SEARCH · Search NASA
Results for “Creep rupture”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Influence of Temperature on Creep, Stress-rupture and Static Properties of Melamine-resin and Silicone-resin Glass-fabric Laminates
Explore the source record for details and available documents.
Creep/Stress Rupture Behavior and Failure Mechanisms of Full CVI and Full PIP SiC/SiC Composites at Elevated Temperatures in Air
SiC/SiC composites fabricated by melt infiltration are being considered as potential candidate materials for next generation turbine components. However these materials are limited to 2400 F application because of the presence of residual silicon in the SiC matrix. Currently there is an increasing interest in developing and using silicon free SiC/SiC composites for structural aerospace applications above 2400 F. Full PIP or full CVI or CVI + PIP hybrid SiC/SiC composites can be fabricated without excess silicon, but the upper temperature stress capabilities of these materials are not fully known. In this study, the on-axis creep and rupture properties of the state-of-the-art full CVI and full PIP SiC/SiC composites with Sylramic-iBN fibers were measured at temperatures to 2700 F in air and their failure modes examined. In this presentation creep rupture properties, failure mechanisms and upper temperature capabilities of these two systems will be discussed and compared with the literature data.
Experimental evaluation of localized creep deformation in grade 91 steel weldments
Spatially resolved measurement of localized creep deformation in heterogeneous creep resistant steel weldments is crucial but challenging for lifetime assessments of critical steam components in power plants. Here, experimental approaches were established to quantitatively evaluate commonly observed localized creep deformation in multi-pass Grade 91 steel weldments. An in-situ digital image correlation (DIC) system was utilized with a creep testing frame to monitor and measure both full-field strain and localized strain accumulation across the weldments during long-term creep testing at elevated temperatures. The in situ DIC method measured not only the creep deformation behavior of the weld metal, heat affected zone (HAZ), and base metal, but also creep strain evolution for each sub-region within the HAZ itself, including coarse-grained HAZ, fine-grained HAZ (FGHAZ), and intercritical HAZ (ICHAZ). The DIC results revealed that local creep strain in the ICHAZ reached up to 90% strain before final rupture, whereas nominal creep strain measured by the standard extensometer of the tested cross-weld specimen was below 10%, indicative of Type IV cracking of the Grade 91 weld. Microstructural analyses revealed that the faster creep degradation/deformation in the HAZ was caused mainly by accelerated matrix grain recrystallization/growth and a reduced pinning effect from the segregated and coarsened precipitates in the FGHAZ and ICHAZ. The ultimate creep rupture occurred in the ICHAZ owing to its lowest creep resistance induced by the largest recrystallized grain size, the lowest fraction of coincidence site lattice, and the lowest local strain energies/dislocation densities.
Creep/Rupture Behavior of Melt-Infiltrated SiC/SiC Composites Being Investigated
The failure behavior of melt-infiltrated SiC/SiC ceramic matrix composites is under investigation at the NASA Glenn Research Center as part of NASA's Ultra-Efficient Engine Technology Program. This material was originally developed under the High Speed Research Office's Enabling Propulsion Materials Program. Creep and rupture data provide accelerated testing information to predict material behavior under engine use situations (1500 to 2400 F). This information gives insights into various material development paths to improve composites as well as improve understanding of failure mechanisms. The left figure shows the fracture surface of a CMC material following over 200 hr of testing at 2400 F. This surface demonstrates the kind of fibrous pullout desirable for maximum crack deflection, hence non-brittle failure. Microscopy suggests that creep and rupture of these materials can best be considered as a probabilistic property, rather than a material property. Fiber failure occurs first in isolated regions, while stronger adjacent fibers remain intact. The right figure shows a region where oxide deposits blur and round the fiber images. Because the oxidation kinetics of SiC are well understood, this oxide scale can be used as a measure of the length of time various regions of the composites have been exposed to the environment, hence providing vital information regarding the sequence of failure. The oxide scale in the right figure indicates an early failure of this tow of fibers, whereas adjacent tows remain oxide free, suggesting failure much later in time. The path of various cracks can be followed throughout the composite in this manner, suggesting failure mechanisms.
