Search NASA⌕ Search

SEARCH · Search NASA

Results for “thermal effect”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 325 records · Page 18

The effects of thermal accretion disk spectra on the emission lines from active galactic nuclei

Although most ratios of AGN emission lines depend primarily on global averages over the ionizing spectrum of the thermal accretion disk, there are some which behave quite differently for different spectra. Using these, it may be possible to infer the shape of the spectrum in the unobservable ultraviolet. Two classes of methods for making this inference are discussed, one based upon as many line ratios as can be observed, the other singling out those best at distinguishing different spectral shapes. Because of a variety of technical difficulties, only the first class, which uses global measures of goodness-of-fit, is practical. Application of this method to a compilation of quasar line ratios yields a weak conclusion, however, with the best fit favoring the presence of a thermal accretion disk with T(b) of roughly 20 eV.

Krolik, Julian H.↗

Crystal growth of CdTe in space and thermal field effects on mass flux and morphology

The primary, long-range goals are the development of vapor phase crystal growth experiments, and the growth of technologically useful crystals in space. The necessary ground-based studies include measurements of the effects of temperature variations on the mass flux and crystal morphology in vapor-solid growth processes. For in-situ mass flux measurements dynamic microbalance techniques will be employed. Crystal growth procedures and equipment will be developed to be compatible with microgravity conditions and flight requirements. Emphasis was placed on the further development of crystal growth and the investigation of relevant transport properties of CdTe. The dependence of the mass flux on source temperature was experimentally established. The CdTe synthesis and pretreatment procedures are being developed that yield considerable improvements in mass transport rates, and mass fluxes which are independent of the amount of source material. A higher degree of stoichiometric control of CdTe than before was achieved during this period of investigation. Based on this, a CdTe crystal growth experiment, employing physical vapor transport, yielded very promising results. Optical microscopy and X-ray diffraction studies revealed that the boule contained several large sized crystal grains of a high degree of crystallinity. Further characterization studies of CdTe crystals are in progress. The reaction chamber, furnace dimensions, and ampoule location of the dynamic microbalance system were modified in order to minimize radiation effects on the balance performance.

Wiedemeier, H.↗

The effect of thermal damage on the mechanical properties of polymer regrinds

Reprocessed polymers are subjected to high processing temperatures that result in the breakdown of molecular chains and changes in the molecular structures. These phenomena are reflected in the mechanical properties of materials. Practically every regrind is seen as a new material. These experiments deal with the molding, regrinding, and reprocessing of test specimens for the study of their mechanical properties. The comparative test data from each recycled material would give students an insight of the molecular structures and property degradation. Three important rheological and mechanical properties such as melt flow, impact strength, and flexural strength are to be determined. These properties play key roles in the selection of engineering materials. The material selected for demonstration was Makrolon 3000L, a polycarbonate thermoplastic from Bayer AG. The thermal degradation due to repeated processing is reflected in the decrease in molecular weight and breakdown of molecular chains causing increase in melt flow. The Izod-impact resistance and the flexural strength deteriorate gradually.

Kundu, Nikhil K.↗

Investigation of the effect of thermal exposure on the mechanical properties of titanium/SiC composites

The objective was to evaluate the influence of thermal exposure, both isothermal and cyclic, on the reaction kinetics, mechanical properties and fracture behavior of Ti-1100 alloy/SiC fiber composites. Previously, it was determined that composites made with TiB2 coated SiC fiber (sigma) reacted at the same rate as SCS-6 fibers. As a result, the thinner surface coating on the Sigma fiber was completely consumed at shorter times than that on the SCS-6. Thermal cycling experiments were conducted on longitudinal and transverse Ti-1100/SCS-6 composites over a temperature range of 150 to 800 C for 500 cycles. The thermal exposures were carried out in air and argon. No appreciable tensile strength degradation was observed for samples cycled in argon, although a strength loss was noted for the samples cycled in air. Fracture surfaces characterization showed brittle matrix failure in regions near the surface and in regions where there was a path for O2 ingress.

Gundel, Douglas B.↗

Effect of thermal shock on fiber-reinforced superalloy composites

An evaluation is presented of the thermal shock behavior of tungsten fiber-reinforced superalloy (FRS) composites with respect to the turbine blade requirements of rocket engine turbopumps. Each composite was reinforced unidirectionally with 40-volume-pct continuous tungsten fibers. The start-up conditions of the first-stage turbine blades of the high-pressure fuel turbopump in the Space Shuttle Main Engine (SSME) were used to investigate the thermal shock behavior of these materials. The FRS composites showed excellent thermal shock resistance, two to nine times better than the turbine blade material used in the SSME. Thermal shock cycling produced microcracks on the surfaces of the irradiated area that were less than 0.13 mm long and 0.005 mm deep. Neither fiber/matrix debonding nor microvoiding was observed.

