Surface and interface of epitaxial CdTe film on CdS buffered van der Waals mica substrate

We report single crystal CdTe films are desirable for optoelectronic device applications. An important strategy of creating films with high crystallinity is through epitaxial growth on a proper single crystal substrate. We report the metalorganic chemical vapor deposition of epitaxial CdTe films on the CdS/mica substrate. The epitaxial CdS film was grown on a mica surface by thermal evaporation. Due to the weak van der Waals forces, epitaxy is achieved despite the very large interface lattice mismatch between CdS and mica (~21–55%). The surface morphology of mica, CdS and CdTe were quantified by atomic force microscopy. The near surface structures, orientations and texture of CdTe and CdS films were characterized by the unique reflection high-energy electron diffraction surface pole figure technique. The interfaces of CdTe and CdS films and mica were characterized by X-ray pole figure technique and transmission electron microscopy. The out-of-plane and in-plane epitaxy of the heteroepitaxial films stack are determined to be CdTe(111)//CdS(0001)//mica(001) and [$\overline{1}2\overline{1}$] CdTe //[$\overline{1}100$] CdS //[010] mica , respectively. The measured photoluminescence (PL), time resolved PL, photoresponse, and Hall mobility of the CdTe/CdS/mica indicate quality films. Finally, the use of van der Waals surface to grow epitaxial CdTe/CdS films offers an alternative strategy towards infrared imaging and solar cell applications.

36 MATERIALS SCIENCE↗

Growth of Epitaxial gamma-Al 2 O 3 Films on Rigid Single-Crystal Ceramic Substrates and Flexible, Single-Crystal-Like Metallic Substrates by Pulsed Laser Deposition

Epitaxial -Al2O3 thin films were grown on diverse substrates using pulsed laser deposition. The high quality of epitaxial growth and cubic structure of -Al2O3 films was confirmed by x-ray diffraction. SrTiO3 and MgO single crystal substrates were used to optimize the growth conditions for epitaxial -Al2O3 film. Under the optimized conditions, epitaxial -Al2O3 thin films were grown on flexible, single-crystal-like, metallic templates. These included untextured Hastelloy substrates with a biaxially textured MgO layer deposited using ion-beam-assisted-deposition and biaxially textured Ni-W metallic tapes with epitaxially grown and a biaxially textured, MgO buffer layer. These biaxially textured, -Al2O3 films on flexible, single-crystal-like substrates are promising for subsequent epitaxial growth of various complex oxide films used for electrical, magnetic and electronic device applications.

36 MATERIALS SCIENCE↗

Pulsed-laser epitaxy of metallic delafossite PdCrO 2 films

Alternate stacking of a highly conducting metallic layer with a magnetic triangular layer found in delafossite PdCrO 2 provides an excellent platform for discovering intriguing correlated quantum phenomena. Thin film growth of delafossites may enable not only the tuning of the basic physical properties beyond what bulk materials can exhibit, but also the development of novel hybrid materials by interfacing with dissimilar materials, yet this has proven to be extremely challenging. Here, we report the epitaxial growth of metallic delafossite PdCrO 2 films by pulsed laser epitaxy (PLE). The fundamental role of the PLE growth conditions, epitaxial strain, and chemical and structural characteristics of the substrate is investigated by growing under various growth conditions and on various types of substrates. While strain plays a large role in improving the crystallinity, the direct growth of epitaxial PdCrO 2 films without impurity phases was not successful. We attribute this difficulty to both the chemical and structural dissimilarities with the substrate and volatile nature of the PdO sublayer, which make nucleation of the right phase difficult. This difficulty was overcome by growing CuCrO 2 buffer layers before PdCrO 2 films were grown. Unlike PdCrO 2 , CuCrO 2 films were readily grown with a relatively wide growth window. Only a monolayer thick buffer layer was sufficient to grow the correct PdCrO 2 phase. This result indicates that the epitaxy of Pd-based delafossites is extremely sensitive to the chemistry and structure of the interface, necessitating near perfect substrate materials. The resulting films are commensurately strained and show an antiferromagnetic transition at 40 K that persists down to as thin as 3.6 nm in thickness. This work provides key insights into advancing the epitaxial growth of the broader class of metallic delafossites for both studying the basic physical properties and developing new spintronic and computing devices.

