Search NASA⌕ Search

SEARCH · Search NASA

Results for “deformable”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

The deformation and burst behavior of Zircaloy-4 cladding tubes with hydride rim features subject to internal pressure loads

This study is motivated by the desire to conduct a separate effects test replicating specific aspects of an in-pile pulse reactor test on high exposure light water reactor (LWR) fuel rods. The principal purpose of the tests was to determine whether temperature and or hydrogen concentration thresholds exist in assessing the vulnerability of a stress relieved zirconium alloy cladding tubes to low strain ruptures. A secondary objective was to determine whether observations of the cladding stress during deformation could aid in the understanding of the crack formation and propagation in cladding tubes with hydride rim features. Here, the study utilized artificially hydrided Zircaloy-4 cladding tubes and an isothermal, internal pressure test that was controlled with an in-situ strain measurement. The test results show a clear transition in failure vulnerability between room temperature and 150 °C. Below 150 °C, cladding tubes rupture at very low uniform plastic strain—even at relatively modest cladding hydrogen levels. At and above 150 °C, cladding tubes only rupture at low uniform plastic strain if the cladding hydrogen content is greater than 500 ppm and usually experience at least some modest amount of plastic deformation prior to rupture. Post-test metallographs from non-ruptured cladding tubes show numerous primary cracks forming in the hydride rim and arresting at the metal/hydride interface. This observation combined with the decrease in bulk yielding of hydrided cladding tubes when compared to fresh non-hydrided tubes leads to the conclusion that the fracture stress of the hydride rims is related to and bounded by the yield stress of the zirconium metal. Some evidence is presented for a change in crack propagation mechanism from one of void formation on hydride plates and linkage at temperatures below 150 °C to more classical ductile shearing beneath the primary crack tip at temperatures above 150 °C. This apparent change in crack propagation mechanism may help explain the observed temperature and hydrogen concentration thresholds.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Soft interface instability and gas flow channeling in low-permeability deformable media

Understanding gas percolation through a clay layer or a shale formation is of great importance for the development of a geologic repository for nuclear waste disposal, a subsurface system for gas storage, and an engineering approach for hydrocarbon extraction from unconventional reservoirs. Gas injection experiments have revealed complex dynamic behaviours of gas percolation through water saturated compacted bentonite, characterized by a high breakthrough pressure, rapid breakthrough, a pressure/stress decay after the breakthrough, a relatively high migration rate, high-frequency periodic/nonperiodic variations in flow rate, stepwise rate reductions during relaxation, and low gas saturation over the whole process, all indicating channelling nature of the processes. Using linear stability analyses, we show that this channelling can autonomously emerge from the instability of the deformable interface between the injected gas and the compacted bentonite matrix driven by local stress concentration, pore dilation, and hydrologic gradient. Channel patterns formed would possess a fractal geometry. We further show that, once a percolating channel is established, the gas injected would percolate through the channel in a chain of gas bubbles, also due to the interface instability, resulting in periodic/chaotic variations in gas flow rate. Our work provides a unified explanation for key features observed for gas percolation in low-permeability deformable media. The work also suggests a possibility of designing an engineered barrier system for a nuclear waste repository that can have controllable gas release while limit water transport.

Bentonite↗

A study of adhesive bonding in metal–metal, metal–CFRP, and CFRP–CFRP material combinations under shear deformation: Fracture morphologies and damage mechanisms

Safe design of adhesive joining in multi-materials in engineered structures requires the accumulation of numerous experimental data on the failure behavior of various adhesively-bonded material combinations under different loading conditions. The deep understanding of mechanical performance, fracturing morphologies, and main damage mechanisms is also quintessential for accelerating the development of proper physics-based and multi-scale models for assisting the design. Towards this goal, this work presents a comprehensive characterization of the failure behavior of adhesively-bonded metal–metal, metal–CFRP, and CFRP–CFRP material combinations under global shear deformation via single lap shear testing. Thanks to a synergistic combination of measurement methods by using Digital Imaging Correlation (DIC) and 3D optical profilometry, adhesive features on the adherend after failure were quantified and the main progressive damage mechanisms were identified. The characterization performed in this work provides quantitative data that contributes to a better understanding of shear failure in adhesive bonding across different bi-material combinations. Finally, the obtained results have practical implications, including the potential to enhance adhesive bonding design, identify failure causes in adhesive joints, and develop or validate computational models capable of capturing the observed behavior in various adhesively-bonded materials under global shear deformation.

