Search NASA⌕ Search

SEARCH · Search NASA

Results for “degradation testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Spatiotemporal Modeling of Real World Backsheets Field Survey Data: Hierarchical (Multilevel) Generalized Additive Models

Assessing photovoltaic module backsheet durability is critical to increasing module lifetime. Laboratory-based accelerating testing has recently failed to predict large scale failures of widely adopted polymeric materials. Additionally, there is a growing concern on characterizing the non-uniformity of field exposure. Therefore, data from field surveys are critical to assess the performance of component lifetimes. Using a documented field survey protocol, 19 field surveys were conducted. The focus of this survey strategy is to investigate spatial continuity in degradation modes. By combining field survey data with real-time satellite weather data, stressor / response models have been trained. Generalized additive Models (GAM) model was created to predict the value of degradation based on measured predictors. Two different GAM constructions were testing using different implementations of basis splines. The model includes variables on the environmental stressors of the system and the location of each measurement in the PV mounting structure. The incorporation of hierarchical structure into the models allowed for material specific degradation rates, while maintaining the assumption of a global trend. The model performed well with an adjusted R2 of 0.975 for yellowness index prediction.

backsheet↗

Updated sustainability status of cadmium telluride thin‐film photovoltaic systems and projections

This paper provides a comprehensive assessment of the up-to-date life-cycle sustainability status of cadmium-telluride based photovoltaic (PV) systems. Current production modules (Series 6 and Series 7) are analyzed in terms of their energy performance and environmental footprint and compared with the older series 4 module production and current single-crystalline Silicon (sc-Si) module production. For fixed-tilt systems with Series 6 modules operating under average US irradiation of 1800 kWh/m 2 /year, the global warming potential (GWP) is reduced from 16 g CO 2eq /kWh in Series 4 systems to 10 CO 2 eq /kWh in Series 6 systems. For operation in US-SW irradiation of 2300 kWh/m 2 /year, the GWP is reduced from 11 to 8 CO 2eq /kWh and for 1-axis tracking systems operating in Phoenix, Arizona, with point-of array irradiation of 3051 kWh/m 2 /year the GWP is reduced to 6.5 CO 2eq /kWh. Similar reductions have happened in all environmental indicators. Energy payback times (EPBT) of currently installed systems range from 0.6 years for fixed–tilt ground–mounted installations at average US irradiation at latitude tilt installations to 0.3 years for one-axis trackers at high US-SW irradiation, considering average fossil-fuel dominated electricity grids with fuel to electricity conversion efficiency of 0.3. The resulting energy return on energy investment (EROI) also depends on the conversion efficiency of the electricity grid and on the operation life expectance. For a 30-year operational life and grid conversion efficiency of 0.3, EROI ranges from 50 (at US average irradiation) to 70 for US-SW irradiation. The EROI declines with increased grid conversion efficiency; for CdTe PV operating in south California with grid conversion efficiency of 49%, the EROI is about 50 and is projected to fall to 30 when the state's 2030 target of 80% renewable energy penetration materializes. Material alternatives that show a potential of further reductions in degradation rates and materials for enhanced encapsulation that would enable longer operation lives have also been investigated. A degradation rate of 0.3%/year, which has been verified by accelerated testing, is assumed in 30-year scenarios; this is projected to be reduced to 0.2%/year in the near-term and potentially to 0.1%/year in the longer term. With such low degradation rates and enhanced edge-sealing, modules can last 40- to 50-years. Consequently, all impact indicators will be proportionally reduced while EROI will increase. This detailed LCA was conducted according to ISO standards and IEA PVPS Task 12 guidelines. Furthermore, the study revealed that the choices of system models, methods and temporal system boundaries can significantly impact the results and points out to the need to include assumptions regarding these choices in the “transparency in reporting” requirements listed in the IEA PVPS Task 12 Guidelines.

