At least 325 records · Page 18

Pursuing graphite-based K-ion O 2 batteries: a lesson from Li-ion batteries

The replacement of lithium metal by lithium intercalated graphite was crucial for developing safe lithium-ion batteries. Superoxide-based potassium–oxygen batteries represent an exciting metal–oxygen battery with the highest energy efficiencies. However, using potassium metal is a more serious safety threat than lithium. Herein, we explore the possibility of graphite-intercalation anodes for potassium-ion oxygen batteries (PIOBs) with enhanced safety. This work demonstrates for the first time that establishing an artificial potassium salt-rich solid electrolyte interphase (SEI) enables a reversible graphite-intercalation anode (249.6 mA h g -1 after 600 cycles) in a potassium bis(trifluoromethanesulfonyl)imide (KTFSI)-based localized high-concentration electrolyte. Such an electrolyte is stable with the superoxide cathode. The PIOB delivers energy efficiencies above 90% at a depth of discharge (DOD) of 25% for 80 cycles. A three-electrode measurement shows that its overpotential mainly comes from the anode. The lifespan is limited to the gradual degradation of the artificial SEI caused by oxygen crossover. This work represents a step towards achieving holistic anode–electrolyte–cathode compatibility in a PIOB and its realistic evaluation under a controlled DOD.

25 ENERGY STORAGE↗

All-organic self-separating three-dimensionally nanoarchitected electrochemical energy storage devices

This work realizes a three-dimensionally (3D) nanoarchitected, all organic, "self-separating" lithium-ion electrochemical energy storage (EES) device that is cycled as a solid-state full cell. The device is enabled by a monolithic carbon anode with a co-continuous pore network, derived from the structure direction of resols by an ultra-large molar mass block copolymer (BCP), poly(styrene-block-2-dimethylaminoethyl methacrylate) (SA). Electropolymerization of a single-phase conductive and redox-active material, poly((2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methyl 9,10-dioxo-9,10-dihydroanthracene-2-carboxylate) (PAQEDOT), into the pore space provides the cathode of the cell. The device is electronically contacted to the relevant electrode network enabled by the co-continuous nature of each electrode. Electrochemical processing via cycling against external lithium in an electrolyte generates a solid electrolyte interphase (SEI) as a separator and lithiates the cell electrodes, after which the EES device is cycled in the solid state. While the full cell does not demonstrate high cyclability, the best full cell demonstrates a discharge capacity of 267 milliamp hours per gram (mAh/g). This work marks, to the best of knowledge of the authors, the first example of an all-organic materials derived 3D nanoarchitected EES device, as well as the first design of "self-separating" cell fabrication. Furthermore, generalization of the design to another co-continuous carbon form factor is demonstrated.

FOS: Physical sciences↗

Sodium trithiocarbonate cathode for high-performance sodium–sulfur batteries

The high abundance and low cost of sodium and sulfur make room-temperature sodium-sulfur (RT Na-S) batteries an attractive technology compared to the current lithium-ion batteries for large-scale grid-storage applications. However, the commercialization of RT Na-S batteries is impeded by the slow kinetics of Na-S chemistry, severe sodium polysulfide shuttling, and uncontrollable growth of dendritic Na. Herein, sodium trithiocarbonate (Na 2 CS 3 ) is applied as a cathode material to facilitate concurrent improvement in both electrodes, leading to a high-rate performance with extended cycle life. The conductive characteristic of the carbon-sulfur resonance bond provides fast ion and electron transfer throughout the cathode, resulting in superior electrochemical reactivity. At the cathode, the presence of Na2CS3 forms an oligomer-structured layer to suppress the dissolution and shuttling of active materials. Meanwhile, when small portions of Na 2 CS 3 intermediates migrate to the anode, a stable solid electrolyte interphase (SEI) layer with uniform Na-ion flux is formed, enabling improved Na stripping and plating performance. A series of electrochemical and materials characterization, accompanied by density functional theory calculations demonstrate that Na 2 CS 3 is a promising candidate to realize high-rate performance long cycle life RT Na-S batteries.

