Auto-adjustable pin tool for friction stir welding

An auto-adjusting pin tool for friction stir welding is presented wherein the pin tool automatically adjusts for welding materials of varying thicknesses, and the pin can be incrementally withdrawn from the workpieces thus eliminating any crater or keyhole in the weld. The inventive apparatus is comprised of a welding head housing a motor connected to a controller instrument package and an arbor supported by bearings. The arbor forms an interior cylinder and is encircled by a stationary slip ring though which are ported hydraulic passageways into the interior cylinder of the arbor such that a piston housed therein may be moved axially. Coupled to the piston is a pin tool which is treaded on its lower end and which is moveably seated in, and extending through, a shoulder housing having concave lower face. When welding, the rotating treaded end of the pin enters and stirs the workpieces while the lower face of the shoulder housing compacts the workpieces. As the welding head traverses the shoulder housing the controller senses any rising pressure on the lower face of the shoulder housing and withdraws the arbor to keep the pressure constant. At the same time, the piston moves towards the workpieces thus extending the pin further from the shoulder. This keeps the pin at a proper depth in the workpieces regardless of their thicknesses. As the weld terminates this same operation can be used to incrementally withdraw the pin during the final part of the traverse, thus eliminating any keyhole or crater that would otherwise be created.

Ding, R. Jeffrey↗

Welding of gamma titanium aluminide alloys

An article made of a gamma titanium aluminide alloy is welded, as for example in the weld repair of surface cracks, by removing foreign matter from the area to be welded, first stress relieving the article, cooling the entire article to a welding temperature of from about 1000.degree. F. to about 1400.degree. F., welding a preselected region in an inert atmosphere at the welding temperature, and second stress relieving the article. Welding is preferably accomplished by striking an arc in the preselected region so as to locally melt the alloy in the preselected region, providing a filler metal having the same composition as the gamma titanium aluminide alloy of the article, and feeding the filler metal into the arc so that the filler metal is melted and fused with the article to form a weldment upon solidification.

Smashey, Russell W.↗

Optically controlled welding system

An optically controlled welding system (10) wherein a welding torch (12) having through-the-torch viewing capabilities is provided with an optical beam splitter (56) to create a transmitted view and a reflective view of a welding operation. These views are converted to digital signals which are then processed and utilized by a computerized robotic welder (15) to make the welding torch responsive thereto. Other features includes an actively cooled electrode holder (26) which minimizes a blocked portion of the view by virtue of being constructed of a single spoke or arm (28) and a weld pool contour detector (14) comprising a laser beam directed onto the weld pool with the position of specular radiation reflected therefrom being characteristic of a penetrated or unpenetrated condition of the weld pool.

Gordon, Stephen S.↗

Making Superconducting Welds between Superconducting Wires

A technique for making superconducting joints between wires made of dissimilar superconducting metals has been devised. The technique is especially suitable for fabrication of superconducting circuits needed to support persistent electric currents in electromagnets in diverse cryogenic applications. Examples of such electromagnets include those in nuclear magnetic resonance (NMR) and magnetic resonance imaging (MRI) systems and in superconducting quantum interference devices (SQUIDs). Sometimes, it is desirable to fabricate different parts of a persistent-current-supporting superconducting loop from different metals. For example, a sensory coil in a SQUID might be made of Pb, a Pb/Sn alloy, or a Cu wire plated with Pb/Sn, while the connections to the sensory coil might be made via Nb or Nb/Ti wires. Conventional wire-bonding techniques, including resistance spot welding and pressed contact, are not workable because of large differences between the hardnesses and melting temperatures of the different metals. The present technique is not subject to this limitation. The present technique involves the use (1) of a cheap, miniature, easy-to-operate, capacitor-discharging welding apparatus that has an Nb or Nb/Ti tip and operates with a continuous local flow of gaseous helium and (2) preparation of a joint in a special spark-discharge welding geometry. In a typical application, a piece of Nb foil about 25 m thick is rolled to form a tube, into which is inserted a wire that one seeks to weld to the tube (see figure). The tube can be slightly crimped for mechanical stability. Then a spark weld is made by use of the aforementioned apparatus with energy and time settings chosen to melt a small section of the niobium foil. The energy setting corresponds to the setting of a voltage to which the capacitor is charged. In an experiment, the technique was used to weld an Nb foil to a copper wire coated with a Pb/Sn soft solder, which is superconducting. The joint was evaluated as part of a persistent-current circuit having an inductance of 1 mH. A current was induced in a loop, and no attenuation of the current after a time interval 1,000 s was discernible in a measurement having a fractional accuracy of 10(exp -4): This observation supports the conclusion that the weld had an electrical resistance <10(exp -10) omega.

