Search NASA⌕ Search

SEARCH · Search NASA

Results for “Electron backscatter diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Pre-compression effect on microstructure evolution of extruded pure polycrystalline magnesium during reversed tension load

Highlights: • Number of twin variants under compression along ED is dependent on grain orientation. • Tension after pre-compression results in low-SF twinning and secondary twinning. • Secondary twinning is facilitated by increasing pre-compression. • Sub-grains due to twinning enhance material strength. - Abstract: The microstructure evolution of extruded pure polycrystalline magnesium under compression followed by subsequent tension in ambient air was investigated. Solid round dog-bone shaped specimens were compressed along the extrusion direction (ED) to − 7.3% and − 12.8% true strains, respectively, and then tensioned along the ED to failure. Electron backscatter diffraction (EBSD) was used to examine the microstructure evolution using companion specimens unloaded at multiple points along the deformation curves. Pre-compression along the ED resulted in {10 1-bar 2} tension twinning which increased in volume with increasing strain until exhaustion at approximately − 10.5% true strain. Tensile reloading of the pre-compressed specimens led to a combination of low Schmid factor twinning, detwinning, and secondary {10 1-bar 2} tension twinning. Detwinning was more significant than secondary twinning in the − 7.3% pre-compressed specimens, where only one secondary twin variant was observed. {10 1-bar 2} secondary twinning was more significant in the − 12.8% pre-compressed specimens, where up to three secondary twin variants were observed. After complete detwinning of primary twins, the secondary twins were retained and appeared as sub-grains. The residual sub-grains resulted from secondary twinning may provide a strengthening mechanism for wrought Mg alloys.

36 MATERIALS SCIENCE↗

Identifying ferroelectric phase and domain structure using angle-resolved piezoresponse force microscopy

We used angle-resolved piezoresponse force microscopy (AR-PFM), vertical PFM (VPFM), and electron backscatter diffraction (EBSD) to provide a systematic interpretation of domain patterns in polycrystalline, near-morphotropic lead zirconate titanate. This material was used to illustrate the power of AR-PFM methods in resolving complex domain patterns where multiple phases may be present. AR-PFM was carried out with a 30° rotation interval, and the resulting data were analysed to identify the orientation of the underlying axis of piezoelectricity. The additional information provided by AR-PFM was studied, comparing its capabilities to those of 3-dimensional PFM, consisting of one VPFM image and two orthogonal lateral PFM (LPFM) images. We show that, in certain conditions, using AR-PFM can identify the phases present at the sub-grain scale. This was confirmed using VPFM and EBSD data. Furthermore, the method can discriminate laminated domain patterns that appear similar in VPFM and can reliably expose domain patterns that may not be seen in LPFM data from a single orientation, or even in 3D PFM data.

36 MATERIALS SCIENCE↗

Effects of V addition on recrystallization resistance of 7150 aluminum alloy after simulative hot deformation

The effects of different V contents (0.01 to 0.19 wt.%) on the recrystallization resistance of 7150 aluminum alloys during post-deformation heat treatment were investigated. The microstructural evolutions at as-cast, as-homogenized conditions and after post-deformation annealing were studied using optical, scanning electron and transmission electron microscopes and using the electron backscattered diffraction technique. The precipitation of Al{sub 21}V{sub 2} dispersoids was observed in alloys containing 0.11 to 0.19 wt.% V after homogenization. The dispersoids were mainly distributed in the dendrite cells, and the precipitate-free zones occurred in the interdendritic regions and near grain boundaries. V addition could significantly enhance the recrystallization resistance during post-deformation annealing, particularly in the presence of a great number of Al{sub 21}V{sub 2} dispersoids. Recrystallized grain growth was effectively restricted because of the dispersoid pinning effect. The alloy containing 0.15 wt.% V exhibited the highest recrystallization resistance amongst all V-containing alloys studied. - Highlights: • Investigated the effect of V level on microstructure and flow stress of 7150 alloys • Characterized microstructures using optical microscopy, SEM, TEM and EBSD • Described the precipitation behavior of V-dispersoids in the dendritic structure • Studied the V effect on recrystallization resistance during post heat treatment • V addition greatly enhanced the recrystallization resistance during annealing.

