Degradation in PV Encapsulant Transmittance: Results of the First PVQAT TG5 Study

Reduced optical transmittance of encapsulants resulting from ultraviolet (UV) degradation has frequently been identified as a cause of decreased PV module performance through the life of service in the field. The present module safety and qualification standards, however, apply short UV doses only capable of examining design robustness or 'infant mortality' failures. The latest versions of the safety and qualification apply ~40 - ~160 days cumulative dose of the AM1.5G total UV radiation. Essential information that might be used to screen encapsulation through product lifetime also remains unknown. For example, the relative efficacy of xenon-arc and UVA-340 fluorescent sources or the typical range of activation energy for degradation is not quantified. We have conducted an interlaboratory experiment to provide the understanding that will be used towards developing a higher fidelity, more rigorous UV weathering test. Five representative, known formulations of EVA were studied in addition to one TPU material. Replicate laminated silica/polymer/silica specimens were examined at 10 institutions using a variety of indoor chambers (including Xenon, UVA-340, and high pressure mercury light sources). Specimens were artificially weathered for 180 cumulative days at pre-designated accelerated test conditions. The solar-weighted transmittance, yellowness index, and the UV cut-off wavelength, determined from the measured hemispherical transmittance, are examined to provide understanding and guidance for the UV light source (lamp type) and temperature used in accelerated UV aging tests.

14 SOLAR ENERGY↗

Physical/chemical modeling for photovoltaic module life prediction

The paper presents a generalized methodology for identification and evaluation of potential degradation and failure of terrestrial photovoltaic encapsulation. Failure progression modeling and an interaction matrix are utilized to complement the conventional approach to failure degradation mode identification. Comparison of the predicted performance based on these models can produce: (1) constraints on system or component design, materials or operating conditions, (2) qualification (predicted satisfactory function), and (3) uncertainty. The approach has been applied to an investigation of an unexpected delamination failure; it is being used to evaluate thermomechanical interactions in photovoltaic modules and to study corrosion of contacts and interconnects.

Moacanin, J.↗

Lessons from the IEC Durability of Adhesion Accelerated Test Sequence

The IEC 62788-1-1 and IEC 63209-2 standards use aging sequences for durability of adhesion in photovoltaic (PV) modules, which may be evaluated using the single cantilever beam (SCB) test. Because the encapsulant forms critical interfaces with the front glass and solar cells, degradation at those interfaces under ultraviolet (UV) exposure, elevated temperature, and humidity can lead to interfacial delamination - compromising the long-term reliability. In this work, adhesion durability of UV-transmitting poly(ethylene-co-vinyl acetate) (EVA) encapsulant to glass and to silicon solar cells is evaluated after sequenced UV and damp heat aging (85C/85%RH). Laminates were prepared using StarPhire solar front glass with thin glass or PERC cells, and two EVA formulations with different concentrations of siloxane coupling agent. Adhesion was quantified by measuring critical debond energy using the SCB method. Both formulations exhibit similar qualitative trends, while different adhesion is observed at the periphery despite the use of low-shrink manufacturing. The results show that while glass/EVA adhesion remains stable or increases after UV exposure and shows only moderate changes after damp heat, the EVA/cell interface exhibits an irreversible loss of adhesion following UV and then damp heat exposure. Although glass/EVA interfaces generally exhibit lower debond energies, the EVA/cell interface is significantly more vulnerable to UV-driven degradation, identifying it as the dominant reliability risk location through early- and intermediate-module life. These results demonstrate that accelerated aging sequences can expose large, interface-specific losses in adhesion durability and underscore the importance of interface engineering for long-term PV module reliability.

