Search NASA⌕ Search

SEARCH · Search NASA

Results for “Waste Form”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Characterization and Leaching Tests of the Fluidized Bed Steam Reforming (FBSR) Waste Form for LAW Immobilization

Several supplemental technologies for treating and immobilizing Hanford low activity waste (LAW) have been evaluated. One such immobilization technology is the Fluidized Bed Steam Reforming (FBSR) granular product. The FBSR granular product is composed of insoluble sodium aluminosilicate (NAS) feldspathoid minerals. Production of the FBSR mineral product has been demonstrated both at the industrial and laboratory scale. Pacific Northwest National Laboratory (PNNL) was involved in an extensive characterization campaign. This goal of this campaign was study the durability of the FBSR mineral product and the mineral product encapsulated in a monolith to meet compressive strength requirements. This paper gives an overview of results obtained using the ASTM C 1285 Product Consistency Test (PCT), the EPA Test Method 1311 Toxicity Characteristic Leaching Procedure (TCLP), and the ASTMC 1662 Single-Pass Flow-Through (SPFT) test. Along with these durability tests an overview of the characteristics of the waste form has been collected using Scanning Electron Microscopy (SEM), X-ray Diffraction (XRD), microwave digestions for chemical composition, and surface area from Brunauer, Emmett, and Teller (BET) theory.

FBSR↗

Crystalline versus Glassy Nature of Iron Phosphate Waste Forms Subjected to Different Slow Cooling Curves

This report provides experimental details and associated results on the elemental distributions (compositions), crystalline/amorphous phase distributions, and microstructures for iron phosphate reference materials (DPF5-336) made with different cooling curves and starting from different temperatures (i.e., 1050°C and 1200°C). The primary goal of this work was to evaluate the properties of the DPF5- 336 reference material after it was melted and cooled at different rates to simulate the cooling profile of different types of canisters. Crystal fractions across the SCC#2, SCC#3, and SCC#5 samples were all similar ranging in crystal content of 35.66–41.14 mass% with amorphous fractions being the balance (64.34–58.86 mass%, respectively). This shows that the heat treatment profile did not seems to greatly affect either the total crystal content or the phase distributions. The quenched sample was almost completely amorphous (99.55 mass%) with very small peaks identified as Li 3 Fe 2 (PO 4 ) 3 whereas the SCC-treated materials showed peaks for what appear to be ten separate phases present in various concentrations. Another goal of these experiments was to see how the phase distribution affected chemical durability of these waste forms, but that information is being collected at Argonne National Laboratory and will be published in a separate report

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced waste form and Melter development for treatment of troublesome high-level wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these “troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating.The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (also with high Al 2 O 3 concentrations). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group. An extended duration CCIM melter test was conducted on an AZ-101 waste simulant using the CCIM platform at the Idaho National Laboratory (INL). The melter was continually operated for approximately 80 hours demonstrating that the AZ-101 high waste loading glass composition could be readily processed using the CCIM technology. The resulting glass was close to the targeted composition and exhibited excellent durability in both the as poured state and after being slowly cooled according to the canister centerline cooling (CCC) profile. Glass formulation development was also completed on other Hanford tank wastes that were identified to further challenge waste loading due to the presence of appreciable quantities (>750 g) of plutonium in the waste tanks. In addition to containing appreciable Pu quantities, the C-102 waste tank and the 244-TX waste tank contain high concentrations of aluminum and iron, respectively that will further challenge vitrification processing. Glass formulation testing also demonstrated that high waste loadings could be achieved with these tank compositions using the attributes afforded by the CCIM technology.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Update to Waste Form Performance Constraints and OWL Status and Inventory Content. Draft

This report provides (1) an updated set of inputs (Sections 1 through 4) on various additional waste forms (WF) for the generic Defense Waste Repository (DWR) inventory represented in the generic disposal system analyses (GDSA); (2) summaries of evaluations initiated to refine particular characteristics of particular WF for future use (Section 5); and (3) status updates (Section 6) for the Online Waste Library (OWL) inventory content, data entry checking process, and external OWL BETA testing initiated in fiscal year 2017. As such, this report represents completion of both deliverables M3SF-17SNO10501022 (SFWD-SFWST-2017-000047 — this actual report) and M4SF-17SN010501012 (SFWD-SFWST-2017- 000112 — to be completed by reference to the first milestone report in the PICSNE system).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Chemical durability and corrosion-induced microstructure evolution of compositionally complex titanate pyrochlore waste forms with uranium incorporation