36 MATERIALS SCIENCE↗

Interface characterization of epitaxial Fe/MgO/Fe magnetic tunnel junctions

Following predictions by first-principles theory of huge tunnel magnetoresistance (TMR) effect in epitaxial Fe/MgO/Fe magnetic tunnel junctions (MTJs), measured magnetoresistance (MR) ratio about 200% at room temperature (RT) have been reported in MgO-based epitaxial MTJs. Recently, MR ratio of about 600% has been reported at RT in MgO-based amorphous MTJs with core structure of CoFeB/MgO/CoFeB grown by magnetron sputtering with amorphous CoFeB layers. The sputtered CoFeB/MgO/CoFeB MTJs shows a great potential application in spintronic devices. Although epitaxial structure will probably not be used in devices, it remains an excellent model system to compare theoretical calculations with experimental results and to enhance our understanding of the spin dependent tunneling. Both theoretical calculations and experimental results clearly indicate that the interfacial structure plays a crucial role on coherent tunneling across single crystalMgO barrier, especially in epitaxial MgO-based MTJs grown by molecular beam epitaxy (MBE). Surface X-ray diffraction, Auger electron spectroscopy, X-ray absorption spectra, and X-ray magnetic circular dichroism have been used for interface characterization. However, no consistent viewpoint has been reached, and this is still an open issue. In this article, recent studies on the interface characterization in MgO-based epitaxial MTJs will be introduced, with a focus on research by X-ray photoelectron spectroscopy, high resolution transmission electron microscopy, and spin dependent tunneling spectroscopy.

Wang, Shouguo↗

Development of Production PVD-AIN Buffer Layer System and Processes to Reduce Epitaxy Costs and Increase LED Efficiency (Final Scientific/Technical Report)

The DOE has set aggressive goals for solid state lighting (SSL) adoption, which require manufacturing and quality improvements for virtually all process steps leading to an LED luminaire product. The goals pertinent to this proposed project are to reduce the cost and improve the quality of the epitaxial growth processes used to build LED structures. The objectives outlined in this proposal focus on achieving cost reduction and performance improvements over state-of-the-art, using technologies that are low in cost and amenable to high efficiency manufacturing. The objectives of the outlined proposal focus on cost reductions in epitaxial growth by reducing epitaxy layer thickness and hetero-epitaxial strain, and by enabling the use of larger, less expensive silicon substrates and would be accomplished through the introduction of a high productivity reactive sputtering system and an effective sputtered aluminum-nitride (AlN) buffer/nucleation layer process. Success of the proposed project could enable efficient adoption of GaN on-silicon (GaN/Si) epitaxial technology on 150mm silicon substrates. The reduction in epitaxy cost per cm 2 using 150mm GaN-on-Si technology derives from (1) a reduction in cost of ownership and increase in throughput for the buffer deposition process via the elimination of MOCVD buffer layers and other throughput and CoO enhancements, (2) improvement in brightness through reductions in defect density, (3) reduction in substrate cost through the replacement of sapphire with silicon, and (4) reduction in non-ESD yield loss through reductions in wafer bow and temperature variation. The adoption of 150mm GaN/Si processing will also facilitate significant cost reductions in subsequent wafer fabrication manufacturing costs. There were three phases to this project. These three phases overlap in order to aggressively facilitate a commercially available production GaN/Si capability. In Phase I of the project, the repeatability of the performance was analyzed and improvements implemented to the Veeco PVD-AlN prototype system to establish a specification and baseline PVD-AlN films on sapphire and in parallel the evaluation of PVD AlN on silicon substrates began. In Phase II of the project a Beta tool based on a scaled-up process module capable of depositing uniform films on batches of 4” or 6” diameter substrates in a production worthy operation was developed and qualified. In Phase III, the means to increase the throughput of the PVD-AlN sy0stem was evaluated and focused primarily on minimizing the impact of the substrate heating and cooling times that dominated the overall cycle time.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Epitaxial Growth of Ga2O3: A Review