25 ENERGY STORAGE↗

Capacity and Coulombic Efficiency Measurements Underestimate the Rate of SEI Growth in Silicon Anodes

Capacity measurements and related quantities are the first layer of information acquired during testing of Li-ion cells. It is generally considered that elevated values of coulombic efficiency and capacity retention are absolute indicators of the existence of a stable solid electrolyte interphase (SEI). Here, we challenge this notion by analyzing how the effect of side reactions on cell capacity depends on the choice of electrodes. More specifically, we demonstrate that the extent of measurable capacity fade due to SEI growth is modulated by the shape of the voltage profile of the cathode and anode at the end of charge and discharge half-cycles. This shape-dependency creates a mismatch between SEI growth and cell capacity loss, which is relatively small for graphite anodes but sizable for silicon-containing electrodes. We illustrate this point by showing that, at the same coulombic efficiency and capacity retention, cells containing silicon-based materials could actually exhibit rates of SEI growth that are as much as ≥ 40% higher than graphite cells. The main implication of this behavior is that, for certain systems, capacity measurements may be an unreliable source of information about the extent of reactions at the SEI, allowing other consequences of these side reactions (such as electrolyte depletion) to proceed unchecked while the cell appears to be stable.

25 ENERGY STORAGE↗

Temperature-Dependent Solubility of Solid Electrolyte Interphase on Silicon Electrodes

The lithium-ion batteries powering mass market electric vehicles must be capable of operating in a wide temperature range. Temperature variation has the possibility to greatly affect the stability of the solid electrolyte interphase (SEI) responsible for mitigating capacity fade due to electrolyte decomposition in the lithium-ion battery. Here, we explore the solubility of the SEI on the silicon (Si) electrode, an alternative anode material to the conventional graphite electrode, at temperatures ranging from -10 to 50 °C. Through use of an electrochemical protocol with a high cathodic cutoff voltage, we measure the evolution of the SEI independently of competing Si mechanical stress. We correlate the electrochemical data with three-dimensional resistivity versus depth profiling as well as atomic force microscopy to show that SEI dissolution occurs at significantly faster rates at higher temperatures.

25 ENERGY STORAGE↗

A new mechanism of stabilizing SEI of Si anode driven by crosstalk behavior and its potential for developing high performance Si-based batteries

Stabilizing solid electrolyte interphase (SEI) is a key factor for determining cell performance of Silicon (Si) anode, such as safety, cycle lifetime, and calendar lifetime. Here, we found a new potential for stabilizing SEI of the Si anode, driven by crosstalk with cathode material. Here we investigated the effect of crosstalk on the chemistry of SEI of the Si anode as a function of three different, representative cathode materials: LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and LiFePO 4 (LFP). Specifically, we observed that crosstalk significantly affected the formation and growth mechanism of SEI layer on the Si anodes. Unexpectedly, dissolved Fe ions from the LFP cathode has a positive impact on the chemistry and electrochemical stability of the SEI layer of Si anode compared to the other cathodes, resulting in better electrochemical performance in terms of initial coulombic efficiency and capacity fade.

25 ENERGY STORAGE↗

Perfluoro Aryl Boronic Esters as Chemical Shuttle Additives in Lithium Ion Batteries

