Highly stretchable polymer semiconductor thin films with multi-modal energy dissipation and high relative stretchability

Abstract Stretchable polymer semiconductors (PSCs) have seen great advancements alongside the development of soft electronics. But it remains a challenge to simultaneously achieve high charge carrier mobility and stretchability. Herein, we report the finding that stretchable PSC thin films (<100-nm-thick) with high stretchability tend to exhibit multi-modal energy dissipation mechanisms and have a large relative stretchability ( rS ) defined by the ratio of the entropic energy dissipation to the enthalpic energy dissipation under strain. They effectively recovered the original molecular ordering, as well as electrical performance, after strain was released. The highest rS value with a model polymer (P4) exhibited an average charge carrier mobility of 0.2 cm 2 V −1 s −1 under 100% biaxial strain, while PSCs with low rS values showed irreversible morphology changes and rapid degradation of electrical performance under strain. These results suggest rS can be used as a parameter to compare the reliability and reversibility of stretchable PSC thin films.

36 MATERIALS SCIENCE↗

Self-healing carbon fiber/epoxy laminates with particulate interlayers of a low-melting-point alloy

In order to prolong the service life of fiber-reinforced polymer composites, the implementation of self-healing ability with the micro-encapsulated healing agent has been extensively studied. However, such microcapsule-based self-healing composites typically suffer from degraded mechanical properties due to the liquid-phase inclusions, thereby limiting their proliferation. Here, in this study, a low-melting-point alloy is utilized as the particulate inclusions of carbon fiber/epoxy laminated composites. Field's Metal particles (melting point: 62 °C) are distributed between woven carbon fiber preforms followed by the resin impregnation to realize laminated composites with a Field's Metal-enhanced interlayer(s). The resulting laminated composites demonstrate the autonomic repair of interlaminar failure with a 40 % of healing efficiency. Most of all, the mechanical properties of these self-healing laminated composites are comparable to the conventional laminated composites attributed to the rigid inclusions that can be compressed to increase the fiber volume. Since the Field's Metal particle inclusions can bestow polymer composites with self-healing ability and the potential increase in mechanical properties, Field's Metal-enhanced fiber-reinforced polymer composites are expected to unlock the practical utility of self-healing composites.

A. polymer-matrix composites (PMCs)↗

Similarity Metric for Data Optimization and Efficient Training of Reactive Machine Learning Force Fields for Hydrocarbon Radiolysis

Radiolysis is a common approach to sterilize polymers, chemically modify them for upcycling, and accelerate their decomposition for recycling purposes. Reactive molecular dynamics (MD) simulations provide a powerful tool to generate atomic-level trajectories of the reactive processes and quantify radiolytic chemical degradation pathways. For this, machine learning (ML) surrogate models for reactive force fields with quantum mechanical accuracy are now widely used, which require ML training data sets that can provide information on atomic environments for target chemical systems. However, radiolysis chemistry can be highly complex and diverse, which poses significant challenges for generating training data to parametrize ML models. In this regard, we developed a method for optimizing the training data set using a cosine similarity metric to help guide training set selection for radiolysis of polyethylene, a model hydrocarbon polymer, as well as to enhance the transferability of our reactive ML force field (MLFF) to a variety of molecular and polymeric systems. Our approach performs atom-by-atom comparisons between local atomic environments to pinpoint important data points associated with rare and localized events, such as radiolysis damage within structures. We apply this approach to train the Chebyshev Interaction Model for Efficient Simulation (ChIMES) MLFF model, which expresses the atomic interaction potentials in terms of linear combinations of many-body Chebyshev polynomials. We first show that our method can reduce our training set size by ∼70% while improving overall accuracy compared to more standard MD model fitting approaches. We then validate our optimum model against diverse hydrocarbon simulation data, including simple alkanes and systems with unsaturated carbon bonds, over a wide range of thermodynamic conditions. Finally, we use our ChIMES model to perform MD simulations of radiolytic damage with large-scale systems that help avoid system size effects. Overall, our approach yields an MD force field that retains most of the accuracy of the underlying quantum method while yielding many orders of improvement in computational efficiency. In conclusion, our efforts will have impact on future hydrocarbon polymer radiolysis studies, where the chemical details of the polymer–radiation interactions can have a strong effect on the resulting products observed in experiments.

