Search NASA⌕ Search

SEARCH · Search NASA

Results for “coating durability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

R&D to Ensure a Scientific Basis for Qualification Tests and Standards (Final Report)

Project return on investment in a photovoltaic (PV) system depends increasingly on maintaining high energy yields, and the system lifetime is a major factor in levelized cost of electricity (LCOE). Thus, the rate of PV deployment and the success of these assets depends upon reliable long-term power generation. The overarching objective of this program is to improve photovoltaic (PV) module reliability via development of tests and standards. Where reliability problems or risk are discovered, we can design tests to ensure that these liabilities don't affect future generations of products. Customers can use these tests to understand which products are susceptible to certain degradation mechanisms, and manufacturers can use the tests to design unwanted characteristics out of their products. The work under this program identifies PV reliability needs, performs characterization that provides scientific understanding of targeted degradation mechanisms, and translates those data into practical and predictive test protocols and standards. Major accomplishments include: A model for polarization-type potential induced degradation (PID-p) was developed and validated against experimental data. NREL is currently leading a new edition of IEC 62804-1 for PID detection. PID-p can cause large losses in current and voltage for some module designs on cloudy days. Finite element modeling (FEM) and experiment was used to determine when cells crack in a module. It was shown that cells in landscape orientation are much more likely to crack than those on portrait orientation. Shortly thereafter, the first products with portrait-oriented cells were introduced. Studies of how to test for light and elevated temperature degradation (LeTID) culminated with the publication of IEC TS 63342. Software to predict the progression of LeTID was developed, validated, and made publicly available. Field validated tests and international standards for durability of PV module coatings abrasion, backsheets, and encapsulants were developed. Examples are IEC 62788-1-1, IEC 62788-2 ED2, IEC TS 62788-7-2, IEC 62788-7-3 ED1, IEC 63209-2. NREL led the development a high-temperature testing technical specification, and published guidelines that enable installers to determine whether higher-temperature testing is needed, simply based on location and mounting configuration. In a number of our case studies, variations in the bills of materials or workmanship have been associated with variations in reliability. These observations emphasize the importance of quality assurance to reliability. A framework for criticality (i.e. Pareto) analysis was developed and published. The framework helps us and other researchers determine what problems should be addressed for reliability research to have the biggest industry impact. NREL continues to participate actively in international standards development and stakeholder engagement activities, including organizing an annual PV Reliability Workshop. These activities are important for ensuring we address issues that are relevant and timely, and that we convey our results to those who may benefit.

14 SOLAR ENERGY↗

Processable Polyimides Containing ATBN Elastomers

Void-free moldings obtained without serious sacrifice in other properties. New synthesis produces high-temperture linear aromatic polyimide processed in imide form to yield tough, void-free components without serious sacrifice in other properties. Linear aromatic condensation polyimides are materials of prime choice for use as adhesives, composite matrix resins, films, coatings, and/or moldings where durability at temperatures as high as 200 to 300oC needed. Finding increasing use in aircraft and spacecraft applications.

St. Clair, Anne K.↗

Effect of an oxygen plasma on uncoated thin aluminum reflecting films

Thin aluminum films were considered for use as a reflective surface for solar collectors on orbiting solar dynamic power systems. A matter of concern is the durability of such reflective coatings against oxidative attack by highly reactive neutral atomic oxygen, which is the predominate chemical specie in low Earth orbit. Research to date was aimed at evaluating the protective merit of thin dielectric coatings over the aluminum or other reflective metals. However, an uncoated aluminum reflector may self-protect by virtue of the oxide formed from its exposed surface, which constitutes a physical barrier to further oxidation. This possibility was investigated, and an attempt was made to characterize the effects of atomic oxygen on thin Al films using photomicrographs, scanning electron microscopy, spectrophotometry, Auger analysis, and mass measurements. Data collected in a parallel effort is discussed for its comparative value. The results of the investigation of uncoated aluminum supported the self-protection hypothesis, and importantly, it was found that long term specular reflectance for uncoated aluminum exceeded that of Al and Ag reflectors with dielectric coatings.