Penanen, Konstantin I.↗

Electron Beam Welding to Join Gamma Titanium Aluminide Articles

A method is provided for welding two gamma titanium aluminide articles together. The method includes preheating the two articles to a welding temperature of from about 1700 F to about 2100 F, thereafter electron beam welding the two articles together at the welding temperature and in a welding vacuum to form a welded structure, and thereafter annealing the welded structure at an annealing temperature of from about 1800 F to about 2200 F, to form a joined structure.

Kelly, Thomas Joseph↗

Microstructural Evolution in Friction Stir Welding of Ti-6Al-4V

Friction stir welding (FSW) is a thermo-mechanical process that utilizes a nonconsumable rotating pin tool to consolidate a weld joint. In the conventional FSW process, the pin tool is responsible for generating both the heat required to soften the material and the forces necessary to deform and combine the weld seam. As such, the geometry of the pin tool is important to the quality of the weld and the process parameters required to produce the weld. Because the geometry of the pin tool is limitless, a reduced set of pin tools was formed to systematically study their effect on the weldment with respect to mechanical properties and resultant microstructure. In this study 0deg, 15deg, 30deg, 45deg, and 60deg tapered, microwave sintered, tungsten carbide (WC) pin tools were used to FSW Ti-6Al-4V. Transverse sections of the weld were used to test for mechanical properties and to document the microstructure using optical microscopy. X-ray diffraction (XRD) was also used to characterize the microstructure in the welds. FSW results for the 45deg and 60deg pin tools are reported in this paper.

Rubisoff, H.↗

Gimballed Shoulders for Friction Stir Welding

In a proposed improvement of tooling for friction stir welding, gimballed shoulders would supplant shoulders that, heretofore, have been fixedly aligned with pins. The proposal is especially relevant to self-reacting friction stir welding. Some definitions of terms, recapitulated from related prior NASA Tech Briefs articles, are prerequisite to a meaningful description of the proposed improvement. In friction stir welding, one uses a tool that includes (1) a rotating shoulder on top (or front) of the workpiece and (2) a pin that rotates with the shoulder and protrudes from the shoulder into the depth of the workpiece. In conventional friction stir welding, the main axial force exerted by the tool on the workpiece is reacted through a ridged backing anvil under (behind) the workpiece. When conventional friction stir welding is augmented with an auto-adjustable pin-tool (APT) capability, the depth of penetration of the pin into the workpiece is varied in real time by a position- or forcecontrol system that extends or retracts the pin as needed to obtain the desired effect. In self-reacting (also known as self-reacted) friction stir welding as practiced heretofore, there are two shoulders: one on top (or front) and one on the bottom (or back) of the workpiece. In this case, a threaded shaft protrudes from the tip of the pin to beyond the back surface of the workpiece. The back shoulder is held axially in place against tension by a nut on the threaded shaft. Both shoulders rotate with the pin and remain aligned coaxially with the pin. The main axial force exerted on the workpiece by the tool and front shoulder is reacted through the back shoulder and the threaded shaft into the friction-stir-welding machine head, so that a backing anvil is no longer needed. A key transmits torque between the bottom shoulder and the threaded shaft, so that the bottom shoulder rotates with the shaft. This concludes the prerequisite definitions of terms.