36 MATERIALS SCIENCE↗

Phase structures and morphologies of tempered CA6NM stainless steel welded by hybrid laser-arc process

The post-weld tempered microstructure of hybrid laser-arc welded CA6NM, a cast low carbon martensitic stainless steel, was investigated. The microstructural evolutions from the fusion zone to the base metal were characterized in detail using optical microscopy, scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), X-ray diffraction (XRD) and microhardness techniques. The fusion zone, in its post-weld tempered condition, consisted of tempered lath martensite, residual delta-ferrite with various morphologies, reversed austenite and chromium carbides. The reversed austenite, which can be detected through both EBSD and XRD techniques, was found to be finely dispersed along the martensite lath boundaries, particularly at triple junctions. Based on the EBSD analysis, the orientation relationship between the reversed austenite and the adjacent martensite laths seemed to follow the Kurdjumov-Sachs (K-S) model. The results also revealed the presence of the reversed austenite in the different regions of the heat affected zone after post-weld tempering. The microindentation hardness distribution was measured, and correlated to the evolution of the corresponding microstructure across the welds. - Highlights: •The EBSD analysis was performed on hybrid laser-arc welded CA6NM. •The FZ consisted of tempered lath martensite, reversed austenite, carbides and δ ferrite after tempering. •The reversed γ was formed along the α′ lath boundaries, particularly at triple junctions.

36 MATERIALS SCIENCE↗

Evolution of grain boundary character distributions in alloy 825 tubes during high temperature annealing: Is grain boundary engineering achieved through recrystallization or grain growth?

Grain boundary engineering (GBE) of nickel-based alloy 825 tubes was carried out with different cold drawing deformations by using a draw-bench on a factory production line and subsequent annealing at various temperatures. The microstructure evolution of alloy 825 during thermal-mechanical processing (TMP) was characterized by means of the electron backscatter diffraction (EBSD) technique to study the TMP effects on the grain boundary network and the evolution of grain boundary character distributions during high temperature annealing. The results showed that the proportion of ∑ 3{sup n} coincidence site lattice (CSL) boundaries of alloy 825 tubes could be increased to > 75% by the TMP of 5% cold drawing and subsequent annealing at 1050 °C for 10 min. The microstructures of the partially recrystallized samples and the fully recrystallized samples suggested that the proportion of low ∑ CSL grain boundaries depended on the annealing time. The frequency of low ∑ CSL grain boundaries increases rapidly with increasing annealing time associating with the formation of large-size highly-twinned grains-cluster microstructure during recrystallization. However, upon further increasing annealing time, the frequency of low ∑ CSL grain boundaries decreased markedly during grain growth. So it is concluded that grain boundary engineering is achieved through recrystallization rather than grain growth. - Highlights: •The grain boundary engineering (GBE) is applicable to 825 tubes. •GBE is achieved through recrystallization rather than grain growth. •The low ∑ CSL grain boundaries in 825 tubes can be increased to > 75%.

36 MATERIALS SCIENCE↗

Grain structure, texture and mechanical property evolution of automotive aluminium sheet during high power ultrasonic welding