14 SOLAR ENERGY↗

Degradation in photovoltaic encapsulant transmittance: Results of the first PVQAT TG5 artificial weathering study

Reduced optical transmittance of encapsulants resulting from ultraviolet (UV) degradation is frequently identified as a cause of decreased performance through the service life of photovoltaic modules. However, the present module safety and qualification standards apply short UV doses, only capable of examining design robustness and 'infant mortality' failures. Furthermore, essential information remains unknown that might be used to screen encapsulants through product lifetime. We conducted an interlaboratory study to provide the understanding that will be used toward developing a higher-fidelity, more-rigorous UV weathering test. Five representative known formulations of poly (ethylene-co-vinyl acetate) were studied, in addition to one thermoplastic polyurethane material. Replicate laminated silica/polymer/silica specimens were examined at seven institutions using a variety of indoor chambers (including xenon, UVA-340, and metal-halide light sources). Specimens were artificially weathered for 180 cumulative days at steady-state accelerated test conditions, predesignated relative to the default irradiance of 1.0 W m-2 nm-1 at 340 nm, chamber temperature of 60 degrees C, and chamber relative humidity of 30%. The solar-weighted transmittance, yellowness index, and the UV cut-off wavelength - each determined from the measured hemispherical transmittance - are examined to provide understanding and guidance for the UV light source (type lamp and filters), temperature, and humidity used in accelerated UV aging tests. The relative efficacy of xenon-arc and UVA-340 fluorescent sources and the typical range of activation energy for degradation is quantified from the experiments.

14 SOLAR ENERGY↗

Al+Si Interface Optical Properties Obtained in the Si Solar Cell Configuration

Al is a commonly used material for rear side metallization in commercial silicon (Si) wafer solar cells. In this study, through-the-silicon spectroscopic ellipsometry is used in a test sample to measure Al+Si interface optical properties like those in Si wafer solar cells. Two different spectroscopic ellipsometers are used for measurement of Al+Si interface optical properties over the 1128-2500 nm wavelength range. For validation, the measured interface optical properties are used in a ray tracing simulation over the 300-2500 nm wavelength range for an encapsulated Si solar cell having random pyramidal texture. The ray tracing model matches well with the measured total reflectance at normal incidence of a commercially available Si module. The Al+Si optical properties presented here enable quantitative assessment of major irradiance/current flux losses arising from reflection and parasitic absorption in encapsulated Si solar cells.

14 SOLAR ENERGY↗

Recovery of Glass and Silicon Solar Cells from Si-Modules Through Laser Processing

This study demonstrates an innovative and environmentally friendly laser-based approach for the efficient recovery of glass and silicon solar cells, allowing the recycling of photovoltaic modules. The methodology involves the use of a high-power pulsed laser beam focusing at various interfaces within the modules. Specifically, the delivery of ultra-short pulse laser energy at the interfaces of glass and polymeric encapsulants, as well as at the encapsulants and silicon solar cells, facilitates the debonding of polymers from both glass and silicon cell surfaces. The debonding occurs through photothermal, ablation, chemical modification, and localized heat generation. The research successfully demonstrates the recovery of glass from commercial mini solar modules of size 11.5 x 6.8 cm 2 and a silicon wafer of size 3.0x1.6 cm 2 . Ongoing efforts aim to extend the effectiveness of this laser-based methodology to comprehensively recycle larger-size components. This innovative approach holds promise for addressing environmental concerns associated with the disposal of solar modules, contributing to sustainable practices in the renewable energy sector.

glass↗

Electrochemical Degradation Modes in Bifacial Silicon Photovoltaic Modules

Motivated by the rapidly rising deployment of bifacial monocrystalline-silicon photovoltaics (PV), we investigate the durability of various PV module packaging configurations with transparent coverings on both the front and rear sides of the module. We use a series of bifacial passivated emitter and rear cell (p-PERC) mini-modules with systematically varying outer cover materials (glass/glass, G/G, or glass/transparent backsheet, G/TB) and encapsulant chemistries (poly [ethylene-co-vinyl acetate], EVA; or polyolefin, POE). We study degradation modes over 1,000 hours of combined damp heat (DH) exposure and high system voltages that can cause potential-induced degradation (PID) under positive, zero, or negative 1,000 V cell-to-frame bias. We analyze the degradation modes using a combination of current-voltage measurements, impedance spectroscopy, external quantum efficiency, and spatially resolved luminescence and thermal imaging. Our results highlight various types of degradation including shunting, enhanced recombination, and series resistance increases, and we use spatially resolved characterization to separately identify the localized effects. We show that multiple PID and moisture-ingress degradation modes severely affect EVA-containing modules, with previously reported PID processes under negative-bias DH and a unique observation of rear-side surface recombination in G/EVA/G modules under positive-bias DH. We observe significantly less degradation in POE-containing modules, where the G/POE/G configuration exhibits minimal degradation under all stress conditions that we employ.

