Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

The Impact of Lithium Anode Interface on Capacity Fade in Polymer Electrolyte-Based Solid-State Batteries

This study investigates the Li stripping-plating morphology and failure mechanisms in full cells consisting of a solid polymer electrolyte (SPE) with two commercial Li anodes: Li chip and Li foil. The primary identified failure mechanism of the SPE cell is capacity fade, regardless of the Li manufacturer. While the cathode’s role in capacity fade is evident, the Li anode significantly influences cycling performance, with Li foil cells cycling 50% longer than Li chip cells, a statistical difference. Further, post-mortem scanning electron microscopy and X-ray photoelectron spectroscopy results attribute the Li chip’s faster capacity fade to a loss of contact and continuous growth of the solid electrolyte interphase (SEI). Conversely, Li foil maintains consistent contact with the solid polymer, displaying a thin and stable SEI. Additionally, failure mechanisms between a gel electrolyte in previous work and the dry SPE are compared.

25 ENERGY STORAGE↗

Atomic-scale constituting stable interface for improved LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathodes of lithium-ion batteries

Ascribed to their higher capacity and lower cost compared to conventional LiCoO 2 , the Ni-rich layered LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) is now considered as one promising cathode for lithium-ion batteries (LIBs). However, it still suffers from some evident performance degradation, especially under high cutoff voltages (i.e., >4.3 V versus Li/Li + ). The performance degradation typically is exhibited as capacity fading and voltage drop, mainly originating from an instable interface between the NMC622 and electrolyte as well as the evolution of the NMC structure. To improve the interfacial and structural stability of NMC cathodes, herein we deposited an ultrathin layer of Al 2 O 3 coatings (<5 nm) conformally over NMC622 composite electrodes directly using atomic layer deposition (ALD). It was found that, under different upper cutoff voltages (4.3, 4.5, and 4.7 V), the ALD Al 2 O 3 coatings enable enhanced performance of NMC622 cathodes with better cyclability and higher capacity. Particularly, the beneficial effects of the ALD Al 2 O 3 coatings are more remarkable at higher upper cutoff voltages (4.5 and 4.7 V). Furthermore, the ALD coatings can significantly improve the rate capability of NMC622. To this end, we utilized a suite of characterization tools and performed a series of electrochemical tests to clarify the effects of the ALD Al 2 O 3 coatings. This study revealed that the beneficial effects of the Al 2 O 3 ALD coatings are multiple: (i) serving as an artificial layer of solid electrolyte interphase to mitigate undesirable interfacial reactions; (ii) acting as a physical barrier to inhibit metal dissolution of NMC; and (iii) forming a reinforced networked overcoating to boost the mechanical integrity of NMC cathodes. This study is favorable for designing high-performance NMC cathodes.

25 ENERGY STORAGE↗

In Situ Study of Silicon Electrode Lithiation with X-ray Reflectivity

Surface sensitive X-ray reflectivity (XRR) measurements were performed to investigate the electrochemical lithiation of a native oxide terminated single crystalline silicon (100) electrode in real time during the first galvanostatic discharge cycle. This allows us to gain nanoscale, mechanistic insight into the lithiation of Si and the formation of the solid electrolyte interphase (SEI). We describe an electrochemistry cell specifically designed for in situ XRR studies and have determined the evolution of the electron density profile of the lithiated Si layer (Li x Si) and the SEI layer with subnanometer resolution. We propose a three-stage lithiation mechanism with a reaction limited, layer-by-layer lithiation of the Si at the Li x Si/Si interface.

36 MATERIALS SCIENCE↗

Nonflammable Electrolytes for Lithium Ion Batteries Enabled by Ultraconformal Passivation Interphases

Occasional fire accidents and continuous battery safety concerns require advanced lithium ion batteries (LIBs) with high safety as well as great battery performances. The electrolyte plays a critical role in electrochemical and safety properties. Organic phosphate solvents next to the state-of-the-art organic carbonates could formulate nonflammable electrolytes and intrinsically eliminate fire hazards, but their poor compatibility with the graphite anodes remains an obstacle for practical applications. This work reports a promising approach by formulating localized high concentration electrolytes based on a phosphate solvent, ethylene carbonate and a partially fluorinated ether. This electrolyte readily generates robust solid electrolyte interphase on graphite anode and cathode electrolyte interphase on LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode. As a result, this electrolyte shows good compatibility with high voltage cathode and graphite anode, and enables long-term cycling stability in graphite||NMC811 cells. This work sheds a new light in development of nonflammable electrolytes for high energy-density LIBs.

