Search NASA⌕ Search

SEARCH · Search NASA

Results for “STEELS - CLEANING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

A Laboratory Corrosion Inhibition Study of Carbon Steel Using 2-Mercaptobenzothiazole (MBT) Under Post-Combustion CO2 Capture Conditions

Corrosion mitigation is an important aspect of amine-based post-combustion carbon dioxide (CO2) capture operations due to the desire to use less expensive but corrosion-vulnerable materials such as low carbon steels in the construction of a capture system. In this study, the corrosion behavior of A106 (grade B) carbon steel with an in-house proprietary amine-based solvent was investigated in a laboratory environment at 80°C using an organic corrosion inhibitor, 2-mercaptobenzothiazole (MBT). The corrosion inhibition mechanism was interpreted by electrochemical methods and surface analyses. The results revealed that the corrosion rates of carbon steel were significantly retarded using MBT. The critical inhibitor concentration was determined to be lie between 10 ppm and 50 ppm under the tested conditions.

Materials Science↗

Pitting Propagation Behavior on Low Alloy AISI 4130 (UNS G41300) Steel Exposed to Various Alkali and Alkaline Earth Metal Chlorides

Pit propagation studies were conducted to elucidate whether alkali and alkali earth metal cations such as Na+ and Rb+ present in the form of metal chloride salts such as RbCl affect pitting behavior in distinctly different manner than NaCl. Pit propagation studies were conducted on a low alloy steel using one-dimensional (1-D) pit method over pit depths from 300-1000 µm. LSV and EIS of planar electrodes of 4130 in a range of Cl- solutions were conducted and revealed no detected differences in impedance, open circuit, corrosion potential (Ecorr), passive current density (ipass), and pitting potential (Epit) as a function of salt type. In the case of one-dimensional pits during fast downward scan rates, the saturation potential (Esat) varied as a function of cation identity when pit depths were shallow. Mass transported limited current density also differed with cations in shallow pits when various alkali metal and alkaline metal cations were present. The limiting current density was increased for RbCl relative to NaCl The pit surface potential (Esurf) of activated pit surfaces reached Ecorr prior to establishing a condition where the pit electrolyte surface concentration (Csurf) was less than the critical concentration for active acidified pitting (i.e. Csurf<Ccrit) in this marginally passivating steel. For various Esurf and pit current density (ipit) combinations at constant Csurf where Ccrit< Csurf < Csat, E-log(i) plots were constructed using the method of Tianshu to create IR ohmic voltage corrected Tafel plots for various fixed pit solution concentrations. Under these conditions, the influence of cation identity on charge transfer controlled kinetics indicated slight differences in Tafel behavior where RbCl was slightly more aggressive than NaCl for low alloy steel oxidation. Differences in metal cation identity exert no effect on passive or breakdown on planar electrodes and only effect pit propagation stage in shallow pits.

Demarest, Chalres↗

Effects of Accident Thermal Loading on In-Plane Shear Behavior of Steel-Plate Composite Walls

Structural walls in safety-related nuclear facilities are required to be designed for seismic and accident thermal (due to postulated high-energy pipe break events) loading combination. Current U.S. and international codes provide limited guidance for analysis and design of walls for this loading combination. This paper describes the experimental results and observations from tests conducted on a laboratory-scale (1:4 to 1:5) test unit representing steel-plate composite (SC) walls subjected to combined in-plane (seismic) and accident thermal loading. The test unit was subjected to surface temperatures of up to 450°F in combination with cyclic in-plane loading. Results of similar experiments recently conducted in Japan are also summarized (with surface temperatures up to 570°F). Surface heating combined with the low thermal conductivity and high specific heat of concrete resulted in nonlinear thermal gradients through the thickness of the specimens. These nonlinear thermal gradients and the associated self- or internal restraint led to extensive concrete cracking. This concrete cracking reduced the initial and secant stiffness of the specimens. The initial stiffness of the heated specimens reduced to 30 to 40% of the initial stiffness of the control (unheated) specimen. The secant stiffness of the heated specimens reduced up to 50% of the secant stiffness of the control (unheated) specimen. However, the in-plane shear strength of the heated SC specimens was still approximately 10 to 30% greater than the nominal in-plane shear strength calculated, for the limit state of steel plate von Mises yielding, using AISC N690 equations and measured material properties. Evaluation of the experimental results and observations suggests that the in-plane shear strength of SC walls subjected to typical accident surface temperatures (up to 570°F) can be estimated conservatively using the current provisions of AISC N690. The stiffness for accident thermal loading combinations can be considered to reduce from cracked composite stiffness at ambient temperature to fully cracked—that is, steel-only stiffness as the surface temperature increases up to typical accident value.