36 MATERIALS SCIENCE↗

Tensile and compressive plastic deformation behavior of medium-entropy Cr-Co-Ni single crystals from cryogenic to elevated temperatures

The equiatomic Cr-Co-Ni medium-entropy alloy has the face-centered cubic (FCC) structure. Bulk single crystals of this alloy were grown and tested in tension and compression between 14 K and 1373 K with the loading axis parallel to [23]. At room temperature, the critical resolved shear stress (CRSS) for {111}<10> slip is 65 ± 5 MPa and does not exhibit a tension-compression asymmetry. It does, however, increase significantly as the test temperature decreases. A dulling of this temperature dependence occurs below 50 K, which may be due to the inertia effect. When the measured values above 50 K are extrapolated to lower temperatures, a value of 225 MPa is estimated for the CRSS at 0 K. This is larger than that (168 MPa) previously determined for the equiatomic Cr-Mn-Fe-Co-Ni high-entropy alloy using a similar procedure. The stacking fault energy of the present Cr-Co-Ni is estimated to be about 14 mJm-2, which is sufficiently low to account for deformation twinning both at 77 K and room temperature. Twinning at 77 K occurs on conjugate (1) planes at an onset shear stress of 482 MPa after primary slip and propagates in the form of Lüders deformation. At room temperature, twinning occurs uniformly throughout the gauge section on primary (111) planes at an onset shear stress of 381 MPa after primary and subsequent conjugate slip. Thin layers with the hexagonal close-packed stacking are observed in association with twinning both at 77 K and room temperature.

36 MATERIALS SCIENCE↗

Deformation, dislocation evolution and the non-Schmid effect in body-centered-cubic single- and polycrystal tantalum

A physically-informed continuum crystal plasticity model is presented to elucidate deformation mechanisms, dislocation evolution and the non-Schmid effect in body-centered-cubic (bcc) tantalum widely used as a key structural material for mechanical and thermal extremes. We show the unified structural modeling framework informed by mesoscopic dislocation dynamics simulations is capable of capturing salient features of the large inelastic behavior of tantalum at quasi-static (10 -3 s -1 ) to extreme strain rates (5000 s -1 ) and at low (77 K) to high temperatures (873 K) at both single- and polycrystal levels. Here we also present predictive capabilities of the model for microstructural evolution in the material. To this end, we investigate the effects of dislocation interactions on slip activities, instability and the non-Schmid behavior at the single crystal level. Furthermore, ex situ measurements on crystallographic texture evolution and dislocation density growth are carried out for polycrystal tantalum specimens at increasing strains. Numerical simulation results also support that the modeling framework is capable of capturing the main features of the polycrystal behavior over a wide range of strains, strain rates and temperatures. The theoretical, experimental and numerical results at both single- and polycrystal levels provide critical insight into the underlying physical pictures for micro- and macroscopic responses and their relations in this important class of refractory bcc materials undergoing large inelastic deformations.

