Search NASA⌕ Search

SEARCH · Search NASA

Results for “superalloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

Rare-earth doped thermal barrier coating bond coat for thermally grown oxide luminescence sensing

A thermal barrier coated component, such as a turbine blade formed from a superalloy substrate, includes a thermal barrier coating applied onto the substrate. A metallic bond coat layer is on the substrate and includes rare-earth luminescent dopants. A ceramic top coat layer is on the bond coat layer. A temperature sensing thermally grown oxide (TGO) layer is formed at the interface of the bond coat layer and ceramic top coat layer. The temperature sensing TGO layer includes grown rare-earth luminescent ions migrated from the metallic bond coat layer in an amount sufficient to enable luminescence sensing of the TGO layer for real-time phosphor thermometry temperature measurements at the TGO layer.

Fouliard, Quentin↗

ADDITIVE MANUFACTURING OF REFRACTORY ALLOYS

Refractory alloys are known for their high temperature capabilities and are intended for use at ultra-high temperatures above even 1200°C, which exceeds the capabilities of conventional superalloys. Additive manufacturing (AM) is an attractive alternative processing route because refractory alloys are difficult to fabricate through traditional methods; AM can form a near net-shape part with a tailored microstructure. This work seeks to evaluate the solidification behavior of refractory alloys under AM conditions and establish corresponding solidification models. Two binary alloys, Mo30Nb and Nb7.5Ta, as well as the commercial Nb alloy, C103, and one refractory high entropy alloy (RHEA), MoNbTaTi, were subjected to single track melts in a laser powder bed fusion (LPBF) machine. Each melt track was evaluated in the scanning electron microscope (SEM), which determined that some AM conditions used led to non-ideal behavior. Electron backscatter diffraction (EBSD) revealed that the Nb7.5Ta, C103, and MoNbTaTi all exhibited new grain nucleation to various extents while the Mo30Nb exhibited primarily epitaxial growth. This was found to be inconsistent with solidification models that were developed for each alloy and each set of AM conditions to predict the columnar to equiaxed transition behavior (CET) of the experimental microstructures. This disparity was largely attributed to the input parameters for the solidification model, which were developed using Thermo-Calc and SYSWELD. These input parameters include the alloy specific Gibbs-Thomson coefficient and thermophysical properties, the solute specific liquidus slopes and partitioning coefficients, as well as the process specific thermal gradients. Each input parameter was evaluated to determine the likely changes required for the modeled values to generate solidification models that better correspond to what was observed experimentally.

Miklas, Abigail↗

Method for forming a temperature sensing layer within a thermal barrier coating

A thermal barrier coated component, such as a turbine blade formed from a superalloy substrate, includes a thermal barrier coating applied onto the substrate. A metallic bond coat layer is on the substrate and includes rare-earth luminescent dopants. A ceramic top coat layer is on the bond coat layer. A temperature sensing thermally grown oxide (TGO) layer is formed at the interface of the bond coat layer and ceramic top coat layer. The temperature sensing TGO layer includes grown rare-earth luminescent ions migrated from the metallic bond coat layer in an amount sufficient to enable luminescence sensing of the TGO layer for real-time phosphor thermometry temperature measurements at the TGO layer.

Fouliard, Quentin↗

High-Strength, High-Ductility, High Entropy Alloys with High-Efficiency Native Oxide Solar Absorbers for Concentrating Solar Power Systems

