Fracture temperature and flaw growth in nitronic 40 at cryogenic temperatures

The fracture resistance and fatigue response of Armco Nitronic 40 austenitic stainless steel were evaluated under cryogenic conditions. Tensile, fracture toughness and fatigue crack growth properties were measured at -275 F. The tensile yield strength was approximately 120 ksi and the fracture toughness was estimated to be 350 ksi-in /2 on the basis of fracture toughness measurements. Testing was conducted to evaluate the behavior of a simulated section of the wing of the Pathfinder 1 model subject to a load and temperature history typical of that for testing in the National Transonic Facility. The wing section model incorporated a proposed brazing technique for pressure-transducer attachment. The simulated wing section performed satisfactorily at stress levels of nearly 60 percent of the material yield strength. The brazing technique proved to be an effective method of transducer attachment under conditions of high stress levels and large temperature excursions.

Domack, M. S.↗

Anisotropic Tensile Properties of a 14YWT Nanostructured Ferritic Alloy: On the Role of Cleavage Fracture

Two plates of nanostructured ferritic alloy NFA-1 were processed by ball milling atomized Fe-14Cr-3W-0.4Ti-0.2Y (wt.%) with FeO powders, canning, and hot-extrusion at 850 °C, followed by annealing and multipass cross-rolling at 1000 °C. This produces a severe (001) brittle cleavage texture on planes running parallel to the plate faces. In the first plate (P1), pre-existing microcracks (MCs) formed on the cleavage planes during cross-rolling. The second plate (P2) contained far fewer, if any, MCs. Here, we compare the tensile data for out-of-plane (S) and in-plane (L) tensile axis orientations, at temperatures from −196 °C to 800 °C. We also assess the tensile property differences between P1 and P2, and the effect of specimen size. The L-orientation strength and ductility were excellent; for example, the room temperature (RT) yield stress, σy ≈ 1042 ± 102 MPa, and the total elongation, εt ≈ 12.9 ± 1.5%. In contrast, the S-orientation RT σy ≈ 708 ± 57 MPa, and εt ≤ 0.2%. These differences were due to cleavage on the brittle (001) planes. Cleavage leads to beneficial delamination toughening, but is deleterious to deformation processing and through-wall heat transfer. Therefore, it is important to quantitatively characterize the pronounced NFA-1 strength anisotropy due to severe crystallographic texturing and cleavage fracture.

Crystallography↗

Sustainable bioplastics derived from renewable natural resources for food packaging

Food packaging is one of the leading sectors for the end use of plastics. Bioplastic is produced from natural renewable resources such as crops, wood pulp, and herbaceous fibers. This article summarizes the rational design of bioplastics from natural resources for food packaging. The bioplastic properties considered include thermal properties, mechanical performance, oxygen/moisture resistance, and biodegradability. Bioplastic degradability and technologies for handling bioplastic waste are discussed. Various aspects of the sustainability of bioplastics (e.g., environmental profile, techno-economic analysis, and societal impact) are investigated. The main challenges of bioplastic application, such as low fracture strain and inferior barrier properties, are discussed. Mitigation approaches to overcome the mechanical properties of bioplastics, such as adding plasticizers, are also discussed. Bioplastic can have properties comparable with fossil-based plastics. In conclusion, bioplastic can be an alternative to conventional plastic in most applications of food packaging, which can reduce the carbon footprint and environmental impact because of its biodegradability.

09 BIOMASS FUELS↗

Supramolecular dynamic binary complexes with pH and salt-responsive properties for use in unconventional reservoirs

Hydraulic fracturing of unconventional reservoirs has seen a boom in the last century, as a means to fulfill the growing energy demand in the world. The fracturing fluid used in the process plays a substantial role in determining the results. Hence, several research and development efforts have been geared towards developing more sustainable, efficient, and improved fracturing fluids. Herein, we present a dynamic binary complex (DBC) solution, with potential to be useful in the hydraulic fracturing domain. It has a supramolecular structure formed by the self-assembly of low molecular weight viscosifiers (LMWVs) oleic acid and diethylenetriamine into an elongated entangled network under alkaline conditions. With less than 2 wt% constituents dispersed in aqueous solution, a viscous gel that exhibits high viscosities even under shear was formed. Key features include responsiveness to pH and salinity, and a zero-shear viscosity that could be tuned by a factor of ~280 by changing the pH. Furthermore, its viscous properties were more pronounced in the presence of salt. Sand settling tests revealed its potential to hold up sand particles for extended periods of time. In conclusion, this DBC solution system has potential to be utilized as a smart salt-responsive, pH-switchable hydraulic fracturing fluid.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing complex subsurface dynamics with continuous seismic monitoring: Observations using distributed acoustic sensing and surface orbital vibrators during hydraulic fracturing