36 MATERIALS SCIENCE↗

A mesoscale crystal plasticity model to predict room-temperature deformation and martensitic transformation of high-strength Quenching and Partitioning (Q&P) Steels and validation with synchrotron X-ray diffraction

Renowned for the superior mechanical properties and adeptness at cold-forming, Quenching and Partitioning (QP) steels have gained prominence as a promising candidate material in fabricating safety-critical components in various industries. The pertinent research on QP steels focus on the martensitic transformation of the Retained Austenite (RA) phase during cold-forming, a crucial mechanism that substantially influences the overall strength and ductility of QP steels. The austenite stability and transformation rate heavily rely on the local strain path and the initial microstructure, which is challenging for analytical prediction. In this paper, a mesoscale model is developed to capture the deformation and transformation kinetics of QP steels inside the microstructure. The model integrates the detailed explicit microstructure, acquired from characterization experiments, into a high-resolution finite element (FE) mesh. It distinctly model the deformation and interaction between the various phases and the effect on the transformation of RA. The model is validated with high energy X-ray diffraction (HEXRD) data, and shows excellent capability in predicting the asymmetric stress-strain behavior under uniaxial tension and compression, as well as the martensitic transformation rate. The model is used to investigate the strain and load partitioning effect of surrounding matrix to the transformation of RA, offering insights into the complex behavior of QP980 and facilitates further material development.

36 MATERIALS SCIENCE↗

Formation of I 1 stacking fault by deformation defect evolution from grain boundaries in Mg

I 1 stacking faults (SFs) in Mg alloys are regarded as the nucleation sites of $\langle \text{c+a} \rangle$ dislocations that are critical for these alloys to achieve high ductility. Previously it was proposed that the formation of I 1 SFs requires the accumulations of a large number of vacancies, which are difficult to achieve at low temperatures. In this study, molecular dynamics (MD) and molecular statics (MS) simulations based on empirical interatomic potentials were applied to investigate the deformation defect evolutions from the symmetric tilt grain boundaries (GBs) in Mg and Mg-Y alloys under external loading along $\langle c \rangle$-axis. The results show the planar faults (PFs) on Pyramidal I planes first appear due to the nucleation and glide of $\langle {\frac {1}{2}}c + p\rangle$ partial dislocations from GBs, where $\langle p\rangle$ = ${\frac {1}{3}} \langle10\bar{1}0\rangle$. These partial dislocations with pyramidal PFs interact with other defects, including pyramidal PFs themselves, GBs, and $\langle p\rangle$ partial dislocations, generating a large amount of I 1 SFs. Detailed analyses show the nucleation and growth of I 1 SFs are achieved by atomic shuffle events and deformation defect reactions without the requirements of vacancy diffusion. Our simulations also suggest the Y clusters at GBs can reduce the critical stress for the formation of pyramidal PFs and I 1 SFs, which provide a possible reason for the experimental observations that Y promotes the $\langle{\text{c+a}}\rangle$ dislocation activities.

36 MATERIALS SCIENCE↗

Effects of Zn and Ca on the deformation texture evolution of Mg–Zn–Ca alloys at elevated temperatures

This work utilized crystal plasticity simulations and experimental thermo-mechanical processing to examine how Zn and Ca content affects texture evolution in Mg–Zn–Ca alloys during simulated hot rolling. Four different compositions were studied: unalloyed Mg and three Mg alloys of ZX0p50 (Mg- 0.5 wt% Zn- 0.1 wt% Ca), ZX30 (Mg-3 wt% Zn- 0.1 wt% Ca), and ZX31 (Mg-3 wt% Zn- 0.3 wt% Ca). Multi-pass Gleeble experiments simulated hot rolling using plane strain conditions. Unalloyed Mg developed a strong basal texture, while the addition of Zn and Ca significantly weakened the texture in ZX30 and ZX31; this reduction was not seen in ZX0p50. Notably, ZX31 exhibited a split basal texture aligned with the rolling direction. Crystal plasticity simulations revealed that the weaker basal texture in ZX30 and ZX31 resulted from reduced activation of basal and twinning modes compared to unalloyed Mg and Zx0p50. Increased Zn and Ca content raised the ratios of basal to pyramidal critical resolved sheer stress (CRSS) and twin to pyramidal CRSS, enhancing pyramidal slip activity and weakening the basal texture. Extension twinning played a critical role in texture development during the first deformation pass. In unalloyed Mg and ZX0p50, twinning led to a strong basal texture, while ZX30 and ZX31 had weak basal textures that increased only slightly with further deformation. The split basal poles simulated in ZX31 were consistent with the experimental findings, highlighting the interplay between alloy composition and texture evolution.