Beta-phase gallium oxide (β-Ga2O3) is a cutting-edge ultrawide bandgap (UWBG) semiconductor, featuring a bandgap energy of around 4.8 eV and a highly critical electric field strength of about 8 MV/cm. These properties make it highly suitable for next-generation power electronics and deep ultraviolet optoelectronics. Key advantages of β-Ga2O3 include the availability of large-size single-crystal bulk native substrates produced from melt and the precise control of n-type doping during both bulk growth and thin-film epitaxy. A comprehensive understanding of the fundamental growth processes, control parameters, and underlying mechanisms is essential to enable scalable manufacturing of high-performance epitaxial structures. This review highlights recent advancements in the epitaxial growth of β-Ga2O3 through various techniques, including Molecular Beam Epitaxy (MBE), Metal-Organic Chemical Vapor Deposition (MOCVD), Hydride Vapor Phase Epitaxy (HVPE), Mist Chemical Vapor Deposition (Mist CVD), Pulsed Laser Deposition (PLD), and Low-Pressure Chemical Vapor Deposition (LPCVD). This review concentrates on the progress of Ga2O3 growth in achieving high growth rates, low defect densities, excellent crystalline quality, and high carrier mobilities through different approaches. It aims to advance the development of device-grade epitaxial Ga2O3 thin films and serves as a crucial resource for researchers and engineers focused on UWBG semiconductors and the future of power electronics.

Chemistry↗

Epitaxial silicon growth for solar cells

The epitaxial procedures, solar cell fabrication, and evaluation techniques are described. The development of baseline epitaxial solar cell structures grown on high quality conventional silicon substrates is discussed. Diagnostic layers and solar cells grown on four potentially low cost silicon substrates are considered. The crystallographic properties of such layers and the performance of epitaxially grown solar cells fabricated on these materials are described. An advanced epitaxial reactor, the rotary disc, is described along with the results of growing solar cell structures of the baseline type on low cost substrates. The add on cost for the epitaxial process is assessed and the economic advantages of the epitaxial process as they relate to silicon substrate selection are examined.

Daiello, R. V.↗

Oxygen Impurities and Defects in Epitaxial Layer SiC and SiC Wafer Characterized by Room and Low Temperatures FTIR

SiC as a highly promising semiconducting material has received increasing attention in the last decade. The impurities such as oxygen and hydrogen have a great effect in electronic properties of semiconducting materials. In this study, the FTIR spectra were measured at room temperature (25 C) and low temperature (-70 C) for an n-type SiC substrate, a p-type epitaxial layer SiC, and patterned Ta on a p-type epitaxial layer SiC sample. The oxygen related IR peaks were measured for all three samples at room and low temperatures. The peak at 1105 cm(exp -1) is the result of a substitutional carbon and a interstitial oxygen in SiC. The concentration of the impurity oxygen increases in the SiC epitaxial layer during the CVD and electron beam processes. For the n-type SiC substrate, this peak does not appear. The peak at 905 cm(exp -1) exists in the IR spectra only for two epitaxial layer on p-type SiC substrate samples. This peak is related to oxygen vacancy centers in SiC, which are introduced in the CVD epitaxial growth process. At low temperature, the peak at 1105 cm(exp -1) shifts down and the peak at 905 cm(exp -1) shifts up for the epitaxial layer SiC samples. It can be explained that, at low temperatures, the stress increases due to the distorted bonds. The study shows that FTIR is a very effective method to evaluate low concentration impurities in SiC.

Lu, W. J.↗

Synchrotron X-Ray Topography Study of Structural Defects and Strain in Epitaxial Structures of Yb- and Tm-Doped Potassium Rare-Earth Double Tungstates and Their Influence on Laser Performance.