Carter, Robert↗

Investigation of Microstructure and Microhardness in Self-Reacting Friction Stir Welded AA2014-T6 and AA2219-T87

Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. This work reports on the microstructure and microhardness of SR-FSW between two dissimilar aluminum alloys. Specifically, the study examines the cross section of the weld joint formed between an AA2014-T6 plate on the advancing side and an AA2219-T87 plate on the retreating side. The microstructural analysis shows an irregularly displaced weld seam from the advancing side past the thermo-mechanical affected zone (TMAZ) into the weld nugget region. There are sharp variations in the microhardness across the weld. These variations are described in the paper and mechanisms for their formation are discussed.

Horton, K. Renee↗

Heat Control via Torque Control in Friction Stir Welding

In a proposed advance in friction stir welding, the torque exerted on the workpiece by the friction stir pin would be measured and controlled in an effort to measure and control the total heat input to the workpiece. The total heat input to the workpiece is an important parameter of any welding process (fusion or friction stir welding). In fusion welding, measurement and control of heat input is a difficult problem. However, in friction stir welding, the basic principle of operation affords the potential of a straightforward solution: Neglecting thermal losses through the pin and the spindle that supports it, the rate of heat input to the workpiece is the product of the torque and the speed of rotation of the friction stir weld pin and, hence, of the spindle. Therefore, if one acquires and suitably processes data on torque and rotation and controls the torque, the rotation, or both, one should be able to control the heat input into the workpiece. In conventional practice in friction stir welding, one uses feedback control of the spindle motor to maintain a constant speed of rotation. According to the proposal, one would not maintain a constant speed of rotation: Instead, one would use feedback control to maintain a constant torque and would measure the speed of rotation while allowing it to vary. The torque exerted on the workpiece would be estimated as the product of (1) the torque-multiplication ratio of the spindle belt and/or gear drive, (2) the force measured by a load cell mechanically coupled to the spindle motor, and (3) the moment arm of the load cell. Hence, the output of the load cell would be used as a feedback signal for controlling the torque (see figure).

Venable, Richard↗

A Micro-Electrochemical Study of Friction Stir Welded Aluminum 6061-T6

The corrosion behavior of friction stir welded Aluminum alloy 606 1-T6 was studied using a micro-electrochemical cell. The micro-electrochemical cell has a measurement area of about 0.25 square mm which allows for measurement of corrosion properties at a very small scale. The corrosion and breakdown potentials were measured at many points inside and outside the weld along lines perpendicular to the weld. The breakdown potential is approximately equal inside and outside the weld; however, it is lower in the narrow border between the weld and base material. The results of electrochemical measurements were correlated to micro-structural analysis. The corrosion behavior of the friction stir welded samples was compared to tungsten inert gas (TIG) welded samples of the same material.

Hintze, Paul E.↗

Laser Ablation Cleaning of Self-Reacting Friction Stir Weld Seam Surfaces: A Preliminary Evaluation

Anodized aluminum panels were cleaned by three lasers at three separate sites with a view to determining whether more economical laser cleaning might supplant current manual cleaning methods for preparation of surfaces to be welded by the self-reacting friction stir process. Uncleaned panels yielded welds exhibiting residual oxide defect (ROD) and failing at very low stresses along the trace of the weld seam. Manually cleaned panels yielded welds without ROD; these welds failed at nominal stress levels along an angled fracture surface not following the weld seam trace. Laser cleaned panels yielded welds failing at intermediate stress levels. The inadequacy of the laser cleaning processes leaves questions: Was the anodized aluminum test too stringent to represent actual cleaning requirements? Were the wrong laser cleaning techniques/parameters used for the study? Is the laser cleaning mechanism inadequate for effective preweld surface cleaning?