14 SOLAR ENERGY↗

Degradation Mechanisms in Advanced MEAs for PEM Water Electrolyzers Fabricated by Reactive Spray Deposition Technology

Proton exchange membrane water electrolyzers (PEMWEs) have demonstrated enormous potential as the next generation hydrogen production technology. The main challenges that the state-of-the-art PEMWEs are currently facing are excessive cost and poor durability. Understanding the failure modes in PEMWEs is a key factor for improving their durability, lowering the precious metal loading, and hence cost reduction. Here, reactive spray deposition technology (RSDT) has been used to fabricate a membrane electrode assembly (MEA) with one order of magnitude lower Pt and Ir catalyst loadings (0.2–0.3 mg PGM cm –2 ) in comparison to the precious metal loadings in the stat-of-the-art commercial MEAs (2–3 mg PGM cm –2 ). As fabricated MEA with an active area of 86 cm 2 , has been tested for over 5000 h at steady-state conditions that are typical for an industrial hydrogen production system. Herein, we present and discuss the results from a comprehensive post-test analysis of the MEA of interest. The main degradation mechanisms, governing the performance loss in the RSDT fabricated MEA with ultra-low precious metal loadings, have been identified and discussed in detail. All failure modes are critically compared and the main degradation mechanism with the highest impact on the MEA performance loss among the others is identified.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Review of Tank 48H Treatment of Tetraphenylborate with Permanganate

Tank 48H contains roughly 270,000 gallons of radioactive waste material. The waste stored in this tank was to be processed in multiple stages utilizing facilities at the Savannah River Site (SRS) almost 30 years ago. The In-Tank Precipitation Process (ITP) was initiated in Tank 48H, which precipitated highly radioactive cesium-137 using sodium tetraphenylborate (NaTPB). While the process succeeded in precipitating the Cs, Sr, and other actinides, it also generated an unexpectedly large amount of benzene. The evolved benzene created a safety concern and made the waste incompatible with further downstream processing. This halted the ITP, and a new method of treatment was required to continue processing the legacy waste contained in Tank 48H. A myriad of treatment options have been proposed with multiple teams of researchers assembled to work on this highly complex issue over the last few decades. This review investigated one potentially viable treatment option, in-tank oxidation with sodium permanganate. Permanganate has been well known in literature as a strong oxidizing agent for organic compounds, as well as being utilized at the Savannah River Site (SRS) in other processes. A small number of studies have been conducted utilizing waste simulants to evaluate the use of permanganate as an oxidant for tetraphenylborate (TPB). A search of the literature and data from these studies indicates that permanganate could be a viable treatment for destruction of TPB in Tank 48H. While the scoping studies had a small number of individual experiments and nonideal conditions, the permanganate decomposed up to 90% of the TPB. A free hydroxide concentration above 1.0 M is required for tank corrosion control. Simulant studies indicate no decrease in TPB decomposition by permanganate until pH 14. The simulant studies show an increase in TPB decomposition as the temperature of the solution is increased to 40 °C. The post-reaction analysis of previous simulant tests did not look at all of the organic degradation products. Investigations into what these organic products are and in what quantity will help guide determinations as to whether the downstream processing facilities are able to handle the material that will be generated. Study on the time frame for the reaction between permanganate and TPB should be investigated as the literature reports only extend out to two weeks reaction time. The permanganate treatment conditions indicate no corrosion control concerns and a longer timescale reaction may be needed for in-tank treatment. In addition, further study would be useful to identify a lower boundary condition for the ratio of TPB and oxidant. The simulant tests applied large excesses of permanganate, and this may be unnecessary. The size constraint of the tank means that there will be practical limitations on the amount of sodium permanganate that can be added to the tank. The amount of permanganate should be minimized as much as possible while still ensuring decomposition of the TPB to minimize the amount of manganese dioxide solids generated.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Molybdenum Oxide Interface Limits the High-Temperature Operational Stability of Unencapsulated Perovskite Solar Cells