Parsons, Roger L.↗

Heat transfer to throat tubes in a square-chambered rocket engine at the NASA Lewis Research Center

A gaseous H2/O2 rocket engine was constructed at the NASA-Lewis to provide a high heat flux source representative of the heat flux to the blades in the high pressure fuel turbopump (HPFTP) during startup of the space shuttle main engines. The high heat flux source was required to evaluate the durability of thermal barrier coatings being investigated for use on these blades. The heat transfer, and specifically, the heat flux to tubes located at the throat of the test rocket engine was evaluated and compared to the heat flux to the blades in the HPFTP during engine startup. Gas temperatures, pressures and heat transfer coefficients in the test rocket engine were measured. Near surface metal temperatures below thin thermal barrier coatings were also measured at various angular orientations around the throat tube to indicate the angular dependence of the heat transfer coefficients. A finite difference model for a throat tube was developed and a thermal analysis was performed using the measured gas temperatures and the derived heat transfer coefficients to predict metal temperatures in the tube. Near surface metal temperatures of an uncoated throat tube were measured at the stagnation point and showed good agreement with temperatures predicted by the thermal model. The maximum heat flux to the throat tube was calculated and compared to that predicted for the leading edge of an HPFTP blade. It is shown that the heat flux to an uncooled throat tube is slightly greater than the heat flux to an HPFTP blade during engine startup.

Nesbitt, James A.↗

Adaptation of an Ammonia Detecting Paint to Commerical Applications

An ammonia-sensitive coating was developed in feasibility studies sponsored by Lockheed Engineering. The paint comprised a cellulosic binder, a dye, a family of solvents, and plasticizer. The resulting coating formulation proved to be very sensitive to trace levels of Lewis-bases and/or nucleophiles, but was limited to concentrations of approximately 1 ppm and higher. In the months following completion of this Lockheed project, efforts to perfect and optimize the paint formulation continued with internal funding. A unique sensitivity enhancing additive was identified and patented which when applied at concentrations of approximately 10% by weight, transcended the 1 ppm sensitivity barrier to fractional ppb. The paint composition was modified by the addition of certain proprietary agents, which promoted a much more intense yellow color in the coating and enhanced its durability in high-vacuum. Paint preparation is a simple one day procedure that can be completed using conventional equipment. Most of the materials are easily obtained.

Graef, Renee C.↗

Investigation of Thermal High Cycle and Low Cycle Fatigue Mechanisms of Thick Thermal Barrier Coatings

Ceramic thermal barrier coatings have attracted increased attention for diesel engine applications. The advantages of using the ceramic coatings include a potential increase in efficiency and power density and a decrease in maintenance cost. Zirconia-based ceramics are the most important coating materials for such applications because of their low thermal conductivity, relatively high thermal expansivity and excellent mechanical properties. However, durability of thick thermal barrier coatings (TBCS) under severe temperature cycling encountered in engine conditions, remains a major question. The thermal transients associated with the start/stop and no-load/full-load engine cycle, and with the in-cylinder combustion process, generate thermal low cycle fatigue (LCF) and thermal high cycle fatigue (HCF) in the coating system. Therefore, the failure mechanisms of thick TBCs are expected to be quite different from those of thin TBCs under these temperature transients. The coating failure is related not only to thermal expansion mismatch and oxidation of the bond coats and substrates, but also to the steep thermal stress gradients induced in the coating systems. Although it has been reported that stresses generated by thermal transients can initiate surface and interface cracks in a coating system, the mechanisms of the crack propagation and of coating failure under the complex LCF and HCF conditions are still not understood. In this paper, the thermal fatigue behavior of an yttria partially stabilized zirconia coating system under simulated LCF and HCF engine conditions is investigated. The effects of LCF and HCF on surface crack initiation and propagation are also discussed.

