SEARCH · Search NASA
Results for “STEEL ALLOYS - STRENGTH”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Dissimilar Brazing of Ti-6Al-4V to Stainless Steel using Silver-Based Braze Alloys
Explore the source record for details and available documents.
State-of-the-art survey of dissimilar metal joining by solid state welding
State-of-the-art of dissimilar metal joining by solid state diffusion bonding and roll and press welding, emphasizing stainless steel and aluminum alloy
Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability (CRADA NFE-21-08888 Final Report)
Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. Eck Industries successfully casted Al-Ce-Mg heat exchanger. ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.
Reconstitution of Sandia's Melt Laboratory: A Strategic Approach to Address Alloy Procurement and Quality Challenges - Part 1
In recent years, the procurement of essential materials such as Stainless Steels, Ni-Alloys, and Kovar has become increasingly challenging. Lead times for these materials have extended to over 24 months, placing significant stress on the reliability of attaining these alloys. This situation is exacerbated by the supplier’s minimum purchase requirement of excessively large quantities to meet unique purchase order (PO) requirements which is usually above the maximum requirements of Sandia National Laboratories (SNL). Additionally, the reluctance of foundries to engage in small lot development for SNL specific needs further complicates the procurement process. This white paper explores the reconstitution of SNL’ Melt Laboratory as a strategic solution to mitigate these challenges.
On the mechanical alloying of novel austenitic dual-precipitation strengthened steels
Not Available
Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability
• Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. • Eck Industries successfully casted Al-Ce-Mg heat exchanger. • ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. • Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. • ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. • In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.
Alloy 625 Qualification Pathway for ASME Section III Division 5 Class A construction
The American Society of Mechanical Engineers Boiler and Pressure Vessel Code Section III Division 5 provides construction and inspection rules to ensure the safety of nuclear components operating at elevated temperatures, defined as those operating above 700°F (370°C) or 800°F (425°C), depending on the material type. At present, there are six materials approved for Class A (high safety significance) component construction under ASME BPVC Section III Division 5. Out of these six materials, five materials are steels or iron-based alloys and one material, Alloy 617, is a nickel alloy. Nickel alloys are stronger than steels; however, Alloy 617 consists of 10-15% cobalt, and activation is a concern under irradiation. Therefore, there is a need to qualify new nickel alloy with lower cobalt content. Alloy 625 is one candidate which has similar mechanical properties at elevated temperature compared to Alloy 617 and has a maximum of 1% cobalt. Although Alloy 625 material properties have been developed in the past to support allowable stress development under ASME Section II, new test results would be needed to qualify this material for elevated temperature component construction under ASME Section III Division 5. The purpose of this report is to describe a path towards developing a Nuclear Code Case to qualify Alloy 625 (UNS N06625; Grade 1 and Grade 2) for elevated temperature nuclear use in accordance with the ASME BPVC rules. This report reviews the existing database on Alloy 625, presents proposed test campaign, and discusses potential paths for accelerating the accelerated material qualification process.
A Modified Embedded-Atom Method Potential for a Quaternary Fe-Cr-Si-Mo Solid Solution Alloy
Ferritic-martensitic steels, such as T91, are candidate materials for high-temperature applications, including superheaters, heat exchangers, and advanced nuclear reactors. Considering these alloys’ wide applications, an atomistic understanding of the underlying mechanisms responsible for their excellent mechano-chemical properties is crucial. Here, we developed a modified embedded-atom method (MEAM) potential for the Fe-Cr-Si-Mo quaternary alloy system—i.e., four major elements of T91—using a multi-objective optimization approach to fit thermomechanical properties reported using density functional theory (DFT) calculations and experimental measurements. Elastic constants calculated using the proposed potential for binary interactions agreed well with ab initio calculations. Furthermore, the computed thermal expansion and self-diffusion coefficients employing this potential are in good agreement with other studies. This potential will offer insightful atomistic knowledge to design alloys for use in harsh environments.