This EPSCoR Project has been investigating the synergy between the excellent high-temperature mechanical behavior of FeMnNiAlCr high entropy alloys (HEA) and the high solar absorptance of their native oxides for high efficiency concentrated solar thermal power (CSP) systems working at >700°C. While HEAs have attracted substantial interest in recent years, most investigations have focused on their applications as structural materials rather than functional materials. This EPSCoR project discovered that FeMnNiAlCr HEAs can potentially be applied synergistically as both a structural and functional material for high-efficiency concentrating solar thermal power (CSP) systems working at >700°C. The HEA itself would be used in high-temperature tubing to carry molten salts or supercritical CO 2 , while its surface oxide would act as a high-efficiency solar thermal absorber. With Fe and Mn being the major components in these HEAs (adding up to ~70 at.% of the alloy), these materials are much more cost-effective than the Ni-based superalloys currently being investigated for high-temperature CSP systems. Through this research, these Fe-Mn based HEAs have demonstrated yield strengths 2-3x greater than that of stainless steel at 700°C and a creep lifetime >800 h at 700ºC under a typical CSP tubing mechanical load of 35 MPa. Their Mn-rich surface oxides maintain a high optical-to-thermal conversion efficiency of ~87% under 1000x solar concentration ratio for 20 simulated day-night thermal cycles between 750ºC and room temperature. In preliminary corrosion studies, these HEAs have sustained immersion in unpurified bromide molten salts for 14 days at 750°C with <2% weight loss, in contrast to 70% weight loss from a 316 stainless steel reference. The simultaneous achievement of promising mechanical, optical, and thermochemical properties in this FeMnNiAlCr system opens the door to new applications of HEAs in solar energy harvesting. Partnerships with Ames Laboratory and Oak Ridge National Laboratory (ORNL) also advanced our understanding of the fundamental structure-property relationships through atomic scale material characterization and first-principles computational modeling. The key research results in this project can potentially be extended to other HEAs and their native oxides. In terms of applications, the proposed FeMnNiAlCr HEA/native oxide system could potentially exceed the mechanical and the optical performance of existing tubing and solar coating materials under EERE’s CSP program at lower cost, which also aligns well with the EPSCoR Science and Technology strategies of New Hampshire in boosting the deployment of renewable energy.

14 SOLAR ENERGY↗

High Temperature Ternary Chloride Molten Salt Pump

This work investigates the design criteria considering thermal, structural, and material selection of a ternary chloride (MgCl2-NaCl-KCl) molten salt pump that is capable of running at temperatures above 720 °C. In this work, preliminary testing of salt-wetted hydrodynamic bearings was done to investigate different material pairings including Colmonoy grades, Stellite grades, and a novel Nickel Tungsten Carbide alloy (HybrimetTM NiWC3b) used as a High Velocity Oxygen Fuel (HVOF) coating. The coating has shown to withstand the corrosive nature of the molten salt. The pump wetted components are made of Inconel 625 and features a carbon ring seal (CIRPAC Seal) flooded with a N2 gas flow on the overhead to keep salt vapors from interacting with the external ambient air. A comprehensive pump test program has been completed. Over 90 hours run time pumping hot chloride salts at temperatures up to 720 °C in which enough data was captured to produce performance curves at 3 different operating speeds. This research showcases a promising design for use in the Concentrated Solar Power (CSP) Gen 3 liquid-pathway and sets the ground for further development and use of the HybrimetTM NiWC3b as a competitive alternative to available superalloys.

14 SOLAR ENERGY↗

Final report on assessment of molten salt corrosion testing of unirradiated and ion irradiated advanced manufactured high entropy alloys