14 SOLAR ENERGY↗

Properties of Encapsulated CIGS Cells in 85 degrees C/85%RH

This paper concerns studies of encapsulated cells subjected to an environment of 85ºC and 85%RH (85/85). Cells are encapsulated with PNNL multi-layer coatings (referred to as PML coatings) utilizing alternating layers of Al2O3, and an advanced polymer. The new polymer has been determined to withstand the 85/85 environment. Two types of cells were used for these studies, namely, SSI mini-modules (which are actually CIGSS devices) and CIGS cells provided by the Institute of Energy Conversion (IEC). Cells were coated and stressed at 85/85 in an environmental chamber. Current-voltage characteristics were acquired before and after coating, and periodically after being subjected to the 85/85 environment. Whereas coated SSI modules were determined to last 1000 hours when stressed at 60ºC/90%RH without degradation, the efficiency of these modules degrade to a level of 60% of the beginning-of-life value when stressed at 85/85. Encapsulated IEC cells, however, have exhibited extraordinary results. The efficiency of several encapsulated cells did not decrease for 1500 hours in an 85ºC/85%RH environment. This results establishes a benchmark for stressed, encapsulated CIGS cells.

14 SOLAR ENERGY↗

Degradation in PV Encapsulation Strength of Attachment: An Interlaboratory Study Towards a Climate-Specific Test

Reduced strength of attachment of the encapsulant resulting from the outdoor environment, including ultraviolet (UV) radiation, may decrease photovoltaic (PV) module lifetime by enabling widespread corrosion of internal components. To date, few studies exist showing how the adhesion of PV components varies with environmental stress. We have conducted an interlaboratory experiment to provide an understanding that will be used to develop climatic specific module tests. Factors examined in the study included the UV light source (lamp type), temperature, and humidity to be proposed for use in accelerated aging tests. A poly (ethylene-co-vinyl acetate) (EVA) formulation often used in veteran PV installations was studied using a compressive shear test - to quantify the strength of attachment at the EVA/glass interface. Replicate laminated glass/polymer/glass coupon specimens were weathered at 12 institutions using a variety of indoor chambers or field aging. Shear strength, shear strain, and toughness were measured using a mechanical load-frame for the compressive shear test, with subsequent optical imaging and electron microscopy of the separated surfaces.

14 SOLAR ENERGY↗

Investigation of Test Methods, Material Properties, and Processes for Solar Cell Encapsulants

The reformulation of a commercial grade of ethylene/vinyl acetate copolymer for use as a pottant in solar cell module manufacture was investigated. Potentially successful formulations were prepared by compounding the raw polymer with antioxidants, ultraviolet absorbers and crosslinking agents to yield stabilized and curable compositions. The resulting elastomer was found to offer low cost (approximately $0.80/lb.), low temperature processability, high transparency (91% transmission), and low modulus. Cured specimens of the final formulation endured 4000 hours of fluorescent sunlamp radiation without change which indicates excellent stability.

Willis, P. B.↗

Study program for encapsulation materials interface for low-cost solar array

The service integrity of the bonded interface in solar cell modules used in solar arrays is addressed. The development of AC impedance as a nondestructive evaluation (NDE) methodology for solar arrays is reported along with development of corrosion models and materials selection criteria for corrosion resistant interfaces.

