Microstructural evolution and hardness response in the laser beam welded joints of pure titanium during recrystallization and grain growth

Highlights: • The LABs and high local misorientations indicate the existence of plastic strains in the as-welded HAZ and FZ. • During heat treatment the recrystallization occurs in the HAZs, decreasing plastic strains, but it doesn't appear in the FZs. • The coarse and unstrained grains gradually replace the fine and strained ones in the HAZs during recrystallization. • The decrease of plastic strains in the HAZs during recrystallization causes the descent of average hardness values based on the strain strengthening. - Abstract: Microstructural evolution and hardness response in the laser beam welded joints of pure titanium during recrystallization and grain growth were investigated by means of electron backscatter diffraction and hardness measurement. The low-angle boundaries (LABs) and high local misorientations, in the as-welded heat affected zone (HAZ) and fusion zone (FZ), indicate the existence of plastic strains caused by the plastic strains due to the thermal stress and the non-equilibrium phase transformations. The recrystallization occurs in the HAZs during heat treatment, but the grain growth after recrystallization does not appear under the heat treatment conditions. Moreover as a result of the slightly high impurity contents in the as-welded FZ, no distinct recrystallization is found in the FZs in this work. During recrystallization in the HAZs, the coarse and unstrained grains with equiaxed shape and smooth boundary gradually consume the fine and strained ones with irregular shape and serrate boundary. Meanwhile, the LABs disappear and the low local misorientations replace the high ones in the modified grains. The recrystallization during heat treatment causes the decrease of plastic strains in the HAZs, which reflects on the descent of average hardness values based on the strain strengthening.

36 MATERIALS SCIENCE↗

Characterization and mechanical properties of cladded stainless steel 316L with nuclear applications fabricated using electron beam melting

The ability to fabricate or join components of 316 L austenitic stainless steel using additive manufacturing (AM) processes such as laser and electron beam melting (EBM®) offers several advantages including enhanced part complexity, narrow or absent heat affected zones, increased part precision, avoidance of filler materials (such as traditional welds), and the ability to create metallurgically sound bonds. These attributes can contribute to improved mechanical properties of the fabricated components and component repair in nuclear, aerospace, and chemical industries. In the present work, we report that austenitic 316 L stainless steel additively manufactured by EBM exhibits a 76% increase in the yield strength and a corresponding increase of 29% in the ultimate tensile strength in contrast to the wrought substrate and commercial forged 316 L stainless steel. The EBM clad 316 L stainless steel elongation was 36%. The wrought substrate equiaxed grain size was ~30 μm in contrast to elongated, columnar grains ~0.1 mm wide and >1 mm in length for the EBM cladding. Transmission Electron Microscopy (TEM) analysis revealed that these columnar grains, which exhibited very straight, and presumably special grain boundaries having a very high (100) texture, contained a variety of sub-grain microstructures consisting of low-angle sub-grain boundaries containing dislocation tangles and stacking-fault arrays, and homogeneously distributed Cr 23 C 6 carbide precipitates, with no preferential carbide precipitation on either the straight, special columnar grain boundaries, or the very low-angle sub-grain boundaries. This observation and the formation of hierarchical microstructures which produce high strength and possibly corrosion resistance as a consequence of the absence of grain boundary carbide precipitation, illustrate the prospects for AM as a novel concept for achieving grain boundary engineering to promote high-strength and corrosion resistant alloys for high-temperature, corrosive environments, including elevated temperature nuclear reactor applications.