Generation IV reactors and future fusion reactor designs have led to more demanding materials performance requirements due to their increased operating temperatures, corrosive coolants, and increased radiation doses compared to the current light-water reactor fleet. Among the innovative nuclear technologies under development, molten salt reactors stand out for their potential to offer superior fuel utilization, intrinsic safety characteristics, and economic viability. Of the proposed Generation IV designs, the gas fast reactor operates at 450 to 850°C and the molten salt reactor operates at 565 to 850°C, with the molten salt reactor design needing molten salt corrosion resistant materials [1, 2]. These increased temperatures and more extreme corrosion environments necessitate higher material performance, such as creep strength, radiation-tolerant microstructures, corrosion resistance, and high-temperature tensile properties. Hastelloy-N, a nickel-based alloy with additions of molybdenum and chromium, has been successfully employed to contain molten fluoride salt at temperatures up to 705°C. However, Hastelloy-N becomes embrittled upon neutron irradiation, primarily due to the accumulation of helium produced by (n,a) transmutation reactions. Furthermore, the corrosive nature of molten fluoride and chloride salts presents a formidable challenge, as these salts can react with and dissolve alloying elements such as Cr, Mo, and Fe, leading to selective leaching, loss of protective oxide layers, and accelerated degradation. High entropy alloys (HEAs) and refractory high entropy alloys (RHEAs) have emerged as a prominent area of interest, due to their ability to achieve tailored chemical compositions for specific applications. Unlike conventional alloys, HEAs are characterized by having multiple principal elements in equimolar or near equimolar ratios, leading to an unconventional alloying strategy [3]. This alloying strategy is believed to promote unique properties, such as single-phase stabilization of chemically compatible elements, lattice distortion effects due to atomic radius differences, and proposed sluggish diffusion effects. For extreme-environment applications, RHEAs have garnered much research interest because of the possibility of creating relatively ductile materials that can operate in extremely high-temperature environments, beyond the operating temperatures where other Ni-based superalloys begin to lose strength [4-6]. Idaho National Laboratory (INL) initiated a joint international effort with the Czech Republic to explore the feasibility of manufacturing HEAs for high-temperature nuclear applications using advanced manufacturing. This effort was funded at INL by the United States Department of Energy's Office of Nuclear Energy under the Advanced Reactor Technologies and Advanced Materials and Manufacturing Technologies (AMMT) Program. The HEAs were specifically designed for the corrosive and irradiation environments experienced in gas-cooled fast reactors, molten salt reactors, and fusion power. These alloys have been manufactured by multiple processes to determine the impact of manufacturing processes on the performance of the alloys in corrosive and irradiation environments. Preliminary molten salt corrosion testing showed that equimolar MoNbTiV and MoNbTi alloys exhibit exceptional performance, with arc-melted variants demonstrating only minimal degradation after 1000 hours of exposure to molten chloride salt at 700°C. Conversely, Nb2TiVZr2 showed significant molten salt corrosion susceptibility and microstructural instability during high-temperature molten salt exposures, and was, therefore deemed unfit for molten salt reactor applications. The MoNbTiV, MoNbTi, and Nb2TiVZr2 alloys were further evaluated through ion irradiation experiments conducted at the Michigan Ion Beam Laboratory at the University of Michigan. The microstructural stability and the evolution of irradiation-induced defects were characterized to assess the irradiation resistance of each of these alloys.

36 - MATERIALS SCIENCE↗

Oxidation of Materials and Coatings at 1000°C and 250 bar for use in Oxy-Combustion Turbine

Combinations of materials and coatings were tested in supercritical CO2 (sCO2) to evaluate their reliability in an oxy-fuel turbine being designed to operate in the 150-300 MWe size range at inlet temperatures of 1,150 °C at 300 bar and exhaust temperatures in the 725-775 °C range. Nickel alloys and stainless steels were exposed to supercritical CO2 at 1,000 °C and 250 bar for a total of over 1,500 hours. The materials were tested bare, with a nanocrystalline MCrAlY bond coat only, or with one of two types of bond coat and a thermal barrier coating. A novel test facility using a localized heat zone generated by an induction heater inside an externally cooled autoclave was developed to perform those tests. The specimens were weighed before and after exposure to determine the oxidation rate. All specimens were inspected visually, and a smaller group of coated specimens were studied using secondary electron microscopy (SEM). The integrity of the coating, and the morphology and composition of the thermally grown oxide were especially of interest for the SEM investigation. This paper presents the up-to-date results of the testing coated and uncoated superalloys in sCO2 at up to 1150 °C and up to 300 bar performed at Southwest Research Institute.

Bocher, Florent [Southwest Research Institute, San↗

Testing of Materials and Coatings at up to 1150°C and 300 bar for use in Oxy-Combustion Turbine

Various materials that may be used in a supercritical carbon dioxide (sCO2) oxy-fuel turbine in the 150-300 MWe size range are being evaluated in various environments of interest. The inlet of the turbine must be capable of 1,150 °C at 300 bar and the exhaust temperature is expected to be within the 725-775 °C range. The design requirements are pushing the known limits of high temperature materials. Little is known about the oxidation of the metallic alloys considered for turbine nozzles and blades or about the resilience of thermal management solutions, such as thermal barrier coatings (TBC), required to accommodate these high temperatures. The combinations of high temperature resistant materials and coatings must be tested in sCO2 to evaluate their reliability in an oxy-fuel turbine environment. A total of 13 alloys were chosen to be tested. They included bare samples, with nano deposited MCrAlY bond coat only, or with the addition of a TBC. A unique test facility was developed to expose those materials in sCO2 at up to 300 bar and 1150 °C for up to 5,000 hours. This was accomplished by placing an induction heater inside an autoclave to achieve those high temperature locally while the pressurized vessel is cooled externally. The specimens are weighed before and after exposure to determine the oxidation rate. The integrity, morphology, and composition of some of the coatings and thermally grown oxide will be investigated by scanning electron microscopy (SEM). This paper presents the up-to-date results of the testing coated and uncoated superalloys in sCO2 at up to 1150 °C and up to 300 bar performed at Southwest Research Institute.