Zhu, Dong-Ming↗

Thermochemical Degradation Mechanisms for Reinforced Carbon/Carbon Panels on the Space Shuttle

The wing leading edge and nose cone of the space shuttle are fabricated from a reinforced carbon/carbon material (RCC). This material attains its durability from a diffusion coating of silicon carbide (SiC) and a glass sealant (ref. 1). During reentry, this material is subjected to an oxidizing high-temperature environment. Joint work between the Ohio State University and the NASA Lewis Research Center led to a survey of potential degradation mechanisms of the reinforced carbon/carbon (RCC) material at high temperatures

Source record↗

Solar Selective Coatings Prepared From Thin-Film Molecular Mixtures and Evaluated

Thin films composed of molecular mixtures of metal and dielectric are being considered for use as solar selective coatings for a variety of space power applications. By controlling molecular mixing during ion-beam sputter deposition, researchers can tailor the solar selective coatings to have the combined properties of high solar absorptance and low infrared emittance. On orbit, these combined properties simultaneously maximize the amount of solar energy captured by the coating and minimize the amount of thermal energy radiated. The solar selective coatings are envisioned for use on minisatellites, for applications where solar energy is used to power heat engines or to heat remote regions in the interior of the spacecraft. Such systems may be useful for various missions, particularly those to middle Earth orbit. Sunlight must be concentrated by a factor of 100 or more to achieve the desired heat inlet operating temperature. At lower concentration factors, the temperature of the heat inlet surface of the heat engine is too low for efficient operation, and at high concentration factors, cavity type heat receivers become attractive. The an artist's concept of a heat engine, with the annular heat absorbing surface near the focus of the concentrator coated with a solar selective coating is shown. In this artist's concept, the heat absorbing surface powers a small Stirling convertor. The astronaut's gloved hand is provided for scale. Several thin-film molecular mixtures have been prepared and evaluated to date, including mixtures of aluminum and aluminum oxide, nickel and aluminum oxide, titanium and aluminum oxide, and platinum and aluminum oxide. For example, a 2400- Angstrom thick mixture of titanium and aluminum oxide was found to have a solar absorptance of 0.93 and an infrared emittance of 0.06. On the basis of tests performed under flowing nitrogen at temperatures as high as 680 C, the coating appeared to be durable at elevated temperatures. Additional durability testing is planned, including exposure to atomic oxygen, vacuum ultraviolet radiation, and high-energy electrons.

Jaworske, Don A.↗

The Characterization of the Selected Materials for Space Shuttle

The harsh conditions to which the Space Shuttles are exposed during flight required the development and use of many unique materials. These materials were specially designed to withstand extreme temperatures, in some cases over 1600 C, while other material must withstand the cryogenic conditions of -253 C, and others must operate while under extreme loads. All of these materials must not only operate in the harsh condition but they must be light weight as well. The Space Shuttle is composed of three major components when configured for launch, Figure 1; the Shuttle, solid rocket boosters, and external tank (ET). The different heat shields of the Shuttle make up the thermal protection system (TPS); this system consists of many different types of components designed to operate on various parts of the vehicle. The body of the Shuttle and ET are composed mainly of aluminum alloy and graphite epoxy. The TPS consists of reinforced carbon-carbon (RCC) used on the wing leading edges and nose cap areas while the upper forward fuselage areas, the entire underside of the Shuttle, the Orbiter maneuvering system, and reaction control system utilize blacc high temperature reusable surface insulation (HRSI) tiles, Figure 2. Other areas of the Orbiter are protected by fibrous refractory composite insulation (FRCI) tiles. Areas where the temperature stays below 649 C, such as the forward fuselage, mid-fuselage, aft fuselage, vertical tail, and upper wing, are protected by other material such as, white low temperature reusable surface insulation (LRSI) tiles, advanced flexible reusable surface insulation (AFRSI) blankets, and felt reusable surface insulation (FRSI) white blankets. The RCC is a pyrolized laminated carbon with the outer surface converted to silicon carbide to prevent oxidation. The FiRST tiles are made of a low-density, high purity silica 99.8-percent amorphous fiber insulation that is made rigid by ceramic bonding resulting in 90-percent void and 10-percent materials. The RCC and HRSI are used in areas where the temperature rises above 1260 T. The FRCI tiles are high strength tiles derived by adding alumina-bososilicate fiber to the pure silica tile slurry that welds the micron-sizes fibers of pure silica into a rigid structure during sintering. The FRCI is composed of 20-percent alumina-borosilicate fibers and 80-percent silica fibers, and provided improved strength, durability and resistance to coating cracking and weight reduction than HRSI.