Crystal plasticity finite element↗

Distributed fiber optic strain sensing of bending deformation of a well mockup in the laboratory

Well integrity is critical to the safety and success of subsurface energy exploration and management, as leakage of fluids from subsurface reservoirs is often induced by compromised wells. This study investigates bending deformation of a mockup of an oil/gas well that is subjected to loads expected in deviated wells under reservoir compaction and assesses the feasibility of utilizing distributed fiber optic strain sensing to monitor the deformation. Here, a well mockup, which consists of outer and inner steel pipes with a cemented annulus, is tested under three-point bending loading and its strain and curvature development is monitored by Brillouin optical time domain reflectometry/analysis (BOTDR/A) as well as optical frequency domain reflectometry (OFDR). The primary objective of this research is to assess the strain sensing performance of newly fabricated fiber optic cables and to identify key cable characteristics which could improve the quality of distributed strain measurements with BOTDR/A. Results show that the tight-buffered cable is best suited for strain sensing as its maximum errors in the strain measurement were -36% and -24% against conventional sensors at the maximum elastic and plastic bending loads, respectively, whereas those of the non-tight-buffered cable were -45% and -71%, respectively. Similar trends were obtained in the bending curvature measurement. The detailed design of the tight-buffered cable is presented to elucidate key characteristics of such a cable, which will facilitate accurate distributed strain sensing in oil and gas wells.

42 ENGINEERING↗

BISON analysis of FeCrAl and Zircaloy cladding deformation during simulated BWR cyclic dryout conditions

The BISON fuel performance analysis code has been used to study FeCrAl and Zircaloy cladding performance to better understand cladding deformation behavior in boiling water reactors during conditions caused by anticipated operational occurrences (AOOs) or by anticipated transients without scram (ATWS). BISON models of novel separate effects tests simulating ATWS events predicted mechanical responses to thermal cycling boundary conditions. Here, we assessed FeCrAl and Zircaloy deformation and burst models to determine those best suited for cyclic dryout event analysis. In addition, we compared diametral strain profiles of the post-experiment claddings to simulation results. The capability of the BISON code for modeling BWR AOO or ATWS events is promising.

36 MATERIALS SCIENCE↗

The effects of microstructures and radiation damage on the deformation behavior of a HT-9 alloy using microtensile testing

Understanding the influence of radiation damage on the mechanical properties of HT-9 and other tempered martensitic alloys is part of the mission in developing radiation-tolerant materials for the next generation of nuclear reactors. Although there has been extensive data on the macroscopic mechanical properties of the irradiated HT-9 alloys and microstructural changes, it is not well-understood how radiation damage and the resulting microstructural changes influence the local mechanical properties. In this study, we utilized in situ SEM microtensile testing to investigate the deformation behavior of specific martensitic boundaries in 1 dpa proton-irradiated HT-9 and answered the question of what is the weakest link. Additionally, we provided the direct observation of the failure modes of microtensiles containing high angle and low angle martensitic boundaries. In the unirradiated condition, the deformation is ductile and no martensitic boundary failure is observed. In the irradiated condition, the high angle martensitic boundaries are more susceptible to radiation-induced boundary failure as compared to the low angle martensitic boundaries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling deformation and failure in AlSi-polyester abradable sealcoating material using microstructure-based finite element simulation

