Recrystallized Arrays of Bismuth Nanowires with Trigonal Orientation.
Abstract not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Explore the source record for details and available documents.
Tin (Sn) whiskers are not a recent development. Studies in the late 1930’s investigated thin filaments that grew spontaneously from Sn coatings used for the corrosion protection of electronic hardware. It was soon recognized that these Sn filaments, or whiskers, could create short circuits in the same electronic equipment. Figure 1a illustrates whisker growth in the hole of a printed circuit board having an immersion Sn surface finish. The engineering solution was to contaminate the Sn with > 3 wt.% of lead (Pb). The result was that whisker growth was replaced with hillock formation (Fig. 1b) that posed a minimal reliability concern to electrical circuits. Today, Pb-containing finishes are being replaced with pure Sn coatings to meet environmental restrictions on Pb use. The same short-circuit concerns have been raised, once again, with respect to Sn whiskers.
Abstract not provided.
Abstract not provided.
Abstract not provided.
In 2012, a pathfinder forward pressure vessel bulkhead (FPVBH) for the Orion Multi-Purpose Crew Vehicle (MPCV) was fabricated using aluminum (Al) alloy 2219. The demonstration article was offered as a replacement for the baseline configuration, which at that time was a multi-piece welded construction using aluminum-lithium (Al-Li) alloy 2195. In 2014, the NASA Engineering and Safety Center (NESC) funded a Phase I effort to explore spin-forming as a manufacturing method to produce a complex-shaped, single-piece FPVBH for the crew module (CM) [1]. The primary focus of the NESC effort was to expand spin-forming technology to the fabrication of an Al-Li 2195 FPVBH. As a result, limited testing and analysis was performed on the original Al 2219 article. In this study, a sufficiently large plate of Al 2219 was not available for the fabrication of a FPVBH. Therefore, the forming blank comprised two plates (from different lots) butt welded together using a single friction stir weld. The welded forming blank was then spin formed into the FPVBH configuration and heat treated to the T62 temper. Mechanical property testing of the spin-formed 2219-T62 FPVBH revealed that the tensile properties were comparable to the Metallic Material Properties Development and Standardization (MMPDS) A-basis allowable for Al 2219-T6 wrought products. However, post-spin forming application of the standard heat treatment produced large, recrystallized grains in the material. The response varied within the two plates; one plate lot exhibited nearly complete recrystallization, while the other lot contained bands of recrystallization. Although no reduction in tensile properties was observed due to these microstructural variations, a more detailed investigation was recommended to better understand the effect of spin forming on the recrystallization mechanism and the impact on other material properties. The current study examined the microstructure and mechanical properties of the fully processed Al 2219-T62 FPVBH with emphasis on comparing differences between the two plates. Testing was limited to the cone region of the FPVBH. The two specific tasks in this study were: a) Characterization of the microstructure and mechanical properties in the two plates used in the FPVBH. b) Isolation of the impact of each step in the thermo-mechanical processing (TMP) sequence of the FPVBH on recrystallization and grain growth. Mechanical property testing sampled regions containing both large, recrystallized and small, unrecrystallized grains. Tensile strengths and elongations were equivalent in both regions and exceeded MMPDS A-basis allowables. Fracture toughness was equivalent in both regions and fracture morphology was typical of aluminum alloys. The fatigue precrack region of the fracture toughness specimens appeared more faceted in the recrystallized plate. This suggests that property testing that is more sensitive to grain size, such as fatigue crack growth rate and stress corrosion cracking, may be warranted. Alcoa reviewed the production records for the two plate lots and confirmed that composition of both plates was within the allowable range for Al 2219 and that plate processing steps were all performed within production limits. However, the Fe content was notably higher in the fully recrystallized plate, resulting in a greater volume fraction of large Fe-bearing inclusions and Al-Cu constituent particles. Alcoa did not provide details regarding plate processing variables for the two plate lots. It was surmised that deformation by hot rolling was the most accurate TMP simulation of commercial spin forming within a laboratory setting. Both hot rolling and spin forming comprise combinations of shear and compressive deformation. The through-thickness strain caused by hot rolling is symmetrical about the mid-plane, as