Construction & Building Technology↗

Corrosion Behavior of Alloy Structural Steels in Catechol and Biomass-Derived Pyrolysis Oils

Electrochemical impedance spectroscopy (EIS) was used to assess the corrosion behavior of three steels, 2.25Cr-1Mo, 5Cr-1Mo and 9Cr-1Mo (UNS K21590, S50200 and K90941) in bio-oils and catechol, an organic constituent commonly found in bio-oils. Two types of biomass pyrolysis oils produced from selected forest residue feedstocks, classified as high-ash and high-moisture (HAHM) and low-ash and low-moisture (LALM) types and 10 wt.% catechol, were used to test the alloys. According to previous results, 10 wt.% catechol in a water and methanol mixture was corrosive to 2.25Cr-1Mo but not to 9Cr-1Mo, highlighting that increasing Cr content in the steels resulted in improved corrosion resistance. 5Cr-1Mo, a steel with an intermediate Cr content, was tested in catechol solutions to better estimate the critical value of Cr for corrosion resistance under these conditions. Also, the three alloys were tested in both HAHM and LALM bio-oils to assess corrosion susceptibility. For EIS measurements, a customized electrochemical setup was employed to minimize the ohmic path through the bio-oils. The corrosion susceptibility was evaluated by determining the resistance at the alloy-corrosive medium interface.

Jun, Jiheon↗

Corrosion of Stainless and Carbon Steel in Aqueous Piperazine for CO2 Capture

Current obstacles that prevent commercial implementation of amine-scrubbing CO2 capture are the high costs. Reducing capital costs by appropriate selection of construction materials, which requires knowledge of material corrosion performance for the process, will improve the economic feasibility of this technology. Corrosion was evaluated in three pilot plant campaigns using aqueous piperazine with the Advanced Stripper (PZAS). 316L stainless steel (SS) experienced higher corrosion than 304 SS and 2205 duplex SS, and the corrosion rate showed strong dependence on the temperature. 304 and 2205 performed well at all locations and should be good construction materials for PZAS. Degraded PZ exacerbated 316L corrosion, and removal of PZ degradation products using a carbon adsorption bed significantly reduced corrosion. Carbon steel (CS) corrosion showed a weak temperature effect because the corrosion was more dependent on the protective siderite film. The protectiveness of the films was related to fluid velocity. Ni-based alloys corroded in PZ, and the rate increased with temperature. Corrosion of C1010 CS and SS (304, 316L, 430) was measured at absorber and water wash conditions on the bench-scale. Corrosion rate decreases with increasing PZ. 8 With more than 0.003 m PZ in solution, CS has acceptable corrosion performance. Corrosion of CS increases with increasing partial pressure of CO2, suggesting loading is another dominant parameter for carbon steel corrosion. Temperature has a less significant effect than PZ concentration and loading. CS corrosion increases with increasing flow velocity at both absorber and water wash conditions. SS had little corrosion at this lower temperature. Performance of siderite (FeCO3) protective films on CS was studied at representative stripper conditions on the bench-scale. Siderite films can deposit on the surface of CS in CO2-loaded PZ solution at temperatures >100 °C and protect CS from corrosion. The protection may fail in degraded PZ. Ethylenediamine (EDA) is one of the major contributors for the loss of film protectiveness or can be the surrogate for the effect of PZ degradation on siderite film protection. A link between protectiveness and the apparent density of siderite films was discovered. The apparent density of siderite films decreases with increasing flow velocity and decreasing CO2 loading, resulting in higher corrosion of CS.