Here, we report on the improved operational stability of unencapsulated perovskite solar cells (PSCs) aged in an ambient atmosphere at elevated temperatures (70 °C) for >1000 h under constant illumination and bias at 30–50% relative humidity. We identify a previously unseen interfacial degradation mechanism concerning the use of a MoO x interlayer, which was originally added to increase operational stability. Specifically, the hole-transport layer/MoO x interface buckles under illumination at 70 °C, which leads to delamination and rapid losses of short-circuit current density corresponding to an average $t_{80}$ of ~55 h. By judiciously evaluating various hole-transport layers, interlayers, and contacts, we find that replacing the MoO x with a VO x interlayer, regardless of the other components in the solar cell, alleviates this buckling issue due to its higher activation barrier toward crystallization, leading to significant gains in PSC operational stability. Unencapsulated devices aged in an ambient atmosphere with a VO x interlayer retain 71% of their initial PCE on average after constant illumination and bias at 70 °C for 1100 h ($t_{80}$ ~ 645 h). Currently, this is the highest temperature reported for the operational stability of unencapsulated n-i-p PSCs aged in air. Identification of a new facet of the complex degradation mechanisms in PSCs will allow for targeted acceleration testing to speed the deployment of low-cost, long-lasting electricity generation under realistic operating temperatures.

14 SOLAR ENERGY↗

NLR CSP Optical Facilities: Illuminating the Path Forward Through Innovation and Impact: Agreement 38490

This initiative is a multi-faceted project at the National Laboratory of the Rockies (NLR) aimed at strengthening its Concentrating Solar Power (CSP) Optical Facilities to advance the development of low-cost, high-performance materials for solar and other applications. The project's strategy is built on three pillars: strategic stakeholder engagement, diligent facility maintenance and utilization, and the development of new research capabilities. The overarching goal is to ensure the facilities remain state-of-the-art resources for industry and academia, thereby accelerating the conversion of concentrated sunlight into energy. A key driver of the project is an international Advisory Board, which provides critical guidance on research priorities and industry needs, leading to new collaborations and secured funding. This external engagement, combined with proactive outreach to industry partners, ensures the lab's work remains aligned with real-world challenges, including materials durability and performance certification. Significant efforts in facility maintenance have addressed challenges with aging infrastructure. Notable achievements include the complete refurbishment of the hail-damaged Ultra-Accelerated Weathering System (UAWS) and the successful replacement of a failing 15-year-old Lambda 1050 spectrophotometer with a new-generation model, substantially upgrading material characterization capabilities. These maintenance activities were complemented by achieving a prestigious ISO 9001:2015 certification for the Advanced Optical Materials Labs, formally recognizing the quality and reliability of NLR's measurement capabilities. Despite these successes, challenges remain, including high demand for the High Flux Solar Furnace (HFSF) and intermittent failures of other key instruments. The project has delivered major advancements in research techniques and capabilities. At the Flatirons campus, a new indoor laboratory, was established to house advanced deflectometry and photogrammetry systems for heliostat characterization. For on-sun testing, a novel, actively cooled turning mirror was developed for the HFSF, enabling more realistic testing of particle receivers and components. A collaboration with Virginia Tech successfully demonstrated the high-temperature durability of a new solar absorber coating through extensive cyclic testing. Concurrently, new modeling took place to better predict material degradation on rough, fractal surfaces. In summary, this project has systematically enhanced NLR's CSP Optical Facilities through strategic upgrades, rigorous maintenance, and stakeholder-guided research. By overcoming equipment failures, budgetary constraints, and logistical hurdles, the project has reinforced NLR's role as a central hub for CSP innovation and materials testing. Future work will focus on securing diverse funding, expanding collaborations, and continuing to provide the critical infrastructure needed to accelerate the development and deployment of next-generation technologies.