Redox shuttles could provide an added measure of control for lithium ion batteries beyond that which is provided by the battery management system. Redox shuttles, which are electrolyte additives, provide electrochemical overcharge protection. Since they possess a reduction-oxidation potential that is slightly above the maximum cathode potential during normal use, they should cause no degradation in cell performance during normal operation, but should shuttle excess electrons during overcharge conditions, effectively limiting the full cell voltage. The goals of the Chemical Shuttle Additives program were to discover and implement a redox shuttle that is compatible with large format lithium ion cells utilizing LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NMC) cathode material and to understand the mechanism of redox shuttle action. Many redox shuttles, both commercially available and experimental, were tested and much fundamental information regarding the mechanism of redox shuttle action was discovered. In particular, studies surrounding the mechanism of the reduction of the oxidized redox shuttle at the carbon anode surface were particularly revealing. Shuttles that were evaluated in various lithium ion cell chemistries include: • 2-(pentafluorophenyl)-tetrafluoro-1,3,2-benzodioxaborole (BDB) supplied by Argonne National Laboratory (ANL), Lemont, Illinois; • 2,5-di-tert-butyl-1,4-dimethoxybenzene (DDB) supplied by 3M, St. Paul, Minnesota; • Li 2 B 12 F 12 supplied by Air Products, Allentown, Pennsylvania (pure compound) and Showa Denko, Japan (in electrolyte); • 1,4-bis(2-methoxyethoxy)-2,5-di-tert-butyl-benzene (ANL-RS2) supplied by Argonne National Laboratory (ANL), Lemont, Illinois; and • A 4.5V class redox shuttle supplied by Argonne National Laboratory (ANL), Lemont, Illinois Although redox shuttles with an appropriate redox potential and sufficient chemical and electrochemical stability for cells utilizing cathodes with potentials higher and lower than that of NMC, a redox shuttle that is viable for use in large format lithium ion cells with NMC cathodes was not found. The effect of the anode on the capacity loss of lithium ion cells with redox shuttles in cells utilizing lithium, lithium titanate, or graphite cells was studied. Molecular imprinting of the redox shuttle molecule during solid electrolyte interphase (SEI) layer formation likely contributes to the successful reduction of oxidized redox shuttle species at carbon anodes. This helps understand how a carbon anode covered with an SEI layer, that is supposed to be electrically insulating, can reduce the oxidized form of a redox shuttle.

25 ENERGY STORAGE↗

The Science of Battery Degradation

This report documents work that was performed under the Laboratory Directed Research and Development project, Science of Battery Degradation. The focus of this work was on the creation of new experimental and theoretical approaches to understand atomistic mechanisms of degradation in battery electrodes that result in loss of electrical energy storage capacity. Several unique approaches were developed during the course of the project, including the invention of a technique based on ultramicrotoming to cross-section commercial scale battery electrodes, the demonstration of scanning transmission x-ray microscopy (STXM) to probe lithium transport mechanisms within Li-ion battery electrodes, the creation of in-situ liquid cells to observe electrochemical reactions in real-time using both transmission electron microscopy (TEM) and STXM, the creation of an in-situ optical cell utilizing Raman spectroscopy and the application of the cell for analyzing redox flow batteries, the invention of an approach for performing ab initio simulation of electrochemical reactions under potential control and its application for the study of electrolyte degradation, and the development of an electrochemical entropy technique combined with x-ray based structural measurements for understanding origins of battery degradation. These approaches led to a number of scientific discoveries. Using STXM we learned that lithium iron phosphate battery cathodes display unexpected behavior during lithiation wherein lithium transport is controlled by nucleation of a lithiated phase, leading to high heterogeneity in lithium content at each particle and a surprising invariance of local current density with the overall electrode charging current. We discovered using in-situ transmission electron microscopy that there is a size limit to lithiation of silicon anode particles above which particle fracture controls electrode degradation. From electrochemical entropy measurements, we discovered that entropy changes little with degradation but the origin of degradation in cathodes is kinetic in nature, i.e. lower rate cycling recovers lost capacity. Finally, our modeling of electrode-electrolyte interfaces revealed that electrolyte degradation may occur by either a single or double electron transfer process depending on thickness of the solid-electrolyte-interphase layer, and this cross-over can be modeled and predicted.

25 ENERGY STORAGE↗

Molecular-Level Insights into the Reactivity of Siloxane-Based Electrolytes at a Lithium-Metal Anode

A molecular-level understanding of the reactions that occur at the lithium-metal anode/electrolyte interphase is essential to improve the performance of Li–O2 batteries. Experimental and computational techniques are applied to explore the reactivity of tri(ethylene glycol)-substituted trimethylsilane (1NM3), a siloxane-based ether electrolyte, at the lithium-metal anode. In situ/ex situ X-ray diffraction and Fourier-transform infrared spectroscopy studies provide evidence of the formation of lithium hydroxide and lithium carbonates at the anode upon gradual degradation of the metallic lithium anode and the solvent molecules in the presence of oxygen. Density functional calculations performed to obtain a mechanistic understanding of the reductive decomposition of 1NM3 indicate that the decomposition does not require any apparent barrier to produce lithium hydroxide and lithium carbonates when the reduced 1NM3 solvent molecules interact with the oxygen crossing over from the cathode. This study indicates that degradation may be more significant in the case of the 1NM3 solvent, compared to linear ethers such as tetraglyme or dioxalone, because of its relatively high electron affinity. Also, both protection of the lithium metal and prevention of oxygen crossover to the anode are essential for minimizing electrolyte and anode decomposition.