Liu, Ching-Ting↗

System and method of making a cast steel alloy crankshaft having low porosity

Systems and methods of making a cast steel alloy crankshaft for an internal combustion engine are provided. The method comprises providing a mold of the crankshaft. The mold has cavities to form the crankshaft. The method further comprises melting a first metallic material at between 1400 degrees Celsius (° C.) and 1600° C. to define a molten metallic material. In addition, the method further comprises feeding the molten metallic material at a riser connection angle of between 30° and 75° in the cavities of the negative sand cast mold. The method further comprises cooling the molten metallic material at a solidification time of between 5 seconds (sec) and 20 sec in the negative sand cast mold with at least one chill member to define a solidified metallic material having dimensions of the cast steel alloy crankshaft. Furthermore, the method comprises separating the solidified metallic material from the negative sand cast mold to define the cast steel alloy crankshaft.

Wang, Liang↗

Effects of chemical segregation on ductility-anisotropy in high strength Fe-Mn-Al-C lightweight austenitic steels

Ductile Fe-Mn-Al-C lightweight steels offer great potential as high specific strength materials for weight critical applications. In the present work, very high yield (~1 GPa) and ultimate tensile strength levels (~1.5 GPa) were obtained along the rolling and transverse directions of Fe-30Mn-8.5Al-0.9Si-0.9C-0.5Mo (wt.%), with high tensile elongation to failure of ~35%. This excellent mechanical behavior was attributed to the nanoscale, ordered κ-carbide precipitates formed during aging after rolling. However, tensile ductility was not isotropic through all directions of the rolled plate. In particular, the ductility was consistently lower than 5% true strain along the normal direction. Upon detailed microstructural investigations, micro-scale lamellar chemical micro-segregation bands were detected, which caused the observed anisotropic embrittlement along certain plate directions. These bands resulted in low failure strains along the normal direction since it is oriented perpendicular to these chemical segregation bands, resulting in a failure type reminiscent of delamination-induced cleavage fracture. Chemical segregation causes an inhomogeneous κ-carbide precipitate distribution upon aging, producing more pronounced mechanical anisotropy after peak-aging as compared to the solution heat treated samples. Surprisingly, deformation twinning was observed after tensile deformation of solution-heat treated specimens via electron-backscatter diffraction experiments, which is anomalous for a high stacking faulty energy (SFE) material. Further, it was proposed that chemical micro-segregation promotes locally different SFE regions, leading to deformation twinning in this nominally high SFE material. Overall, this work demonstrates the effects of chemical segregation on mechanical properties and microstructural evolution in a high performance, lightweight Fe-Mn-Al-C steel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Radiation induced amorphization of carbides in additively manufactured and conventional ferritic-martensitic steels: In-situ experiments on extraction replicas

In-situ irradiations using 1 MeV Kr 2+ ions in a transmission electron microscope were performed on extraction replica samples containing M 23 C 6 carbides and MX carbonitrides from two ferritic-martensitic (FM) steels: (i) 9%Cr-1%W-TaV based Eurofer97 and (ii) 9%Cr-1%Mo-VNb (all in wt.%) based additively manufactured (AM) Grade91 steel. The irradiations were performed between 100 and 773 K up to a maximum dose of ~2.4 displacements per atom (dpa). The M 23 C 6 carbides are highly susceptible to radiation induced amorphization (RIA), while the MX type nanoprecipitates are highly amorphization resistant across the entire irradiation temperature range. Between 100 and 423 K, RIA of M 23 C 6 carbides occurs very rapidly with critical amorphization doses ranging between ~0.35 and 0.9 dpa, increasing to higher doses at 573 K. Complete amorphization of the M 23 C 6 carbides up to doses of ~2.4 dpa is not possible at 773 K under the present irradiation conditions. The critical amorphization dose of M 23 C 6 carbides increases nearly exponentially with irradiation temperature. The critical temperature for the crystalline-to-amorphous phase transformation (T c→a ) of M 23 C 6 carbides irradiated as replica samples, i.e. without the surrounding metal matrix, was estimated to be ~812 K. Comparing the present results with neutron irradiation data on bulk samples reveals a decrease in the critical amorphization dose for M 23 C 6 and an increase of T c→a , highlighting the effect of dose rate on the amorphization behavior that is qualitatively consistent with literature on other non-metals. Changes in the minor chemistry of M 23 C 6 , such as presence or absence of W, V, Nb, Mo, seems to have little effect on the amorphization behavior. Here, in-situ irradiations on extraction replica samples provide a novel pathway to explore radiation tolerance of nanoprecipitates in nuclear structural materials