Hydrocarbons↗

Structured for success: conjugated polymer binders with tailored composition and architecture for lithium-ion batteries

Conjugated polymer binders are replacing conventional binders in lithium-ion batteries. Herein, we examine how molecular engineering and hierarchical nanostructuring govern binder functionality and electrochemical performance. Lithium-ion batteries (LIBs) are the leading energy storage technology, yet enhancing their energy density and cycle life remains critical. Significant progress has been made in high-capacity anodes and high-voltage cathodes, but their performance is hindered by electrode degradation, where it is related to the behaviors of binders at the surface and interface. Conventional non-conductive binders like poly(vinylidene difluoride) (PVDF), combined with conductive additives, often fail to maintain electrical pathways under repeated volume changes. Alternatively, conjugated polymer binders have emerged as a superior alternative, simultaneously offering intrinsic conductivity, mechanical flexibility, and strong adhesion through π-conjugated backbones and functional groups. Their tunable molecular structure enables efficient electron/ion transport while mitigating electrode cracking. Additionally, the development of hierarchically ordered nanostructures in conjugated polymer binder can further enhance their electrochemical performance. This review examines the design principles of conjugated polymer binders, focusing on molecular engineering and nanostructural control to optimize their performance in high-loading electrodes, such as silicon-based anodes. By addressing key challenges in binder functionality, these advanced materials pave the way for next-generation high-energy-density LIBs.

Jin, Xiuyu↗

Alkylidene functionalization produces highly recyclable and scalable polyhydroxyalkanoates

Recyclable polymers that can be produced at scale and readily tuned within the same polymer framework for specific properties are important to achieving a circular materials economy. To this end, synthetic poly(3-hydroxyalkanoate)s (PHAs) have emerged as high-performance, chemically recyclable variants of biological PHAs, but their difficult monomer syntheses and suboptimal recycling efficiencies pose challenges for large-scale deployment. In this study, we investigated a β-isopropylidene PHA, i-PHA, for which the lactone monomer can be synthesized by existing industrial methods from biomass-derived isobutyric acid. The alkylidene substituent prevents decarboxylative degradation typically observed during PHA depolymerization, enabling near-quantitative chemical recycling to monomer. Controlled hydrogenation of the β-isopropylidene side group produces PHAs with diverse performance metrics that are competitive with a range of commodity polymers, spanning strong fibers to ductile thermoplastics to superglue epoxy resins.

36 MATERIALS SCIENCE↗

H-Mat Hydrogen Compatibility of Polymers and Elastomers

The H2@Scale program of the U.S. Department of Energy (DOE) Fuel Cell Technologies Office is supporting work on the hydrogen compatibility of polymers to improve the durability and reliability of materials for hydrogen infrastructure. The hydrogen compatibility program (H-Mat) seeks “to address the challenges of hydrogen degradation by elucidating the mechanisms of hydrogen-materials interactions with the goal of providing science-based strategies to design materials, (micro)structures, and morphology with improved resistance to hydrogen degradation.” This research has observed interactions of hydrogen and pressure with model rubber-material compounds resulting in volume change and compression-set differences in the materials. The materials were investigated using helium-ion microscopy (HeIM), which revealed significant morphological changes in the plasticizer-incorporating compounds after exposure, as evidenced by time-of-flight secondary ion mass spectrometry. Additional studies using transmission electron microscopy and nuclear magnetic resonance were performed to correlate morphological change to potential chemical change in the materials.

08 HYDROGEN↗

Standardized protocols for evaluating platinum group metal-free oxygen reduction reaction electrocatalysts in polymer electrolyte fuel cells

Platinum group metal (PGM)-free electrocatalysts for the oxygen reduction reaction at the polymer electrolyte fuel cell cathode have shown substantial improvements in activity—especially those derived from transition metals, nitrogen and carbon. However, their stability and durability remain insufficient. A key to enabling future improvements and performance comparisons lies in the development of test protocols that are relevant to the operating conditions of the fuel cell cathode, can be completed within a reasonable time and are ubiquitously adopted. Here we propose and validate such protocols, designed with special attention to typical catalyst degradation mechanisms of PGM-free catalysts. The results of the cross-laboratory validation study using two different catalysts attest to the strength and feasibility of the proposed approach. We hope that the information provided here can serve as a broad and effective platform for assessing the performance and durability of PGM-free catalysts for polymer electrolyte fuel cells.