36 MATERIALS SCIENCE↗

Effect of the surface preparation techniques on the EBSD analysis of a friction stir welded AA1100-B{sub 4}C metal matrix composite

Aluminum based metal matrix composites (MMCs) have been used in various automobile, aerospace and military industries. Yet characterization of the microstructure in these materials remains a challenge. In the present work, the grain structure in the matrix of B{sub 4}C particulate reinforced MMCs and their friction stir welds is characterized by using optical metallography and the electron backscatter diffraction (EBSD) technique. Optical metallography can partially reveal the grain structure in the matrix of AA1100-16 vol.% B{sub 4}C composite. The EBSD technique has been successfully applied to characterize the grain structure in the AA1100-16 vol.% B{sub 4}C friction stir welds, which provides a powerful tool to follow the microstructural evolution of MMC materials during friction stir welding (FSW). Both mechanical polishing and ion beam polishing are used for the EBSD sample preparation. The effect of the sample preparation on the EBSD data acquisition quality is studied. Some typical examples, such as the identification of grains and subgrains, grain size distribution, deformation fields and the texture components are given. - Highlights: {yields} EBSD has been used to characterize the grain structure of Al-B{sub 4}C MMCs. {yields} Mechanical and ion beam polishing are compared for EBSD sample preparation of MMCs. {yields} EBSD shows great advantages over optical microscopy for microtexture analysis of MMCs.

36 MATERIALS SCIENCE↗

The effect of weld stresses on weld quality

A narrow heat source raises the temperature of a spot on a solid piece of material like metal. The high temperature of the spot decreases with distance from the spot. This is true whether the heat source is an arc, a flame, an electron beam, a plasma jet, a laser beam, or any other source of intense, narrowly defined heat. Stress and strain fields around a moving heat source are organized into a coherent visible system. It is shown that five stresses act across the weld line in turn as an arc passes. Their proportions and positions are considerably altered by weld parameters or condition changes. These pushes and pulls affect the metallurgical character and integrity of the weld area even when there is no apparent difference between after-the-fact examples.

Chihoski, R. A.↗

Dissimilar metal joining of Ti-6Al-4V and Inconel 625

The dissimilar joining of Ti-6Al-4V and Inconel 625 by using a suitable interlayer shows potential design flexibility by avoiding the brittle intermetallic phases from direct welding. These phases include NiTi , NiTi 2 , and Ni 3 Ti . The objective of this work is to facilitate laser welding of Ti-6Al-4V and Inconel 625 through a vanadium interlayer to form an intermetallic free, strong, and corrosion resistant joint. Vanadium was chosen based on binary phase diagram solubilities, literature, and theoretical CalPhaD calculations in PanDat. Laser welding was systematically explored from based on beam mode, offset, power, and scan speed. Varied parameters include laser power from 325 to 650 watts, laser scan speed from 80 to 160 in/min, and beam offset up to a ¼ of the beam diameter. Parameters were chosen based on previous dissimilar joining research and those found in the literature. Metallography, including optical and scanning electron microscopy, was used to analyze the weld chemical composition, grain structure, and defects through both the fusion and heat affected zones. The results and discussion will examine the relationship between process parameters, microstructure, and observed weld defects. Our findings will not only assess the weldability of vanadium and Inconel 625 but also establish a transferable framework for studying other dissimilar material combinations, providing valuable insights for future research in this field.

36 MATERIALS SCIENCE↗

Experimental Investigations on Pulsed Nd:YAG Laser Welding of C17300 Copper-Beryllium and 49Ni-Fe Soft Magnetic Alloys

Copper-beryllium and soft magnetic alloys must be joined in electrical and electro-mechanical applications. There is a high difference in melting temperatures of these alloys which cause to make the joining process very difficult. In addition, copper-beryllium alloys are of age hardenable alloys and precipitations can brittle the weld. 49Ni-Fe alloy is very hot crack sensitive. Moreover, these alloys have different heat transfer coefficients and reflection of laser beam in laser welding process. Therefore, the control of welding parameters on the formation of adequate weld puddle composition is very difficult. Laser welding is an advanced technique for joining of dissimilar materials since it can precisely control and adjust the welding parameters. In this study, a 100W Nd:YAG pulsed laser machine was used for joining 49Ni-Fe soft magnetic to C17300 copper-beryllium alloys. Welding of samples was carried out autogenously by changing the pulse duration, diameter of beam, welding speed, voltage and frequency. The spacing between samples was set to almost zero. The ample were butt welded. It was required to apply high voltage in this study due to high reflection coefficient of copper alloys. Metallography, SEM analysis, XRD and microhardness measurement was used for survey of results. The results show that the weld strength depends upon the chemical composition of the joints. To change the wells composition and heat input of the welds, it was attempted to deviate the laser focus away from the weld centerline. The best strength was achieved by deviation of the laser beam away about 0.1mm from the weld centerline. The result shows no intermetallic compounds if the laser beam is deviated away from the joint.