Chemical durability of compositionally-complex rare-earth titanate pyrochlore solid solutions with or without uranium incorporation was investigated by semi-dynamic leaching testing. A Ti-enriched amorphous passivation film formed on the surface due to the surface alteration-reorganization mechanism with preferential release of the weakly oxygen-bonded rare earth elements. Elemental release was found to be strongly correlated with chemical disorder, with a negligible correlation with entropy. The release rate of the uranium gradually decreased with increasing numbers of components, implying a possibility of designing and optimizing waste form performance with enhanced chemical durability by controlling composition complexity and chemical disorder for effective nuclear waste management.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Iodosodalite Waste Forms from Low-Temperature Aqueous Process

ABSTRACT Nuclear energy is one option to meet rising electricity demands, although one concern of this technology is the proper capture and storage of radioisotopes produced during fission processes. One of the more difficult radioisotopes is 129 I due to its volatility and poor solubility in traditional waste forms such as borosilicate glass. Iodosodalite has been previously proposed as a viable candidate to immobilize iodine due to high iodine loading and good chemical durability. Iodosodalite was traditionally synthesized using solid state and hydrothermal techniques, but this paper discusses an aqueous synthesis approach to optimize and maximize the iodosodalite yield. Products were pressed into pellets and fired with glass binders. Chemical durability and iodine retention results are included.

iodosodalite↗

Fiscal Year 2010 Summary Report on the Epsilon-Metal Phase as a Waste Form for 99 Tc

Epsilon metal (ε-metal) is generated in nuclear fuel during irradiation. This metal consists of Pd, Ru, Rh, Mo, and some Te. These accumulate at the UO 2 grain boundaries as small (ca 5 µm) particles. These metals have limited solubility in the acid used to dissolve fuel during reprocessing and in typical borosilicate glass. These must be treated separately to improve overall waste loading in glass. This low solubility and their survival in 2 Gy-old natural reactors led us to investigate them as a waste form for the immobilization of 99 Tc and 107 Pd, two very long-lived isotopes.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Laboratory Testing of Bulk Vitrified Low-Activity Waste Forms to Support the 2005 Integrated Disposal Facility Performance Assessment. Erratum

This report refers to or contains K g values for glasses LAWA44, LAWB45 and LAWC22 affected by calculations errors as identified by Papathanassiu et al. (2011). The corrected K g values are reported in an erratum included in the revised version of the original report. The revised report can be referenced as follows: Pierce E. M. et al. (2004) Waste Form Release Data Package for the 2005 Integrated Disposal Facility Performance Assessment. PNNL-14805 Rev. 0 Erratum. Pacific Northwest National Laboratory, Richland, WA, USA.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Form Release Calculations for the 2005 Integrated Disposal Facility Performance Assessment. Erratum

This report refers to or contains K g values for glasses LAWA44, LAWB45 and LAWC22 affected by calculations errors as identified by Papathanassiu et al. (2011). The corrected K g values are reported in an erratum included in the revised version of the original report. The revised report can be referenced as follows: Pierce E. M. et al. (2004) Waste Form Release Data Package for the 2005 Integrated Disposal Facility Performance Assessment. PNNL-14805 Rev. 0 Erratum. Pacific Northwest National Laboratory, Richland, WA, USA.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Consolidation of Glass-Ceramic Waste forms by Hot Isostatic Pressing: Sample Optimisation - 16581

Zirconolite based glass-ceramics were developed for the disposition of plutonium residues at the UK's Sellafield site. Glass-ceramics act as double barrier systems, separating Pu into a durable ceramic phase and retaining miscellaneous material in the amorphous phase. Here we discuss the optimisation of processing parameters and formulations of these alternative waste-forms. All samples were HIPed at 1250 deg. C, 100 MPa for 4 hrs. By investigating the effects of different pre-HIP heat treatments on sample quality and throughput, and glass phase compositions on the crystalline phase assemblage, an optimised method and wasteform composition were achieved. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Form Release Data Package for the 2005 Integrated Disposal Facility Performance Assessment. Erratum

This report refers to or contains K g values for glasses LAWA44, LAWB45 and LAWC22 affected by calculations errors as identified by Papathanassiu et al. (2011). The corrected K g values are reported in an erratum included in the revised version of the original report. The revised report can be referenced as follows: Pierce E. M. et al. (2004) Waste Form Release Data Package for the 2005 Integrated Disposal Facility Performance Assessment. PNNL-14805 Rev. 0 Erratum. Pacific Northwest National Laboratory, Richland, WA, USA.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Materials for Tc capture to increase Tc retention in glass waste form - A review - 15553