Environmental Molecular Sciences Laboratory↗

Bis(trimethylsilyl) 2-fluoromalonate derivatives as electrolyte additives for high voltage lithium ion batteries

Three trimethylsilyl based malonate esters, bis(trimethylsilyl) 2-methyl-2-fluoromalonate (BTMSMFM), bis(trimethylsilyl) 2-ethyl-2-fluoromalonate (BTMSEFM) and bis(trimethylsilyl) 2-propyl-2-fluoromalonate (BTMSPFM), have been used as additives in 1.0 M LiPF 6 /ethylene carbonate (EC)-dimethyl carbonate (DMC)-diethyl carbonate (DEC) (1-1-1, by v) baseline electrolyte for LiNi 0.80 Co 0.15 Al 0.05 O 2 (NCA) based high voltage lithium ion batteries. The NCA half-cells with 5 wt% BTMSMFM exhibit higher capacity retention than that in the baseline electrolyte at different upper cut off voltages, that is, 4.2, 4.3, 4.4 and 4.5 V vs. Li/Li + . Scanning electron microscope (SEM) show that the additive successfully prevents the formation of thick solid electrolyte interphase (SEI) films on the surface of the NCA electrodes. X-ray diffraction (XRD) further reveals that the crystal structure of NCA is also maintained in the electrolyte with 5 wt% BTMSMFM at high cut off voltages. Finally, besides beneficial to NCA cathode, the BTMSMFM additive also ensures better cycling performance of the graphite based half-cells and NCA/graphite full-cells, and thus is a promising additive for application in rechargeable lithium ion batteries.

25 ENERGY STORAGE↗

Anode‐Free Lithium–Sulfur Cells Enabled by Rationally Tuning Lithium Polysulfide Molecules

Abstract The two major barriers of practical lithium–sulfur batteries are the poor reversibility of lithium‐metal anode and sluggish kinetics of sulfur cathode. Here, we report a simple yet cogent, molecular tailoring approach for lithium polysulfides, enabling a synergistic enhancement of anode reversibility and cathode kinetics. We show that SnI 4 coordinates with lithium polysulfides to form soluble complexes, resulting in a Li 2 SnS 3 ‐rich anode interphase layer. As Li 2 SnS 3 is stable against parasitic reactions and has a lower ionic resistance over cycling, the Li plating/stripping efficiency is greatly improved. In addition, the formation of soluble complexes between SnI 4 and lithium polysulfides play a non‐negligible role in suppressing the clustering behavior of lithium polysulfide molecules, resulting in a significant enhancement in sulfur conversion kinetics under lean electrolyte conditions. The synergistic improvement is validated in anode‐free, lean‐electrolyte pouch cells with a Li 2 S cathode that displays capacity retention of 78 % after 100 cycles.