36 MATERIALS SCIENCE↗

3D Characterization of the Columnar-to-Equiaxed Transition in Additively Manufactured Inconel 718

Additive manufacturing (AM) provides enormous processing flexibility, enabling novel part geometries and optimized designs. Access to a local heat source further permits the potential for local microstructure control on the scale of individual melt pools, which can enable local control of part properties. In order to design tailored processing strategies for target microstructures, models predicting the columnar-to-equiaxed transition must be extended to the high solidification velocities and complex thermal histories present in AM. Here, we combine 3D characterization with advanced modeling techniques to develop a more complete understanding of the solidification process and evolution of microstructure during electron beam melting (EBM) of Inconel 718. Full calibration of existing microstructure prediction models demonstrates the differences between AM processes and more conventional welding techniques, underlying the need for accurate determination of key parameters that can only be measured directly in 3D. The ability to combine multisensor data in a consistent 3D framework via data fusion algorithms is essential to fully leverage these advanced characterization approaches. Thermal modeling provides insight on microstructure development within isolated solidification events and demonstrates the role of Marangoni effects on controlling solidification behavior.

Polonsky, Andrew↗

Additive Manufacturing of Advanced High Temperature Masking Fixtures for EBPVD TBC Coating

The purpose of this Manufacturing Demonstration Facility (MDF) technical collaboration project between Praxair Surface Technologies, Inc. (PST) and Oak Ridge National Laboratory (ORNL) was to develop an additive manufacturing process to fabricate next generation high temperature masking fixtures for coating of turbine airfoils with ceramic Thermal Barrier Coatings (TBC) by the Electron Beam Physical Vapor Deposition (EBPVD) process. Typical masking fixtures are sophisticated designs and require complex part manipulation in order to achieve the desired coating distribution. Fixtures are typically fabricated from high temperature nickel (Ni) based superalloys. The fixtures are fabricated from conventional processes by welding of thin sheet material into a complex geometry, to decrease the weight load for the manipulator and to reduce the thermal mass of the fixture. Recent attempts have been made in order to fabricate the fixtures through casting, but thin walled sections are difficult to cast and have high scrap rates. This project focused on understanding the potential for fabricating high temperature Ni based superalloy fixtures through additive manufacturing. Two different deposition processes; electron beam melting (EBM) and laser powder bed fusion were evaluated to determine the ideal processing route of these materials. Two different high temperature materials were evaluated. The high temperature materials evaluated were Inconel 718 and another Ni base alloy, designated throughout the remainder of this document as Alloy X, as the alloy composition is sensitive. Inconel 718 is a more widely utilized material for additive manufacturing although it is not currently the material utilized for current fixtures. Alloy X is the alloy currently used for the fixtures, but is not a commercially available alloy for additive manufacturing. Praxair determined it was possible to build the fixture using laser powder bed technology from Inconel 718. ORNL fabricated the fixture geometry using the EBM technology in order to compare deposition features such as surface roughness, geometric accuracy, deposition rate, surface and subsurface porosity, and material quality. It was determined that the laser powder bed technology was ideal for the geometry and requirements of the fixture set by Praxair, and Praxair moved forward with the purchase of a laser powder bed system. The subsequent portion of the project focused on determining the ideal processing parameters for alloy X for the laser powder bed system using ORNL’s Renishaw laser powder bed system. Praxair supplied gas atomized powders of alloy X material with properties specified by ORNL. ORNL printed text cube arrays in order to determine the ideal combination of laser powder and laser travel speed in order to maximize material density, improve surface quality, and maintain geometric accuracy. Additional powder supplied by Praxair was used to fabricate a full-scale fixture component.

