surfaces of metal-ceramic couples correlates with the metals total surface energy in the real area of contact gamma A (which is the product of the surface energy per unit area of the metal gamma and the real area of contact (A)). The coefficient of friction increases as gamma A increases. Furthermore, gamma A is associated with the wear and transfer of the metal at the metal-ceramic interface: the higher the value of gamma A, the greater the wear and transfer of the metal.

Miyoshi, Kazuhisa↗

Fibre-matrix bond strength studies of glass, ceramic, and metal matrix composites

An indentation test technique for compressively loading the ends of individual fibers to produce debonding has been applied to metal, glass, and glass-ceramic matrix composites; bond strength values at debond initiation are calculated using a finite-element model. Results are correlated with composite longitudinal and interlaminar shear behavior for carbon and Nicalon fiber-reinforced glasses and glass-ceramics including the effects of matrix modifications, processing conditions, and high-temperature oxidation embrittlement. The data indicate that significant bonding to improve off-axis and shear properties can be tolerated before the longitudinal behavior becomes brittle. Residual stress and other mechanical bonding effects are important, but improved analyses and multiaxial interfacial failure criteria are needed to adequately interpret bond strength data in terms of composite performance.

Grande, D. H.↗

Theoretical study of the bonding of the first-row transition-metal positive ions to ethylene

Ab initio calculations were performed to study the bonding of the first-row transition-metal ions with ethylene. While Sc(+) and Ti(+) insert into the pi bond of ethylene to form a three-membered ring, the ions V(+) through Cu(+) form an electrostatic complex with ethylene. The binding energies are compared with those from experiment and with those of comparable calculations performed previously for the metal-acetylene ion systems.

Sodupe, M.↗

Porus electrode comprising a bonded stack of pieces of corrugated metal foil

An electrode suitable for use in an electrochemical cell is described. The electrode is composed of a porous conductive support with a bonded stack of pieces of thin corrugated nickel foil where the corrugations are oriented approximately perpendicular to the sides of the electrode and form an array of passages through the electrode. Active material such as cadmium hydroxide or nickel hydroxide is uniformly distributed within the passages. The support may comprise also a piece of thin flat nickel foil between adjacent pieces of the corrugated foil, forming a barrier between the passages formed on each side of it. Typically the corrugations in the odd corrugated layers are oriented at a small angle from the perpendicular in one direction and the corrugations in the even corrugated layers are oriented at a small angle from the perpendicular in the opposite direction.

Mccallum, J.↗

Mechanical and physical properties of plasma-sprayed stabilized zirconia

Physical and mechanical properties were determined for plasma-sprayed MgO- or Y2O3-stabilized ZrO2 thermal barrier coatings. Properties were determined for the ceramic coating in both the freestanding condition and as-bonded to a metal substrate. The properties of the NiCrAlY bond coating were also investigated.

Siemers, P. A.↗

Preliminary Investigations of Joining Technologies for Attaching Refractory Metals to Ni-Based Superalloys

In this study, a range of joining technologies has been investigated for creating attachments between refractory metal and Ni-based superalloys. Refractory materials of interest include Mo-47%Re, T-111, and Ta-10%W. The Ni-based superalloys include Hastelloy X and MarM 247. During joining with conventional processes, these materials have potential for a range of solidification and intermetallic formation-related defects. For this study, three non-conventional joining technologies were evaluated. These included inertia welding, electro-spark deposition (ESD) welding, and magnetic pulse welding (MPW). The developed inertia welding practice closely paralleled that typically used for the refractory metals alloys. Metallographic investigations showed that forging during inertia welding occurred predominantly on the nickel base alloy side. It was also noted that at least some degree of forging on the refractory metal side of the joint was necessary to achieve consistent bonding. Both refractory metals were readily weldable to the Hastelloy X material. When bonding to the MarM 247, results were inconsistent. This was related to the higher forging temperatures of the MarM 247, and subsequent reduced deformation on that material during welding. ESD trials using a Hastelloy X filler were successful for all material combinations. ESD places down very thin (5- to 10- m) layers per pass, and interactions between the substrates and the fill were limited (at most) to that layer. For the refractory metals, the fill only appeared to wet the surface, with minimal dilution effects. Microstructures of the deposits showed high weld metal integrity with maximum porosity on the order of a few percent. Some limited success was also obtained with MPW. In these trials, only the T-111 tubes were used. Joints were possible for the T-111 tube to the Hastelloy X bar stock, but the stiffness of the tube (resisting collapse) necessitated the use of very high power levels. These power levels resulted in damage to the equipment (concentrator) during welding. It is of note that the joint made showed the typical wavy bond microstructure associated with magnetic pulse/explosion bond joints. Joints were not possible between the T-111 tube and the MarM 247 bar stock. In this case, the MarM 247 shattered before sufficient impact forces could be developed for bonding.

Gould, Jerry E.↗

Method of making an explosively welded scarf joint

A method is presented for obtaining a bond joint between thin metal members without the addition of a bonding agent. The method yields bond strengths comparable to the parent metal. The method comprises overlapping the materials at the edges and bonding them by explosive welding while also making use of the explosive force to shape the materials into an essentially planar configuration.

Bement, L. J.↗

Shear strength of metal-sapphire contacts

The shear strength of polycrystalline Ag, Cu, Ni, and Fe contacts on clean (0001) sapphire has been studied in ultrahigh vacuum. Both clean metal surfaces and surfaces exposed to O2, Cl2, and C2H4 were used. The results indicate that there are two sources of strength of Al2O3-metal contacts: an intrinsic one that depends on the particular clean metal in contact with Al2O3 and an additional one due to intermediate films. The shear strength of the clean metal contacts correlated directly with the free energy of oxide formation for the lowest metal oxide, in accord with the hypothesis that a chemical bond is formed between metal cations and oxygen anions in the sapphire surface. Contacts formed by metals exposed to chlorine exhibited uniformly low shear strength indicative of van der Waals bonding between chlorinated metal surfaces and sapphire. Contacts formed by metals exposed to oxygen exhibited enhanced shear strength, in accord with the hypothesis that an intermediate oxide layer increases interfacial strength.