Understanding hydraulic fracturing is crucial to improving the stimulation of unconventional reservoirs and increasing fluid production. This study develops a novel seismic monitoring technology using distributed acoustic sensing (DAS) and surface orbital vibrators (SOV) to capture fracture seismic response and mechanical properties at high temporal intervals. We analyze continuous time-lapse vertical seismic profiling (VSP) data acquired every hour during the first nine days of treatment of an unconventional reservoir in the Austin Chalk/Eagle Field Laboratory. The VSP data contain clear seismic signals scattered from the activated fractures. The spatiotemporal changes of the fracture reflectivity revealed by the SOV/DAS data correlate well with the observations of fracture locations inferred from low-frequency DAS data. These results capture the fracture opening and closure processes, as well as highlight potential prestage activations of the fractures due to hydraulic connectivity with preexisting fracture systems. Therefore, analysis of the presented data set provides a unique opportunity to understand fracture initiation and subsequent evolution, not only in the context of unconventional resources but also in enhanced geothermal systems.

Correa, Julia↗

Measuring Mechanical Properties Of Optical Glasses

Report discusses mechanical tests measuring parameters of strength and fracture mechanics of optical glasses. To obtain required tables of mechanical properties of each glass of interest, both initial-strength and delayed-fracture techniques used. Modulus of rupture measured by well-known four-point bending method. Initial bending strength measured by lesser-known double-ring method, in which disk of glass supported on one face near edge by larger ring and pressed on its other face by smaller concentric ring. Method maximizes stress near center, making it more likely specimen fractures there, and thereby suppresses edge effects. Data from tests used to predict reliabilities and lifetimes of glass optical components of several proposed spaceborne instruments.

Tucker, Dennis S.↗

Gear Crack Propagation Path Studies: Guidelines for Ultra-Safe Design

Design guidelines have been established to prevent catastrophic rim fracture failure modes when considering gear tooth bending fatigue. Analysis was performed using the finite element method with principles of linear elastic fracture mechanics. Crack propagation paths were predicted for a variety of gear tooth and rim configurations. The effects of rim and web thicknesses, initial crack locations, and gear tooth geometry factors such as diametral pitch, number of teeth, pitch radius, and tooth pressure angle were considered. Design maps of tooth/rim fracture modes including effects of gear geometry, applied load, crack size, and material properties were developed. The occurrence of rim fractures significantly increased as the backup ratio (rim thickness divided by tooth height) decreased. The occurrence of rim fractures also increased as the initial crack location was moved down the root of the tooth. Increased rim and web compliance increased the occurrence of rim fractures. For gears with constant pitch radii, coarser-pitch teeth increased the occurrence of tooth fractures over rim fractures. Also, 25 deg pressure angle teeth had an increased occurrence of tooth fractures over rim fractures when compared to 20 deg pressure angle teeth. For gears with constant number of teeth or gears with constant diametral pitch, varying size had little or no effect on crack propagation paths.

Lewicki, David G.↗

Influence of heat treatment on mechanical properties of 300M Steel

The plane strain fracture toughness and tensile strength response of 300M Steel to a wide variety of austenitizing and tempering temperatures were investigated. The results make it possible for one to select heat treatments which provide an optimum combination of strength and toughness for a variety of structural applications. In particular, improvements in toughness on the order of 20% were found possible with no loss in tensile properties by increasing the austenitizing temperature from the currently employed 1144 K to 1255 K or higher, and this change in heat treatment therefore appears worthy of general implementation.