Ren, Yuxun↗

Cr{sub 2}O{sub 5} as new cathode for rechargeable sodium ion batteries

Chromium oxide, Cr{sub 2}O{sub 5}, was synthesized by pyrolyzing CrO{sub 3} at 350 °C and employed as a new cathode in rechargeable sodium ion batteries. Cr{sub 2}O{sub 5}/Na rechargeable batteries delivered high specific capacities up to 310 mAh/g at a current density of C/16 (or 20 mA/g). High-resolution solid-state {sup 23}Na NMR both qualitatively and quantitatively revealed the reversible intercalation of Na ions into the bulk electrode and participation of Na ions in the formation of the solid-electrolyte interphase largely at low potentials. Amorphization of the electrode structure occurred during the first discharge revealed by both NMR and X-ray diffraction data. CrO{sub 3}-catalyzed electrolyte degradation and loss in electronic conductivity led to gradual capacity fading. The specific capacity stabilized at >120 mAh/g after 50 charge-discharge cycles. Further improvement in electrochemical performance is possible via electrode surface modification, polymer binder incorporation, or designs of new morphologies. - Graphical abstract: Electrochemical profile of a Cr{sub 2}O{sub 5}/Na battery cell and high-resolution solid-state {sup 23}Na MAS NMR spectrum of a Cr{sub 2}O{sub 5} electrode discharged to 2 V. - Highlights: • Cr{sub 2}O{sub 5} was synthesized and used as a new cathode in rechargeable Na ion batteries. • A high capacity of 310 mAh/g and an energy density of 564 Wh/kg were achieved. • High-resolution solid-state {sup 23}Na NMR was employed to follow the reaction mechanisms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Molecular dynamics simulations of the first charge of a Li-ion—Si-anode nanobattery

Rechargeable lithium-ion batteries are the most popular devices for energy storage but still a lot of research needs to be done to improve their cycling and storage capacity. Silicon has been proposed as an anode material because of its large theoretical capacity of ~3600 mAh/g. Therefore, focus is needed on the lithiation process of silicon anodes where it is known that the anode increases its volume more than 300%, producing cracking and other damages. In this study, we performed molecular dynamics atomistic simulations to study the swelling, alloying, and amorphization of a silicon nanocrystal anode in a full nanobattery model during the first charging cycle. A dissolved salt of lithium hexafluorophosphate in ethylene carbonate was chosen as the electrolyte solution and lithium cobalt oxide as cathode. External electric fields are applied to emulate the charging, causing the migration of the Li-ions from the cathode to the anode, by drifting through the electrolyte solution, thus converting pristine Si gradually into Li 14 Si 5 when fully lithiated. When the electric field is applied to the nanobattery, the temperature never exceeds 360 K due to a temperature control imposed resembling a cooling mechanism. The volume of the anode increases with the amorphization of the silicon as the external field is applied by creating a layer of LiSi alloy between the electrolyte and the silicon nanocrystal and then, at the arrival of more Li-ions changing to an alloy, where the drift velocity of Li-ions is greater than the velocity in the initial nanocrystal structure. Charge neutrality is maintained by concerted complementary reduction-oxidation reactions at the anode and cathode, respectively. Also, the nanobattery model developed here can be used to study charge mobility, current density, conductance and resistivity, among several other properties of several candidate materials for rechargeable batteries and constitutes the initial point for further studies on the formation of the solid electrolyte interphase in the anode.

25 ENERGY STORAGE↗

Enabling Ether-Based Electrolytes for Long Cycle Life of Lithium-Ion Batteries at High Charge Voltage

Lithium-ion batteries (LIBs) with high-nickel (Ni) content LiNi x Mn y Co z O 2 ( x + y + z = 1) (NMC with Ni ≥ 0.6) cathodes operated at high charge voltages have been considered as one of the most promising candidates for addressing the challenge of increasing energy density demand. Conventional LiPF 6 –organocarbonate electrolytes exhibit incompatibility with such cell chemistries under certain testing conditions because of the instability of electrode/electrolyte interphases. In response to this challenge, ether-based electrolytes with finely tuned structure and composition of solvation sheaths were developed and evaluated in graphite (Gr)∥NMC811 cell chemistry in 2.5–4.4 V, despite ethers being conventionally considered to be unfavorable electrolyte solvents for LIBs because of their anodic instability above 4.0 V and cointercalation into Gr electrodes. Furthermore, the functional ether-based electrolytes in this work enable both excellent cycle life and high rate capability of Gr∥NMC811 cells. Mechanistic studies reveal that the unique structure and composition of the solvation sheath of the functional ether electrolytes are the main reasons behind their excellent anodic stability and effective protection of the Gr electrode and, consequently, the extraordinary cell performances when operated at high charge cutoff voltages. This work also provides a feasible approach in developing highly stable functional electrolytes for high-energy density LIBs.