Determination of structural engineering properties of incoloy 903 and CTX-1 alloys
Tension, notched tension, compression, density, thermal conductivity, and thermal expansion tests were conducted on Incoloy 903 over the temperature range 20 K (-423 F) through 1033 K (1400 F). Fracture toughness tests were performed at room temperature (RT). Creep and rupture tests were conducted at 811 K (1000 F), 922 K (1200 F), and 1033 K (1400 F) for this alloy. Transverse unnotched and notched fatigue tests at R = 0.1 were performed at RT and 922 K (1200 F). For CTX-1 alloy, tension, Charpy V-notch impact, density, thermal conductivity, and thermal expansion tests were conducted over the temperature range 20 K (-423 F) through 1033 K (1400 F). Poisson's ratio was determined at RT, 811 K (1000 F), 922 K (1200 F), and 1033 K (1400 F). Notched tension and compression tests were performed at 20 K (-423 F), RT, and 922 K (1200 F); plane strain fracture toughness tests were conducted at RT, 77 K (-320 F), and 20 K (-423 F). Creep and rupture tests were performed at 811 K (1000 F), 922 K (1200 F), and 1033 K (1400 F); longitudinal unnotched and notched fatigue tests at R = 0.1 were conducted at RT and 922 K (1200 F). Results are presented and discussed.
A linear time-temperature relation for extrapolation of creep and stress-rupture data
Explore the source record for details and available documents.
Ultra High Temperature (UHT) SiC Fiber (Phase 2)
Silicon-carbide fiber-reinforced silicon-carbide ceramic matrix composites (SiCSiC CMC) are emerginglightweight re-usable structural materials not only for hot section components in gas turbine engines, but also for controlsurfaces and leading edges of reusable hypersonic vehicles as well as for nuclear propulsion and reactor components. Ithas been shown that when these CMC are employed in engine hot-section components, the higher the upper usetemperature (UUT) of the SiC fiber, the more performance benefits are accrued, such as higher operating temperatures,reduced component cooling air, reduced fuel consumption, and reduced emissions. The first generation of SiCSiC CMC with a temperature capability of 2200-2400F are on the verge of being introduced into the hot-section components ofcommercial and military gas turbine engines.Today the SiC fiber type currently recognized as the worlds best in terms ofthermo-mechanical performance is the Sylramic-iBN fiber. This fiber was previously developed by the PI at NASA GRC using patented processes to improve the high-cost commercial Sylramic fiber, which in turn was derived from anotherlow-cost low-performance commercial fiber. Although the Sylramic-iBN fiber shows state-of-the art creep and rupture resistance for use temperatures above 2550oF, NASA has shown by fundamental creep studies and model developmentthat its microstructure and creep resistance could theoretically be significantly improved to produce an Ultra HighTemperature (UHT) SiC fiber.This Phase II Seedling Fund effort has been focused on the key objective of effectively repeating the similar processes used for producing the Sylramic-iBN fiber using a design of experiments approach to first understand the cause of the less than optimum Sylramic-iBN microstructure and then attempting to develop processconditions that eliminate or minimize these key microstructural issues. In so doing, it is predicted that that theseadvanced process could result in an UHT SiC fiber with 20 times more creep resistance than the Sylramic-iBN fiber,which in turn would allow SiCSiC CMC to operate up to 2700oF and above, thereby further enhancing the performancebenefits of SiCSiC components in aero-propulsion engines. It was also envisioned that the fiber processes developedduring Phase II efforts would not only reduce production costs for the UHT fiber by using low-cost precursor fibers andcombined processes, but also allow the UHT fibers to be directly produced in preforms of the precursor fibers, possibly atthe facilities of the CMC fabricator.
Fracture of flash oxidized, yttria-doped sintered reaction-bonded silicon nitride
The oxidation behavior of a slip cast, yttria-doped, sintered reaction-bonded silicon nitride after 'flash oxidation' was investigated. It was found that both the static oxidation resistance and flexural stress rupture life (creep deformation) were improved at 1000 C in air compared to those of the same material without flash oxidation. Stress rupture data at high temperatures (1000 to 1200 C) are presented to indicate applied stress levels for oxidation-dependent and independent failures.