Youngblood, J. L.↗

Reactive flash sintering of TiZrN and TiAlN ternary metal nitrides

Here, this study demonstrated the reactive flash sintering (RFS) for two powder mixtures: TiN-ZrN (both conducting) and AlN-TiN (TiN conducting but AlN insulating), targeting ternary metal nitrides (TMN) of Ti 0.5 Zr 0.5 N and Ti 0.5 Al 0.5 N, respectively. A constant volage and pressure (e.g., 8 V DC, ∼15 MPa) at room temperature triggered the flash (current density up to 27 A/mm 2 ) without pre-heating, and the entire RFS process finished in a few minutes. For TiZrN, the flash was instantaneous whereas for TiAlN, there was a long incubation before the flash followed by a quick and dramatic flash. Both conventional ex situ XRD and in situ synchrotron study had been carried out. They showed a uniform Ti 0.57 Zr 0.43 N solution formed in RFS and persisted upon cooling, while (Ti, Al) N solid solution formed at high temperature was not stable and likely went through a very quick phase separation in the cooling process. The final products from RFS had been characterized using SEM/EDS for microstructure. Both TiZrN and TiAlN were dense. Distribution of Ti, Zr, and N was uniform for TiZrN; for TiAlN, Ti and N distribution was uniform, while association of Al with oxygen was observed. TGA-DSC revealed the onset oxidation temperature for TiZrN was comparable to TiN and ZrN, while it was higher by ∼200 °C for TiAlN, likely due to the formation of Al 2 O 3 . In terms of mechanical properties such as hardness or fracture toughness, forming a single-phase solid solution (like TiZrN) does not offer obvious benefits. while large grain size from RFS seemed to be unfavorable. Future optimization of RFS condition and in-depth study by both experiments and simulation are needed to fully understand the composition-processing-structure-property relationships for such TMN from the reactive flash sintering process.

Flash Sintering↗

A Multi-Parameter Approach for Calculating Crack Instability

An accurate fracture control analysis of spacecraft pressure systems, boosters, rocket hardware and other critical low-cycle fatigue cases where the fracture toughness highly impacts cycles to failure requires accurate knowledge of the material fracture toughness. However, applicability of the measured fracture toughness values using standard specimens and transferability of the values to crack instability analysis of the realistically complex structures is refutable. The commonly used single parameter Linear Elastic Fracture Mechanics (LEFM) approach which relies on the key assumption that the fracture toughness is a material property would result in inaccurate crack instability predictions. In the past years extensive studies have been conducted to improve the single parameter (K-controlled) LEFM by introducing parameters accounting for the geometry or in-plane constraint effects]. Despite the importance of the thickness (out-of-plane constraint) effects in fracture control problems, the literature is mainly limited to some empirical equations for scaling the fracture toughness data] and only few theoretically based developments can be found. In aerospace hardware where the structure might have only one life cycle and weight reduction is crucial, reducing the design margin of safety by decreasing the uncertainty involved in fracture toughness evaluations would result in lighter hardware. In such conditions LEFM would not suffice and an elastic-plastic analysis would be vital. Multi-parameter elastic plastic crack tip field quantifying developments combined with statistical methods] have been shown to have the potential to be used as a powerful tool for tackling such problems. However, these approaches have not been comprehensively scrutinized using experimental tests. Therefore, in this paper a multi-parameter elastic-plastic approach has been used to study the crack instability problem and the transferability issue by considering the effects of geometrical constraints as well as the thickness. The feasibility of the approach has been examined using a wide range of specimen geometries and thicknesses manufactured from 7075-T7351 aluminum alloy.

Zanganeh, M.↗

High-strength silicon carbides by hot isostatic pressing

Silicon carbide has strong potential for heat engine hardware and other high-temperature applications because of its low density, good strength, high oxidation resistance, and good high-temperature creep resistance. Hot isostatic pressing (HIP) was used for producing alpha and beta silicon carbide (SiC) bodies with near-theoretical density, ultrafine grain size, and high strength at processing temperatures of 1900 to 2000 C. The HIPed materials exhibited ultrafine grain size. Furthermore, no phase transformation from beta to alpha was observed in HIPed beta-SiC. Both materials exhibited very high average flexural strength. It was also shown that alpha-SiC bodies without any sintering aids, when HIPed to high final density, can exhibit very high strength. Fracture toughness K (sub C) values were determined to be 3.6 to 4.0 MPa m (sup 1/2) for HIPed alpha-SiC and 3.7 to 4.1 MPa m (sup 1/2) for HIPed beta-SiC. In the HIPed specimens strength-controlling flaws were typically surface related. In spite of improvements in material properties such as strength and fracture toughness by elimination of the larger strength-limiting flaws and by grain size refinement, HIPing has no effect on the Weibull modulus.