25 ENERGY STORAGE↗

Research Progress and Perspectives on Pre‐Sodiation Strategies for Sodium‐Ion Batteries

Sodium‐ion batteries (SIBs) with abundant elements have garnered significant attention from researches as a promise compensation to lithium‐ion batteries (LIBs). However, the large‐scale commercial application of SIBs is partially hindered by the limited initial coulombic efficiency (ICE) due to the irreversible formation of solid electrolyte interphase (SEI) and intercalation into the defects in the anode. Similar to pre‐lithiation techniques, pre‐sodiation approaches are considered to be one of the most direct and effective way to compensate for the loss of active sodium at the anode side of SIBs during the initial cycle. In this context, additional sodium ions are pre‐injected to the cathode/anode material by chemical/electrochemical methods, aiming to improve battery span life and energy density. Here, this review delves into the necessity and impact of pre‐sodiation techniques, compiling the latest research progress, for instance, self‐sacrificing cathode additives, over‐sodiated cathode materials, direct contact and solution chemical pre‐sodiation. Notably, the research mechanisms underlying solution chemical pre‐sodiation are highlighted. This comprehensive overview aims to foster a deeper understanding of the pre‐sodiation techniques and expects to provide guidance for realizing the commercial application of high energy density sodium‐ion batteries.

25 ENERGY STORAGE↗

Hybrid Lithium-Sulfur Batteries with an Advanced Gel Cathode and Stabilized Lithium-Metal Anode

The insulating nature of sulfur, polysulfide shuttle effect, and lithium metal deterioration cause a decrease in practical energy density and fast capacity fade in lithium-sulfur batteries. Here, we present an integrated strategy for the development of hybrid Li-S batteries based on a gel sulfur cathode, a solid electrolyte, and a protective anolyte composed of highly-concentrated salt electrolyte containing mixed additives. The dense solid electrolyte completely blocks polysulfide diffusion, and also makes it possible to investigate the cathode and anode independently. This gel cathode effectively traps the polysulfide active material while maintaining a low electrolyte to sulfur ratio (E/S) of 5.2 mL/g. The anolyte effectively protects the Li metal and suppresses the consumption of liquid electrolyte, enabling stable long-term cycling for over 700 hours in Li symmetric cells. This advanced design can simultaneously suppress the polysulfide shuttle, protect Li metal, and reduce the liquid electrolyte usage. The assembled hybrid batteries exhibit remarkably stable cycling performance over 300 cycles with high capacity. Finally, surface-sensitive techniques were carried out to directly visualize and to probe the interphase formed on the surface of the LAGP pellet, which may help stabilize the solid-liquid interface.

25 ENERGY STORAGE↗

Non‐Linear Kinetics of The Lithium Metal Anode on Li 6 PS 5 Cl at High Current Density: Dendrite Growth and the Role of Lithium Microstructure on Creep

Abstract Interfacial instability, viz., pore formation in the lithium metal anode (LMA) during discharge leading to high impedance, current focusing induced solid–electrolyte (SE) fracture during charging, and formation/behaviour of the solid–electrolyte interphase (SEI), at the anode, is one of the major hurdles in the development of solid‐state batteries (SSBs). Also, understanding cell polarization behaviour at high current density is critical to achieving the goal of fast‐charging battery and electric vehicle. Herein, via in situ electrochemical scanning electron microscopy (SEM) measurements, performed with freshly deposited lithium microelectrodes on transgranularly fractured fresh Li6PS5Cl (LPSCl), the LiǀLPSCl interface kinetics are investigated beyond the linear regime. Even at relatively small overvoltages of a few mV, the LiǀLPSCl interface shows non‐linear kinetics. The interface kinetics possibly involve multiple rate‐limiting processes, i.e., ion transport across the SEI and SE|SEI interfaces, as well as charge transfer across the LiǀSEI interface. The total polarization resistance R P of the microelectrode interface is determined to be ≈ 0.8 Ω cm 2 . It is further shown that the nanocrystalline lithium microstructure can lead to a stable LiǀSE interface via Coble creep along with uniform stripping. Also, spatially resolved lithium deposition, i.e., at grain surface flaws, grain boundaries, and flaw‐free surfaces, indicates exceptionally high mechanical endurance of flaw‐free surfaces toward cathodic load (>150 mA cm −2 ). This highlights the prominent role of surface defects in dendrite growth.