Bocher, Florent↗

Multi-Modal Characterization of Interfacial Corrosion of Ni-based Alloys in Chloride-based Molten Salts

The United States Department of Energy (DOE) is committed to the advancement of nuclear reactor technology through initiatives such as the Advanced Reactor Development Program (ARDP), to diversify the United States energy portfolio towards more sustainable energy options. The ARDP includes demonstration by industry partners of molten salt fast reactors (MSRs). Construction of molten salt reactor technology requires qualified nuclear structural materials. Unfortunately, there are no current materials that meet current qualification requirements dictated by the Nuclear Regulatory Commission for construction of MSRs. Adapting current structural material qualifications requires expansion of our current knowledgebase on corrosion performance. In this investigation, we assess microstructural changes in a Ni-based superalloy after exposure to a chloride-containing salt system through a correlated multi-modal approach combining several advanced characterization techniques. Namely we will highlight the impact of grain boundary phenomena at the onset of corrosion attack, including the role of intergranular crack propagation and development of internal corrosion products. The findings from this investigation will further expand our assessment of the corrosion performance of structural materials being investigated for construction of MSR components.

36 - MATERIALS SCIENCE↗

Influence of interrupted cooling on the development of bimodal γ' precipitate distributions in ATI 718Plus

The influence of aging treatments on the evolution of the γ' precipitates in ATI 718Plus was studied using scanning electron microscopy, energy dispersive spectroscopy, transmission electron microscopy, and atomic probe tomography. A set of aging treatments was performed on solution-treated samples to obtain various γ' size distributions. The aging temperatures ranged from 720 to 900°C with holding times of either two hours (for the 900°C aging temperature) or 10 h (for the 720°C and 750°C aging temperatures) followed by either air cooling, furnace cooling, or water quenching. The cooling method and aging temperature influenced the distribution of the solute elements. This work discussed the evolution of the γ' precipitation during single-step aging and two-step aging involving continuous cooling or interrupted cooling. Finally, a bimodal size distribution of the γ' precipitates was obtained through interrupted cooling two-step aging treatments, while single-step aging resulted in unimodal γ' precipitate distributions.

36 MATERIALS SCIENCE↗

Exploring Material Solutions for Supercritical CO 2 Applications above 800 °C

There has been recent interest in exploring revolutionary supercritical CO 2 (sCO 2 ) power cycles, and this exploratory investigation was seeking materials with CO 2 compatibility at up to 1200 °C. Here, initial exposures were conducted at 0.1 and 2 MPa CO 2 for up to 1000 h at 900–1200 °C. As expected, specimens of Mo and W that might be used as matrix materials in cermets were rapidly attacked under these conditions. Even an alumina-forming FeCrAlMo alloy showed high mass gains in less than 100 h at 1200 °C due to the formation of Fe-rich oxide. However, at 900–1100 °C, more protective behavior was observed for FeCrAlMo specimens, with or without pre-oxidation, in 0.1 MPa CO 2 , but increased attack was observed in 2 MPa CO 2 . In contrast, most Ni-based alloys exposed at 900–1100 °C showed higher mass gains and thicker reaction products than formed in air. Thus, Ni-based alloys appear less compatible with CO 2 environments above 800 °C compared to lower temperatures. Low mass gains were observed for CVD SiC at 900–1200 °C, but MoSi 2 and Mo(Si,Al) 2 specimens did not form protective scales under these conditions at 1000 and 1100 °C.