Kaelble, D. H.↗

Advancing the Fork detector for quantitative spent nuclear fuel verification

The Fork detector is widely used by the safeguards inspectorate of the European Atomic Energy Community (EURATOM) and the International Atomic Energy Agency (IAEA) to verify spent nuclear fuel. Fork measurements are routinely performed for safeguards prior to dry storage cask loading. Additionally, spent fuel verification will be required at the facilities where encapsulation is performed for acceptance in the final repositories planned in Sweden and Finland. The use of the Fork detector as a quantitative instrument has not been prevalent due to the complexity of correlating the measured neutron and gamma ray signals with fuel inventories and operator declarations. A spent fuel data analysis module based on the ORIGEN burnup code was recently implemented to provide automated real-time analysis of Fork detector data. This module allows quantitative predictions of expected neutron count rates and gamma units as measured by the Fork detectors using safeguards declarations and available reactor operating data. This study describes field testing of the Fork data analysis module using data acquired from 339 assemblies measured during routine dry cask loading inspection campaigns in Europe. Assemblies include both uranium oxide and mixed-oxide fuel assemblies. More recent measurements of 50 spent fuel assemblies at the Swedish Central Interim Storage Facility for Spent Nuclear Fuel are also analyzed. An evaluation of uncertainties in the Fork measurement data is performed to quantify the ability of the data analysis module to verify operator declarations and to develop quantitative go/no-go criteria for safeguards verification measurements during cask loading or encapsulation operations. The goal of this approach is to provide safeguards inspectors with reliable real-time data analysis tools to rapidly identify discrepancies in operator declarations and to detect potential partial defects in spent fuel assemblies with improved reliability and minimal false positive alarms. Finally, the results are summarized, and sources and magnitudes of uncertainties are identified, and the impact of analysis uncertainties on the ability to confirm operator declarations is quantified.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Uniform Mechanical Loading Can Test for Nonuniform Loading Durability

In this work, we present a method to evaluate the equivalency between any module mechanical loading conditions. The method is developed to address the specific failure mode of glass fracture and is based on Weibull analysis and weakest link theory. It considers the varying stress profile across the module to calculate the probability of glass fracture, which is used as the metric of equivalency. An idealized nonuniform loading scheme is employed to demonstrate the method and introduce the concept of the equivalent uniform load factor: a factor applied to the maximum pressure of the nonuniform load to obtain the equivalent uniform load value. It is demonstrated that this factor is less than unity for all nonuniform load cases considered, including snow and various characters of wind loading. These significant results suggest that uniform loading may be reliably, and practically, employed to evaluate photovoltaic module glass for nonuniform loading durability.

14 SOLAR ENERGY↗

Surface Stress Characterization and Trends in Thermally Strengthened Photovoltaic Module Glass

Simultaneous changes in photovoltaic (PV) module architecture-such as increased area, replacing the polymeric backsheet with a glass backsheet, and reducing glass thickness from 3.2 to 2.0 mm-have resulted in a novel failure called spontaneous glass breakage. Spontaneous glass breakage results in front and/or rear glass failure without any obvious cause. The resulting low-energy fracture patterns have raised concerns about the thermal strengthening in 2.0-mm glass. We present validation of a nondestructive method for measuring the glass surface stress in PV modules. We use a scattered light polariscope to examine the glass properties of 11 modules from 6 solar fields, with and without spontaneous glass breakage. Based on a Mann-Whitney test p-value of 1.4 x 10-6, we conclude that there is a correlation between lower surface stress and susceptibility to spontaneous breakage. A Kendall's Tau test p-value of 2.0 x 10-4 indicates a correlation between increased module area and lower surface stress. We find that 2.0-mm glass can be, and often is, fully tempered (surface stress ≥69 MPa), but inspecting the fracture pattern is not a reliable way to assess the amount of thermal strengthening. A combination of factors, not just surface stress, influences glass breakage.

14 SOLAR ENERGY↗

EFG solar modules

Six photovoltaic modules using solar cells fabricated from silicon ribbons were assembled and delivered to JPL. Each module was comprised of four separate submodules which were parallel connected. The submodules contained 45 EFG cells which were series interconnected by a shingle or overlapping design. The inherent rectangular shape of the cells allowed a high packing factor to be achieved. The average efficiency of the six modules, corrected to AM1 at 28 C was 8.7%, which indicates that the average encapsulated cell efficiency was 10.0%.

Source record↗