42 ENGINEERING↗

Development of Fiber Laser Weld Parameters for Stainless Steel and Refractory Metals

Laser welds were made in 21-6-9 stainless steel, vanadium and tantalum using LLNL's new 6kW fiber laser to target 1 mm penetration depths. The materials were machined into flat coupon samples with standard step-joint geometries, and were welded in a continuous wave mode. The laser was characterized using the Primes laser beam diagnostic system so that the beams can be reproduced in the future. The optical configuration consisted of a 200 {micro}m fiber, 200 mm collimator and 250 mm focusing lens, which delivered electron-beam level power densities in the 5 to 20 kW/mm2 range. The three different materials required different power densities to produce the desired penetration, and this report summarizes the results of this screening study that was directed at developing a first approximation to the proper welding parameters for future work. The results show that 1 mm penetrations can be achieved using a 400W beam for 21-6-9 stainless steel, a 600W beam for vanadium, and a 1,100W beam for tantalum using sharp focus and a travel speed of 40 inch/min. Future welds should incorporate a trailing gas shield to prevent discoloration of the surface and to prevent oxygen and nitrogen pickup in the welds.

36 MATERIALS SCIENCE↗

Geometry-Induced Spatial Variation of Microstructure Evolution During Selective Electron Beam Melting of Rene-N5

High gamma prime (γ') nickel-based alloys produced by selective electron beam melting are of interest to the turbine industry which requires control of microstructure in relation to loading conditions within complex component geometry. Welding literature predicts cracking and microstructure evolution as a function of alloy composition and process parameters in this class of alloys. In addition, Additive manufacturing causes variations in the above conditions due to the interaction of geometry on processing and heat transfer. The influence of geometry on processing conditions was explored for alloy Rene N5 by characterizing the solidification grain microstructure and solid-state precipitation. A Semi-Analytical Heat Transfer Model was employed to explain the resulting variation in solidification grain morphology that occurred due to the part geometry. Finally, the as-built precipitation structure was found to vary as a function of build height and had no correlation to the solidification grain structure or the layer geometry.

36 MATERIALS SCIENCE↗

Chloride-Induced Stress Corrosion Cracking Characteristics of the Used Nuclear Fuel Canister Material

The used nuclear fuel (UNF) dry storage systems are located in the coastal and lake/river-side regions, the service time of which is 60 years and more. One type of dry storage systems is composite of a thin-walled austenitic stainless steel (SS) welded canister and a concrete overpack. The air flows through the canister surface and brings away the decay heat. Meanwhile, the air brings the salt species into the canister and make them deposit on the surface. The salt deposit will be deliquescent when absorbing the moisture air, being corrosive to the surface. NRC and other programs claimed that chloride induced stress corrosion cracking (CISCC) would lead to the canister failure, being one of the major technical gaps for extended dry storage systems. CISCC is induced by the combined influence of the aggressive environment (chloride ions in our case) and tensile stresses (residual stresses in our case) on the susceptible materials (the austenitic SS in our case). Chrome (Cr), as one of the chemical compositions of SSs, plays an important role in the corrosion resistance. It can form a chrome-rich inner barrier oxide layer to prevent the SS from corrosion. However, chloride ions can easily break down the barrier and accelerate dissolution of the underlying metal, the phenomena of which is pitting corrosion. Pitting is the precursor to CISCC as which provides the combination of a local aggressive solution chemistry and a stress concentrating feature. Accordingly, CISCC invariably originates from the pits, and cracks that have nucleated on pit walls can grow around the pit and coalesce to form a complete through-crack. Significant tensile residual stresses, caused by the welding process, exist throughout the thickness of the canister wall. Enos and Bryan found that large residual stresses were in the full-scale mockup container simulating a canister, which supports the SCC propagation. It is therefore interesting to achieve a good knowledge about the effect of welding on the durability of SSs, especially in the corrosive environment. In order to understand the fundamental of the cracking behaviors, it's vital to elucidate the microstructure and microchemistry of cracking. This study focused on observing the CISCC characteristics of the UNF canister material exposed to the humid environment with salt deposit. Extensive micro-characteristics have been achieved by the techniques include focused ion beam/ scanning electron microscope (FIB/SEM), transmission electron microscopy (TEM), energy dispersive spectroscopy (EDS), and optical profiler. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Limiting current in electron-beam welders

Damage to workpiece by excessive current in electron-beam welder is prevented by mechanism that accurately adjusts anode-to-cathode spacing. Mechanism is installed on standard Sciaky (or equivalent) electron-beam gun with only minimal modification. By turning knurled knob and observing digital readout of anode/cathode separation, machine operator adjusts welder for safe maximum current before welding begins.