Recent progress in the design of the K-DEMO divertor
The preliminary conceptual design of the Korean fusion demonstration reactor (K-DEMO) with a major radius of 6.8 m and the fusion power of 2200 MW has been studied since 2012. The overall configuration of the K-DEMO divetor system based on the ITER-like water-cooled tungsten technology is a double-null type symmetric divertor subdivided into 32 toroidal modules for the vertical maintenance. A detached divertor scenario with impurity seeding was considered as the primary approach for the power exhaust to reduce the peak heat flux lower than the engineering limit of 10 MW/m 2 . The power exhaust performance at the scrap off layer was estimated by using UEDGE-2D code, a two-dimensional fluid transport code for collisional edge plasma and neutral species like N, Ne, and Ar. Particle and heat flux on inboard and outboard divertor targets were calculated for the detached cased depending on parameters such as the impurity seeding rate, pumping rate, and the pedestal density. On the other hand, a magnetic solution like X-divertor, snowflake divertor, and super X-divertor to expand the plasma wet area was considered for K-DEMO since the detached divertor increasing a radiation fraction by impurity seeding might be able to be unstable. However, the extremely high current of poloidal coils was required more than the engineering limit, 20 MA, to form magnetic field lines for the alternative divertors. Based on the physical calculation of the edge plasma, engineering analyses were carried out to find out the thermal and structural reliability. The thermo-hydraulic analysis confirmed thermal stability, whether all comprising materials are operating within their allowable temperature windows when the case of the peak heat flux is set to 10 MW/m 2 on the outboard divertor target. The response surface optimization method derived two optimal design candidates employing two kinds of heat sink materials, respectively: the reduced activation ferritic martensitic (RAFM) steel and CuCrZr alloy. Additionally, the drawbacks and merits of the two materials were definite. The optimal design with applying RAFM steel was vulnerable to withstand thermal and mechanical loads since low thermal conductivity caused too thin thickness of the heat sink. On the other hand, the CuCrZr alloy has critical drawbacks in terms of activation and radioactive waste despite its high thermal conductivity. Meanwhile, preliminary electromagnetic (EM) analysis was carried out to estimate the EM loads caused by the abnormal behaviors of plasma since EM loads are one of the most critical external loads for designing a DEMO divertor.
Internal carburization and scale formation on austenitic steels in supercritical carbon dioxide
Direct-fired supercritical CO 2 (sCO 2 ) power cycles are being commercialised to revolutionise fossil energy as a low-emission power source. In order to lower the cost of this technology, less expensive steels are needed in the lower temperature segments of the cycle. However, there are concerns about internal carburisation of steels in sCO 2 . A consistent observation is that thin, Cr-rich oxides appear to reduce C ingress compared to thick Fe-rich oxides formed on 9–12% Cr ferritic-martensitic steels. Advanced austenitic stainless steels (SS) like alloy 709 (20Cr-25Ni) are able to continue to form Cr-rich oxides at 650°C, while a conventional type 316 H SS formed a Fe-rich scale. The C diffusion profiles in SS specimens were quantified at 550°C–650°C using glow discharge optical emission spectroscopy and electron probe microanalysis. Analytical transmission electron microscopy was used to compare the thin protective Cr-rich oxide formed on alloy 709 in sCO 2 at 650°C to that formed in ambient air.
Additive manufacturing of amorphous metal soft magnetic composites
Soft magnet alloys are used as magnetic cores for electric motors, transformers, wind turbines and other power generation systems. Soft magnetic cores are expensive and time consuming to manufacture in the complex shapes required for next-generation devices using conventional press and sinter powder metallurgy. The objective of this effort is to additively manufacture high performance soft magnets, with reduced cost and reduced material waste and 10x lower energy (core) loss at the high operating frequencies of many electric machines. Laser powder bed fusion additive manufacturing is used as the fabrication method. Electrical steel and amorphous alloys atomized powders are used as a feedstock materials. Magnetic cores are printed in topology optimized structures such as the Hilbert curve because this has been shown to reduce energy losses by minimizing the eddy currents that circulate within the magnet at high frequencies. In our project, we succeed in printing FeSi 3.5wt% and FeSi 6.5wt% electrical steels, and iron-based soft magnetic amorphous alloys in the shape of Hilbert and Peano curve topology optimized structures. We found that the Peano curve has a higher cut-off frequency than the Hilbert curve, and that amorphous alloys have high cut-off frequencies and higher mechanical hardness than electrical steels. Processing conditions such as laser power, scan speed, and hatching pattern were optimized to achieve high density prints, and optimize magnetic performance. We find that the printing of amorphous alloy soft magnetic cores may be technoeconomically feasible for large scale applications such as transformers, for which supply chain issues and the labor costs of manual fabrication of magnetic cores is prohibitive in some cases.