High power ultrasonic spot welding (HPUSW) is a joining technique which is performed within less than a second and provides a more energy-efficient alternative to friction stir spot welding (FSSW), which is considered a longer cycle manufacturing process for joining automotive alloys. To date, only a few reports exist on the deformation mechanisms that take place during high power ultrasonic spot welding. In this work, dynamic recrystallization and grain growth were examined using electron backscatter diffraction (EBSD). HPUSW causes extensive deformation within the weld zone where the temperature increases to 440 °C. An ultra-fine grain structure was observed in a thin band of flat weld interface within a short welding time of 0.10 s. With increasing welding time the interface was displaced and ‘folds’ or ‘crests’ appeared together with shear bands. The weld interface progressively changed from flat to sinusoidal and eventually to a convoluted wave-like pattern when the tool fully penetrated the workpiece, having a wavelength of ~ 1 mm after 0.40 s. Finally, the microstructure and texture varied significantly depending on the location within the weld. Although the texture near the weld interface was relatively weak, a shift was observed with increasing welding time from an initially Cube-dominated texture to one where the typical β-fibre Brass component prevailed. - Highlights: •Lap shear strength of ~2.9 kN was achieved in 0.30 sec welding time. •Temperature approached 440 °C along the weld centreline for the highest welding time. •The texture near the teeth was dominated by Brass, P and S components at optimum condition. •The weld interface showed typical β-fibre deformation texture at optimum condition.

36 MATERIALS SCIENCE↗

Micromechanisms of grain refinement during extrusion of Mg–0.3 at.% Al at low homologous temperature

Coarse grained Mg–0.3 at.% Al (0.33 in wt.%) alloy was processed by direct extrusion with a reduction ratio of 25:1 at a temperature of ∼ 433 K. The extrusion remainder was removed from the die and analysed in three distinct zones: the cast billet, the conical zone of extrusion die, and the as-extruded rod. The zones were characterized by electron backscatter diffraction (EBSD) and light microscopy techniques to identify the processes responsible for grain refinement. Complex networks of (10–12) twins in practically all grains produced a noticeable microstructural fragmentation even before the material reached the conical zone of the die. Deformation twinning extended up to the entrance zone of the conical die where it was followed by a continuous dynamic recrystallization (CDRX) that gradually changed low angle boundaries to high angle boundaries. It is apparent that geometrically necessary dislocations play a crucial role in the formation of new grain boundaries. CDRX results in a bimodal structure with grain diameters ∼ 3 and ∼ 30 μm. As a material flows through the conical zone, the ratio of large to small grains is progressively decreased by CDRX in favour of fine grains. The as-extruded microstructure (a rod 8 mm in diameter), with an average grain diameter of ∼ 2.1 μm, shows a strong texture where the vast majority of grains (99.99%) have the c-axis oriented at least 30° from the extrusion direction. - Highlights: • Coarse grained Mg–0.3 at.% Al alloy was extruded at temperature of ∼ 433 K. • Processes responsible for grain refinement were analysed in extrusion remainder. • In the first stage, complex (10–12) twinning produced a noticeable fragmentation. • Deformation twinning was followed by continuous dynamic recrystallization. • 99.99% of grains in extruded rod have c-axis oriented > 30° from extrusion direction.

36 MATERIALS SCIENCE↗

Characterization of as-welded microstructure of heat-affected zone in modified 9Cr–1Mo–V–Nb steel weldment

Non-equilibrium microstructure of the heat-affected zone (HAZ) in the as-welded modified 9Cr–1Mo–V–Nb pipe steel (P91) weldment deposited by gas tungsten arc welding (GTAW) and flux core arc welding (FCAW) has been characterized by field-emission scanning electron microscope (FESEM) and electron backscatter diffraction (EBSD). The heterogeneous structures in the sub-layers of the as-welded HAZ are attributable to phase transformations caused by the welding thermal cycles and the local structure variations in the as-received base metal. Coarse-grained heat-affected zone (CGHAZ) has a prior austenite grain (PAG) size of 20 μm. Fine uniformly-distributed precipitates and a higher fraction of MX carbonitrides are observed in the CGHAZ. Fine-grained heat-affected zone (FGHAZ) consists of the finest grains (1.22 μm measured by EBSD, 5 μm PAG size), coarse undissolved M{sub 23}C{sub 6} carbides within the PAG boundaries and fine nucleated M{sub 23}C{sub 6} particles within the martensite laths. Inter-critical heat-affected zone (ICHAZ) consists of partially austenitized grains and over-tempered martensite laths. EBSD kernel average misorientation (KAM) map in the FGHAZ close to the ICHAZ illustrates the greatest local strain variations with a moderate normalized KAM value of 0.92°. The majority (88.1%) of the matrix grains in the CGHAZ are classified as deformed grains by EBSD grain average misorientation (GAM) evaluation. The FGHAZ close to the ICHAZ has the most recrystallized grains with an area fraction of 14.4%. The highest density variation of precipitates within grains in the FGHAZ originates from the inhomogeneous chemistry in the base metal. - Highlights: •A comprehensive characterization of the as-welded HAZ of P91 weldment is conducted. •Structural features in the each layer of the HAZ are quantified by EBSD. •Structural heterogenities in HAZ are due to welding cycle and base metal structure. •FGHAZ contains the finest grain structure and largest precipitate density variation.