25 ENERGY STORAGE↗

Recent developments in catalyst-related PEM fuel cell durability

Cost and durability remain the two major barriers to the widespread commercialization of polymer electrolyte membrane fuel cell (PEMFC)-based power systems, especially for the most impactful but challenging fuel cell electric vehicle (FCEV) application. Commercial FCEVs are now on the road; however, their PEMFC systems do not meet the cost targets established by the U.S. Department of Energy, primarily due to the high platinum loading needed on the cathode to achieve the requisite performance and lifetime. Furthermore, while the activities of a number of commercial Pt-based alloy cathode catalysts exceed the beginning-of-life (BOL) targets, these activities, and the overall cathode performance, degrade via a variety of mechanisms described herein. Degradation is mitigated in current FCEVs by utilizing a cathode catalyst with a lower BOL activity (e.g., much lower transition metal alloy content and larger BOL nanoparticle size), necessitating higher catalyst loadings, and through the utilization of system controls that avoid conditions known to exacerbate degradation processes, such as limiting the fuel cell stack voltage range. The design and development of active and robust materials and eliminating the need for vehicle mitigation strategies would greatly simplify the operating system, allowing for greater transient operation, avoiding large hybridization, and curtailing of fuel cell power. Although system mitigation strategies have provided the near-term pathway for FCEV commercialization, material-specific solutions are required to further reduce costs and improve operability and efficiency. Future material developments should focus on stabilization of the electrode structure and minimization of the catalyst particle susceptibility to dissolution caused by oxide formation and reduction over PEMFC cathode-relevant operating potentials plus minimization of support corrosion. Ex situ accelerated stress tests have provided insight into the processes responsible for material and performance degradation and will continue to provide useful information on the relative stability of materials and benchmarks for robust and stable materials-based solutions not requiring system mitigation strategies to achieve adequate lifetime.

25 ENERGY STORAGE↗

Ion Chromatography and Combustion Ion Chromatography Analysis of Fuel Cell Effluent Water During Open Circuit Voltage

Open circuit voltage tests were conducted on sixteen 3M Ionomer and eight Nafion™ NR211 membranes. Lifetime distributions were determined, and ion chromatography (IC) techniques were used to measure fluoride, sulfate, trifluoro acetate, and oxalate ions. Combustion Ion Chromatography (CIC) was used to determine the total organic fluoride (TOF) associated with water soluble membrane degradation fragments. The ratio of these products relative to the fluoride release rates were used to infer the likely degradation mechanism for each membrane. Peroxide attack at the sulfonic acid side chain was determined to be the least relevant reaction pathway while the long-proposed polymer chain end unzipping appears to be the dominant mechanism. Abstraction of the tertiary fluorine in the NR211 backbone and side chain is evident by organic fluoride release rates higher than can be explained by unzipping alone.

25 ENERGY STORAGE↗

Durable Mn-Based PGM-Free Catalysts for Polymer Electrolyte Membrane Fuel Cells

This proposed project aims to develop and evaluate novel manganese based, nitrogen-derived, PGM-free electrocatalysts (denoted as Mn-N-C) to fully address the membrane electrolyte assemblies (MEA)’s ionomer degradation issue resulting from iron. Four thrusts will be pursed in this proposed project. First, advanced first-principles computation methods will be employed to accelerate the rational catalyst design and synthesis. Second, an effective hydro-gel method will be used to maximize atomic Mn active sites embedded in carbon matrix. Next, state-of-the art methods in fuel cell companies will be used to fabricate MEAs containing the Mn-N-C catalysts. Finally, industry standards will be rigorously followed to evaluate fuel cell performance and durability of the Mn-N-C catalysts. With successful completion of the project, it is expected that the following outcomes will be achieved. (1) A set of MEAs containing the Mn-N-C catalysts and with active area large than 50 cm 2 for independent testing, (2) testing results demonstrating that the MEAs of Mn-N-C catalysts have mass activity of 0.044 A/cm 2 at 0.9 VIR-free and H 2 /air performance of 0.50 V at 1.0 A/cm 2 ; (3) fundamental understanding of the composition-structure-property relation of the PGM-free Mn- N-C catalysts, and (4) computational data, measurement data, and publications deposited into the database of ElectroCat Consortium.

08 HYDROGEN↗

Proposed synthesis of a linear poly-ethylenimine with hydroxyl pendants substituents at the adjacent carbon

The synthesis of a linear poly-ethylenimine with pendant hydroxyl groups bonded to backbone carbons adjacent to the backbone amine groups is investigated and compared to the conventional method of functionalizing branched poly-ethylenimine using epoxides for use in direct air capture of carbon dioxide. The addition of hydroxyl groups imparts stability against both oxidative degradation and the formation of urea by reducing the number of primary amines, while the novel method of bonding to the adjacent backbone carbon rather than directly to the amine is hypothesized to retain the higher capacity for carbon dioxide of secondary amines when compared to tertiary amines. We also expect that the hydroxyl substituents will impart stronger hydrogen bonding capabilities, resulting in stronger interactions between adjacent polymer chains and a subsequent decrease in mobility.