36 MATERIALS SCIENCE↗

High-Temperature Corrosion of Chromia-Forming Ni-Based Alloys in CO 2 Containing Impurities

Future technologies require structural materials resistant to environmental degradation in high-temperature CO 2 -rich environments. In this work, we exposed several commercially available Ni-based alloys (230, 263, 282, 617, 625, and 740H) to atmospheric pressure gases intended to simulate the compositions expected in future direct-fired supercritical CO 2 power cycles. The alloys were exposed to 95% CO 2 + 4% H 2 O + 1% O 2 and the same gas containing 0.1% SO 2 at temperatures of 600, 650, 700, 750, and 800 °C for 2500 h. With minor exceptions, chromia scales formed on all alloys at all temperatures in the SO 2 -free gas, yielding parabolic growth rates that followed an Arrhenius temperature dependence. Behavior in the SO 2 -containing gas was more complex. Generally, the alloys performed well at temperatures of 650, 750, and 800 °C. While some alloys further performed relatively well across the whole temperature range, several of the alloys experienced chromia failure resulting in non-protective duplex oxide scales and high oxidation rates, at temperatures of 600 and 700 °C. Deviation from protective behavior was associated with internal sulfide formation and, additionally for the case of 600 °C, external sulfate formation. Extensive carburization accompanied growth of the non-protective duplex oxide scales, which made it more difficult for the alloy to recover after initiation of the sulfur-induced accelerated corrosion process. The thermodynamic and kinetic factors influencing the accelerated corrosion in the presence of sulfur are discussed. The results suggest that caution is required when assessing compatibility of Ni-based alloys for CO 2 -based systems when sulfur-based impurities are expected.

36 MATERIALS SCIENCE↗

Long-Term Creep-Rupture Behavior of Alloy Inconel 740/740H

To explore potential application of Ni-based alloys for power generation at the higher temperatures and pressures needed to achieve high thermal to electrical-energy conversion efficiency, an extensive creep-rupture dataset covering up to 875 °C and almost 70,000 h for Inconel 740/740H was analyzed using Larson–Miller parameter and Wilshire approaches. The results were used to assess the relative effectiveness of the two analytical methods, both in describing the experimental data and, because of the breadth of the dataset, using analyses of its shorter-time data to make creep lifetime predictions for much more extended times, which were then directly compared to the measured rupture times. The respective methods were also used to predict creep-limited lifetimes relevant to power production (that is, 100,000 h or greater). Despite the complexity of the precipitation-strengthened Inconel 740/740H alloy and the generalized parametric approach of these methodologies, the predictions based on such were reasonably accurate when the entire dataset was analyzed. However, when the analysis was confined to only data for conditions yielding creep-rupture times < 5,000 h( about 65 % of the entire dataset), the Wilshire correlation yielded better prediction for longer time lifetimes due to the inherent instability of the specific Larson–Miller formalism used in this analysis when extrapolated significantly outside its analysis range.

36 MATERIALS SCIENCE↗

Powder Metallurgy HIP Process Study and Mechanical Property Evaluations for IN740H

The effects of hot isostatic pressing (HIP) parameters and powder size distribution (PSD) on the resulting microstructure and properties of powder metallurgy (P/M) IN740H have been investigated. Properties can be substantially tailored through the appropriate management of these parameters. Applying a thermal presoak to the input powder prior to the sintering stage of HIP can significantly increase average grain size and coarse grain fraction, enabling a trade for improved creep resistance at the expense of tensile strength. Here, powder thermal presoak was found to have a larger impact on microstructure and properties than the use of a coarser PSD alone. Additionally, substantial grain growth and grain boundary migration is observed in P/M IN740H at HIP temperatures above 1260°C. Given its inherently finer grain size, P/M HIP IN740H typically outperforms its cast and wrought counterparts in tensile response. Creep life at 700–800°C was inferior to wrought due to PPBs coincident with grain boundaries which served as cavity nucleation sites, leading to lower creep ductility. The ability to adjust the microstructure toward a more balanced creep and tensile behavior allows P/M HIP IN740H to be considered for high-temperature applications in advanced ultra-supercritical steam and supercritical carbon dioxide power cycles.

