Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Progressive growth of the solid–electrolyte interphase towards the Si anode interior causes capacity fading

The solid–electrolyte interphase (SEI), a layer formed on the electrode surface, is essential for electrochemical reactions in batteries and critically governs the battery stability. Active materials, especially those with extremely high energy density, such as silicon (Si), often inevitably undergo a large volume swing upon ion insertion and extraction, raising a critical question as to how the SEI interactively responds to and evolves with the material and consequently controls the cycling stability of the battery. Here, by integrating sensitive elemental tomography, an advanced algorithm and cryogenic scanning transmission electron microscopy, we unveil, in three dimensions, a correlated structural and chemical evolution of Si and SEI. Furthermore, corroborated with a chemomechanical model, we demonstrate progressive electrolyte permeation and SEI growth along the percolation channel of the nanovoids due to vacancy injection and condensation during the delithiation process. Consequently, the Si–SEI spatial configuration evolves from the classic ‘core–shell’ structure in the first few cycles to a ‘plum-pudding’ structure following extended cycling, featuring the engulfing of Si domains by the SEI, which leads to the disruption of electron conduction pathways and formation of dead Si, contributing to capacity loss. The spatially coupled interactive evolution model of SEI and active materials, in principle, applies to a broad class of high-capacity electrode materials, leading to a critical insight for remedying the fading of high-capacity electrodes.

36 MATERIALS SCIENCE↗

Quantum chemical calculations of lithium-ion battery electrolyte and interphase species

Abstract Lithium-ion batteries (LIBs) represent the state of the art in high-density energy storage. To further advance LIB technology, a fundamental understanding of the underlying chemical processes is required. In particular, the decomposition of electrolyte species and associated formation of the solid electrolyte interphase (SEI) is critical for LIB performance. However, SEI formation is poorly understood, in part due to insufficient exploration of the vast reactive space. The Lithium-Ion Battery Electrolyte (LIBE) dataset reported here aims to provide accurate first-principles data to improve the understanding of SEI species and associated reactions. The dataset was generated by fragmenting a set of principal molecules, including solvents, salts, and SEI products, and then selectively recombining a subset of the fragments. All candidate molecules were analyzed at the ω B97X-V/def2-TZVPPD/SMD level of theory at various charges and spin multiplicities. In total, LIBE contains structural, thermodynamic, and vibrational information on over 17,000 unique species. In addition to studies of reactivity in LIBs, this dataset may prove useful for machine learning of molecular and reaction properties.

25 ENERGY STORAGE↗

Determination of the Solid Electrolyte Interphase Structure Grown on a Silicon Electrode Using a Fluoroethylene Carbonate Additive

In this work we explore how an electrolyte additive (fluorinated ethylene carbonate – FEC) mediates the thickness and composition of the solid electrolyte interphase formed over a silicon anode in situ as a function of state-of-charge and cycle. We show the FEC condenses on the surface at open circuit voltage then is reduced to C-O containing polymeric species around 0.9 V (vs. Li/Li + ). The resulting film is about 50 Å thick. Upon lithiation the SEI thickens to 70 Å and becomes more organic-like. With delithiation the SEI thins by 13 Å and becomes more inorganic in nature, consistent with the formation of LiF. This thickening/thinning is reversible with cycling and shows the SEI is a dynamic structure. We compare the SEI chemistry and thickness to 280 Å thick SEI layers produced without FEC and provide a mechanism for SEI formation using FEC additives.

25 ENERGY STORAGE↗

Molecular Dynamics of Lithium Ion Transport in a Model Solid Electrolyte Interphase

Here, Li + transport within a solid electrolyte interphase (SEI) in lithium ion batteries has challenged molecular dynamics (MD) studies due to limited compositional control of that layer. In recent years, experiments and ab initio simulations have identified dilithium ethylene dicarbonate (Li 2 EDC) as the dominant component of SEI layers. Here, we adopt a parameterized, non-polarizable MD force field for Li 2 EDC to study transport characteristics of Li + in this model SEI layer at moderate temperatures over long times.

