Trapping helium in Y{sub 2}Ti{sub 2}O{sub 7} compared to in matrix iron: A first principles study
Pyrochlore Y{sub 2}Ti{sub 2}O{sub 7} is a primary precipitate phase in nano-structured ferritic alloys (NFAs) for fission and fusion energy applications. We report a theoretical study for assessing the relative stability of trapping helium in Y{sub 2}Ti{sub 2}O{sub 7} versus in matrix iron. Various defect structures and the associated energies are examined and compared. Results reveal that helium can be deeply trapped in Y{sub 2}Ti{sub 2}O{sub 7} and that the corresponding self-interaction is essentially repulsive. Transmutant helium in NFAs prefers to occupy individual octa-interstitial sites in Y{sub 2}Ti{sub 2}O{sub 7}, before forming small clusters in Y{sub 2}Ti{sub 2}O{sub 7}. Helium partitioning in NFAs depends on the number and dispersion of Y{sub 2}Ti{sub 2}O{sub 7}; and thus initially, bubble formation and growth in iron matrix can be largely suppressed. Charge transfer occurs from helium to neighboring oxygen anions, but not to neighboring metal cations, suggesting a general effectiveness of trapping helium in oxides. Reasons for the ultimate fate of helium to form small nm-scale interface bubbles are also discussed.