Monoclinic potassium rare-earth double tungstates [KRE(WO{sub 4}){sub 2}, RE = Y, Lu, Yb; KREW] are well suited as hosts for active lanthanide ion (Ln{sup 3+}) dopants for diode-pumped solid-state lasers, with particular interest in thin-disk laser configurations when they are grown as thin films. Using synchrotron white-beam x-ray topography, we have imaged defects and strain in top-seeded solution-grown (TSSG) bulk substrates of different rare-earth tungstates as well as within Yb{sup 3+}- and Tm{sup 3+}-doped epitaxies for thin-disk laser applications grown on these substrates by liquid-phase epitaxy. Higher structural stress in Yb:KYW/KYW epitaxies compared with Yb:KLuW/KLuW epitaxies is found to lower efficiency in laser operation. The quality of Tm:KLuW/KLuW epitaxial films is sensitive to doping level, film thickness, and growth rate. Inhomogeneous stresses within the layers are dominated by lattice-mismatch effects rather than by crystallographic anisotropy.

36 MATERIALS SCIENCE↗

X-ray Microdiffraction from α-Ti 0.04 Fe 1.96 O 3 (0001) Epitaxial Film Grown Over α-Cr 2 O 3 Buffer Layer Boundary

Ti-doped hematite (α-Ti 0.04 Fe 1.96 O 3 ) film grown over patterned α-Cr 2 O 3 buffer layer on α-Al 2 O 3 (0001) substrate was characterized with synchrotron X-ray microdiffraction. The film was grown by oxygen plasma assisted molecular beam epitaxy method. The film growth mode was correlated to buffer layer boundary and Ti concentration variation. Epitaxial α-Ti 0.04 Fe 1.96 O 3 film was formed on bare substrate adjacent to the buffer layer. The epitaxial film was connected laterally to a strain-relaxed epitaxial α-Ti 0.04 Fe 1.96 O 3 film grown on the buffer layer. On bare α-Al2O3 substrate with diminished Ti concentration only a small portion of α-Ti x Fe 1-x O 3 film was epitaxial either as coherent to the substrate or strain-relaxed form.

36 MATERIALS SCIENCE↗

Epitaxial Growth of MgO/TiN Multilayers on Cu

The growth of epitaxial MgO/TiN multilayer films on (001) Cu has been investigated. In particular, epitaxial structures were grown on (001) Cu layers that were epitaxial on (001) SrTiO{sub 3}. X-ray diffraction and reflection high-energy electron diffraction indicate that the multilayer structures are epitaxial on the (001) Cu surface. The motivation is the use of crystalline MgO/TiN multilayers as a diffusion barrier to both copper and oxygen. MgO/TiN multilayers are potentially useful as diffusion barriers for Cu interconnects on semiconductors as well as for superconducting wires based on the epitaxial growth of cuprate superconductors on biaxially textured copper.

36 MATERIALS SCIENCE↗

Ultrathin Ruthenium Films on Graphene Buffered SiO 2 via Quasi Van der Waals Epitaxy

In this study, we demonstrate a quasi van der Waals epitaxy approach to prepare single crystalline Ru ultrathin film on large scale, monolayer graphene. Physical and epitaxial properties of bulk, near surface and surface of ultrathin Ru films were comprehensively studied using various structural, morphological, compositional, and electrical characterization techniques. Here, we confirm that Ru can epitaxially grow on single, monolayer graphene using magnetron sputtering at elevated temperature of 600 °C. The epitaxial Ru films with film thickness ranging from 94.2 nm down to 3.9 nm show the (0001) out-of-plane orientation. The epitaxial relationships between Ru and graphene are out-of-plane Ru(0001) || graphene(0001) and in-plane Ru[$11\bar20$] || graphene[$11\bar20$]. All the Ru films show smooth surfaces with root-mean-square roughness less than 0.8 nm and have negligible oxide layer on the surfaces. The Ru films on graphene demonstrate significantly reduced electrical resistivity comparing to their counterpart grown on bare SiO 2 , which show polycrystalline nature. For 7.1 to 3.9 nm film thicknesses, the resistivity of Ru on graphene shows 38 to 45% resistivity decrease from that of Ru film on bare SiO 2 without graphene. Our observations suggest the existence of the above-classical van der Waals interaction between Ru and graphene. On the other hand, graphene is capable of effectively blocking the inter-diffusion/interaction between Ru and SiO 2 during a 1000 °C annealing process.