A plasma-sprayed aluminum-silicon (AlSi)/polyester coating is applied in modern gas turbine engines as an abradable sealcoating to maintain tight clearances between the rotating blades and the static casing. While running the engine, the rotating blades “rub” with the abradable coating, which results in extreme strain rate (up to 10 6 ) dynamics and a high-temperature environment. Due to the difficulty of collecting direct measurements, predictive computational models are important for analyzing the deformation and failure of the abradable material, to help meet the design target of avoiding damage to the blade tip and maintaining high fuel efficiency. In this research, a microstructure-based finite element (FE) computational model was developed to capture the complex mechanical behavior of the AlSi/polyester microstructure. The model is based on a virtual representative-volume-element (RVE) of a metal-polymer microstructure, reconstructed from x-ray computed tomography. It models the plastic deformation of, and damage to, each AlSi and polyester constituents, as well as the failure at their interface. The model was calibrated and validated with uniaxial tension and compression experiments, conducted at two temperatures (298 K and 533 K) at an applied strain rate of 10 3 - 10 4 s -1 . The material exhibited strongly asymmetric tension-compression behavior and a sensitivity to temperature, which was well captured by the model. The model was further applied to investigate changes in mechanical behavior due to variations in constituents’ volume fractions, which provides guidance to the microstructural design of AlSi/polyester abradable materials. The model is expected to facilitate the development of improved abradable materials by bypassing the conventional trial-and-error approach and extensive testing requirements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploring pressure-dependent inelastic deformation and failure in bonded granular composites: An energetic materials perspective

In polymer-filled granular composites, damage may develop in mechanical loading prior to material failure. Damage mechanisms such as microcracking or plastic deformation in the binder phase can substantially alter the material’s mesostructure. For energetic materials, such as solid propellants and plastic bonded explosives, these mesostructural changes can have far reaching effects including degraded mechanical properties, potentially increased sensitivity to further insults, and changes in expected performance. Unfortunately, predicting damage is nontrivial due to the complex nature of these composites and the entangled interactions between inelastic mechanisms. In this work, we assess the current literature of experimental knowledge, focusing on the pressure-dependent shear response, and propose a simple simulation framework of bonded particles to study four limiting-case material formulations at both meso- and macro-scales. Further, to construct the four cases, we systematically vary the relative interfacial strength between the polymer binder and granular filler phase and also vary the polymer’s glass transition temperature relative to operating temperature which determines how much the binder can plastically deform. These simulations identify key trends in global mechanical response, such as the emergence of strain hardening or softening regimes with increasing pressure which qualitatively resemble experimental results. By quantifying the activation of different inelastic mechanisms, such as bonds breaking and plastically straining, we identify when each mechanism becomes relevant and provide insight into potential origins for changes in mechanical responses. The locations of broken bonds are also used to define larger, mesoscopic cracks to test various metrics of damage. We primarily focus on triaxial compression, but also test the opposite case of triaxial extension to highlight the impact of Lode angle on mechanical behavior.

36 MATERIALS SCIENCE↗

Deformation behavior of nanoscale Al–Al 2 Cu eutectics studied by in situ micropillar compression

We report deformation behavior of nanoscale laser processed Al–Al 2 Cu eutectics at room temperature is characterized through in situ micro-pillar compression testing in a scanning transmission microscope. Interlamellar spacing of Al–Al 2 Cu eutectics varies from hundreds of nanometers to 20 nm. Three different sizes of micro-pillars are fabricated in order to study the deformation behaviors of single colony and multiple colonies, corresponding to the single crystal and polycrystal respectively. For single colonies, lamellar orientations parallel, normal or inclined to the loading direction were tested. The main findings are: 1) the plasticity mechanisms strongly depend on loading orientation: buckling and kinking in the parallel-loaded eutectics, planar sliding along Al–Al 2 Cu lamellar interfaces in the incline-loaded eutectics and localized shearing in the normal-loaded eutectics. 2) the incline-loaded eutectics exhibits the lowest compression flow strength, and the normal-loaded eutectics has the highest compression flow strength. 3) with decreasing inter-lamellar spacing, the strength increases and plasticity is uniformly distributed, as opposed to shear localization. Highest compressive plasticity is observed in polycrystalline eutectics with an ensemble of lamellar orientations with ~20 nm average spacing: 17.9% at flow stress of 1.63 GPa, and degenerate, bimodal morphology: 11.1% at flow stress of 1.36 GPa.