Non-flammable electrolyte, lithium ion battery, lo↗

Tracking the evolution of processes occurring in silicon anodes in lithium ion batteries by 3D visualization of relaxation times

An unconventional electroanalytical method has been used for tracking processes in silicon anodes in lithium ion batteries: a 3D visualization of relaxation times. Impedance data of the electrodes were collected at different potentials and different cycles during cyclic voltammetry, and were treated by means of the Distribution of Relaxation Times (DRT) method. A 3D visualization of the results allowed to identify the formation of a solid electrolyte interphase on the anode, composed of two layers with different relaxation times. Such findings are not possible by conventional analysis of impedance data by modeling with equivalent circuits, nor by simple DRT alone. Additionally, it was possible to observe that the characteristic relaxation time of the lithiation of the Si anode becomes smaller upon cycling, indicating that the material experiences structural transformations that allow it to lithiate faster. The result is relevant to motivate the use of micron-sized particles in the anode.

25 ENERGY STORAGE↗

Lithium metal stripping mechanisms revealed through electrochemical liquid cell electron microscopy

An understanding of lithium stripping is as important as that of lithium plating to achieve significant advances in using lithium metal anodes for high-energy rechargeable batteries. However, there have been limited studies on lithium stripping compared to lithium plating. Here we report the lithium stripping mechanisms revealed through in-situ electrochemical liquid cell transmission electron microscopy (TEM). We directly observe and compare the stripping behavior of the in-situ grown lithium dendrites and lithium nanograins covered by a lithium fluoride-rich solid-electrolyte interphase (SEI). Furthermore, we find the sporadic lithium stripping behavior and three important modes that can describe the stripping of individual lithium deposits, regardless of their morphology: (i) symmetric stripping, (ii) surface-preferred asymmetric stripping, and (iii) interface-preferred asymmetric stripping. In addition, SEI chemical mapping with high spatial resolution shows a remarkable SEI loss at the end of the lithium metal stripping, which illustrates the importance of SEI protection in the subsequent cycles.

25 ENERGY STORAGE↗

Micelle-Like Bulk Structure of Localized High-Concentration Electrolytes

In the recent article by Efaw et al. published in Nature Materials, a unique micelle-like bulk structure of localized high-concentration electrolytes (LHCEs) is revealed to provide beneficial characteristics with respect to solid electrolyte interphase (SEI) stability on lithium metal anodes. This work adds to the pertinent discussions on design rules of LHCE, providing tangible guidelines for its improvement.

DIRECT ENERGY CONVERSION↗

Understanding the Effect of Cathode Composition on the Interface and Crosstalk in NMC/Si Full Cells

Crosstalk between the cathode and the anode in lithium-ion batteries has a great impact on performance, safety, and cycle lifetime. Still, no report exists for a systematic investigation on crosstalk behavior in silicon (Si)-based cells as a function of transition metal composition in cathodes. We studied the effect of crosstalk on degradation of Si-rich anodes in full cells with different cathodes having the same crystal structure but different transition metal compositions, such as LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NM111), LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811). We found that the transition metal composition in cathodes, especially Mn ion concentration, significantly affects electrolyte decomposition reactions, even from very early cycles. This change causes differences in the solid electrolyte interphase (SEI) chemistry of each aged Si sample. As a result, each of the aged Si samples has a different electrochemistry, in terms of initial Coulombic efficiency and the mechanism of capacity fade.

25 ENERGY STORAGE↗

Stable metal anodes enabled by a labile organic molecule bonded to a reduced graphene oxide aerogel

Significance Rechargeable batteries based on metal anodes are highly desirable due to their high energy density. However, the electrochemical interface is generally not favorable for metal deposition, resulting in dendritic metal growth and an unstable solid–electrolyte interphase (SEI). We altered the interface using a labile organic molecule, benzenesulfonyl fluoride. This molecule was bonded to the surface of a reduced graphene oxide aerogel, which not only guides uniform metal deposition but also enables formation of a stable SEI layer. The lithium metal batteries showed stable cycling and excellent tolerance to low-temperature operation. Stable sodium and zinc anodes were also realized, demonstrating the versatility of this concept.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Integrative Additive Design for Robust SEI Formation in NMC811||Silicon Batteries