14 SOLAR ENERGY↗

The Impact of Operational Strategies and Load Fluctuations on Anion Exchange Membrane Water Electrolyzer Degradation

This study reports on the durability of anion exchange membrane water electrolyzers (AEMWEs) at the cell level in a supporting electrolyte (1 M) and the impact of operational profiles on cell degradation. While constant load shows significant voltage loss, including a current hold at 1 A cm −2 and a potential hold at 2 V, it generally occurs in the first 70 h of testing. These losses are likely due to passivation altering site reactivity and cell kinetics, and are largely recoverable upon load cycling and diagnostics at the end of test. Furthermore, square and triangular-wave cycling do not show cell degradation and indicate that AEMWEs are not vulnerable to load cycling. When operating outside of this potential window (1.45–2 V), cell voltage decay rates markedly increase and the losses are not recoverable. This includes a current density hold at 4.0 A cm −2 with high cell voltages (>2.4 V for test duration) and cycling between 0 and 2 V to simulate start–stop, where more than a 50% loss in current density occurs over 50 h. The findings presented here demonstrate the high durability of AEMWEs, particularly when operating with load fluctuations, and may allow for durability advantages compared to iridium and proton exchange membrane systems.

08 HYDROGEN↗

Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li + ) and operating temperature (25 °C and 60 °C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiO x formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiO x formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiO x phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiO x phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiO x phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.

electrochemical impedance spectroscopy↗

Evaluation of Nanostructured β-Mn 2 V 2 O 7 Thin Films as Photoanodes for Photoelectrochemical Water Oxidation

β-Mn 2 V 2 O 7 (β-MVO) was recently reported to be a promising candidate for photoelectrochemical (PEC) water splitting, with a suitable band gap and band edge positions and reasonable stability and photoactivity in preliminary tests in alkaline solution. Here, we present an in-depth evaluation of the PEC performance and stability of phase-pure nanostructured β-Mn 2 V 2 O 7 films made by calcination of a spin-cast molecular ink. We show that β-Mn 2 V 2 O 7 dissolves in pure water, corrodes in aqueous electrolytes at pH 7 and 9, and converts to amorphous manganese (hydr)oxides within minutes at pH 13. Our β-Mn 2 V 2 O 7 films yielded only miniscule photocurrents (~uA cm -2 ) for the oxidation of iodide, sulfite, or water and the reduction of iodate or water in borate- and phosphate-buffered electrolytes at pH 7 and 9, the oxidation of [Fe(CN) 6 ] 4- or water at pH 13, and the oxidation of bromide in acetonitrile, regardless of film calcination temperature and time, film thickness, and illumination geometry. Minimal photoactivity was observed even in electrolytes in which film degradation was insignificant over the duration of the PEC tests. Ultrafast transient absorption spectroscopy shows that the poor photoactivity is likely the result of fast hole trapping and recombination at the MVO surface that leaves few free charge carriers beyond the picosecond time scale. Given its poor charge transport/extraction and chemical stability, native nanostructured β-Mn 2 V 2 O 7 is ineffective for solar water splitting and future research on this material should focus on the development of superior syntheses and film morphologies, MVO alloys, heterostructures, and surface coatings to alleviate recombination and boost operational stability. This work underscores the importance of careful follow-up studies of materials identified as "hits" in combinatorial materials discovery campaigns.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Computational Study of the Shear Behavior of Reinforced Concrete Beams Affected from Alkali–Silica Reactivity Damage

In this study, an investigation of the shear behavior of full-scale reinforced concrete (RC) beams affected from alkali–silica reactivity damage is presented. A detailed finite element model (FEM) was developed and validated with data obtained from the experiments using several metrics, including a force–deformation curve, rebar strains, and crack maps and width. The validated FEM was used in a parametric study to investigate the potential impact of alkali–silica reactivity (ASR) degradation on the shear capacity of the beam. Degradations of concrete mechanical properties were correlated with ASR expansion using material test data and implemented in the FEM for different expansions. The finite element (FE) analysis provided a better understanding of the failure mechanism of ASR-affected RC beam and degradation in the capacity as a function of the ASR expansion. The parametric study using the FEM showed 6%, 19%, and 25% reduction in the shear capacity of the beam, respectively, affected from 0.2%, 0.4%, and 0.6% of ASR-induced expansion.