36 MATERIALS SCIENCE↗

Performance stability of plastics for neutron-gamma pulse shape discrimination

The introduction of the first commercially available plastic scintillators with pulse shape discrimination (PSD) offered by Eljen Technology marked progress towards potentially replacing liquid scintillators in neutron detection. However, use of these plastics over several recent years has revealed an important flaw in these materials: the eventual degradation of scintillation light output and PSD performance. Here, studies described in this paper considered possible reasons for this degradation. Experiments conducted with numerous lab-prepared and commercial EJ-276 samples showed that the main factor affecting the instability is oxidation that involves highly reactive radicals generated during the polymerization process or from the further breakdown of polymer chains under oxygen/air exposure. Based on the obtained results, the stability of scintillation performance for PPO (2,5-Diphenyloxazole)-based PSD plastics has been improved through modifications of the composition via the utilization of scintillation dyes and compounds with antioxidant properties that diminish the effects of oxidation. Elements of these studies were used in the commercial production of the most recent EJ-276D PSD plastic version for fast neutron detection and 6Li-loaded plastics for thermal neutron and antineutrino detection applications. Performance projections of the new PSD plastics indicate a likely degradation of less than 10 % over 5–10 years in comparison to previous EJ-276 that might lose up to 30–40 % of the scintillation light during 1–2 years of storage or deployment under ambient conditions.

36 MATERIALS SCIENCE↗

1,4-cineole: a bio-derived solvent for highly stable graphene nanoplatelet suspensions and well-dispersed UHMWPE nanocomposite fibers

The exceptional properties of carbon nanoparticles, such as graphene, promise to expand the performance and functionality of many materials. The reinforcement of polymers is of keen interest due to their low density and flexible manufacturing methods. However, dispersing graphene in them has proven to be an enduring challenge due to the particles’ propensity to form performance degrading agglomerations. Furthermore, effective solvents for nanoparticle dispersion are commonly harmful, non-renewable, petrochemicals. In this work, a bio-derived solvent, 1,4-cineole, is demonstrated as a renewable alternative to these solvents that can be used to form highly stable graphene nanoplatelet (GnP) suspensions and used to gel spin well-dispersed UHMWPE/GnP nanocomposite fibers. The GnP concentration in the fibers was varied across three orders of magnitude, 0.01 wt% to 1 wt%, to examine its effect on fiber microstructure and properties. At low concentrations the particles act as point defects without affecting the fiber microstructure, and poor particle/matrix interfacial adhesion results in significantly reduced mechanical properties. At 1 wt% GnPs, a network effect takes hold thereby reinforcing the fibers, but the particles also impede the growth and orientation of crucial load-carrying crystalline structures in the fiber. Furthermore, unveiling the microstructural effects of GnPs on highly oriented and crystalline polymers in this study provides crucial insights for future work developing high-performance polymer nanocomposite fibers.

36 MATERIALS SCIENCE↗

3D printed water-stable Cd-doped Cs 4 MnBi 2 Cl 12 /polylactic acid perovskite/polymer composites for high-flux X-ray scintillation

Stable and efficient X-ray scintillators are crucial for medical diagnostics, industrial, and defense applications. However, conventional scintillator technologies face a trade-off between stability, optimal performance, and sustainability. Herein, we introduce 3D-printed Cs 4 MnBi 2 Cl 12 (Pero1) and Cs 4 Cd 0.68 Mn 0.32 Bi 2 Cl 12 (Pero2) perovskite microcrystals embedded within a polylactic acid (PLA) polymer composite as X-ray scintillators, combining efficiency, stability, and sustainability. The orange luminescent perovskite powder phosphors exhibited poor water stability, which was successfully addressed through incorporation into PLA via filament extrusion and fused deposition modeling (FDM) 3D printing. The resulting composite films demonstrated remarkable water stability while maintaining uniform orange emission throughout the polymer matrix, as confirmed by 3D topography scanning and X-ray fluorescence mapping. Structural characterization revealed minimal chemical interaction between the perovskite and PLA matrix, with the composites retaining their crystalline properties. The PLA-Pero2 composite exhibited superior optical properties, with a photoluminescence quantum yield of 47%, nearly 17 times higher than that of PLA-Pero1 (2.8%), attributed to the effective suppression of non-radiative decay pathways through Cd 2+ doping. Under hard X-ray irradiation at synchrotron beamlines, both composites exhibited excellent radioluminescence, with emission peaks at 605 nm, a linear response across a wide X-ray flux range, and remarkable radiation stability, showing less than 3% intensity degradation after 600 seconds of continuous high-dose exposure. The PLA-Pero2 composite achieved a spatial resolution of 5 line pairs per millimeter and a contrast ratio of 0.255. These performance metrics, combined with the polymer's biodegradability and scalability through additive manufacturing, position PLA-based composites as a more sustainable alternative to conventional petroleum-based polymer scintillators for next-generation medical imaging, radiation monitoring, and industrial radiography applications.