the rollers contact both sides of the material. Shear strains are maximum at the inner and outer surfaces and trend toward zero at the mid-thickness. In contrast, spin forming utilizes a single roller on the outer surface, producing a gradient in shear stress through the thickness. Shear strains in spin-formed material are highest at the outer surface due to direct contact with the roller, and trend toward zero at the inner surface. Consequently, there will undoubtedly be some discrepancies in the mechanical response of hot-rolled and spin-formed products in the through-thickness direction. Interrupted TMP simulations were performed on remnant plate from the FPVBH forming blank in order to isolate the effects of a post-weld anneal, spin-forming deformation/thermal cycling, and solution heat treatment (SHT) on development of the recrystallized microstructures. Analysis confirmed that large, recrystallized grains formed exclusively during SHT and only after a certain deformation level was exceeded. Remnant plate from both lots that received thermal processing only did not exhibit recrystallization but exhibited fully recrystallized microstructures when processed by hot rolling. This indicates that (1) the level of deformation exceeded the critical level for recrystallization in both plates and (2) that the level of deformation during hot rolling was greater than that which accumulated during spin forming of the FPVBH. Comparison of the hot-rolled plate with the spin-formed material showed that the recrystallized grain size was larger in the FPVBH, providing further evidence that deformation levels were lower in the FPVBH. The most plausible explanation for the differing degrees of recrystallization in the two plates is particle stimulated nucleation (PSN) at the Fe-bearing inclusions and large Al-Cu constituent particles. In the plate with higher solute content, the greater volume fraction of these particles reduces the deformation level required to promote recrystallization. During spin forming the critical deformation level was likely exceeded for the higher Fe content plate resulting in a fully recrystallized microstructure. The lower Fe content plate developed a microstructure that exhibited bands of recrystallization due to the combination of a non-uniform distribution of particles and deformation. The critical deformation required for recrystallization was likely only exceeded during spin forming in regions of higher particle content. While there were differences in Fe content between these lots of Al 2219 plate, the composition of both was within defined alloy limits and Alcoa reported no anomalies during plate production. The observed differences in recrystallization after spin forming may reflect the inherent variability between these two lots of plate. The spin-forming vendor, Spincraft, reported that similar variations in recrystallized microstructures have been observed during examination of multiple spin-forming trials of a different 2xxx series aluminum alloy. Hence, tighter chemical specification limits on impurity levels in Al 2219 plate may help ensure uniform, predictable microstructures. Finally, the tensile and fracture toughness properties were not affected by the microstructural variations noted.
Highlights: • A superior fcc HEA with the strength of 1.5 GPa at the cryogenic condition is developed. • The strengthening mechanisms of HEAs at different temperatures are clarified. • The temperature dependence of MBIP effect is revealed. - Abstract: The uniaxial mechanical properties of the high entropy alloy (HEA) Fe{sub 40.4}Ni{sub 11.3}Mn{sub 34.8}Al{sub 7.5}Cr{sub 6} doped with 1.1 at.% C have been determined for both the as-cast and recrystallized states at temperatures from 77 to 973 K. Very high yield strengths were obtained at 77 K of 928 MPa for the as-cast HEA and 1037 MPa for the recrystallized HEA. The yield strength decreased sharply to 293 K and more slowly to 973 K, where it was ~200 MPa [11] in both conditions. The lattice friction stress, which results from the increase of the Peierls barrier, was the major contributor to the large yield strength at 77 K. On the other hand, the grain boundaries lose their strengthening ability at a high temperature, which largely accounts for the sharp drop in yield strength of the fine-grained (5 μm) recrystallized HEA at 973 K. The elongation to failure was highest at 293 K and 673 K with the lowest values at 77 K. Transmission electron microscopy was used to study the effects of temperature on the deformation mechanisms of the HEAs, especially the temperature dependence of the microband-induced plasticity effect. At temperatures ranging from 77 K to 673 K microbands form in the as-cast HEA, while dislocation clusters were observed in the recrystallized HEA over this temperature range. Only tangled dislocations were found at 973 K for both the as-cast and recrystallized HEA due to thermally-activated deformation.