36 MATERIALS SCIENCE↗

Recent developments in catalyst-related PEM fuel cell durability

Cost and durability remain the two major barriers to the widespread commercialization of polymer electrolyte membrane fuel cell (PEMFC)-based power systems, especially for the most impactful but challenging fuel cell electric vehicle (FCEV) application. Commercial FCEVs are now on the road; however, their PEMFC systems do not meet the cost targets established by the U.S. Department of Energy, primarily due to the high platinum loading needed on the cathode to achieve the requisite performance and lifetime. Furthermore, while the activities of a number of commercial Pt-based alloy cathode catalysts exceed the beginning-of-life (BOL) targets, these activities, and the overall cathode performance, degrade via a variety of mechanisms described herein. Degradation is mitigated in current FCEVs by utilizing a cathode catalyst with a lower BOL activity (e.g., much lower transition metal alloy content and larger BOL nanoparticle size), necessitating higher catalyst loadings, and through the utilization of system controls that avoid conditions known to exacerbate degradation processes, such as limiting the fuel cell stack voltage range. The design and development of active and robust materials and eliminating the need for vehicle mitigation strategies would greatly simplify the operating system, allowing for greater transient operation, avoiding large hybridization, and curtailing of fuel cell power. Although system mitigation strategies have provided the near-term pathway for FCEV commercialization, material-specific solutions are required to further reduce costs and improve operability and efficiency. Future material developments should focus on stabilization of the electrode structure and minimization of the catalyst particle susceptibility to dissolution caused by oxide formation and reduction over PEMFC cathode-relevant operating potentials plus minimization of support corrosion. Ex situ accelerated stress tests have provided insight into the processes responsible for material and performance degradation and will continue to provide useful information on the relative stability of materials and benchmarks for robust and stable materials-based solutions not requiring system mitigation strategies to achieve adequate lifetime.

25 ENERGY STORAGE↗

Understanding (La,Sr)(Co,Fe)O$_{3-δ}$ Phase Instability within SOECs Using a Combined Experimental and Atomistic Modeling Approach

Understanding the onset of degradation in the air electrode within solid oxide electrolysis cells (SOECs), and the subsequent impact on cell performance, is a critical step in mitigating the performance losses and stability issues of SOECs. In an effort to identify early onset degradation phenomena, SOECs were characterized as fabricated and after testing potentiostatically at 1.3 V for 1000 h at 750 °C. SOEC air electrodes composed of a 1:1 composite of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3–δ (6428-LSCF) and Gd 0.1 Ce 0.9 O 1.95 (GDC) were studied using synchrotron X-ray diffraction (XRD), scanning transmission electron microscopy coupled with energy dispersive X-ray spectroscopy (STEM-EDS), and X-ray absorption near-edge spectroscopy (XANES) to evaluate the changes in the air electrode structurally and chemically. These techniques show the migration of Sr species from the air electrode through pores in the GDC barrier layer, progressing to the electrolyte boundary, where it accumulates and reacts with (Zr 0.84 Y 0.16 )O 2–δ (YSZ) to form SrZrO 3 . Microscopy results are paired with atomistic simulations to better understand the relationship between the thermodynamic instability of 6428-LSCF and cell fabrication/testing conditions. First-principles calculations reveal that LSCF-6428 is not stable during cell manufacturing and testing conditions, which supports the experimental identification of secondary phases in both as-fabricated and tested cells. Together, these results demonstrate that the challenging environments encountered by SOECs during cell manufacturing and operation lead to instabilities of the target 6428-LSCF anode material and underscore the need for more durable, high-performing SOEC components.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fabrication of α-Fe 2 O 3 Nanoparticles/g-C 3 N 4 Direct Z-Scheme Heterojunction of Durable Photocatalytic Activity