Pepper, S. V.↗

Electrostatically focused intensified charge coupled devices

Work performed to develop intensified charge coupled devices (ICCDs) is presented. Four ICCDs, containing 100 x 160 arrays, were fabricated. Electron gains up to 3200 at 15 keV were achieved. Photocathode sensitivities ranged from 190 to 410 micro A/lumen. Dark currents varied from 11 nA/sq cm to 37 nA/sq cm. There was serious concern about the reliability of the bonding scheme for ICCDs due to occassional bond failure. Two solutions to this problem were developed. One involved a modification of the existing bonding technique, and the other was the development of a protected bond pad employing a barrier metal between the aluminum metallization and the gold bond wire. An accumulation process was characterized with respect to its most critical variable. This characterization led to the achievement of reproducible spectral response and the discovery and elimination of dark current increase associated with this process.

Walker, J. W.↗

Production of an ion-exchange membrane-catalytic electrode bonded material for electrolytic cells

A good bond is achieved by placing a metal salt in solution on one side of a membrane and a reducing agent on the other side so that the reducing agent penetrates the membrane and reduces the metal. Thus, a solution containing Pt, Rh, etc., is placed on one side of the membrane and a reducing agent such as NaBH, is placed on the other side. The bonded metal layer obtained is superior in catalytic activity and is suitable as an electrode in a cell such as for solid polymer electrolyte water electrolysis.

Takenaka, H.↗

On the extension of the MCSCF/CI method

Research conducted during this period was focused on two main areas: (1) bonding in transition metal oxides; and (2) adsorption of CO on Al and Ni. In both of these theoretical studies a major interest was to obtain a better understanding of the nature of the bonding in transition metal containing systems. The studies used self consistent field (SCF), multi-configuration self cosistent field (MCSCF) and configuration interaction (CI) methods in the treatment of the transition metal oxides and only the SCF method in the adsorption studies. The reports of three principle investigators who contributed to this work during the tenure of the project are presented along with associated published papers.

Bauschlicher, C., Jr.↗

Comparison of the bonding between ML(+) and ML2(+) (M = metal, L = noble gas)

Ab initio calculations are reported of the spectroscopic constants for the low-lying states of the molecular ions ML2(+), where M = Li, Na, Mg, V, Fe, Co, Ni and Cu, and where L is usually Ar. Comparison with existing analogous calculations on the ML(+) ions shows how the bonding and binding energy change with the addition of a second noble gas atom. The second binding energy is predicted to be essentially the same as the first for the Li, Na, Mg, and V ions, but larger for the Fe, Co, Ni and Cu ions. The binding energies of the transition metal noble gas ions are not accurately predicted at the SCF level, because correlation is required to describe their M(0)Ln(+) character. All trends can be explained in terms of promotion and hybridization on the metal ion.

Bauschlicher, Charles W., Jr.↗

Adhesion and friction of thin metal films

Sliding friction experiments were conducted in vacuum with thin films of titanium, chromium, iron, and platinum sputter deposited on quartz or mica substrates. A single crystal hemispherically tipped gold slider was used in contact with the films at loads of 1.0 to 30.0 and at a sliding velocity of 0.7 mm/min at 23 C. Test results indicate that the friction coefficient is dependent on the adhesion of two interfaces, that between the film and its substrate and the slider and the film. There exists a relationship between the percent d bond character of metals in bulk and in thin film form and the friction coefficient. Oxygen can increase adhesive bonding of a metal film (platinum) to a substrate.

Buckley, D. H.↗

Impacting device for testing insulation

An electro-mechanical impacting device for testing the bonding of foam insulation to metal is descirbed. The device lightly impacts foam insulation attached to metal to determine whether the insulation is properly bonded to the metal and to determine the quality of the bond. A force measuring device, preferably a load cell mounted on the impacting device, measures the force of the impact and the duration of the time the hammer head is actually in contact with the insulation. The impactor is designed in the form of a handgun having a driving spring which can propel a plunger forward to cause a hammer head to impact the insulation. The device utilizes a trigger mechanism which provides precise adjustements, allowing fireproof operation.

Redmon, J. W.↗

Bonding and Joining Technology: a Compilation

A collection of articles concerning the methods and uses of aerospace bonding and joining techniques in industrial processes is presented. Data include methods to bond and join metal components, joining techniques for adhesive materials, and shop hints for bonding and joining a variety of other items and materials.

Source record↗

Investigation of the feasibility of developing low permeability polymeric films

The feasibility of reducing the gas permeability rate of Mylar and Kapton films without drastically effecting their flexibility characteristics at cryogenic temperatures was considered. This feasibility was established using a concept of diffusion bonding two layers of metallized films together forming a film-metal-film sandwich laminate. The permeability of kapton film to gaseous helium was reduced from a nominal ten = to the minus 9 power cc-mm/sq cm sec. cm Hg to ten to the minus 13 power cc-mm/ sq cm - sec. cm Hg with some values as low as ten to the minus 15 power cc - mm/sq cm m-sec - cm Hg being obtained. Similar reductions occurred in the liquid hydrogen permeability at -252 C. In the course of the program the permeability, flexibility and bond strength of plain, metalized and diffusion bond film were determined at +25 C, -195 C and -252 C. The cryogenic flexibility of Kapton film was reduced slightly due to the metallization process but no additional loss in flexibility resulted from the diffusion bonding process.

Hoggatt, J. T.↗