36 MATERIALS SCIENCE↗

Synthesis of monocrystalline Ca{sub 3}SiO{sub 5} using the optical floating zone method

Alite (Ca{sub 3}SiO{sub 5}/C{sub 3}S with low concentrations of foreign ions) is the main constituent of Ordinary Portland Cement. Normally it forms during sintering but with quite low crystal sizes (ca. 30 μm). For experiments on alite hydration behavior monocrystalline grains are required. Due to its incongruent melting behavior and its thermodynamic instability below 1250 °C it is very challenging to obtain large alite single crystals. In the present study, the floating zone method was used for annealing polycrystalline rods of monoclinic and triclinic C{sub 3}S just below the melting point of the phase. Large monocrystalline grains (> 500 μm) of the monoclinic (Al, Mg-doped) and triclinic polymorphs could successfully be obtained. Monocrystallinity was demonstrated by electron backscatter diffraction (EBSD). The chemical composition regarding incorporation of foreign ions and thus the resulting crystallographic modification of the C{sub 3}S can easily be adjusted. Chemical homogeneity of the synthesized monocrystalline grains was proven by electron probe microanalysis (EPMA).

36 MATERIALS SCIENCE↗

Information or resolution: Which is required from an SEM to study bulk inorganic materials?: Evaluate SEMs’ practical performance

Significant technological advances in scanning electron microscopy (SEM) have been achieved over the past years. Different SEMs can have significant differences in functionality and performance. This work presents the perspectives on selecting an SEM for research on bulk inorganic materials. Understanding materials demands quantitative composition and orientation information, and informative and interpretable images that reveal subtle differences in chemistry, orientation/structure, topography, and electronic structure. The capability to yield informative and interpretable images with high signal-to-noise ratios and spatial resolutions is an overall result of the SEM system as a whole, from the electron optical column to the detection system. The electron optical column determines probe performance. The roles of the detection system are to capture, filter or discriminate, and convert signal electrons to imaging information. The capability to control practical operating parameters including electron probe size and current, acceleration voltage or landing voltage, working distance, detector selection, and signal filtration is inherently determined by the SEM itself. As a platform for various accessories, e.g. an energydispersive spectrometer and an electron backscatter diffraction detector, the properties of the electron optical column, specimen chamber, and stage greatly affect the performance of accessories. Ease-of-use and ease-of-maintenance are of practical importance. It is practically important to select appropriate test specimens, design suitable imaging conditions, and analyze the specimen chamber geometry and dimensions to assess the overall functionality and performance of an SEM. Finally, for an SEM that is controlled/operated with a computer, the stable software and user-friendly interface significantly affect the usability of the SEM.