36 MATERIALS SCIENCE↗

In-situ synchrotron diffraction study of the localized phase transformation and deformation behavior in NiTi SMA

The accumulation of dislocation defect was generally recognized as the origin of residual strain and the pseudoelastic instability in NiTi shape memory alloys (SMAs). In the present work, the pseudoelastic instability was studied by comparing the characteristics of Luders-type and uniform transformation mechanism via in-situ synchrotron-based high-energy X-ray diffraction (XRD) characterization. The experimental results showed that the Liiders-type mechanism could result in an intense and sharp increase of stress-induced martensite at the expense of austenite. The residual austenite with high lattice strain within the Luders band might be fully martensitic beyond the stress plateau of the E-a curve. With the accumulation of dislocation defect, the uniform martensitic transformation took place by the progressively homogeneous nucleation and growth of martensite in a local region. While the residual martensite and dislocation density was stabilized during mechanical cycling, the deformation of NiTi SMA turned into a mixture of (i) a balanced forward and reverse phase transformation between austenite and martensite, as well as (ii) the elastic deformation of the aggregate. As a result, there was no apparent increase in dislocation density detected during further cycling.

36 MATERIALS SCIENCE↗

Collapse of helium-filled voids in extreme deformation: Dislocation mechanisms

The mechanisms responsible for the collapse of helium-filled bubbles during the passage of shock waves in monocrystalline copper are revealed. Both internal pressure (caused by pre-existing helium atoms) and bubble size are varied in molecular dynamics simulations to understand the atomistic scale deformation as they are subjected to shock compression at pressures of 48, 123, and 170 GPa, corresponding to particle velocities of 1.0, 2.0, and 2.5 km/s. Both empty and helium filled bubbles serve as dislocation sources, generating intense, localized plastic regions. There are distinct differences in the collapse of empty voids compared to He-filled bubbles, the former requiring less stress and generating a greater density of dislocations for a given shock strength. Additionally, a generalized model for dislocation emission is proposed, where the inclusion of shear stress generated by the helium bubble increases the critical stress to generate dislocations at the defect surface, demonstrating the change in plastic deformation.

36 MATERIALS SCIENCE↗

In-situ neutron diffraction investigation of two-stage martensitic transformation in a 13%Mn steel with serrated deformation

Two stage austenite →ε-martensite →α-martensite phase transformation, phase-specific lattice strain evolution and load sharing during tensile deformation of a 13%Mn hot-rolled austenitic steel are revealed by in-situ neutron diffraction. In conclusion, direct evidence is provided that serrated deformation behavior is attributed to discontinuous martensitic transformation.

Austenitic steel↗

Transformation and twinning induced plasticity in metastable Ti-Mo alloys under high strain rate deformation

The development of metastable titanium (Ti) alloys provides an unprecedented opportunity to expand their use in plasticity and damage critical applications like protective structures. However, such applications require knowledge of quasi-static to dynamic mechanical behavior, which is currently lacking. Here we perform in-situ, ultrafast synchrotron x-ray diffraction during high strain rate (Kolsky) pressure bar testing in tension and post-mortem electron microscopy to study TRansformation Induced Plasticity (TRIP) and TWinning Induced Plasticity (TWIP) in metastable Ti-Mo alloys. Two alloys, namely Ti-12Mo and Ti-15Mo (wt.%), were selected for study having different β -phase chemical stabilities. TWIP was observed in both Ti-12Mo and Ti-15Mo by in-situ synchrotron diffraction during high strain rate testing. Post-mortem microstructural characterization also revealed the presence of TRIP in Ti-12Mo. TWIP in Ti-15Mo was found to under-perform in terms of total elongation compared to TRIP/TWIP in Ti-12Mo. Ti-12Mo exhibited an average elongation of 17% compared to only 12% for Ti-15Mo with deformation at 1000 s -1 . In conclusion, TRIP resulted in significantly finer microstructure evolution and alleviated local strain accumulations in Ti-12Mo, suggesting TRIP can be used to tune available strength/ductility combinations in metastable Ti alloys under high strain rate deformation conditions.

36 MATERIALS SCIENCE↗