The fabrication of a nanohybrid photocatalyst that combines α-Fe 2 O 3 nanoparticles with graphitic carbon nitride (g-C 3 N 4 ) is reported. The ensuing direct Z-scheme heterojunction greatly boosts the photocatalytic activity of the α-Fe 2 O 3 /g-C 3 N 4 nanohybrids. This results in organic dye degradation rates more than two times higher than its individual components, promoted by the efficient charge separation and transfer of the Z-scheme heterojunction mechanism of the nanohybrid photocatalyst. In addition, recyclability tests show an outstanding stability of the nanohybrids spanning five consecutive dye degradation experiments, during which the degradation rate is slightly improved. The origin of the improved photocatalytic performance of the nanohybrid lies in the intimate interaction between α-Fe 2 O 3 and g-C 3 N 4 afforded by the two-step fabrication process, which enables the direct and controlled growth of α-Fe 2 O 3 nanoparticles on g-C 3 N 4 . A first ultrasound impregnation step promotes the effective anchoring of stable Fe species via Fe–N and C–N/C–O bonding, while a second microwave phase conversion step induces the subsequent growth of α-Fe 2 O 3 nanoparticles on the g-C 3 N 4 sheets. Careful control of the FeCl 3 precursor concentration up to a threshold value of 0.25 M during impregnation enables complete control over their size and phase. This approach clearly highlights the benefits of microwave reactor systems in the fabrication of hematite-based Z-scheme photocatalytic, overcoming the limitations of conventional thermal treatment technology.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Susceptibility to polarization type potential induced degradation in commercial bifacial p-PERC PV modules

Potential induced degradation (PID) is a reliability issue affecting photovoltaic (PV) modules, mainly when PV strings operate under high voltages in hot/humid conditions. Polarization-type PID (PID-p) has been known to decrease module performance quickly. PID-p can be reduced or recovered under the light in some cases, but this effect, as expected, would be less pronounced on the rear side of bifacial PV modules receiving lower irradiance. As bifacial PV modules are projected to dominate the PV market within the next 10 years, it is crucial to understand the PID-p issue in bifacial modules better. In this study, we performed indoor PID testing to induce PID-p on 14 commercial bifacial p-PERC modules with three different module constructions from three manufacturers. Here, four rounds (+ve and –ve polarities for front and rear sides) of PID testing are done at 25°C, 54% relative humidity (RH) for 168 h using the aluminum foil method. Each module side (front cell side and back cell side) is tested individually under both negative and positive voltage bias. The results show that the highest degradation of 32% in maximum power (Pmax) at standard test conditions (1000 W/m 2 ) and 51% at low irradiance (200 W/m 2 ) has been observed in some cases. Recovery under sunlight is also done, and outcomes show a near-complete recovery in Pmax. This study presents an extensive experimental methodology and a detailed analysis to systematically and simultaneously/sequentially evaluate multiple construction types of bifacial modules to the PID-p susceptibility and recovery.

14 SOLAR ENERGY↗

Lessons from the IEC Durability of Adhesion Accelerated Test Sequence

The IEC 62788-1-1 and IEC 63209-2 standards use aging sequences for durability of adhesion in photovoltaic (PV) modules, which may be evaluated using the single cantilever beam (SCB) test. Because the encapsulant forms critical interfaces with the front glass and solar cells, degradation at those interfaces under ultraviolet (UV) exposure, elevated temperature, and humidity can lead to interfacial delamination - compromising the long-term reliability. In this work, adhesion durability of UV-transmitting poly(ethylene-co-vinyl acetate) (EVA) encapsulant to glass and to silicon solar cells is evaluated after sequenced UV and damp heat aging (85C/85%RH). Laminates were prepared using StarPhire solar front glass with thin glass or PERC cells, and two EVA formulations with different concentrations of siloxane coupling agent. Adhesion was quantified by measuring critical debond energy using the SCB method. Both formulations exhibit similar qualitative trends, while different adhesion is observed at the periphery despite the use of low-shrink manufacturing. The results show that while glass/EVA adhesion remains stable or increases after UV exposure and shows only moderate changes after damp heat, the EVA/cell interface exhibits an irreversible loss of adhesion following UV and then damp heat exposure. Although glass/EVA interfaces generally exhibit lower debond energies, the EVA/cell interface is significantly more vulnerable to UV-driven degradation, identifying it as the dominant reliability risk location through early- and intermediate-module life. These results demonstrate that accelerated aging sequences can expose large, interface-specific losses in adhesion durability and underscore the importance of interface engineering for long-term PV module reliability.