Silicon (Si) is considered a promising replacement for graphite anodes in lithium-ion batteries (LIBs) due to its high abundance and exceptional specific capacity, but its widespread commercialization has been hindered by poor electrochemical performance. Among various strategies, the use of functional additives has emerged as one of the most effective and cost-efficient methods to enhance the electrochemical properties of LIBs. In this study, several additives—vinylene carbonate (VC), vinyl ethylene carbonate (VEC), lithium difluorophosphate (LiDFP), lithium difluoro(oxalato)borate (LiDFOB), lithium tetrafluorooxalatophosphate (LiTFOP), and lithium difluorobis(oxalato)phosphate (LiDFBOP)—were systematically investigated in LiNi₀.₈Mn₀.₁Co₀.₁O₂ (NMC811)||Si full cells. Notably, LiDFBOP, a lithium salt containing two oxalate groups, outperformed all other additives, delivering the best capacity retention after 300 cycles. Comprehensive characterizations, including FTIR, SEM, and XPS, revealed that LiDFBOP's superior performance stems from its ability to form a more stable solid electrolyte interphase (SEI) on the Si anode, owing to its favorable molecular structure that integrates the beneficial features of the other additives.

25 ENERGY STORAGE↗

Stable Li Metal Anode by a Hybrid Lithium Polysulfidophosphate/Polymer Crosslinking Film

The practical application of rechargeable lithium (Li) metal batteries has long been hindered by the unstable Li metal anode with problems like Li dendrite growth, low Coulombic efficiency (CE), and short cycle life. Here, we demonstrate a multifunctional sulfur-containing hybrid Li polysulfidophosphate and poly(2-chloroethyl acrylate) cross-linking film that can provide effective protection for Li metal anode. This film can facilitate Li metal anode generating a stable organic/inorganic hybrid solid electrolyte interphase (SEI) layer containing multiple components such as polymer-tethered organo(poly)sulfide, inorganic Li polysulfidophosphate, Li sulfides, and Li salts. Thanks to this hybrid robust SEI layer, dendrite-free Li deposition and stable cycling of Li metal anode can be achieved (e.g. CE >98.7% over 950 cycles). We demonstrated this Li protection technique enables both the protected Li metal anode and Li-metal-free anode cycling with significantly improved CEs and stability in full cells using LiFePO 4 (~2.4 mAh/cm 2 ) cathode.

25 ENERGY STORAGE↗

Electrolyte-phobic Surface for the Next-Generation Nanostructured Battery Electrodes

Nanostructured electrodes are among the most important candidates rationally designed to enable high capacity battery chemistry. Nanostructures can solve issues such as the volume change and mechanical fragmentations. However, the high surface area they usually possess would decrease the Coulombic efficiencies, since the side chemical reactions scale with surface area. Moreover, electrodes comprised of nanomaterials have significant intakes of liquid electrolytes, which reduces the overall energy density and increases the cost of the battery. Here we present a new strategy of limiting effective surface area by introducing an “electrolyte-phobic surface”. In this study, a porous Si anode functions as a model material to demonstrate this concept. Silicon boasts high theoretical capacity, but experiences large volume change during its lithiation and delithiation processes. Porous Si can address this volume change problem with the buffer effect of its inner pores. However, porous silicon shows low initial Coulombic efficiencies and high irreversible lithium loss, owing to its intrinsic high surface area. In this report, a covalently linked perfluorinated surface coating layer on porous Si particles serves as an electrolyte-phobic protection layer, minimizing the accessible surface area for the electrolytes, decreasing the side reactions between the electrolyte and Si surface, and thus significantly enhancing the initial Coulombic efficiencies, up to ~88% compared to ~60% for the pristine porous silicon. Meanwhile, the electrolyte-phobic protection layer of Si particles keeps the silicon surface compatible with the conventional polyvinylidene fluoride (PVDF) binder, which helps to stabilize the Si electrode for long-term battery cycling.

Qian, Chenxi↗

Synergetic Dual‐Additive Electrolyte Enables Highly Stable Performance in Sodium Metal Batteries

Sodium (Na)-metal batteries (SMBs) are considered one of the most promising candidates for the large-scale energy storage market owing to their high theoretical capacity (1,166 mAh g -1 ) and the abundance of Na raw material. However, the limited stability of electrolytes still hindered the application of SMBs. Herein, sulfolane (Sul) and vinylene carbonate (VC) are identified as effective dual additives that can largely stabilize propylene carbonate (PC)-based electrolytes, prevent dendrite growth, and extend the cycle life of SMBs. The cycling stability of the Na/NaNi 0.68 Mn 0.22 Co 0.1 O 2 (NaNMC) cell with this dual-additive electrolyte is remarkably enhanced, with a capacity retention of 94% and a Coulombic efficiency (CE) of 99.9% over 600 cycles at a 5 C (750 mA g -1 ) rate. The superior cycling performance of the cells can be attributed to the homogenous, dense, and thin hybrid solid electrolyte interphase consisting of F- and S-containing species on the surface of both the Na metal anode and the NaNMC cathode by adding dual additives. Such unique interphases can effectively facilitate Na-ion transport kinetics and avoid electrolyte depletion during repeated cycling at a very high rate of 5 C. This electrolyte design is believed to result in further improvements in the performance of SMBs.