Yuen, J. L.↗

Measurements of the effects of thermal contact resistance on steady state heat transfer in phosphoric-acid fuel cell stack

The influence of the thermal contact resistance on the heat transfer between the electrode plates, and the cooling system plate in a phosphoric-acid fuel-cell stack was experimentally investigated. The investigation was conducted using a set-up that simulates the operating conditions prevailing in a phosphoric acid fuel-cell stack. The fuel-cell cooling system utilized three types of coolants, water, engine oil, and air, to remove excess heat generated in the cell electrode and to maintain a reasonably uniform temperature distribution in the electrode plate. The thermal contact resistance was measured as a function of pressure at the interface between the electrode plate and the cooling system plate. The interface pressure range was from 0 kPa to 3448 kPa, while the Reynolds number for the cooling limits varied from 15 to 79 for oil, 1165 to 6165 for water, and 700 to 6864 for air. Results showed that increasing the interface pressure resulted in a higher heat transfer coefficient.

Abdul-Aziz, Ali↗

Effect of thermal cycling on interface bonding requirements in Al2O3 fiber-reinforced superalloy composites

CTE (coefficient of thermal expansion) mismatch-induced stresses as they affect the fiber-matrix bond integrity of Al2O3 fiber-reinforced superalloy composites are examined. Of the three individual stress components, only the radial stress directly affects the integrity of the fiber-matrix interface. It is noted that a compressive radial stress leads to a clamping action on the fiber and is therefore beneficial to the integrity of the fiber-matrix bond. A radial tensile stress, on the other hand, can cause debonding of the fiber from the matrix for a weak fiber-matrix bond.

Misra, Ajay K.↗

Thermal history effects on electrical relaxation and conductivity for potassium silicate glass with low alkali concentrations

Electrical response measurements from 10 Hz to 100 kHz between 120 and 540 C were made on potassium-silicate glasses with alkali oxide contents of 2, 3, 5 and 10 mol percent. Low alkali content glasses were chosen in order to try to reduce the Coulombic interactions between alkali ions to the point that frozen structural effects from the glass could be observed. Conductivity and electrical relaxation responses for both annealed and quenched glasses of the same composition were compared. Lower DC conductivity (sigma(sub DC)) activation energies were measured for the quenched compared to the annealed glasses. The two glasses with the lowest alkali contents exhibited a non-Arrhenius concave up curvature in the log(sigma(sub DC)) against 1/T plots, which decreased upon quenching. A sharp decrease in sigma(sub DC) was observed for glasses containing K2O concentrations of 5 mol percent or less. The log modulus loss peak (M'') maximum frequency plots against 1/T all showed Arrhenius behavior for both annealed and quenched samples. The activation energies for these plots closely agreed with the sigma(sub DC) activation energies. A sharp increase in activation energy was observed for both series as the potassium oxide concentration decreased. Changes in the electrical response are attributed to structural effects due to different alkali concentrations. Differences between the annealed and quenched response are linked to a change in the distribution of activation energies (DAE).

Angel, Paul W.↗

Effects of thermal and moisture cycling on the internal structure of stitched RTM laminates

Conventional aerospace composites are strong and stiff in the directions parallel to the carbon fibers, but they are prone to delaminations and damage in the through-the-thickness directions. Recent research has shown that substantial improvements in damage tolerance are obtained from textile composites with Z-direction reinforcement provided by stitching, weaving, or braiding. Because of the mismatch in thermal and moisture expansion properties of the various material components, there is a potential for microcracks to develop in the resin matrix. These cracks can form to relieve the mechanical stresses that are generated during curing or in-service temperature cycles.

Walker, Jeff↗

Effects of thermal and electrical stressing on the breakdown behavior of space wiring

Several failures in the electrical wiring systems of many aircraft and space vehicles have been attributed to arc tracking and damaged insulation. In some instances, these failures proved to be very costly as they have led to the loss of many aircraft and imperilment of space missions. Efforts are currently underway to develop lightweight, reliable, and arc track resistant wiring for aerospace applications. In this work, six wiring constructions were evaluated in terms of their breakdown behavior as a function of temperature. These hybrid constructions employed insulation consisting of Kapton, Teflon, and cross-linked Tefzel. The properties investigated included the 400 Hz AC dielectric strength at ambient and 200 C, and the lifetime at high temperature with an applied bias of 40, 60, and 80% of breakdown voltage level. The results obtained are discussed, and conclusions are made concerning the suitability of the wiring constructions investigated for aerospace applications.

Hammoud, Ahmad↗

Investigation of Thermal Creep and Thermal Stress Effects in Microgravity Physical Vapor Transport

Reported here are the results of our numerical investigation into the mechanisms which affect the transport and growth processes in physical vapor transport (PVT) crystal growth ampoules. The first part of the report consists of a brief summary of the major accomplishments and conclusions of our work. The second part consists of two manuscripts, submitted to the Journal of Crystal Growth, which provided a detailed description of the findings in our investigation.