36 MATERIALS SCIENCE↗

Ultrasmooth Epitaxial Pt Thin Films Grown by Pulsed Laser Deposition

Platinum (Pt) thin films are useful in applications requiring high-conductivity electrodes with excellent thermal and chemical stability. Ultrasmooth and epitaxial Pt thin films with single-crystalline domains have the added benefit of providing ideal templates for the subsequent growth of heteroepitaxial structures. Here, we grow epitaxial Pt (111) electrodes (ca. 30 nm thick) on sapphire (α-Al 2 O 3 (0001)) substrates with pulsed laser deposition. This versatile technique allows control of the growth process and fabrication of films with carefully tailored parameters. X-ray scattering, atomic-force microscopy, and electron microscopy provide structural characterization of the films. Various gaseous atmospheres and temperatures were explored to achieve epitaxial growth of films with low roughness. A two-step (500 °C/300 °C) growth process was developed, yielding films with improved epitaxy without compromising roughness. The resulting films possess ultrasmooth interfaces (<3 Å) and high electrical conductivity (6.9 × 10 6 S/m). Finally, Pt films were used as current collectors and templates to grow lithium manganese oxide (LiMn 2 O 4 (111)) epitaxial thin films, a cathode material used in Li-ion batteries. In conclusion, using a solid-state ionogel electrolyte, the films were highly stable when electrochemically cycled in the 3.5-4.3 V vs Li/Li + range.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Engineering metal oxidation using epitaxial strain

The oxides of platinum group metals are promising for future electronics and spintronics due to the delicate interplay of spin-orbit coupling and electron correlation energies. However, their synthesis as thin films remains challenging due to their low vapour pressures and low oxidation potentials. Here we show how epitaxial strain can be used as a control knob to enhance metal oxidation. Using Ir as an example, we demonstrate the use of epitaxial strain in engineering its oxidation chemistry, enabling phase-pure Ir or IrO 2 films despite using identical growth conditions. The observations are explained using a density-functional-theory-based modified formation enthalpy framework, which highlights the important role of metal-substrate epitaxial strain in governing the oxide formation enthalpy. We also validate the generality of this principle by demonstrating epitaxial strain effect on Ru oxidation. The IrO 2 films studied in our work further revealed quantum oscillations, attesting to the excellent film quality. The epitaxial strain approach we present could enable growth of oxide films of hard-to-oxidize elements using strain engineering.

36 MATERIALS SCIENCE↗

Epitaxially Grown Single-Crystalline SrTiO 3 Membranes Using a Solution-Processed, Amorphous SrCa 2 Al 2 O 6 Sacrificial Layer