25 ENERGY STORAGE↗

Balancing formation time and electrochemical performance of high energy lithium-ion batteries

Most lithium-ion batteries still rely on intercalation-type graphite materials for anodes, and the formation process for them typically takes several days or even more to provide a stable solid electrolyte interphase (SEI). The slow formation step results in lower LIB production rates, requires a large number of battery cyclers, and constitutes the second highest cost during battery manufacturing. In an effort to decrease the high manufacturing cost associated with long formation times, here we studied five different formation protocols in nickel-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)/graphite cells where the total formation time varied from 10 to 86 h. Electrochemical characterization and post mortem analysis show that very long formation time do not necessarily improve long-term performance while very short formation protocols result in lithium plating and poorer electrochemical performance. Finally, we find the optimum formation cycling protocol is intermediate in length to minimize impedance growth, improve capacity retention, and avoid lithium plating.

25 ENERGY STORAGE↗

Novel Low-Temperature Electrolyte Using Isoxazole as the Main Solvent for Lithium-Ion Batteries

A novel electrolyte system with an excellent low temperature performance for lithium-ion batteries (LIBs) has been developed and studied. It was discovered for the first time, in this work, that when isoxazole (IZ) was used as the main solvent, the ionic conductivity of the electrolyte for LIBs is more than doubled in a temperature range between -20 and 20 °C compared to the baseline electrolyte using ethylene carbonate–ethyl methyl carbonate as solvents. To solve the problem of solvent cointercalation into the graphite anode and/or electrolyte decomposition, the lithium difluoro(oxalato)borate (LiDFOB) salt and fluoroethylene carbonate (FEC) additive were used to form a stable solid electrolyte interphase on the surface of the graphite anode. Benefitting from the high ionic conductivity at low temperature, cells using a new electrolyte with 1 M LiDFOB in FEC/IZ (1:10, vol %) solvents demonstrated a very high reversible capacity of 187.5 mAh g -1 at -20 °C, while the baseline electrolyte only delivered a reversible capacity of 23.1 mAh g -1 .

25 ENERGY STORAGE↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

A Systematic Study on the Effects of Solvating Solvents and Additives in Localized High‐Concentration Electrolytes over Electrochemical Performance of Lithium‐Ion Batteries

Abstract Localized high‐concentration electrolytes (LHCEs) based on five different types of solvents were systematically studied and compared in lithium (Li)‐ion batteries (LIBs). The unique solvation structure of LHCEs promotes the participation of Li salt in forming solid electrolyte interphase (SEI) on graphite (Gr) anode, which enables solvents previously considered incompatible with Gr to achieve reversible lithiation/delithiation. However, the long cyclability of LIBs is still subject to the intrinsic properties of the solvent species in LHCEs. Such issue can be readily resolved by introducing a small amount of additive into LHCEs. The synergetic decompositions of Li salt, solvating solvent and additive yield effective SEIs and cathode electrolyte interphases (CEIs) in most of the studied LHCEs. This study reveals that both the structure and the composition of solvation sheaths in LHCEs have significant effect on SEI and CEI, and consequently, the cycle life of energetically dense LIBs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

LiH formation and its impact on Li batteries revealed by cryogenic electron microscopy

Little is known about how evolved hydrogen affects the cycling of Li batteries. Hypotheses include the formation of LiH in the solid-electrolyte interphase (SEI) and dendritic growth of LiH. Here, we discover that LiH formation in Li batteries likely follows a different pathway: Hydrogen evolved during cycling reacts to nucleate and grow LiH within already deposited Li metal, consuming active Li. We provide the evidence that LiH formed in Li batteries electrically isolates active Li from the current collector that degrades battery capacity. We detect the coexistence of Li metal and LiH also on graphite and silicon anodes, showing that LiH forms in most Li battery anode chemistries. Last, we find that LiH has its own SEI layer that is chemically and structurally distinct from the SEI on Li metal. Our results highlight the formation mechanism and chemical origins of LiH, providing critical insight into how to prevent its formation.

25 ENERGY STORAGE↗