36 MATERIALS SCIENCE↗

Spall damage mechanisms in laser powder bed fabricated stainless steel 316L

This paper reports on spall damage mechanisms in laser powder bed fusion (LPBF) fabricated stainless steel 316L (SS316L) subjected to uniaxial, strain plate-impact loading and explores failure evolution with increasing impact velocity and peak pressure. Analysis of velocimetry profiles reveals a heterogeneous failure response with several different failure mechanisms activated during impact and resulting spall. The analysis is supported by optical microscopy and electron backscattered diffraction (EBSD) observation of soft recovered impacted samples, which show evidence of localized nano-twinning, twin growth, severe grain rotation, and grain refinement along the spall plane, in addition to pore nucleation, coalescence, and growth. Furthermore, the observed failure mechanisms, including crack formation and propagation along high angle grain boundaries (HAGBs), are not consistently indicative of ductile fracture typical of wrought stainless steel.

36 MATERIALS SCIENCE↗

Superior strength-ductility synergy by hetero-structuring high manganese steel

Lacking of forest hardening makes low ductility in steels long challenge particularly at high yield strength. Here, we report to make good use of hetero-structuring for superior strength-ductility synergy in high manganese steel. The point is to retain original deformed structure of large quantity, along with recrystallized ultrafine-grains and fine grains, jointly for most effective heterogeneous deformation-induced (HDI) hardening especially at high strength. The residual plastic strain of larger than 0.2% and large proportion of HDI stress over 60% indicate the crucial role in ductility by HDI hardening. This renders a significantly upgraded strength-ductility combination within high strength scope.

36 MATERIALS SCIENCE↗

A Model to Account for the Effects of Load Ratio and Hydrogen Pressure on the Fatigue Crack Growth Behavior of Pressure Vessel Steels

A phenomenological model for estimating the effects of load ratio R and hydrogen pressure P H2 on the hydrogen-assisted fatigue crack growth rate (HA–FCGR) behavior in the transient and steady-state regimes of pressure vessel steels is described. The “transient regime” is identified with crack growth within a severely embrittled zone of intense plasticity at the crack tip. The “steady-state” behavior is associated with the crack growing into a region of comparatively lower hydrogen concentration located further away from the crack tip. The model treats the effects of R and P H2 as being functionally separable. In the transient regime, the effects of the hydrogen pressure on the HA–FCGR behavior were negligible but were significant in the steady-state regime. The hydrogen concentration in the steady-state region is modeled as being dependent on the kinetics of lattice diffusion, which is sensitive to pressure. Experimental HA–FCGR data from the literature were used to validate the model. The new model was shown to be valid over a wide range of conditions that ranged between –1 ≤ R ≤ 0.8 and 0.02 ≤ P H2 ≤ 103 MPa for pressure vessel steels.