A laboratory-scale hot extrusion setup was designed to investigate recrystallization and grain growth behavior of an AA7050 alloy during extrusion and subsequent heat treatments. Compared with industrial extrusion, the laboratory-scale process enabled rapid water quenching of extrudate with less delay so that the dynamic grain structure development was captured. After extrusion, static microstructure evolution in the extrudates was studied using salt bath annealing for 5 and 15 s at 490 °C and solutionization treatment for 1 h at 490 °C. The salt bath annealing was a simulation of the delay of press quenching in typical industrial extrusion practices. In the as-quenched extrudates, the peripheral region mainly exhibited continuous dynamic recrystallization and geometric dynamic recrystallization, whereas in the core region discontinuous dynamic recrystallization dominated. A <100> and <111> double fiber texture was identified in extrudates, and recrystallization behavior was found to be orientation dependent. The <100> oriented grains contained more sub-grain boundaries and better-defined sub-grains and had a higher tendency to fragment via continuous recrystallization, while the <111> oriented grains produced less sub-grain boundaries and did not recrystallize. Subsequent heat treatments resulted in static recrystallization and abnormal growth of the continuously recrystallized grains. Additionally, the effects of extrusion temperature (440, 480 and 520 °C) and punch speed (0.7, 1.4 and 2.1 mm/s) on grain structure were discussed. A revised grain structure evolution mechanism based on the observation of 7050 extrusion was proposed.
Specimens cut from a rolled tin bronze sheet were annealed at 400–800 °C for 1 h and evolution of their microstructures was then characterized in details by electron channeling contrast imaging and electron backscatter diffraction techniques. Particularly, statistics on special boundaries (SBs) with Σ ≤ 29 and network connectivity of random high angle boundaries (HABs) in the annealed specimens were examined to probe optimization potentials of grain boundary character distribution (GBCD) for this material. Results show that the deformed microstructure in the as-received material begins to be recrystallized when the annealing temperature increase to 500 °C and average grain sizes surge with further increasing temperatures. As a result of the recrystallization, a large number of annealing twins (with Σ3 misorientation) are produced, leading to remarkably increased fractions of SBs (f{sub SBs}). Thanks to preexisting dense low angle boundaries, the majority of SBs in the 500 °C specimen with only partial recrystallization are Σ3{sub ic} (incoherent) boundaries, which effectively disrupt connectivity of random HABs network. Although the f{sub SBs} can be further increased (up to 72.5%) in specimens with full recrystallization (at higher temperatures), the Σ3{sub ic} boundaries would be replaced to some extent by Σ3{sub c} (coherent) boundaries which do not contribute directly to optimizing the GBCD. This work should be able to provide clear suggestions on applying the concept of grain boundary engineering to tin bronze alloys. - Highlights: • The rolled tin bronze begins to be recrystallized as temperature increases to 500 °C. • A lot of SBs are produced after recrystallization and the highest f{sub SBs} is 72.5%. • Partially recrystallized specimen has the optimum GBCD due to more Σ3{sub ic} boundaries. • The Σ3{sub ic} boundaries are replaced by Σ3{sub c} boundaries after full recrystallization.
Highlights: • A non-isothermal annealing process that is concurrent with precipitation is investigated. • The mechanism of grain refinement through the interactions of precipitation, recovery and recrystallization is identified. • The combination of non-isothermal annealing and proper pre-deformation temper condition tetrads recovery. • Massive recrystallization nucleation is achieved by delaying recovery. • The growth of recrystallized grains is controlled by coarsening of precipitates that pin the grain boundaries. - Abstract: Interactions between precipitation, recovery and recrystallization during a non-isothermal annealing process in an Al-Mg-Si-Cu alloy have been investigated through a comprehensive experimental analysis. Non-isothermal annealing with a slow heating rate that starts from a low temperature is found to promote homogeneous nucleation of precipitates. The uniformly distributed precipitates limit the extent of recovery, which in turn facilitates extensive nucleation of new grains within the deformed microstructure. The growth of the recrystallized grains is strongly controlled through pinning of grain boundaries by precipitates. During the final stages of annealing, enhanced diffusion at the recrystallization front leads to preferential precipitate coarsening, release of grain boundaries from precipitates pinning, and completion of recrystallization. These interactive microstructural phenomena explain the effectiveness of a non-isothermal annealing route combined with an adequate level of deformation in obtaining a fine-grained recrystallized structure.