25 ENERGY STORAGE↗

An interphase pool of KIF11 localizes at the basal bodies of primary cilia and a reduction in KIF11 expression alters cilia dynamics

KIF11 is a homotetrameric kinesin that peaks in protein expression during mitosis. It is a known mitotic regulator, and it is well-described that KIF11 is necessary for the formation and maintenance of the bipolar spindle. However, there has been a growing appreciation for non-mitotic roles for KIF11. KIF11 has been shown to function in such processes as axon growth and microtubule polymerization. We previously demonstrated that there is an interphase pool of KIF11 present in glioblastoma cancer stem cells that drives tumor cell invasion. Here, we identified a previously unknown association between KIF11 and primary cilia. We confirmed that KIF11 localized to the basal bodies of primary cilia in multiple cell types, including neoplastic and non-neoplastic cells. Further, we determined that KIF11 has a role in regulating cilia dynamics. Upon the reduction of KIF11 expression, the number of ciliated cells in asynchronously growing populations was significantly increased. We rescued this effect by the addition of exogenous KIF11. Lastly, we found that depleting KIF11 resulted in an increase in cilium length and an attenuation in the kinetics of cilia disassembly. These findings establish a previously unknown link between KIF11 and the dynamics of primary cilia and further support non-mitotic functions for this kinesin.

59 BASIC BIOLOGICAL SCIENCES↗

Evaluating the solid electrolyte interphase formed on silicon electrodes: A comparison of ex situ X-ray photoelectron spectroscopy and in situ neutron reflectometry

This work details the in situ characterization of the interface between a silicon electrode and an electrolyte using a linear fluorinated solvent molecule, 0.1 M lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) in deuterated dimethyl perfluoroglutarate (d6-PF5M 2 ) (1.87 x 10 -2 mS/cm -1 ). The solid electrolyte interphase (SEI) composition and thickness determined via in situ neutron reflectometry (NR) and ex situ X-ray photoelectron spectroscopy (XPS) were compared. The data show that SEI expansion and contraction (breathing) during electrochemical cycling was observed via both techniques; however, ex situ XPS suggests that the SEI thickness increases during Si lithiation and decreases during delithiation, while in situ NR suggests the opposite. The most likely cause of this discrepancy is the selective removal of SEI components (top 20 nm of the SEI) during the electrode rinse process, required to remove electrolyte residue prior to ex situ analysis, demonstrating the necessity of performing SEI characterizations in situ.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Breathing and oscillating growth of solid-electrolyte-interphase upon electrochemical cycling

We report the first direct experimental evidence of the dynamic behavior of the solid-electrolyte-interphase (SEI) on copper electrodes upon electrochemical cycling. Synchrotron-based soft X-ray absorption spectroscopy (sXAS) and time-of-flight secondary ion mass spectrometry (TOF-SIMS) consistently show that both the chemical composition and the thickness of the SEI change with electrochemical potential throughout the slow formation process. In particular, sXAS results show that the nascent carbonate species in SEI show redox reversibility and decompose during the delithiation (oxidation) process, which leads to a significant shrinking of the SEI thickness as confirmed by TOF-SIMS. Meanwhile, the carbonates also matures and become more and more inactive at every lithiation (reduction) process. These experimental observations reveal unambiguously that SEI formation is much more complicated than a simple and monotonous deposition of electrolyte decomposition product; instead, it could be an oscillating process with a breathing growth.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Deliberate modification of the solid electrolyte interphase (SEI) during lithiation of magnetite, Fe 3 O 4 : impact on electrochemistry

Here, magnetite is a conversion anode material displaying multi-electron transfer during lithiation and delithiation. The solid electrolyte interphase (SEI) on magnetite, Fe 3 O 4 , electrodes for lithium ion batteries was deliberately modified through the use of fluoroethylene carbonate (FEC) electrolyte additive, improving both capacity retention and rate capability. Analysis showed reduction of FEC at higher voltage compared to non-fluorinated solvents with formation of a modified lithium flouride containing electrode surface.