Kim, Hae-Soo↗

Effect of fuel to air ratio on Mach 0.3 burner rig hot corrosion of ZrO2-Y2O3 thermal barrier coatings

A Mach 0.3 burner rig test program was conducted to determine how the fuel to air mass ratio affects the durability of ZrO2-Y2O3/Ni-16Cr-6Al-0.31Y thermal barrier coating systems in combustion products containing 5 ppm Na and 2 ppm V. As the fuel to air mass ratio was increased from 0.039 to 0.049, the durability of ZrO2-6Y2O3, ZrO2-8Y2O3 and ZrO2-12Y2O3 coatings decreased. ZrO2-8Y2O3 coatings were approximately 2X and 1.3X more durable than ZrO2-12Y2O3 and ZrO2-6Y2O3 coatings respectively at the fuel to air mass ratio of 0.039. The number of one hour cycles endured by ZrO2-8Y2O3 coatings varied from averages of 53 to 200 for the fuel to air mass ratios of 0.049 and 0.039, respectively. At the fuel to air mass ratio of 0.049, all ZrO2-Y2O3 coated specimens failed in 40 to 60 one hour cycles

Hodge, P. E.↗

Derivation of a Levelized Cost of Coating (LCOC) metric for evaluation of solar selective absorber materials

A new metric, the Levelized Cost of Coating (LCOC), is derived in this paper to evaluate and compare alternative solar selective absorber coatings against a baseline coating (Pyromark 2500). In contrast to previous metrics that focused only on the optical performance of the coating, the LCOC includes costs, durability, and optical performance for more comprehensive comparisons among candidate materials. The LCOC is defined as the annualized marginal cost of the coating to produce a baseline annual thermal energy production. Costs include the cost of materials and labor for initial application and reapplication of the coating, as well as the cost of additional or fewer heliostats to yield the same annual thermal energy production as the baseline coating. Results show that important factors impacting the LCOC include the initial solar absorptance, thermal emittance, reapplication interval, degradation rate, reapplication cost, and downtime during reapplication. The LCOC can also be used to determine the optimal reapplication interval to minimize the levelized cost of energy production. As a result, similar methods can be applied more generally to determine the levelized cost of component for other applications and systems.

14 SOLAR ENERGY↗

Enhanced Catalyst Durability and Sulfur Tolerance by Atomic Layer Deposition (CRADA Final Report)

This CRADA advanced the use of atomic layer deposition (ALD) catalyst coatings to improve sulfur tolerance and demonstrate improved catalyst durability for biomass conversion chemistries. This project leveraged National Laboratory and industry expertise for ALD catalyst coating development between NREL, ALD NanoSolutions, Inc. ("ALD NanoSolutions"), and Johnson Matthey PLC ("Johnson Matthey"). To better understand the role of ALD coatings on catalyst activity and durability, a joint experimental and computational effort combined bench-scale ALD catalyst synthesis, material characterization, catalyst testing, and modeling of catalyst surface energetics. In addition, to demonstrate the commercial relevance of this technology, scaled ALD coated catalysts were subjected to continuous testing and accelerated aging to validate performance gains. Results were used to inform ALD catalyst coating manufacturing cost models, as well as biobased chemical process cost models.