Dutta, Sunil↗

High-strength silicon carbides by hot isostatic pressing

Silicon carbide has strong potential for heat engine hardware and other high-temperature applications because of its low density, good strength, high oxidation resistance, and good high-temperature creep resistance. Hot isostatic pressing (HIP) was used for producing alpha and beta silicon carbide (SiC) bodies with near-theoretical density, ultrafine grain size, and high strength at processing temperatures of 1900 to 2000 C. The HIPed materials exhibited ultrafine grain size. Furthermore, no phase transformation from beta to alpha was observed in HIPed beta-SiC. Both materials exhibited very high average flexural strength. It was also shown that alpha-SiC bodies without any sintering aids, when HIPed to high final density, can exhibit very high strength. Fracture toughness K (sub C) values were determined to be 3.6 to 4.0 MPa m (sup 1/2) for HIPed alpha-SiC and 3.7 to 4.1 MPa m (sup 1/2) for HIPed beta-SiC. In the HIPed specimens strength-controlling flaws were typically surface related. In spite of improvements in material properties such as strength and fracture toughness by elimination of the larger strength-limiting flaws and by grain size refinement, HIPing has no effect on the Weibull modulus.

Dutta, Sunil↗

Molecular scale insight of pore morphology relation with mechanical properties of amorphous silica using ReaxFF

Porous materials are typically heterogeneous and they contain large variations of micro-/nano-pore structures, causing complicated behaviors. In continuum models, most mechanical properties of porous materials are estimated based on porosity, while the variations of micro/nano structures are ignored. That could be problematic as the microscopic heterogeneity may affect the mechanical response of porous materials. Thus, understanding micro/nano heterogeneity impact has been the focus in many scientific and engineering subjects. In the present study, we investigated the effect of nanopore structure (including pore shape and orientation) as well as porosity on mechanical properties of amorphous silica (a-SiO 2 ). The pore sizes in our simulations are comparable to the corresponding ones observed in a-SiO 2 based materials. We found that the existing of nanopores strongly influences Young’s modulus (E) and critical energy release rate (G IC ). These properties decrease with increasing porosity. Importantly, the impact of nanopores was characterized by structural parameters of porous materials. In addition to dependency on porosity, Young’s modulus also was found to vary as a function of potential energy per atom, which highly depends on nanopore shape. Furthermore, critical energy release rate was found to increase with increasing ligament length (also known as pore wall thickness). Finally, the results highlighted the importance of nanopore structures, which must be taken into account when studying fracture mechanisms in porous materials. Based on our findings, it was proposed that mechanical properties of porous materials can be controlled by nano-engineering pore structures.

36 MATERIALS SCIENCE↗

Friction stir processing: A thermomechanical processing tool for high pressure die cast Al-alloys for vehicle light-weighting

This study uses friction stir processing (FSP) for thermomechanical processing of high-pressure die-casting (HPDC) to modify microstructure and improve mechanical properties. FSP is carried out on two different HPDC aluminum alloys: (a) general-purpose, high-iron, HPDC A380 alloy and (b) premium quality, low-iron HPDC Aural-5 alloy in thin wall, flat plate geometry. Subsequent mechanical testing shows ~30 % and ~65 % enhancement in yield strength and tensile ductility. In addition, FSP leads to ~10 times improvement in fatigue life for A380 alloy and ~70 % improvement in fracture toughness for Aural-5 alloy. These findings emphasize the capability of FSP to modify the microstructure of HPDC Al-alloys-based structural components so that they can demonstrate a good combination of strength, ductility, fracture toughness, and high fatigue properties for long-term durability and reliability.