25 ENERGY STORAGE↗

The role of the solid electrolyte interphase layer in preventing Li dendrite growth in solid-state batteries

Lithium (Li) metal anodes have regained intensive interest in recent years due to the ever-increasing demand for next-generation high energy battery technologies. Li metal, unfortunately, suffers from poor cycling stability and low efficiency as well as from the formation of dangerous Li dendrites, raising safety concerns. Utilizing solid-state electrolytes (SSEs) to prevent Li dendrite growth provides a promising approach to tackle the challenge. However, recent studies indicate that Li dendrites easily form at high current densities, which calls for full investigation of the fundamental mechanisms of Li dendrite formation within SSEs. Herein, the origin and evolution of Li dendrite growth through SSEs have been studied and compared by using Li6.1Ga0.3La3Zr2O12 (LLZO) and NASICON-type Li2O–Al2O3–P2O5–TiO2–GeO2 (LATP) pellets as the separators. We discover that a solid electrolyte interphase (SEI)-like interfacial layer between Li and SSE plays a critical role in alleviating the growth of dendritic Li, providing new insights into the interface between SSE and Li metal to enable future all solid-state batteries.

Wu, Bingbin↗

Role of conductive binder to direct solid–electrolyte interphase formation over silicon anodes

In this study, with the use of in situ neutron reflectometry (NR) we show how the addition of an electronically conductive polymeric binder, PEFM, mediates the solid–electrolyte interphase (SEI) formation and composition on an amorphous Si (a-Si) electrode as a function of the state-of-charge. Upon initial contact with the electrolyte a Li rich, 41 Å thick, layer forms on the surface of the anode below the polymer layer. At 0.8 V (vs. Li/Li + ), a distinct SEI layer forms from the incorporation of electrolyte decomposition products in the reaction layer that is organic in nature. In addition, solvent uptake in the PEFM layer occurs resulting in the layer swelling to ~200 Å. Upon further polarization to 0.4 and 0.15 V (vs. Li/Li + ) a thick layer (800 Å) on the surface of the Si is evident where a diffuse interface between the PEFM and SEI occurs resulting in a matrix between the two layers, as the binder has taken up a large amount of electrolyte. The two layers appear to be interchanging solvent molecules from the PEFM to the SEI to the Si surface preventing the lithiation of the a-Si. By 0.05 V (vs. Li/Li + ) a Li rich, 72 Å thick, SEI layer condenses on the surface of the anode, and a 121 Å intermixed layer on top of the SEI with LiF and Li–C–O species is present with the rest blended into the electrolyte.

36 MATERIALS SCIENCE↗

Polar polymer–solvent interaction derived favorable interphase for stable lithium metal batteries

Lithium metal has long been regarded as one of the most promising anode materials for future rechargeable batteries. However, the severe reaction of Li with carbonate electrolytes and the rapid growth of Li-dendrites at high current densities hinder its practical application in Li-metal batteries. In this work, we report a polar polymer protective layer to suppress highly corrosive cyclic carbonates by tuning polymer–solvent interactions. The C≡N groups of polyacrylonitrile (PAN) polymer chains in the polar polymer network can effectively reduce high reactivity of the C=O groups of carbonate solvents leading to a stable solid electrolyte interphase (SEI) layer with higher inorganic components. In situ optical and electron microscopes demonstrate that the polar polymer network effectively restrained the formation and growth of Li-dendrites, which helps to stabilize the plating/stripping behavior of Li in a symmetric Li|Li cell and a Li|LiNi 1/3 Co 1/3 Mn 1/3 O 2 cell. This study provides a useful perspective of controlling electrolyte coordination to form a stable SEI layer in carbonate electrolytes for Li-metal batteries.

25 ENERGY STORAGE↗

A functional SrF 2 coated separator enabling a robust and dendrite-free solid electrolyte interphase on a lithium metal anode

An unstable solid electrolyte interphase (SEI) and accompanying Li metal dendrites are the key impediments to commercialization of high-energy lithium metal batteries (LMBs). We employ a strontium fluoride (SrF 2 ) microsphere coated polypropylene (PP) separator to stabilize the SEI and to prevent dendrites from growing. This approach is tested with Li∥Cu half-cells, Li∥Li symmetrical cells, and Li∥NMC full LMBs, there being a major improvement in each case. The Li∥Cu cell with SrF 2 maintains a stable coulombic efficiency (CE) of 80% after 100 cycles, when tested at 0.25 mA cm -2 to a capacity of 0.5 mA h cm -2 . By comparison, the uncoated PP reference has a CE of 10% in cycle 60. The Li∥Li cell with SrF 2 exhibits a markedly smaller voltage polarization and is able to stably cycle for approximately 340 h vs. the reference which begins to display severe voltage instability at 200 h. The Li∥NMC full LMB with SrF 2 shows an initial discharge capacity of 173 mA h g -1 , with 167 mA h g -1 (96.5%) being retained after 200 cycles at 200 mA g -1 (1C rate). The SrF 2 containing LMB also has a substantially improved rate capability over the reference, the difference being drastic even at the highest testing rate of 20C. First-principles calculations based on DFT indicate that lithium ions prefer to adsorb onto the SrF 2 surface, which should create a more uniform ion flux and reduce the propensity for dendrite nucleation. Finally in parallel, the SrF 2 spheres bind with the SEI layer, creating a tough in situ formed composite membrane that mechanically stabilizes a planar metal interface.