14 SOLAR ENERGY↗

In Situ Reliability Investigation of All-Vanadium Redox Flow Batteries by a Stable Reference Electrode

Redox flow batteries (RFBs) have been studied over the past several decades as a promising candidate for stationary energy storage applications. It is therefore important to understand the reliability of RFBs and the mechanisms that cause degradation with time. Contributions from individual electrodes (cathode or anode) are difficult to separate especially for long-term cycle testing, due to the lack of a stable reference electrode. In our work, the reliability and degradation mechanisms of an all-vanadium RFB were investigated by a stable reference electrode based on the dynamic hydrogen electrode (DHE). With factor exploration and design optimization, the newly developed DHE reference electrode demonstrated high accuracy and long-term stability that enables in-situ monitoring of individual electrode signals (potentials and impedances) over hundreds of cycles in a vanadium RFB. This approach enables the full cell degradation to be separated and the degradation attributed to contributions from the cathode and anode. The cathode and anode were found to play quite different roles in the increase in overpotential of the vanadium RFB during long-term cycling. The anode reaction limited both the charge and discharge capacity over 100 cycles. In addition, the negative side also appeared to be the rate limiting factor throughout cycling as determined by EIS measurement. The cathode contributed to the performance degradation as cycling exceeded 50 cycles.

Huang, Qian↗

Spatio-Temporal Modeling of Field Surveyed Backsheet Degradation

Assessing photovoltaic module backsheet durability is critical to increasing module lifetime. Lab based accelerating testing has recently failed to predict large scale failures of widely adopted polymeric materials. Field surveyed data is critical to assess the performance of component lifetime. Using a documented field survey protocol, 13 field surveys where conducted. Each measurement is encoded with it's spatial location in respect to the other modules. By combining field survey data on degradation predictors with real time satellite weather data, data-driven predictive models of backsheet degradation were trained. LOESS models were constructed to investigate the spatial dependence of measurements. It was found that micro-climatic effects like tree-lines, ground surface changes, and elevation changes effected the magnitude and variance of the measurements. A GAM model was created to predict the value of degradation based on measured predictors. The model includes variables on the climate of the system and the location of each measurement in the PV mounting structure. The model performed well with an adj.R 2 of 0.95 for yellowness index prediction. The model was cross-validated using k-folds.

backsheet↗

Glass/Glass Photovoltaic Module Reliability and Degradation: A Review - Figures

Glass/glass (G/G) photovoltaic (PV) module construction is quickly rising in popularity due to increased demand for bifacial PV modules, with additional applications for thin-film and building-integrated PV technologies. G/G modules are expected to withstand harsh environmental conditions and extend the installed module lifespan to greater than 30 years compared to conventional glass/backsheet (G/B) modules. With the rapid growth of G/G deployment, understanding the outdoor performance, degradation, and reliability of this PV module construction becomes highly valuable. In this review, we present the history of G/G modules that have existed in the field for the past 20 years, their subsequent reliability issues under different climates, and methods for accelerated testing and characterization of both cells and packaging materials. We highlight some general trends of G/G modules, such as greater degradation when using poly(ethylene-co-vinyl acetate) (EVA) encapsulants, causing the industry to move toward polyolefin-based encapsulants. Transparent backsheets have also been introduced as an alternative to the rear glass for decreasing the module weight and aiding the effusion of trapped gaseous degradation products in the laminate. New amendments to IEC 61215 standard protocols for G/G bifacial modules have also been proposed so that the rear side power generation and UV exposure will be standardized. We further summarize a suite of destructive and non-destructive characterization techniques, such as current-voltage scans, module electro-optical imaging, adhesion tests, nanoscale structural/chemical investigation, and forensic analysis, to provide deeper insights into the fundamental properties of the module materials degradation and how it can be monitored in the G/G construction. This will set the groundwork for future research and product development.

transparent backsheet↗