Nunes, A. C., Jr.↗

Prediction of Tensile Strength of Friction Stir Weld Joints with Adaptive Neuro-Fuzzy Inference System (ANFIS) and Neural Network

Friction-stir-welding (FSW) is a solid-state joining process where joint properties are dependent on welding process parameters. In the current study three critical process parameters including spindle speed (𝑁), plunge force (𝐹𝑧), and welding speed (𝑉) are considered key factors in the determination of ultimate tensile strength (UTS) of welded aluminum alloy joints. A total of 73 weld schedules were welded and tensile properties were subsequently obtained experimentally. It is observed that all three process parameters have direct influence on UTS of the welded joints. Utilizing experimental data, an optimized adaptive neuro-fuzzy inference system (ANFIS) model has been developed to predict UTS of FSW joints. A total of 1200 models were developed by varying the number of membership functions (MFs), type of MFs, and combination of four input variables (𝑁,𝑉,𝐹𝑧,𝐸𝐹𝐼) utilizing a MATLAB platform. Note EFI denotes an empirical force index derived from the three process parameters. For comparison, optimized artificial neural network (ANN) models were also developed to predict UTS from FSW process parameters. By comparing ANFIS and ANN predicted results, it was found that optimized ANFIS models provide better results than ANN. This newly developed best ANFIS model could be utilized for prediction of UTS of FSW joints.

Mohammad W Dewan↗

Friction Stir Welding – an Advanced Approach to Repair Nuclear Power Plant Components

Solid phase joining technique friction stir welding (FSW) has been shown to mitigate helium-related issues in fusion welding of irradiated steels. Here, we present detailed characterization results of the first friction stir weld of an irradiated 304L stainless steel (SS) coupon contained 5.2 atomic parts per million (appm) helium. Scanning electron microscopy (SEM) was used to characterize a cross section specimen removed from the friction stir weld. No macro helium induced crack was observed at the analyzed cross-section, and only 1 – 1.5 µm size pores were found in the stir zone (SZ) and the thermal-mechanical affected zone (TMAZ). Moreover, some minor helium aggregations (Maximum ~20 µm in length) appeared along grain boundaries inside the TMAZ. Thereafter, miniature tensile specimens were extracted from the SZ, TMAZ and heat affected zone (HAZ), and base metal (BM) and tested. All welded specimens showed high total elongations (> 60%) and strengths (> 75% BM strengths). Overall, the weld made by FSW showed much better results comparing with traditional fusion welding on irradiated SS.

Tang, Wei↗

Numerical and Experimental Analysis of Dissimilar Repair Welding Residual Stress in P91 Steel Considering Solid-State Phase Transformation

Repair welding is a popular method to repair the cracked zones of pipes in power plants. However, residual stresses induced by repair welding are inevitably generated and have a significant effect on the performance of repair-welded components during service. The purpose of this research is to investigate the effects of solid-state phase transformation (SSPT) on the repair welding residual stress distribution of multi-layer and multi-pass welding in P91 steel. Based on thermal elastic-plastic theory, a three-dimensional thermal–metallurgical–mechanical finite element model considering the SSPT is established, and shielded metal arc welding (SMAW) heat input is modelled as one double elliptical heat source. The effect of phase transformation on residual stress is investigated by considering effects with and without phase transformation in the database of materials. The results show that transverse compressive stress and a low longitudinal stress area are generated in the final pass due to martensite transformation. Compared with different zones along the thickness direction, the effect of SSPT is greater around the outer surface than around the internal fusion zone. The rationality of the developed finite element model is verified by the experimental method, and good agreement is obtained between those results from the numerical analysis and experimental methods.

36 MATERIALS SCIENCE↗

Neutron diffraction illustrates residual stress behavior of welded alloys used as radioactive confinement boundary

Corrosion-resistant welded alloys are frequently used as a leak-tight boundary in critical applications that require confinement of hazardous and/or radioactive substances, including an increasing population of spent nuclear fuel (SNF) canisters. The behavior of residual stresses generated as a result of irregular elastic–plastic deformation during processes such as welding is one of today's key issues to a full understanding of the aging mechanisms that may compromise the confinement boundary. Whether such processes and any subsequent weld repairs, not subjected to post-weld heat treatment, would negatively affect the initial material by introducing through-thickness tensile stresses remains an open question. Here we report the first residual stress measurements using neutron diffraction on the welded joints of a SNF canister. We found significant tensile residual stresses in the as welded sample, indicating that initiation and through-thickness growth of cracks may be possible. Following repair, we observed a stress redistribution and introduction of beneficial compressive stresses. We anticipate our results will improve understanding of confinement susceptibility to aging and guide improvements in repair techniques.