09 BIOMASS FUELS↗

Performance of Al-rich Oxidation Resistant Coatings for Fe-Base Alloys

Aluminum-rich coatings made by chemical vapor deposition and pack cementation on ferritic (e.g. Fe-9Cr-1Mo) and austenitic (Type 304L) substrates are being evaluated at 650-800 C. For oxidation testing, a humid air environment was used to quantify coating performance, as uncoated substrates experience rapid oxidation at these temperatures. A main goal of this work is to demonstrate the potential benefits and problems with alumina-forming coatings. The higher exposure temperatures were selected to accelerate the degradation of the coating by interdiffusion with the substrate. A general conclusion of this testing was that coatings with less Al and a ferritic Fe(Al) structure could be more durable than higher Al content aluminide coatings which have a large thermal expansion mismatch with these substrates. A lifetime model has been developed using diffusion and oxidation observations to predict coating performance as a function of temperature and initial coating composition. To test and improve the model, additional experiments are now being conducted to determine the effect of substrate composition (e.g. Cr content using Fe-12Cr and Fe-9Cr-2W substrates) and exposure temperature on the critical Al content for coating failure. Because of the unexpectedly low level of Al measured at coating failure ({approx}3.5 at.% at 700 C), exposures of specimens with thick ({approx}200 {micro}m) high Al content coatings were stopped after 10kh at 800 C and 20kh at 700 C because extremely long times to failure were predicted. Post-exposure Al concentration profiles for these specimens were measured using electron microprobe.

36 MATERIALS SCIENCE↗

Performance of Al-Rich Oxidation Resistant Coatings for Fe-Base Alloys

Aluminum-rich coatings made by chemical vapor deposition and pack cementation on ferritic (e.g. Fe-9Cr-1Mo) and austenitic (Type 304L) substrates are being evaluated at 650-800 C. For oxidation testing, a humid air environment was used to quantify coating performance, as uncoated substrates experience rapid oxidation at these temperatures. A main goal of this work is to demonstrate the potential benefits and problems with alumina-forming coatings. The higher exposure temperatures were selected to accelerate the degradation of the coating by interdiffusion with the substrate. A general conclusion of this testing was that coatings with less Al and a ferritic Fe(Al) structure could be more durable than higher Al content aluminide coatings which have a large thermal expansion mismatch with these substrates. A lifetime model has been developed using diffusion and oxidation observations to predict coating performance as a function of temperature and initial coating composition. To test and improve the model, additional experiments are now being conducted to determine the effect of substrate composition (e.g. Cr content using Fe-12Cr and Fe-9Cr-2W substrates) and exposure temperature on the critical Al content for coating failure. Because of the unexpectedly low level of Al measured at coating failure ({approx}3.5at.% at 700 C), exposures of specimens with thick ({approx}200 {micro}m) high Al content coatings were stopped after 10kh at 800 C and 20kh at 700 C because extremely long times to failure were predicted. Post-exposure Al concentration profiles for these specimens were measured using electron microprobe.

36 MATERIALS SCIENCE↗

Performance of Al-Rich Oxidation Resistant Coatings For Fe-Base Alloys

Aluminum-rich coatings made by chemical vapor deposition and pack cementation on ferritic (e.g. Fe-9Cr-1Mo) and austenitic (Type 304L) substrates are being evaluated at 650-800 C. For oxidation testing, a humid air environment was used to quantify coating performance, as uncoated substrates experience rapid oxidation at these temperatures. A main goal of this work is to demonstrate the potential benefits and problems with alumina-forming coatings. The higher exposure temperatures were selected to accelerate the degradation of the coating by interdiffusion with the substrate. A general conclusion of this testing was that coatings with less Al and a ferritic Fe(Al) structure could be more durable than higher Al content aluminide coatings which have a large thermal expansion mismatch with these substrates. A lifetime model has been developed using diffusion and oxidation observations to predict coating performance as a function of temperature and initial coating composition. To test and improve the model, additional experiments are now being conducted to determine the effect of substrate composition (e.g. Cr content using Fe-12Cr and Fe-9Cr-2W substrates) and exposure temperature on the critical Al content for coating failure. Because of the unexpectedly low level of Al measured at coating failure ({approx}3.5at.% at 700 C), exposures of specimens with thick ({approx}200 {mu}m) high Al content coatings were stopped after 10kh at 800 C and 20kh at 700 C because extremely long times to failure were predicted. Post-exposure Al concentration profiles for these specimens were measured using electron microprobe.