Hydrogen environment embrittlement of astroloy and Udimet 700 (nickel-base) and V-57 (iron-base) superalloys
The sensitivity to hydrogen environment embrittlement of three superalloys was determined. Astroloy forgings were resistant to embrittlement during smooth tensile, notched tensile, and creep testing in 3.5-MN/sq m hydrogen over the range 23 to 760 C. The notched tensile strength of Udimet 700 bar stock in hydrogen at 23 C was only 50 percent of the baseline value in helium. Forgings of V-57 were not significantly embrittled by hydrogen during smooth tensile testing over the range 23 to 675 C; creep and rupture lives of V-57 were degraded by hydrogen. Postcreep tensile ductility of V-57 was reduced by 40 percent after creep exposure in hydrogen.
Tensile Creep and Fatigue of Sylramic-iBN Melt-Infiltrated SiC Matrix Composites: Retained Properties, Damage Development, and Failure Mechanisms
An understanding of the elevated temperature tensile creep, fatigue, rupture, and retained properties of ceramic matrix composites (CMC) envisioned for use in gas turbine engine applications are essential for component design and life-prediction. In order to quantify the effect of stress, time, temperature, and oxidation for a state-of-the-art composite system, a wide variety of tensile creep, dwell fatigue, and cyclic fatigue experiments were performed in air at 1204 C for the SiC/SiC CMC system consisting of Sylramic-iBN SiC fibers, BN fiber interphase coating, and slurry-cast melt-infiltrated (MI) SiC-based matrix. Tests were either taken to failure or interrupted. Interrupted tests were then mechanically tested at room temperature to determine the residual properties. The retained properties of most of the composites subjected to tensile creep or fatigue were usually within 20% of the as-produced strength and 10% of the as-produced elastic modulus. It was observed that during creep, residual stresses in the composite are altered to some extent which results in an increased compressive stress in the matrix upon cooling and a subsequent increased stress required to form matrix cracks. Microscopy of polished sections and the fracture surfaces of specimens which failed during stressed-oxidation or after the room-temperature retained property test was performed on some of the specimens in order to quantify the nature and extent of damage accumulation that occurred during the test. It was discovered that the distribution of stress-dependent matrix cracking at 1204 C was similar to the as-produced composites at room temperature; however, matrix crack growth occurred over time and typically did not appear to propagate through thickness except at final failure crack. Failure of the composites was due to either oxidation-induced unbridged crack growth, which dominated the higher stress regime (> 179 MPa) or controlled by degradation of the fibers, probably caused by intrinsic creep-induced flaw growth of the fibers or internal attack of the fibers via Si diffusion through the CVI SiC and/or microcracks at the lower stress regime (< 165 MPa).
Advanced Constituents and Processes for Ceramic Composite Engine Components
The successful replacement of metal alloys by ceramic matrix composites (CMC) in hot-section engine components will depend strongly on optimizing the processes and properties of the CMC microstructural constituents so that they can synergistically provide the total CMC system with improved temperature capability and with the key properties required by the components for long-term structural service. This presentation provides the results of recent activities at NASA aimed at developing advanced silicon carbide (Sic) fiber-reinforced hybrid Sic matrix composite systems that can operate under mechanical loading and oxidizing conditions for hundreds of hours at 2400 and 2600 F, temperatures well above current metal capability. These SiC/SiC composite systems are lightweight (-30% metal density) and, in comparison to monolithic ceramics and carbon fiber-reinforced ceramic composites, are able to reliably retain their structural properties for long times under aggressive engine environments. It is shown that the improved temperature capability of the SiC/SiC systems is related first to the NASA development of the Sylramic-iBN Sic fiber, which displays high thermal stability, creep resistance, rupture resistance, and thermal conductivity, and possesses an in-situ grown BN surface layer for added environmental durability. This fiber is simply derived from Sylramic Sic fiber type that is currently produced at ATK COI Ceramics. Further capability is then derived by using chemical vapor infiltration (CVI) to form the initial portion of the hybrid Sic matrix. Because of its high creep resistance and thermal conductivity, the CVI Sic matrix is a required base constituent for all the high temperature SiC/SiC systems. By subsequently thermo- mechanical-treating the CMC preform, which consists of the S ylramic-iBN fibers and CVI Sic matrix, process-related defects in the matrix are removed, further improving matrix and CMC creep resistance and conductivity.