36 MATERIALS SCIENCE↗

A complete grain-level assessment of the stress-strain evolution and associated deformation response in polycrystalline alloys

Polycrystalline alloys are used pervasively across structural applications contingent upon extensive experimental testing. A statistically representative number of tests are required to expose the variability in the material's performance, as a result of non-uniform microstructures and associated micromechanical fields. In a more direct means of capturing this pertinent information, multi-modal experimental techniques are presented to measure and track the complete micromechanical state, evolving during loading, of each and every grain within the regions of interest. Specifically, a combination of high-energy X-ray diffraction microscopy and digital image correlation coupled with electron backscatter diffraction are conducted on a specimen for each of the alloys, Haynes 282 and Ti7Al. The results of the multi-modal analysis definitively demonstrate that the degree of heterogeneity increases with deformation level and is used to assess the number of grains necessary for a representative volume element description of the stress state for each of these materials. Moreover, higher resolution imaging is used for identification of the slip system activity and subsequently used to study slip transmission events. An accurate knowledge of the resolved shear stress in adjacent grains (grain interactions) is demonstrated to be a key descriptor of the slip transmission events.

36 MATERIALS SCIENCE↗

Development of grain-scale slip activity and lattice rotation fields in Inconel 718

Using a combination of in-situ high-resolution digital image correlation (HR-DIC), Heaviside-DIC method (H-DIC), and crystal plasticity finite element (CPFE), we investigate the evolution of intragranular lattice rotations and slip activity during monotonic and cyclic loading in a high performance, polycrystalline face centered cubic material. The CPFE employs a quasi-3D model microstructure, which is a highly resolved mirror representation of the experimental in-situ test sample. In agreement, the measurements and calculations reveal that most grains, regardless of their size and lattice orientation, develop intragranular lattice rotation gradients that span the grain. For a small cluster of grains on the deformed material, we perform HR-DIC analysis of slip lines to demonstrate agreement in the active slip systems and changes in this local slip activity across the individual grains. The combined analysis reveals that deforming grains are divided into sub-granular regions of uniform lattice rotation and these regions are most often associated with only one or two active slip systems. The gradient lines that divide them correspond to changes in the predominant slip system. The model is used to examine the evolution of intragranular lattice rotation in a single fully reversed tension-compression cycle. The calculations indicate that intragranular gradients intensify during the reverse loading path as nearest neighboring regions appear to shed lattice rotation, increasing the lattice rotation in some regions, while shutting down rotation in neighboring regions. So these findings provide insight into the irreversible changes that develop within deforming grains at the scale of the grain, particularly the heterogeneous development of intragranular lattice rotation in early stages of deformation, which could serve as precursors to localization.

36 MATERIALS SCIENCE↗

Temperature-dependent mechanical properties and crystal plasticity parameters for additively manufactured Haynes-214 alloy: Experiments and numerical modeling

Our experimental mechanical testing data demonstrated that the additively manufactured (AM) laser powder bed fusion (L-PBF) Haynes-214 alloy exhibits non-linear mechanical properties as the temperature rises from ambient to 870 °C. Crystal plasticity (CP) simulations provide an effective approach to gaining deeper insights into microstructure-property linkages under thermomechanical loading. This method can reduce the need for costly high-temperature mechanical testing while accounting for the effects of crystallographic texture and grain morphology on the mechanical behavior of AM materials. However, calibrating a CP model is time-consuming because individual simulations are computationally expensive and hundreds (or more) of iterations over parameter sets may be required. To address this issue, we have designed a machine learning-differential evolution (ML-DE) CP framework that can accurately interpolate the tensile properties of AM L-PBF Haynes-214 alloy across a wide temperature range from ambient to 870 °C, with minimal reliance on experimental data. The framework uses electron backscatter diffraction (EBSD) measurements to generate statistically equivalent microstructural volume elements to serve as inputs to the CP modeling framework. Stress–strain curves were generated from 1000 CP simulations, which serve as the training data set for the three ML regression algorithms explored: linear, extra-trees, and multi-layer perceptron. These three regression models were independently evaluated to compare their efficiency and identify the most suitable algorithm for the given problem. Results revealed that the extra-trees ML regressor outperforms the other models in both qualitative and quantitative aspects with an R 2 of 0.98. Subsequently, the differential evolution optimization approach is employed to calibrate the ML-based CP material parameters with experimental results obtained at various temperatures. Finally, temperature-dependent CP material parameters are formulated. The effectiveness and efficiency of the designed framework are validated through comparison with experimental results, demonstrating a high degree of agreement. These calibrated parametric constitutive equations enable further use of the CP model to study the deformation behavior of this alloy under a wide range of thermo-mechanical loading conditions.

36 MATERIALS SCIENCE↗