3D Printing↗

Atomic-scale modeling of C/N kinetic stability descriptors for PGM-free electrocatalysts at finite temperatures

The durability of platinum group metal-free (PGM-free) electrocatalysts is a major barrier to their usage in polymer electrolyte fuel cell cathodes. C and N removal from active sites may play an important role in the catalyst’s ability to maintain high activity. While C degradation mechanisms are kinetically controlled, previous studies have focused on thermodynamic descriptors. In this work, we develop a temperature-dependent kinetic descriptor of C and N stability using an electron beam-damage model. Our approach considers the electron beam energy threshold (EBET) describing the knock-on displacement of C and N atoms as a stability descriptor for atomic structures. The stability of different sites is calculated to be different showing this approach can discriminate between similar sites with varied configurations. Additionally, we provide important insight regarding TEM beam damage of proposed active sites. We calculate 60 keV electrons can damage some proposed active site structures even at room temperature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Recent progress in the durability of Fe-N-C oxygen reduction electrocatalysts for polymer electrolyte fuel cells

This mini-review article review focuses on the very recent advancements in the stability and durability under operating fuel cell conditions of Fe-N-C electrocatalysts oxygen reduction reaction (ORR) catalysts. The most prominent degradation mechanisms of active site demetallation and carbon corrosion, both resulting in a relatively rapid initial performance loss, are introduced and elaborated on through recent published work, with emphasis on the role of H 2 O 2 radicals in these two likely catalysts degradation mechanisms. Here, the current state of Fe-N-C electrocatalysts is also discussed and several specific improvements are proposed as necessary to advance these materials towards a state of competitive stability and durability.

25 ENERGY STORAGE↗

Dose Rate Effects in the Aging of Nuclear Cable Insulation Subjected to Gamma Radiation

In nuclear power plants (NPPs), the aging of polymer-based electrical cable insulation must be effectively monitored to ensure the safe and reliable operation of NPPs. Gamma radiation is one of the main environmental stressors causing degradation of cable insulation. For a given total dose of absorbed gamma radiation, damage due to gamma irradiation may be dose rate dependent. The purpose of this work is to confirm whether a dose rate effect exists for the cable insulation made by crosslinked polyethylene (XLPE) and ethylene propylene rubber (EPR), quantify the relationship between degradation rate and dose rate, and explore the correlation of different measured properties. The dose rate effects at 1800 Gy/h, 200 Gy/h, and 100 Gy/h using 60Co gamma irradiation on cable aging was studied. Different types of cable insulation, including two XLPEs and one EPR, were irradiated at the different dose rates with a total dose around 300 kGy at 26 °C. The properties of unirradiated and irradiated samples were characterized by mass change, yellowness index, and other ongoing measurements. Dose rate effects were observed for mass change data of XLPE and EPR.

Li, Donghui↗

Effect of Catalyst and Catalyst Layer Composition on Catalyst Support Durability

Polymer electrolyte membrane fuel cells (PEMFCs) are efficient, zero-emission engines for the automotive sector. However, cost and durability are major barriers for the commercialization of PEMFCs. Degradation of the carbon support in the cathode catalyst layer due to high potential excursions caused by unmitigated events like H 2 starvation, or start-up/shutdown are still a major durability issue in PEMFCs. Catalyst support durability was studied by accelerated stress tests (ASTs) that included repeated potential cycling from 1.0 to 1.5 V. The effect of catalyst layer composition on carbon corrosion was studied using membrane electrode assemblies with different catalysts (Pt, PtCo), catalyst composition (catalyst wt.%, supports), ionomer composition (loading, and equivalent weights). The corrosion of the carbon support is similar between Pt and PtCo catalysts. However, the performance degradation rate is higher for the alloy catalysts due to differences in catalyst particle size and the transition metal’s leaching accelerating the performance degradation. The carbon loss is lower for catalysts with lower initial carbon loading (or higher catalyst wt.%), which is better for durability. However, the cumulative loss of carbon is identical for electrodes with the same catalyst support irrespective of catalyst and ionomer composition in the catalyst layer.

25 ENERGY STORAGE↗