36 MATERIALS SCIENCE↗

Process-driven roadmap for depositing super duplex stainless steel via wire Arc additive manufacturing

Here, this study systematically investigates the effects of shielding gas, bead spacing, weld mode, and travel speed on the phase balance, porosity, and hardness of wire arc additively manufactured (WAAM) super duplex stainless steel (ER2594). Robotic WAAM was employed to fabricate multilayer walls under systematically varied process conditions, followed by phase transformation simulations, X-ray computed tomography (XCT), electron backscatter diffraction (EBSD), and microhardness evaluation. Thermodynamic simulations predicted rapid cooling of AM process can suppress the potential formation of deleterious precipitates which was later validated via cross-sectional microstructure analyses of printed samples. XCT revealed porosity levels below 0.2% for all deposits, with reduced travel speed significantly lowering defect volume. Microstructural analyses revealed the evolution of various austenite precipitates, including grain boundary austenite (GBA), Widmanstätten austenite (WA), and intergranular austenite (IGA), sequentially upon cooling of the ferrite phase. Among all process parameters, weld transfer mode exhibited the strongest influence on phase balance; pulsed mode promoted higher ferrite retention (~ 36%) compared to RapidX mode. No consistent relationship between stabilized phase fraction and captured microhardness was observed. This work provides critical insights for optimizing WAAM parameters to control phase balance and mechanical performance, which is essential for producing high-integrity super duplex stainless-steel components for nuclear and marine applications.

Grain orientation↗

Thermodynamics and kinetics of precipitation and austenite reversion during aging of Ti-free grade 300 maraging steel manufactured by laser powder bed fusion (LPBF)

Austenite reversion and intermetallic precipitation are two key phase transformations in maraging steels which determine the strength and ductility. Usually, an optimum aging temperature/time is determined using trial and error approach with inputs from thermodynamic databases and a-posteriori microscopy/hardness evaluations. In this study, a thermo-kinetic model is developed to predict the precipitation and austenite reversion kinetics during various post-fabrication heat treatments in a Ti-free variant of grade 300 maraging steel manufactured using laser powder bed fusion. The thermo-kinetic model was based on the principles of Scheil solidification and the classical nucleation theory. The predictions from the thermo-kinetic model were verified using suitable microscopy techniques, and the results from the thermo-kinetic model agree well with the experimental measurements. Overall, results highlight the fact that an Integrated Computational Materials Engineering approach can be used to predict the precipitation and austenite reversion kinetics, and be used as an input for an efficient design of heat treatments for achieving optimum mechanical properties.

36 MATERIALS SCIENCE↗

Methods to Observe Tribological Failures in Self-Mated Steel Contacts

Scuffing, a type of wear found in highly stressed or poorly lubricated contacts, is characterized by a rapid increase in friction and severe plastic deformation of the near-surface material. Scuffing has proven difficult to study because it initiates unpredictably, progresses rapidly, and typically develops within an inaccessible contact interface. Although there have been successful in-situ studies of scuffing in real-time, the transparent counter body needed for these studies changes the interactions between the surfaces and the lubricant, which affects the scuffing process in unknown ways. This paper describes the development of X-ray-compatible tribometry to study the scuffing of self-mated steels in-situ and in real-time. The method uses a crossed cylinders configuration with a thin (500 μm thick) stationary component and a small (≈200 μm) contact width to maximize X-ray interactions with atoms within the stress field generated by the contact. The resulting instrument and method are used to benchmark the scuffing response of self-mated 52,100 steel under tribologically challenging ‘oil-off’ lubrication conditions. The results demonstrate reliable scuffing in this configuration despite the relatively small contact areas and loads used. Following scuffing, gross plastic deformation was observed on both surfaces along with significant subsurface grain refinement and flow only on the stationary surface, which experienced constant contact. Interestingly, high friction initiated at specific locations of the migratory surface, which experienced intermittent contact, and then propagated across the track over time, suggesting that local conditions of the migratory surface dominated friction leading into the failure event.