Advanced SiC/SiC Ceramic Composites For Gas-Turbine Engine Components
NASA Glenn Research Center (GRC) is developing a variety of advanced SiC/SiC ceramic composite (ASC) systems that allow these materials to operate for hundreds of hours under stress in air at temperatures approaching 2700 F. These SiC/SiC composite systems are lightweight (approximately 30% metal density) and, in comparison to monolithic ceramics and carbon fiber-reinforced ceramic composites, are able to reliably retain their structural properties for long times under aggressive gas-turbine engine environments. The key for the ASC systems is related first to the NASA development of the Sylramic-iBN Sic fiber, which displays higher thermal stability than any other SiC- based ceramic fibers and possesses an in-situ grown BN surface layer for higher environmental durability. This fiber is simply derived from Sylramic Sic fiber type that is currently produced at ATK COI Ceramics (COIC). Further capability is then derived by using chemical vapor infiltration (CVI) and/or polymer infiltration and pyrolysis (PIP) to form a Sic-based matrix with high creep and rupture resistance as well as high thermal conductivity. The objectives of this study were (1) to optimize the constituents and processing parameters for a Sylramic-iBN fiber reinforced ceramic composite system in which the Sic-based matrix is formed at COIC almost entirely by PIP (full PIP approach), (2) to evaluate the properties of this system in comparison to other 2700 F Sylramic-iBN systems in which the matrix is formed by full CVI and CVI + PIP, and (3) to examine the pros and cons of the full PIP approach for fabricating hot-section engine components. A key goal is the development of a composite system with low porosity, thereby providing high modulus, high matrix cracking strength, high interlaminar strength, and high thermal conductivity, a major property requirement for engine components that will experience high thermal gradients during service. Other key composite property goals are demonstration at high temperatures of high environmental resistance and high creep resistance, which in turn will result in long component life. Data are presented from a variety of laboratory tests on simple two-dimensional panels that examine these properties and compare the performance of the optimized full PIP system with those of the full CVI and CVI + PIP hybrid systems. Underlying mechanisms for performance differences in the various systems are discussed. Remaining issues for further property enhancement and for application of the full PIP approach for engine components are also discussed, as well as on-going approaches at NASA to solve these issues.
A thermochemical database from high-throughput first-principles calculations and its application to analyzing phase evolution in AM-fabricated IN718
A comprehensive thermochemical database is constructed based on high–throughput first-principles phonon calculations of over 3000 atomic structures in limited concentrations in Ni, Fe, and Co alloys involving a total of 26 elements including Al, B, C, Cr, Cu, Hf, La, Mn, Mo, N, Nb, O, P, Re, Ru, S, Si, Ta, Ti, V, W, Y, and Zr, providing thermochemical data largely unavailable from existing experiments. Here, the database can be employed to predict the equilibrium phase compositions and fractions directly from first-principles by minimizing the chemical potential of a multicomponent system with a fixed overall chemical composition and a fixed temperature. It is applied to the additively manufactured nickel-based IN718 superalloy to analyze the phase evolution with temperature. IN718 is known for its great performance in tensile, fatigue, creep, and rupture strength, combined with easy fabrication and corrosion resistance. In particular, we successfully predicted the formation of L1 0 -FeNi, γ’-Ni 3 (Fe,Al), α-Cr, δ-Ni 3 (Nb,Mo), γ”-Ni 3 Nb, and η-Ni 3 Ti at low temperatures (below 680 K), γ’-Ni 3 Al, δ-Ni 3 Nb, γ”-Ni 3 Nb, α-Cr, and γ-Ni(Fe,Cr,Mo) at intermediate temperatures (between 680 and 1140 K), and δ-Ni 3 Nb and γ-Ni(Fe,Cr,Mo) at high temperatures (above 1140 K) in IN718. These predictions are validated by EDS mapping of compositional distributions and corresponding identifications of phase distributions. The database is expected to be a valuable source for future thermodynamic analysis and microstructure prediction of alloys involving the 26 elements.