Spiegel, K. W.↗

CHARACTERIZATION OF FATIGUE BEHAVIORS OF NOTCHED 316L DED AM SPECIMENS

ASME Codification of Additive Manufacturing • Integration of AM into ASME Codes and Standards • The ASME goal is to have AM requirements in ASME Code Cases preceding the 2025 Edition. • The ASME Special Committee on AM has drafted criteria for two Code Cases for Additive Manufacturing. • AM Construction of Pressure Equipment using the Direct Energy Deposition Process with Wire Feedstock. • Includes Gas Metal Arc Welding. • Time-independent material properties. • Status - Criteria endorsed by AM Committee. • AM Construction of Pressure Equipment using the Powder Bed Fusion AM Process. • Includes Laser and Electron Beam Energy Sources. • Austenitic and Nonferrous materials. • Time-independent material properties. • Status – Approval ballot circulating to the AM Committee.

Krentz, Timothy M.↗

Development of Ultra Small Scale Mechanical Testing and Localized He Implantation for Nuclear Applications

Mechanical properties degradation of components deployed in nuclear applications has been a concern since the deployment of first generation nuclear power plants. Radiation damage along with environmental degradation, elevated temperatures, and long term deployment of nuclear structures pose a challenging environment for all materials in these applications. Traditionally, the mechanical properties are assessed by standardized macroscopic testing methods. While those are providing engineering relevant data these techniques do have limitations, especially on reactor irradiated materials, due to the large size of the samples. Limitations on the amount of radioactivity of large samples must be applied for research applications as they are conducted at universities. In addition it can be difficult to retrieve sufficiently large amounts of material from an operating reactor component. Therefore smaller sample sizes are desirable and reduce the amount of radioactive material which needs to be handled or material which needs to be retrieved. In addition, the number of tests which can be performed on materials irradiated in a test reactor program is limited due to limited space in specific dose and temperature positions. Downsizing of the mechanical test can overcome this issue and perform more tests on the same amount of irradiated materials, reducing the statistical uncertainties. In addition, smaller scale samples allow access to specific regions of interest in a material or component, be it the zone in front of a crack tip or the sampling of very small components like springs or welded areas. In addition ion beam irradiation has become an integral part of nuclear materials research to enhance the understanding of radiation damage in materials in a time and cost effective fashion. The drawback of ion beam irradiation is the small penetration depth of the ions into the material making localized microstructural characterization as well as small scale mechanical testing necessary. Another more fundamental motivation is the fact that since the beginning of electron microscopy, one has been concerned about imaging and quantifying defects in materials. Multiscale tools to image a large range of radiation induced defects have been established starting from atom probe tomography to transmission electron microscopy, up to scattering techniques. Mechanical testing, however, has always been performed on a large scale, and an attempt to match the same scale where a defect is observed with the materials' mechanical property response has not yet been realized. However, the question of separate effects testing on specific radiation induced defects remains and is an additional driving force for small scale mechanical testing. In this work we present an approach for small scale mechanical testing in irradiated materials and the variety of possible test methods developed today. We also present recent efforts of performing localized ion beam implantation to achieve a number of different doses in the same region of interest enhancing comparability and quantification of observed phenomena. It is the intention to give the reader an overview of the different microscale mechanical testing techniques possible today as well as an introduction of a novel ion beam irradiation method using a newly established capability. In this paper we can't discuss all aspects of all small scale mechanical testing of irradiated materials However, It does give an overview over the techniques enabled due to recent effort and enhanced instrument capability. While indentation or micro compression testing has been performed previously tensile testing and ion beam irradiation using the He ion beam microscope are novel approaches not attempted previously. (authors)