Brazing titanium to stainless steel
Titanium and stainless-steel members are usually joined mechanically for lack of any other effective method. New approach using different brazing alloy and plating steel member with nickel resolves problem. Process must be carried out in inert atmosphere.
Impact of Hydrogen Combustion on the Oxidation-induced Degradation of Heavy-duty Diesel Engine Piston Materials
High temperature ferritic-martensitic steels are candidate materials for heavy-duty diesel engine pistons. The envisioned transition to hydrogen blended fuels is expected to alter the post-combustion atmosphere in the engines, primarily resulting in a higher water vapor content (> 20 vol%) and potentially higher exhaust gas temperatures. The oxidation resistance of existing and newly developed alloys will be a critical life-limiting mechanism under these conditions. In the present work, the oxidation behavior of candidate piston alloys was evaluated in air+10 vol.% H2O and air+30 vol.% H2O at 700°C. Thermal cyclic (1h cycle) exposures were conducted for two variants of commercial UNSS42200 ferritic-martensitic steel and two developmental alloy steels for up to 300h. The developmental alloys each have similar compositions but with one containing elevated Cu levels of 3 wt.%, A significant reduction in resistance to breakaway oxidation was observed for the commercial alloys in the higher water vapor atmosphere. Microstructural characterization (optical metallography, scanning electron microscopy and electron microprobe analysis) revealed the formation of thick Fe-rich oxides even for the high Cr (~12 wt.%) steels after an initial stage of protective oxidation with MnCr-rich spinels. The impact of the evaporation-induced loss of Cr on the time and temperature dependent compositional changes in the alloys was correlated with experimental findings. For the developmental alloys, Cu additions appear to play a role in significantly reducing oxidation kinetics in air+30 vol.% H2O at 700°C.
Design of an additively manufactured functionally graded material of 316 stainless steel and Ti-6Al-4V with Ni-20Cr, Cr, and V intermediate compositions
This study presents a method for designing a computationally informed gradient pathway to fabricate a functionally graded material (FGM) with terminal alloys of 316 stainless steel (SS316) and Ti-6Al-4V via directed energy deposition additive manufacturing with powder feedstock. In this work, the grading is accomplished through the introduction of intermediate elements and alloys (Ni-20Cr, Cr, and V) to avoid the brittle Fe-Ti intermetallic phases that form in the direct liquid phase joining of Ti-alloys and stainless steels. Using a combination of equilibrium calculations and Scheil-Gulliver simulations, a compositional pathway was designed to avoid deleterious phases. FGM samples were fabricated and experimentally characterized to determine the viability of the pathway. A change in phases from fcc to bcc was predicted to occur within the Ni-20Cr/Cr gradient region, and this was validated through experimental characterization. No detrimental phases (intermetallic, Laves, or σ phases) formed along the gradient path, demonstrating a successful computationally-informed design and fabrication of an FGM from SS316 to Ti-6Al-4V.
Characterization of Precipitation-Strengthening Heat-Resistant Austenitic Stainless Steels for Life-Prediction Modeling
In this study, the role of minor alloying additions in 347H stainless steels (UNS34709, ASTM A240/240M) on creep-rupture properties at 650-750°C and microstructure evolution during isothermal exposure at 750°C has been investigated, aiming to provide the experimental dataset as boundary conditions of physics-based modeling for material/component life prediction. Four different 347H heats containing various amounts of boron and nitrogen additions were prepared and evaluated. The combined additions of B and N are found to stabilize the strengthening secondary M23C6 carbides and retarding the transition from M23C6 to sigma phase precipitates during thermal exposure. The observed kinetics of microstructure evolution reasonably explains the improvement of creep-rupture properties of 347H stainless steels with the B and N additions.
Burner rig alkali salt corrosion of several high temperature alloys
The hot corrosion of five alloys was studied in cyclic tests in a Mach 0.3 burner rig into whose combustion chamber various aqueous salt solutions were injected. Three nickel-base alloys (IN-792, IN-738, and IN-100), a cobalt-base alloy (MM-509), and an iron-base alloy (304 stainless steel) were studied at temperatures of 700, 800, 900, and 1000 C with various salt concentrations and compositions. The relative resistance of the alloys to hot corrosion attack was found to vary with temperature and with both the concentration and composition of the injected salt solution. Results indicate that the corrosion of these alloys is a function of both the presence of salt condensed as a liquid on the surface and of the composition of the gas phases present.