25 ENERGY STORAGE↗

Salt-rich solid electrolyte interphase for safer high-energy-density Li metal batteries with limited Li excess

We propose a carbonate-based electrolyte optimized with dual cations and ionic liquid for high-efficiency Li metal batteries with a high-voltage cathode. An average coulombic efficiency of Li deposition of 99.6% is achieved due to the salt-rich solid electrolyte interphase and Na guided uniform Li plating. The Li||NCM811 cells can be cycled with limited Li (N/P = 1) over 90 cycles. An additional advantage is that it improves the thermal stability of the NCM811 cathode.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unveiling the mechanisms of lithium dendrite suppression by cationic polymer film induced solid–electrolyte interphase modification

It is crucial to suppress lithium dendrite formation in lithium metal batteries. Formation of a good solid–electrolyte interphase (SEI) has been considered to be effective in limiting lithium dendrite growth. However, how the SEI may be modified during lithium deposition is hard to resolve due to challenges in in situ investigation of the SEI with fine details. Here, we report an in situ study that uncovers the lithium dendrite suppression mechanism arising from SEI modification by a poly(diallyldimethylammonium chloride) (PDDA) cationic polymer film, using electrochemical liquid cell transmission electron microscopy (TEM). Lithium nanogranules are obtained in the presence of the polymer film. Chemical mapping of the deposits provides remarkable details of the SEI on individual nanogranules. It shows that lithium fluorides are uniformly distributed within the inner SEI layer of individual lithium nanogranules, arising from the instantaneous reaction of the deposited lithium with PF 6 – ions accumulated by the cationic polymer film, and thus the dendritic growth of lithium is prohibited. The ability to directly measure SEI chemistry at the nanoscale down to the individual nanograins in situ and unveil its correlation with the lithium deposition behavior opens future opportunities to explore unsolved mechanisms in batteries.

25 ENERGY STORAGE↗

A solid electrolyte interphase to protect the sulfurized polyacrylonitrile (SPAN) composite for Li–S batteries: computational approach addressing the electrolyte/SPAN interfacial reactivity

This study addresses the reactivity of multiple solvents and lithium bis(fluorosulfonyl)imide (LiFSI) at the interface with sulfurized polyacrylonitrile (SPAN) in multiple stages of lithiation via ab initio molecular dynamics simulations. Here, both ether 1,3-dioxolane (DOL) and dimethyl carbonate (DMC) proved stable on the lithiated SPAN surface regardless of the lithium content, meaning that neither of these species likely contributes to growing a solid electrolyte interphase (SEI) coating to protect the SPAN composite. Conversely, cyclic carbonates, ethylene carbonate (EC) and fluoroethylene carbonate (FEC) are shown to be very active. The EC reduction occurs only on a highly lithiated surface with a 3.0 Li/S molar ratio, the equivalent of the SPAN composite in an over-discharge regime with voltages close to 0.0 V vs. Li/Li + . The FEC reduction starts with a 2.0 Li/S molar ratio and above, suggesting that FEC could act as a useful additive in electrolyte formulations with EC. Both EC and FEC follow multiple reduction mechanisms to produce complex reduction products and LiF in the FEC case. We provide a mechanistic description for each detected decomposition path. The LiFSI salt also proves reactive against the lithiated SPAN surface. The FSI – defluorination is the dominant reduction path. However, the SO 2 NSO 2 F – and SO 2 NSO 2 2– species proved stable against S–N cleavage. This behavior makes the LiFSI salt a potential candidate for SPAN-based Li–S batteries because it produces LiF without releasing SO 2 .

25 ENERGY STORAGE↗