Highlights: • Hot forging of AD730 led to formation of large non-recrystallized grains. • Similarity in chemical compositions of the non-recrystallized zones and the matrix. • Increase in strain level promoted recrystallization. - Abstract: Design and control of microstructure of engineering parts made from nickel based superalloys with superior mechanical properties for high temperature applications, require the parts to be subjected to certain thermo-mechanical processing during forging. This often includes sequential straining and annealing at elevated temperatures followed by subsequent aging heat treatments at lower temperatures. In this study, the effect of strain magnitude on the evolution of microstructure during hot forging of a recently developed AD730 nickel based superalloy has been investigated. Microstructural heterogeneity was observed in a forged material manifested in a form of large non-recrystallized grains within the recrystallized matrix that is observed to be dependent on the level of deformation (i.e. strain magnitude). Analyses of microstructure indicated significant reduction in the fraction of low-angle grain boundaries and sub-structures with an increase in the applied strain, suggesting higher fraction of recrystallization with higher levels of strains. It was concluded that the lower strain levels were insufficient to provide enough driving force for complete recrystallization throughout the entire microstructure of the forged material.
Here, in a magnetic fusion energy (MFE) device, the plasma-facing materials (PFMs) will be subjected to tremendous fluxes of ions, heat, and neutrons. The response of PFMs to the fusion environment is still not well defined. Tungsten metal is the present candidate of choice for PFM applications such as the divertor in ITER. However, tungsten's microstructure will evolve in service, possibly to include recrystallization. How tungsten's response to plasma exposure evolves with changes in microstructure is presently unknown. In this work, we have exposed hot-worked and recrystallized tungsten to an 80 eV helium ion beam at a temperature of 900 °C to fluences of 2 × 10 23 or 20 × 10 23 He/m 2 . This resulted in a faceted surface structure at the lower fluence or short but well-developed nanofuzz structure at the higher fluence. There was little difference in the hot-rolled or recrystallized material's near-surface (≤50 nm) bubbles at either fluence. At higher fluence and deeper depth, the bubble populations of the hot-rolled and recrystallized were different, the recrystallized being larger and deeper. This may explain previous high-fluence results showing pronounced differences in recrystallized material. The deeper penetration in recrystallized material also implies that grain boundaries are traps, rather than high-diffusivity paths.
The irradiation responses of Ca2La8(SiO4)6O2 and Sr2Nd8(SiO4)6O2 with the apatite structure are investigated to predict their long-term behaviour as host phases for immobilization of actinide elements from the nuclear fuel cycle. Different ions and energies are used to study the effects of dose, temperature, atomic displacement rate and ionization rate on irradiation-induced amorphization and recrystallization. The dose for amorphization increases with temperature in two stages, below and above 150 K. In the high temperature stage relevant to actinide immobilization, the increase of amorphization dose with temperature exhibits a strong dependence on the ratio of ionization rate to displacement rate for the different ions. Data analysis using a dynamic model for amorphization reveals that ionization-induced processes, with activation energy of 0.15 0.02 eV, dominate dynamic recovery for ions from Ne through Xe. For heavier Au ions or for alpha-recoil nuclei emitted in alpha decay of actinides, ionization becomes less dominant and dynamic recovery is controlled primarily by thermally-driven processes. In post-irradiation annealing studies of amorphous samples, epitaxial thermal recrystallization is observed at 1123 K, and irradiation-enhanced nucleation of nanocrystallites is observed under irradiation with heavier ions. The recrystallization temperature under irradiation decreases with increasing ion mass to a value of ~ 823 K, which also defines the thermally-driven critical temperature for amorphization under irradiation with heavy ions. Some partial recovery due to alpha particle irradiation at 300 K is observed that suggests a self-healing mechanism in apatite phases containing actinides. Based on the results and dynamic model, the temperature and time dependences of amorphization in silicate-apatite host phases for actinide immobilization are predicted.