{sup 99}Technetium is a long-lived fission product found in the tank waste at the Hanford site in Washington State. In its hepta-valent species, it is volatile at the temperatures used in Hanford Tank Waste Treatment and Immobilization Plant vitrification melters, and thus is challenging to incorporate into waste glass. In order to decrease volatility and thereby increase retention, technetium can be converted into more thermally stable species. Several mineral phases, such as spinel, are able to incorporate tetravalent technetium in a chemically durable and thermally stable lattice, and these hosts may promote the decreased volatility that is desired. In order to be usefully implemented, there must be a synthetic route to these phases that is compatible with both technetium chemistry and current Hanford Tank Waste Treatment and Immobilization Plant design. Synthetic routes for spinel and other potential host phases are examined. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Cold crucible induction melter test for crystalline ceramic waste form fabrication: A feasibility assessment

The first scaled proof-of-principle cold crucible induction melter (CCIM) test to process a multiphase ceramic waste form from a simulated combined (Cs/Sr, lanthanide and transition metal fission products) commercial used nuclear fuel waste stream was recently conducted in the United States. X-ray diffraction, 2-D X-ray absorption near edge structure (XANES), electron microscopy, inductively coupled plasma-atomic emission spectroscopy (and inductively coupled plasma-mass spectroscopy for Cs), and product consistency tests were used to characterize the fabricated CCIM material. Characterization analyses confirmed that a crystalline ceramic with a desirable phase assemblage was produced from a melt using a CCIM. We identified primary hollandite, pyrochlore/zirconolite, and perovskite phases in addition to minor phases rich in Fe, Al, or Cs. The material produced in the CCIM was chemically homogeneous and displayed a uniform phase assemblage with acceptable aqueous chemical durability.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

OWL and Waste Form Characteristics (Annual Status Update)

This report represents completion of milestone deliverable M2SF-21SN010309012 “Annual Status Update for OWL and Waste Form Characteristics” that provides an annual update on status of fiscal year (FY 2020) activities for the work package SF-20SN01030901 and is due on January 29, 2021. The Online Waste Library (OWL) has been designed to contain information regarding United States (U.S.) Department of Energy (DOE)-managed (as) high-level waste (DHLW), spent nuclear fuel (SNF), and other wastes that are likely candidates for deep geologic disposal, with links to the current supporting documents for the data (when possible; note that no classified or official-use-only (OUO) data are planned to be included in OWL). There may be up to several hundred different DOE-managed wastes that are likely to require deep geologic disposal. This draft report contains versions of the OWL model architecture for vessel information (Appendix A) and an excerpt from the OWL User’s Guide (Appendix B and SNL 2020), which are for the current OWL Version 2.0 on the Sandia External Collaboration Network (ECN).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fabrication of Large Size GCM Waste Forms Containing I 2 or CH 3 I Loaded AgI-MOR

Two large size Glass Composite Material (GCM) waste forms containing AgI-MOR were fabricated. One contained methyl iodide-loaded AgI-MOR that was received from Idaho National Laboratory (INL, Test 5, Beds 1 – 3) and the other contained iodine vapor loaded AgIMOR that was received from Oak Ridge National Laboratory (ORNL, SHB 2/9/15 ). The composition for each GCM was 20 wt% AgI-MOR and 80 wt% Ferro EG2922 low sintering temperature glass along with enough added silver flake to prevent any I2 loss during the firing process. The silver flake amounts were 1.2 wt% for the GCM with the INL AgI-MOR and 3 wt% for the GCM contained the ORNL AgI-MOR. The GCMs, nominally 100 g, were first uniaxially pressed to 6.35 cm (2.5 inch) diameter disks then cold isostatically pressed, before firing in air to 550°C for 1hr. They were cooled slowly (1°C/min) from the firing temperature to avoid any cracking due to temperature gradients. The final GCMs were ~5 cm in diameter (~2 inches) and non-porous with densities of ~4.2 g/cm³. X-ray diffraction indicated that they consisted of the amorphous glass phase with small amounts of mordenite and AgI. Furthermore, the presence of the AgI was confirmed by X-ray fluorescence. Methodology for the scaled up production of GCMs to 6 inch diameter or larger is also presented.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