36 MATERIALS SCIENCE↗

Reactive Transport Modeling of Mineral Precipitation and Carbon Trapping in Discrete Fracture Networks

In this study we use numerical experiments to analyze reactive flow and transport behavior in discrete intersecting fracture networks, focusing on (a) how reaction-induced changes in physical and chemical properties affect flow connectivity and (b) how fracture networks developed in the Earth's critical zone contribute to carbon sequestration via mineral weathering reactions. In the first part of the study, we used two-dimensional reactive flow and transport simulations to analyze the impacts of mixing in a natural discrete fracture network. We concluded that reaction-induced changes can substantially alter the flow connectivity, especially at fracture intersections. The second set of simulations considered the problem of natural weathering of fractured mafic and ultramafic rocks in the partially saturated Earth's critical zone as a function of infiltration rates, fracture permeability, and partially saturated flow parameters. As a model system, we considered an incongruent reaction network with dissolution of forsterite and precipitation of magnesite. The behavior is complex in terms of the rate-controlling processes because of the multicomponent nature of the system as shown by the grid Peclet number: the CO 2 behavior is gas diffusion-controlled in the partially saturated zone, while the rate of water flow via the Damkӧhler number controls Mg 2+ transport through the fracture network. The amounts of carbon that can be trapped are modest, but the naturally fractured domain considered here provides a useful “base case” against which various engineered solutions can be compared.

58 GEOSCIENCES↗

Admittance Survey of Type 1 Coronae on Venus: Implications for Elastic Thickness

Coronae are volcano-tectonic features on Venus which range from 60km to 2600km and are defined by their nearly circular patterns of fractures. Type 1 (regular) coronae are classified as having >50% complete fracture annuli. Previous work has examined the factors controlling the morphology, size, and fracture pattern of coronae, using lithospheric properties, loading signature and geologic characteristics. However, these studies have been limited to Type 2 (topographic) coronae (e.g. coronaes with <50% fracture annuli), and the factors controlling the formation of Type 1 coronae remain poorly understood. In this study, we apply the methodology of to survey the admittance signature for Type 1 coronae to determine the controlling parameters which govern Type 1 coronae formation.

Hoogenboom, T.↗

Gear Crack Propagation Path Studies-- Guidelines Developed for Ultrasafe Design

Effective gear designs balance strength, durability, reliability, size, weight, and cost. However, unexpected gear failures may occur even with adequate gear tooth design. To design an extremely safe system, the designer must ask and address the question "What happens when a failure occurs?" With regard to gear-tooth bending fatigue, tooth or rim fractures may occur. For aircraft, a crack that propagated through a rim would be catastrophic, leading to the disengagement of a rotor or propeller, the loss of an aircraft, and possible fatalities. This failure mode should be avoided. However, a crack that propagated through a tooth might or might not be catastrophic, depending on the design and operating conditions. Also, early warning of this failure mode might be possible because of advances in modern diagnostic systems. An analysis was performed at the NASA Glenn Research Center to develop design guidelines to prevent catastrophic rim fracture failure modes in the event of gear-tooth bending fatigue. The finite element method was used with principles of linear elastic fracture mechanics. Crack propagation paths were predicted for a variety of gear tooth and rim configurations. The effects of rim and web thicknesses, initial crack locations, and gear-tooth geometry factors such as diametral pitch, number of teeth, pitch radius, and tooth pressure angle were considered. Design maps of tooth and rim fracture modes, including the effects of gear geometry, applied load, crack size, and material properties were developed. The occurrence of rim fractures significantly increased as the backup ratio (rim thickness divided by tooth height) decreased. The occurrence of rim fractures also increased as the initial crack location was moved down the root of the tooth. Increased rim and web compliance increased the occurrence of rim fractures. For gears with constant-pitch radii, coarser-pitch teeth increased the occurrence of tooth fractures over rim fractures. Also, 25 degree pressure angle teeth increased the occurrence of tooth fractures over rim fractures in comparison to 20 pressure angle teeth. For gears with a constant number of teeth or for gears with constant diametral pitch, varying size had little or no effect on crack propagation paths.

Lewicki, David G.↗

Ethynyl-Terminated Imidothioethers And Derived Resins

New toughened epoxies exhibit excellent properties, but temperatures at which used limited. Bismaleimide resins some of base materials being formulated to develop materials used at moderate temperatures. Work conducted on use of acetylenic (ethynyl) group to cross-link and extend chains of oligomers and polymers to obtain materials that perform at high temperatures. Work extended to ethynyl-terminated imidothioethers (ETI's). Tested primarily as adhesives and composite matrices and found to have useful properties in terms of processing, resistance to high temperature, fracture toughness, and resistance to solvents. Also have desirable mechanical properties. Potentially useful for aerospace and nonaerospace applications.

Hergenrother, Paul M.↗