36 MATERIALS SCIENCE↗

Quantifying the mechanical effects of He, W and He + W ion irradiation on tungsten with spherical nanoindentation

Here, recent advances in spherical nanoindentation protocols have proven very useful for capturing the grain-scale mechanical response of different metals. This is achieved by converting the load–displacement response into an effective indentation stress–strain response which reveals latent information such as the elastic–plastic transition or indentation yield strength and work-hardening behavior and subsequently correlating the response with the material structure (e.g., crystal orientation) at the indentation site. Using these protocols, we systematically study and quantify the microscale mechanical effects of He, W, and He + W ion irradiation on commercially pure, polycrystalline tungsten. The indentation stress–strain response is correlated with the crystal orientation from electron backscatter diffraction, the defect structure from transmission electron microscopy micrographs, and the stopping range of ions in matter calculations of displacement damage and He concentration. He-implanted grains show a much higher indentation yield strength and saturation stress compared to W-ion-irradiated grains for the same displacement damage. There is also good agreement between the dispersed barrier hardening model with a barrier strength of 0.5–0.8 and void models (Bacon–Kochs–Scattergood and Osetsky–Bacon models) with the experimentally observed changes in indentation strength due to the presence of He bubbles. This finding indicates that a high density (~ 9 × 10 23 m –3 ) and concentration (~ 1.5 at.%) of small (~ 1 nm diameter) He bubbles can be moderate to strong barriers to dislocation slip in tungsten.

36 MATERIALS SCIENCE↗

Relating microstructure to defect behavior in AA6061 using a combined computational and multiscale electron microscopy approach

In this paper, a multiscale electron microscopy-based approach is applied to understanding how different aspects of the microstructure in a notched AA6061-T6, including grain boundaries, triple junctions, and intermetallic particles, promote localized dislocation accumulation as a function of applied tensile strain and depth from the sample surface. Experimental measurements and crystal plasticity simulations of dislocation distributions as a function of distance from specified microstructural features both showed preferential dislocation accumulation near intermetallic particles relative to grain boundaries and triple junctions. High resolution electron backscatter diffraction and site-specific transmission electron microscopy characterization showed that high levels of dislocation accumulation near intermetallic particles led to the development of an ultrafine sub-grain microstructure, indicative of a much higher level of local plasticity than predicted from the coarser measurements and simulations. In addition, high resolution measurements in front of a crack tip suggested a compounding influence of intermetallic particles and grain boundaries in dictating crack propagation pathways.

36 MATERIALS SCIENCE↗

Direct observation of annealing-driven recrystallization behavior in magnesium alloy at low strain condition

Grain-twin interactions are significant in texture modification under thermodynamic driving force. In this study, annealing-driven twinning/detwinning behavior, grain growth, and corresponding texture evolution in a pre-deformed AZ31 magnesium alloy were systematically tracked and investigated via in-situ heating synchrotron X-ray diffraction and quasi in-situ electron backscattered diffraction techniques. A twinning texture is generated in the pre-deformed sample due to the activation of {$10\bar{1}2$} tensile twinning. During annealing, dislocation annihilation occurs between 100 and 280 °C, and recrystallization occurs above 280 °C, manifesting as the initial residual matrix and twins being competitively swallowed by each other, forming a bimodal texture. The recrystallization process is completed by boundary movement, which depends on the energy difference across the boundary. In addition, it is found that the grain boundaries favor movement towards the side with higher stored energy, regardless of the boundary type or the boundary energy.