36 MATERIALS SCIENCE↗

Microstructural Characteristics and Mechanical Properties in the Laser Beam Welded Joints of High-Strength Microalloyed Steel

The laser beam welded joints of the high-strength microalloyed steel consist of the base metal (BM), the partially transformed heat-affected zone I (PTHAZ-I), the partially transformed heat-affected zone II (PTHAZ-II), the fully transformed heat-affected zone (FTHAZ) and the fusion zone (FZ). The martensite/austenite (M/A) islands of the bainites in the PTHAZ-II are dense versus those in the PTHAZ-I, and the martensites exist in the FTHAZ and the FZ together with the bainites under the slow welding speed. The M/A islands of the bainites and/or the martensites in the PTHAZ become denser under the high welding speed, and the martensites in the FTHAZ and the FZ predominate. The low-angle boundary density and the high local misorientation proportion are used to identify the constituents roughly, consistent with the microstructural characteristics in the welded joints. The misorientation angle distributions are employed to evaluate the degree of the phase transformation, reflecting the change law of the degree of the phase transformation in the welded joints. The hardness and the tensile tests indicate that the HAZ and the FZ are stronger than the BM, dependent on the microstructures in the welded joints. The strengthening in the HAZ and the FZ is mainly attributed to the products of non-equilibrium phase transformation with the high dislocation density.

36 MATERIALS SCIENCE↗

A Weighting Grade-Based Optimization Method for Determining Refill Friction Stir Spot Welding Process Parameters

The welding process used in fabricating thin-walled structures by refill friction stir spot welding (RFSSW) should be characterized by a high strength of welds and high process repeatability which is demonstrated by a small dispersion of the load capacity of the joints. The present work is designed to optimize RFSSW process parameters for 7075-T6 Alclad aluminum alloy sheets used to fabricate aircraft structures. The optimization was performed by scalarization of the objective function using the weighting grades method. The study considers the effect of process parameters, i.e., tool plunge depth, duration of welding, tool rotational speed, on the tensile/shear strength of the joints, and dispersion of the load capacity. It was found that it was possible to choose the optimal welding parameters taking into account maximization of the load capacity and minimization of the dispersion of the joint strength via a best compromise between the tool rotational speed ensuring adequate plasticization of the base material and the duration of welding ensuring that a fine-grained joint microstructure is obtained.

36 MATERIALS SCIENCE↗

The effect of filament peaking on electron beam weld quality

Electron beam welding uses high intensity beams that are generated by an electron emitting cathode under high vacuum conditions. The cathode, typically a ribbon or wire filament of refractory metal, must be heated to sufficiently high temperatures for electron emission to occur and must be carefully controlled to produce the desired beam current while at the same time optimizing filament lifetime. Traditional methods for doing this in commonly used triode gun assemblies consist of first finding the filament knee point in the filament current versus beam current relationship that produces the desired beam current for a given beam voltage. The filament current is then increased by some amount, typically 5–10%, per conventional wisdom to produce a peaked beam. This investigation studies and quantifies the beam and weld quality produced by underkneed and overpeaked filaments using electron beam diagnostics to measure the power density distribution of these beams. Underkneed filaments are shown to have power densities that drop off very quickly below the traditional knee, resulting in poor weld penetration. Kneed filaments do not reach the full beam intensity and also produce shallow welds. Increasing the filament current 10% above the traditional knee was shown to produce a circular Gaussian-like beam with peaked intensity optimized for welding and for filament lifetime. Further increases in the filament current that produce overpeaked beams do not significantly change the beam or weld quality and would only contribute to a reduced filament lifetime.

Electron Beam Welding↗