Conceptual Designs for Irradiation Creep Testing of SiC in HFIR
Understanding irradiation creep of nuclear fuel cladding is important to properly size the initial fuel-cladding gap and understand when pellet-cladding contact is expected to occur due to a combination of fuel swelling and cladding creep-down. Irradiation creep also plays a role in relaxing stresses that develop in-pile. Silicon carbide fiber–reinforced silicon carbide matrix (SiC/SiC) composites are the leading long-term accident-tolerant fuel cladding concept for light-water reactors (LWRs). Although some limited data are available regarding irradiation creep of the individual constituents (fibers, matrix), data regarding irradiation creep of SiC/SiC composites are currently insufficient. Additional data regarding irradiation creep compliance and the rupture lifetime (combination of creep and slow crack growth) are needed to understand material limitations. This work describes the design and development of two irradiation vehicles that are being pursued for testing SiC/SiC concepts in the High Flux Isotope Reactor (HFIR). The first is a passive experiment, referred to as the PRECISE experiment, that leverages the constant coolant pressure of HFIR to compress a metallic bellows and provide a well-characterized load to drive creep in a SiC/SiC dog bone specimen. The total creep strain would be quantified post-irradiation by measuring dimensional changes of the specimen length as well as local dimensional changes within the gauge region. Non-stressed specimens would also be irradiated under the same conditions to provide an indication of dimensional changes due to radiation-induced swelling in the absence of creep. A second, more complex experiment, referred to as the INSITE experiment, is being designed in parallel that would use pneumatics to pressurize a metal bellows and linear variable differential transformers (LVDTs) to measure the specimen displacement in situ during irradiation. Such an experiment would provide significantly more data regarding the evolution of the creep compliance as a function of dose and applied stress within a single experiment but would require significantly more development time and cost to execute. The primary concern with the INSITE experiment is the accuracy, reliability, and expected lifetime of the LVDTs during irradiation at elevated temperatures. Efforts are being made to adjust the experiment design and operating procedure to limit LVDT temperatures and mitigate or otherwise compensate for uncertainties due to factors such as temperature fluctuations, creep in the surrounding structural materials, and drift of the LVDTs. This work describes the experiment designs, thermal and structural analysis that were performed to ensure that the desired temperature and stress conditions can be achieved, some initial sensitivity analyses to predict the evolution of the radiation-induced specimen displacements, and potential sources of uncertainty in the measurements. Out-of-pile testing is being performed in parallel to confirm that the test trains achieve the expected stress states in the specimens and do not result in prohibitive stress concentrators (e.g., in the grip regions) that might risk pre-mature failure. The PRECISE experiments are proceeding toward fabrication and assembly with HFIR insertion planned during fiscal year 2026. The INSITE experiment is progressing toward out-of-pile demonstrations, which will provide more conclusive evidence regarding the feasibility of executing these tests in HFIR or whether alternative displacement monitoring techniques may need to be considered.
Analysis of temperature and pressure distribution of containers for nuclear waste material disposal in space
A computer program was adapted from a previous generation program to analyze the temperature and internal pressure response of a radioactive nuclear waste material disposal container following impact on the earth. This program considers component melting, LiH dissociation, temperature dependent properties and pressure and container stress response. Analyses were performed for 21 cases with variations in radioactive power level, container geometry, degree of deformation of the container, degree of burial and soil properties. Results indicated that the integrity of SS-316 containers could be maintained with partial burials of either underformed or deformed containers. Results indicated that completely buried waste containers, with power levels above 5 kW, experienced creep stress rupture failures in 4 to 12 days.
Fabrication of aluminum-carbon composites
A screening, optimization, and evaluation program is reported of unidirectional carbon-aluminum composites. During the screening phase both large diameter monofilament and small diameter multifilament reinforcements were utilized to determine optimum precursor tape making and consolidation techniques. Difficulty was encountered in impregnating and consolidating the multifiber reinforcements. Large diameter monofilament reinforcement was found easier to fabricate into composites and was selected to carry into the optimization phase in which the hot pressing parameters were refined and the size of the fabricated panels was scaled up. After process optimization the mechanical properties of the carbon-aluminum composites were characterized in tension, stress-rupture and creep, mechanical fatigue, thermal fatigue, thermal aging, thermal expansion, and impact.
Fabrication of angleply carbon-aluminum composites
A study was conducted to fabricate and test angleply composite consisting of NASA-Hough carbon base monofilament in a matrix of 2024 aluminum. The effect of fabrication variables on the tensile properties was determined, and an optimum set of conditions was established. The size of the composite panels was successfully scaled up, and the material was tested to measure tensile behavior as a function of temperature, stress-rupture and creep characteristics at two elevated temperatures, bending fatigue behavior, resistance to thermal cycling, and Izod impact response.