36 MATERIALS SCIENCE↗

Ceramic thermal-barrier coatings for cooled turbines

Ceramic thermal-barrier coatings on hot engine parts have the potential to reduce metal temperatures, coolant requirements, cost, and complexity of the cooling configuration, and to increase life, turbine efficiency and gas temperature. Coating systems consisting of a plasma-sprayed layer of zirconia stabilized with either yttria, magnesia or calcia over a thin alloy bond coat have been developed, their potential analyzed and their durability and benefits evaluated in a turbojet engine. The coatings on air-cooled rotating blades were in good condition after completing as many as 500 two-minute cycles of engine operation between full power at a gas temperature of 1644 K and flameout, or as much as 150 hours of steady-state operation on cooled vanes and blades at gas temperatures as high as 1644 K witn 35 start and stop cycles. On the basis of durability and processing cost, the yttria-stabilized zirconia was considered the best of the three coatings investigated.

Liebert, C. H.↗

Development of a Long-Life-Cycle, Highly Water-Resistant Solar Reflective Retrofit Roof Coating

Highly water-resistant and solar-reflective coatings for low-slope roofs are potentially among the most economical retrofit approaches to thermal management of the building envelope. Therefore, they represent a key building technology research program within the Department of Energy. Research efforts in industry and the Department of Energy are currently under way to increase long-term solar reflectance on a number of fronts. These include new polymer coatings technologies to provide longer-lasting solar reflectivity and improved test methodologies to predict long-term soiling and microbial performance. The focus on long-term improvements in soiling and microbial resistance for maximum reflectance does not address the single most important factor impacting the long-term sustainability of low-slope roof coatings: excellent water resistance. The hydrophobic character of asphaltic roof products makes them uniquely suitable for water resistance, but their low albedo and poor exterior durability are disadvantages. A reflective coating that maintains very high water resistance with increased long-term resistance to soiling and microbial activity would provide additional energy savings and extend roof service life.

36 MATERIALS SCIENCE↗

MoVN-Cu Coatings for In Situ Tribocatalytic Formation of Carbon-Rich Tribofilms in Low-Viscosity Fuels

Inhibiting the tribological failure of mechanical assemblies which rely on fuels for lubrication is an obstacle to maintaining the lifetime of these systems with low-viscosity and low-lubricity fuels. Here in the present study, a MoVN-Cu nanocomposite coating was tribologically evaluated for durability in high- and low-viscosity fuels as a function of temperature, load, and sliding velocity conditions. The results indicate that the MoVN-Cu coating is effective in decreasing wear and friction relative to an uncoated steel surface. Raman spectroscopy, transmission electron microscopy, and electron-dispersive spectroscopy analysis of the MoVN-Cu worn surfaces confirmed the presence of an amorphous carbon-rich tribofilm which provides easy shearing and low friction during sliding. Further, the characterization of the formed tribofilm revealed the presence of nanoscale copper clusters overlapping with the carbon peak intensities supporting the tribocatalytic origin of the surface protection. The tribological assessment of the MoVN-Cu coating reveals that the coefficient of friction decreased with increasing material wear and initial contact pressure. These findings suggest that MoVN-Cu is a promising protective coating for fuel-lubricated assemblies due to its adaptive ability to replenish lubricious tribofilms from hydrocarbon environments.

36 MATERIALS SCIENCE↗