In-situ observation↗

Microstructure and coercivity in alnico 9

Magnetic property enhancement of alnico, a rare-earth free permanent magnet, is highly dependent on both the initial microstructure and the evolution of the spinodal decomposition (SD) inside each grain during the heat treatment process. The size, shape and distribution of the magnetic FeCo-rich (α 1 ) phase embedded in continuous non-magnetic AlNi-rich (α 2 ) phase as well as a minor Cu-enriched phase residing in between are shown to be crucial in controlling coercivity. Phase and magnetic domain morphology in a commercial alnico 9 alloy was studied using a combination of structural characterization techniques, including scanning electron microscopy, electron backscatter diffraction, aberration-corrected scanning transmission electron microscopy and Lorentz microscopy. Our results showed that casting created structural nonuniformity and defects, such as porosity, TiS 2 precipitates and grain misorientation, are heterogeneously distributed, with the center section having the best crystallographic orientation and minimal defects. The optimal spinodal is a “mosaic structure”, composed of rod-shape α1 phase with {110} or {100} planar faceting and diameter of ~30–45nm. There is also a Cu-enriched phase residing at the corners of two < 110 > facets of the α1 phase. Furthermore, it was observed that grain boundary phase reverse magnetization direction at lower external magnetic field compared to the SD region inside the grain. Improving grain orientation uniformity, reducing detrimental grain boundary phase volume fraction, and the branching of the α 1 rods, as well as their diameter, are promising routes to improve energy product of alnico.

36 MATERIALS SCIENCE↗

Enhanced mechanical properties of carbon-doped FeNiMnAlCr high entropy alloy via hot-rolling

This work demonstrates an improvement in the mechanical performance of the high entropy alloy Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 containing 1.1 at. % carbon (CHEA) by hot-rolling followed by annealing at 1323 K. The microstructure was examined using scanning electron microscopy, electron backscatter diffraction, X-ray diffraction, and transmission electron microscopy. Room-temperature tensile tests were used to assess the alloy's mechanical properties. The presence of dense dislocation walls indicate that the alloy has not fully recrystallized and, moreover, the deformation substructure and the large fraction of Σ3 twin boundaries contribute to the high room temperature yield strength (~523 MPa). Despite the presence of substantial dislocation density, the annealed, hot-rolled CHEA displays an improvement in elongation to fracture (~33%) compared to the negligible ductility (< 2%) observed for the alloy after it has been simply annealed. Finally, the present work shows that hot rolling can produce good strength and ductility in the alloy while establishing the processing conditions necessary for the large-scale manufacture and utilization of its remarkable properties.

36 MATERIALS SCIENCE↗

Fundamental Study of Fatigue Crack Initiation at Grain and Twin Boundaries in Austentic Stainless Steel (Final Technical Report)

The overarching goal of this project was to understand the dislocation-based mechanisms driving fatigue crack initiation at grain and twin boundaries. The hypothesis of the work is that dislocation structures equivalent to persistent slip bands (PSBs) form in the boundaries, leading to local stress concentrations and fatigue crack initiation. The sub-goals associated with this work include: • Understanding the evolution of the dynamic stress state and dislocation density surrounding PSB/grain boundary interactions. This will require the development of new techniques that couple high resolution electron backscatter diffraction (HREBSD) with in situ scanning electron microscopy (SEM) deformation. • Uncover the mechanisms by which dislocations are accommodated in grain and twin boundaries during fatigue. The proposed approach here is to conduct in situ transmission electron microscopy (TEM) deformation experiments on fatigued samples. • Establish correlations between microstructure, deformation accommodation, and crack initiation across time and length scales. This work primarily focuses on understanding fatigue crack initiation in austenitic stainless steels, though promising work by an undergraduate researcher extended the work to high purity Al.

42 ENGINEERING↗

Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S32750

In the present work, the effect of grain size on deleterious phase precipitation in a superduplex stainless steel was investigated. The materials studied were heat treated isothermally at 800 deg. C, 850 deg. C and 900 deg. C for times up to 120 min. Hardness tests, light optical microscopy, scanning electron microscopy and X-ray diffraction were carried out to detect sigma and other harmful precipitate phases. The ferritic and austenitic grain sizes in the solution treated condition of the two steels analyzed were measured by electron backscattered diffraction (EBSD). Cyclic polarization corrosion tests were performed to evaluate the effect of grain size on the corrosion resistance. The results presented show that the precipitation of deleterious phases such as {chi}, {sigma} and {gamma}{sub 2}, which can occur during welding and forming operations, is retarded by grain growth.

36 MATERIALS SCIENCE↗