Water-soluble sacrificial layers based on epitaxially-grown, single crystalline (Ca, Sr, Ba) 3 Al 2 O 6 layer are widely used for creating free-standing perovskite oxide membranes. However, obtaining these sacrificial layers with intricate stoichiometry remains a challenge, especially for molecular beam epitaxy (MBE). In this study, we demonstrate the hybrid MBE growth of epitaxial, single crystalline SrTiO 3 films using a solution processed, amorphous SrCa 2 Al 2 O 6 sacrificial layer onto SrTiO 3 (001) substrates. Prior to the growth, the oxygen plasma exposure was used to first create the crystalline SrCa 2 Al 2 O 6 layer with well-defined surface crystallinity. Utilizing reflection high energy electron diffraction, x-ray diffraction, and atomic force microscopy, we observe an atomic layer-by-layer growth of epitaxial, single crystalline SrTiO 3 film on the SrCa 2 Al 2 O 6 layer with atomically smooth surfaces. The SrCa 2 Al 2 O6 layer was subsequently dissolved in de-ionized water to create free-standing SrTiO3 membranes that were transferred onto a metal-coated Si wafer. Membranes created with Sr-deficiency revealed ferroelectric-like behavior measured using piezo force microscopy whereas stoichiometric films remained paraelectric-like. Furthermore, these findings underscore the viability of using ex-situ deposited amorphous SrCa2Al2O6 for epitaxial, single crystalline growth, as well as the importance of point defects in determining the ferroic properties in membranes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling two-dimensional solid-phase epitaxial regrowth using level set methods

Modeling the two-dimensional (2D) solid-phase epitaxial regrowth (SPER) of amorphized Si (variously referred to as solid-phase epitaxial growth, solid-phase epitaxy, solid-phase epitaxial crystallization, and solid-phase epitaxial recrystallization) has become important in light of recent studies which have indicated that relative differences in the velocities of regrowth fronts with different crystallographic orientations can lead to the formation of device degrading mask edge defects. Here, a 2D SPER model that uses level set techniques as implemented in the Florida object oriented process simulator to propagate regrowth fronts with variable crystallographic orientation (patterned material) is presented. Apart from the inherent orientation dependence of the SPER velocity, it is established that regrowth interface curvature significantly affects the regrowth velocity. Specifically, by modeling the local SPER velocity as being linearly dependent on the local regrowth interface curvature, data acquired from transmission electron microscopy experiments matches reasonably well with simulations, thus providing a stable model for simulating 2D regrowth and mask edge defect formation in Si.

36 MATERIALS SCIENCE↗

Substrate doping effects on Raman spectrum of epitaxial graphene on SiC

In this paper, we reported a Raman scattering study of epitaxial graphene on different doped 6H-SiC (0001) substrates and investigated the substrate induced charge-transfer doping to the epitaxial graphene. We found that the charge carrier type and concentration of epitaxial graphene can be altered by SiC substrates with different doping level and doping type. This effect is comparable to that obtained by electrochemical doping. As Raman scattering is very sensitive to the doping level, the charge carrier concentration of epitaxial graphene can be estimated by the Raman G-peak shift. Our results are fundamental and may have implications for future epitaxial-graphene-based micro/nanoelectronic devices.

36 MATERIALS SCIENCE↗

Epitaxial Ni{sub 3}FeN thin films: A candidate for spintronic devices and magnetic sensors

A new type of epitaxial ferromagnetic nitride (Ni{sub 3} Fe N = permalloy nitride = 'PyN') compound films were grown on Al{sub 2}O{sub 3}(1120) substrates using reactive triode magnetron sputtering. The results of electron back-scattering diffraction and x-ray diffraction techniques indicate a high quality epitaxial crystalline structure with growth normal of (100). Magnetization measurements of epitaxial PyN films revealed several unique results. (1) A textbook square hysteresis loop that suggest existence of single magnetic domain in these films. (2) A coercive field is tunable from a few mOe up to a few Oe by changing the film thickness. (3) A magnetization that switches (rotate) over a very small field range of {delta}H{sub C} {<=} 0.05 Oe, independent of the film thickness. This small {delta}H indicates a very large resistive sensitivity ({delta}R/{delta}H) of the epitaxial PyN. (4) The epitaxial PyN thermal cycling through several cycles between '2 and 800 K' (-271 Degree-Sign C to +527 Degree-Sign C) shows much less degradation only about 2-5% compared to 40% degradation of a simple Py film. Four-probe transport measurements give an anisotropic magnetoresistance of Almost-Equal-To 6%, sufficiently higher than other known ferromagnetic materials. These interesting properties are ideal for a variety of spintronic devices and magnetic sensors.

36 MATERIALS SCIENCE↗