36 MATERIALS SCIENCE↗

Automated Grain Boundary (GB) Segmentation and Microstructural Analysis in 347H Stainless Steel Using Deep Learning and Multimodal Microscopy

Austenitic 347H stainless steel offers superior mechanical properties and corrosion resistance required for extreme operating conditions such as high temperature. The change in microstructure due to composition and process variations is expected to impact material properties. Identifying microstructural features such as grain boundaries thus becomes an important task in the process-microstructure-properties loop. Applying convolutional neural network (CNN)-based deep learning models is a powerful technique to detect features from material micrographs in an automated manner. In contrast to microstructural classification, supervised CNN models for segmentation tasks require pixel-wise annotation labels. However, manual labeling of the images for the segmentation task poses a major bottleneck for generating training data and labels in a reliable and reproducible way within a reasonable timeframe. Microstructural characterization especially needs to be expedited for faster material discovery by changing alloy compositions. Here, in this study, we attempt to overcome such limitations by utilizing multimodal microscopy to generate labels directly instead of manual labeling. We combine scanning electron microscopy images of 347H stainless steel as training data and electron backscatter diffraction micrographs as pixel-wise labels for grain boundary detection as a semantic segmentation task. The viability of our method is evaluated by considering a set of deep CNN architectures. We demonstrate that despite producing instrumentation drift during data collection between two modes of microscopy, this method performs comparably to similar segmentation tasks that used manual labeling. Additionally, we find that naïve pixel-wise segmentation results in small gaps and missing boundaries in the predicted grain boundary map. By incorporating topological information during model training, the connectivity of the grain boundary network and segmentation performance is improved. Finally, our approach is validated by accurate computation on downstream tasks of predicting the underlying grain morphology distributions which are the ultimate quantities of interest for microstructural characterization.

36 MATERIALS SCIENCE↗

Stress relaxation cracking susceptibility evaluation in 347H stainless steel welds

Abstract Stress relaxation cracking (SRC) has been reported as a dominant failure mechanism for 347H stainless steel welds at elevated service temperatures, occurring in either the heat-affected zone (HAZ) or fusion zone (FZ). In this study, SRC susceptibility of physically simulated HAZ and cross-welded E347-347H stainless steel welds was studied using a four-step accelerated SRC test with a thermomechanical physical simulator. The stress and temperature range studied represents weld-induced residual stress at 150–600 MPa and post-weld heat treatment temperatures between 800 and 1050 °C. For all temperature conditions, the cross-welded samples failed at a lower critical stress threshold than the simulated HAZ. A finite element model of a 50.8-mm-thick single-V groove weld was used to generate the residual stress maps induced by a 40-pass welding procedure, which in combination with the experimental threshold stress map predicted potential SRC failure locations. Postmortem microstructural evaluations were performed to identify contributing characteristics to SRC. It was found that HAZ samples exhibited a combination of creep void development, secondary cracks with intergranular fracture near grain boundary carbides, and eutectic phases. FZ samples showed brittle fracture with cracks propagating along straight, non-tortuous interdendritic grain boundaries.

42 ENGINEERING↗

Effects of heat treatment and build orientation on the evolution of $ϵ$ and $α'$ martensite and strength during compressive loading of additively manufactured 304L stainless steel

In this paper, the effect of heat-treatment and build orientation on martensitic phase transformation in additively manufactured (AM) 304L stainless steel is studied and compared with conventionally produced wrought material. The relationships between observed martensitic transformations and material microstructures and their effects on mechanical strength are established through experimental observations. In situ high-energy X-ray powder diffraction measurements were performed to monitor the evolution of $ϵ$ and $α'$ martensite during compressive loading of stainless steel. Electron backscatter diffraction (EBSD) was used to provide insight on initial grain morphology, crystallographic misorientation within grains, and crystallographic texture. Heat treatment alters the microstructure of AM samples creating different initial conditions. This difference in starting microstructure resulted in variability in martensitic transformation during compressive deformation. The rate of martensitic transformation decreased for AM samples treated with temperatures up to 1100°C, after which the AM microstructures recrystallized, resulting in increased rate of martensitic transformation for those samples treated at higher temperatures. It was also observed that aligning the axis of compression with the AM build direction resulted in a lower rate of strain-induced martensite formation as opposed to aligning the compression axis perpendicular to it. More favorable distribution of crystal orientations in the latter loading orientation promoted martensitic transformation. These and additional experimental observations from EBSD in terms of kernel average misorientation, mean grain orientation spread, and mean crystallite size reveal strong microstructural effects on strength of additively manufactured metallic materials.

304L stainless steel↗