36 MATERIALS SCIENCE↗

Additive Manufacturing Modeling and Simulation A Literature Review for Electron Beam Free Form Fabrication

Additive manufacturing is coming into industrial use and has several desirable attributes. Control of the deposition remains a complex challenge, and so this literature review was initiated to capture current modeling efforts in the field of additive manufacturing. This paper summarizes about 10 years of modeling and simulation related to both welding and additive manufacturing. The goals were to learn who is doing what in modeling and simulation, to summarize various approaches taken to create models, and to identify research gaps. Later sections in the report summarize implications for closed-loop-control of the process, implications for local research efforts, and implications for local modeling efforts.

Seufzer, William J.↗

The real mission of ITER

For future machines, the plasma stored energy is going up by factors of 20-40x, and plasma currents by 2-3x, while the surface to volume ratio is at the same time decreasing. Therefore the disruption forces, even for constant B, (which scale like IxB), and associated possible localized heating on machine components, are more severe. Notably, Tore Supra has demonstrated removal of more than 1 GJ of input energy, over nearly a 400 second period. However, the instantaneous stored energy in the Tore Supra system (which is most directly related to the potential for disruption damage) is quite small compared to other large tokamaks. The goal of ITER is routinely described as studying DT burning plasmas with a Q {approx} 10. In reality, ITER has a much more important first order mission. In fact, if it fails at this mission, the consequences are that ITER will never get to the eventual stated purpose of studying a burning plasma. The real mission of ITER is to study (and demonstrate successfully) plasma control with {approx}10-17 MA toroidal currents and {approx}100-400 MJ plasma stored energy levels in long-pulse scenarios. Before DT operation is ever given a go-ahead in ITER, the reality is that ITER must demonstrate routine and reliable control of high energy hydrogen (and deuterium) plasmas. The difficulty is that ITER must simultaneously deal with several technical problems: (1) heat removal at the plasma/wall interface, (2) protection of the wall components from off-normal events, and (3) generation of dust/redeposition of first wall materials. All previous tokamaks have encountered hundred's of major disruptions in the course of their operation. The consequences of a few MA of runaway electrons (at 20-50 MeV) being generated in ITER, and then being lost to the walls are simply catastrophic. They will not be deposited globally, but will drift out (up, down, whatever, depending on control system), and impact internal structures, unless 'ameliorated'. Basically, this represents an extraordinarily robust e-beam welding machine, capable of deep penetration into any armor tiles, to the cooling channels which are embedded less than 1 cm below the tile surface. When energy is deposited in a fraction of a second on (or in) a tile, the presence of underlying water cooling does no good for the purposes of heat removal.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Characteristics of laser welded wrought Mg-Al-Mn alloy

Magnesium alloys have gained increased attention in recent years as a structural metal because of their property merits, which necessitates the development of welding techniques qualified for applications in the aeronautic and automotive industries. Laser welding is known to be an excellent method for joining metals. In this paper, a 3 kW CO{sub 2} laser beam was used to weld the wrought Mg-Al-Mn alloy. The characteristics of the microstructure and the mechanical properties of the joints were analyzed by optical microscopy (OM), energy dispersive spectrometry (EDS), scanning electron microscopy (SEM), tensile testing and hardness testing. The experimental results show that the wrought Mg-Al-Mn alloy can be joined successfully using optimized welding conditions. The results of tensile testing show that the highest ultimate tensile strength (UTS) of the joints is up to 94% of that of the base metal. The base metal consists of a typical rolled structure, the narrow heat affected zone (HAZ) has no obvious grain coarsening, and the fusion zone consists of fine grains with a high density of {gamma}-Mg{sub 17}Al{sub 12} precipitates. The hardness test results indicate that the microhardness in the fusion zone is higher than that of the base metal. The elemental analysis reveals that the Mg content in the weld is lower than that of the base metal, but the Al content is slightly higher.

36 MATERIALS SCIENCE↗