Mackowski, D. W.↗

Experimental Investigation at Mach Number 3.0 of the Effects of Thermal Stress and Buckling on the Flutter of Four-Bay Aluminum Alloy Panels with Length-Width Ratios of 10

Skin-stiffener aluminum alloy panels consisting of four bays, each bay having a length-width ratio of 10, were tested at a Mach number of 3.0 at dynamic pressures ranging from 1,500 psf to 5,000 psf and at stagnation temperatures from 300 F to 655 F. The panels were restrained by the supporting structure in such a manner that partial thermal expansion of the skins could occur in both the longitudinal and lateral directions. A boundary faired through the experimental flutter points consisted of a flat-panel portion, a buckled-panel portion, and a transition point at the intersection of the two boundaries. In the region where a panel must be flat when flutter occurs, an increase in panel skin temperature (or midplane compressive stress) makes the panel more susceptible to flutter. In the region where a panel must be buckled when flutter occurs, the flutter trend is reversed. This reversal in trend is attributed to the panel postbuckling behavior.

Dixon, Sidney C.↗

Thermal Processing Effects on the Adhesive Strength of PS304 High Temperature Solid Lubricant Coatings

In this paper the effects of post deposition heat treatments on the cohesive and adhesive strength properties of PS304, a plasma sprayed nickel-chrome based, high temperature solid lubricant coating deposited on stainless steel, are studied. Plasma spray deposited coating samples were exposed in air at temperatures from 432 to 650 C for up to 500 hr to promote residual stress relief, enhance particle to particle bonding and increase coating to substrate bond strength. Coating pull-off strength was measured using a commercial adhesion tester that utilizes 13 mm diameter aluminum pull studs attached to the coating surface with epoxy. Pull off force was automatically recorded and converted to coating pull off strength. As deposited coating samples were also tested as a baseline. The as-deposited (untreated) samples either delaminated at the coating-substrate interface or failed internally (cohesive failure) at about 17 MPa. Samples heat treated at temperatures above 540 C for 100 hr or at 600 C or above for more than 24 hr exhibited strengths above 31 MPa, nearly a two fold increase. Coating failure occurred inside the body of the coating (cohesive failure) for nearly all of the heat-treated samples and only occasionally at the coating substrate interface (adhesive failure). Metallographic analyses of heat-treated coatings indicate that the Nickel-Chromium binder in the PS304 appears to have segregated into two phases, a high nickel matrix phase and a high chromium precipitated phase. Analysis of the precipitates indicates the presence of silicon, a constituent of a flow enhancing additive in the commercial NiCr powder. The exact nature and structure of the precipitate phase is not known. This microstructural change is believed to be partially responsible for the coating strength increase. Diffusion bonding between particles may also be playing a role. Increasing the heat treatment temperature, exposure time or both accelerate the heat treatment process. Preliminary measurements indicate that the heat treatment also results in a one time, permanent coating thickness increase of about 3%. Based upon these results, the incorporation of a heat treatment prior to final finishing has been incorporated in the application process of this coating technology.

DellaCorte, Christopher↗

Effect of Thermal Exposure on the Tensile Properties of Aluminum Alloys for Elevated Temperature Service

Tensile properties were evaluated for four aluminum alloys that are candidates for airframe applications on high speed transport aircraft. These alloys included the Al-Cu-Mg-Ag alloys C415 and C416 and the Al-Cu-Li-Mg-Ag alloys RX818 and ML377. The Al-Cu-Mg alloys CM001, which was used on the Concorde SST, and 1143, which was modified from the alloy used on the TU144 Russian supersonic aircraft, were tested for comparison. The alloys were subjected to thermal exposure at 200 F, 225 F and 275 F for times up to 30,000 hours. Tensile tests were performed on thermally-exposed and as-received material at -65 F, room temperature, 200 F, 225 F and 275 F. All four candidate alloys showed significant tensile property improvements over CM001 and 1143. Room temperature yield strengths of the candidate alloys were at least 20% greater than for CM001 and 1143, for both the as-received and thermally-exposed conditions. The strength levels of alloy RX818 were the highest of all materials investigated, and were 5-10% higher than for ML377, C415 and C416 for the as-received condition and after 5,000 hours thermal exposure. RX818 was removed from this study after 5,000 hours exposure due to poor fracture toughness performance observed in a parallel study. After 30,000 hours exposure at 200 F and 225 F, the alloys C415, C416 and ML377 showed minor decreases in yield strength, tensile strength and elongation when compared to the as-received properties. Reductions in tensile strength from the as-received values were up to 25% for alloys C415, C416 and ML377 after 15,000 hours exposure at 275 F.

Edahl, Robert A., Jr.↗