Search NASA⌕ Search

SEARCH · Search NASA

Results for “laser testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Long term reliability study and life time model of quantum cascade lasers

Here, we present results of quantum cascade laser lifetime tests under various aging conditions including an accelerated life test. The total accumulated life time exceeds 1.5 × 106 device hours. The longest single device aging time was 46 500 hours without failure in the room temperature aging test. Four failures were found in a group of 19 devices subjected to the accelerated life test with a heat-sink temperature of 60 °C and a continuous-wave current of 1 A. Failure mode analyses revealed that thermally induced oxidation of InP in the semi-insulating layer is the cause of failure. An activation energy of 1.2 eV is derived from the dependence of the failure rate on laser core temperature. The mean time to failure of the quantum cascade lasers operating at a typical condition with the current density of 5 kA/cm2 and heat-sink temperature of 25 °C is expected to be 809 000 hours.

Xie, Feng↗

Diborane Electrode Response in 3D Silicon Sensors for the CMS and ATLAS Experiments

Unusually high leakage currents have been measured in test wafers produced by the manufacturer SINTEF containing 3D pixel silicon sensor chips designed for the ATLAS (A Toroidal LHC ApparatuS) and CMS (Compact Muon Solenoid) experiments. Previous data has shown the CMS chips as having a lower leakage current after processing than ATLAS chips. Some theories behind the cause of the leakage currents include the dicing process and the usage of copper in bump bonding, and with differences in packaging and handling between the ATLAS and CMS chips causing the disparity between the two. Data taken at SLAC from a SINTEF wafer with electrodes doped with diborane and filled with polysilicon, before dicing, and with indium bumps added contradicts this past data, as ATLAS chips showed a lower leakage current than CMS chips. It also argues against copper in bump bonding and the dicing process as main causes of leakage current as neither were involved on this wafer. However, they still display an extremely high leakage current, with the source mostly unknown. The SINTEF wafer shows completely different behavior than the others, as the FEI3s actually performed better than the CMS chips. Therefore this data argues against the differences in packaging and handling or the intrinsic geometry of the two as a cause in the disparity between the leakage currents of the chips. Even though the leakage current in the FEI3s overall is lower, the current is still significant enough to cause problems. As this wafer was not diced, nor had it any copper added for bump bonding, this data argues against the dicing and bump bonding as causes for leakage current. To compliment this information, more data will be taken on the efficiency of the individual electrodes of the ATLAS and CMS chips on this wafer. The electrodes will be shot perpendicularly with a laser to test the efficiency across the width of the electrode. A mask with pinholes has been made to focus the laser to a beam smaller than the width of an electrode in order to properly scan it. This will provide more information on whether something in the electrodes, such as the polysilicon filling, is contributing to the leakage current or if there is another cause to be found. It will also reveal whether the diborane doping method and the new polysilicon filling has increased the electrode efficiency as expected. Thus, the cause of these leakage currents on the wafers from SINTEF has yet to be definitively found.

43 PARTICLE ACCELERATORS↗

Effect of Heat Treatment on Microstructure and Mechanical Properties of Laser Additively Manufactured AISI H13 Tool Steel

The effect of heat treatment on microstructure and mechanical properties (microhardness, wear resistance and impact toughness) of laser additively manufactured AISI H13 tool steel was systemically investigated. To understand the variation of microstructure and mechanical properties under different heat treatments, the as-deposited samples were treated at 350, 450, 550, 600 and 650 °C/2 h, respectively. Microstructure and phase transformation were investigated through optical microscopy, scanning electron microscope and transmission electron microscope. The mechanical properties were characterized by nanoindentation tests, Charpy tests and high-temperature wear tests. The microstructure of as-deposited samples consisted of martensite, ultrafine carbides and retained austenite. After the tempering treatment, the martensite was converted into tempered martensite and some fine alloy carbides which precipitated in the matrix. When treated at 550 °C, the greatest hardness and nanohardness were 600 HV{sub 0.3} and 6119.4 MPa due to many needle-like carbides precipitation. The value of hardness increased firstly and then decreased when increasing the temperature. When tempered temperatures exceeded 550 °C, the carbides became coarse, and martensitic matrix recrystallized at the temperature of 650 °C. The least impact energy was 6.0 J at a temperature of 550 °C. Samples tempered at 550 °C had larger wear volume loss than that of others. Wear resistances of all samples under atmospheric condition at 400 °C showed an oxidation mechanism.

36 MATERIALS SCIENCE↗

Pulsed Laser System to Simulate Effects of Cosmic Rays in Semiconductor Devices

Spaceflight system electronic devices must survive a wide range of radiation environments with various particle types including energetic protons, electrons, gamma rays, x-rays, and heavy ions. High-energy charged particles such as heavy ions can pass straight through a semiconductor material and interact with a charge-sensitive region, generating a significant amount of charge (electron-hole pairs) along their tracks. These excess charges can damage the device, and the response can range from temporary perturbations to permanent changes in the state or performance. These phenomena are called single event effects (SEE). Before application in flight systems, electronic parts need to be qualified and tested for performance and radiation sensitivity. Typically, their susceptibility to SEE is tested by exposure to an ion beam from a particle accelerator. At such facilities, the device under test (DUT) is irradiated with large beams so there is no fine resolution to investigate particular regions of sensitivity on the parts. While it is the most reliable approach for radiation qualification, these evaluations are time consuming and costly. There is always a need for new cost-efficient strategies to complement accelerator testing: pulsed lasers provide such a solution. Pulsed laser light can be utilized to simulate heavy ion effects with the advantage of being able to localize the sensitive region of an integrated circuit. Generally, a focused laser beam of approximately picosecond pulse duration is used to generate carrier density in the semiconductor device. During irradiation, the laser pulse is absorbed by the electronic medium with a wavelength selected accordingly by the user, and the laser energy can ionize and simulate SEE as would occur in space. With a tightly focused near infrared (NIR) laser beam, the beam waist of about a micrometer can be achieved, and additional scanning techniques are able to yield submicron resolution. This feature allows mapping of all of the sensitive regions of the studied device with fine resolution, unlike heavy ion experiments. The problematic regions can be precisely identified, and it provides a considerable amount of information about the circuit. In addition, the system allows flexibility for testing the device in different configurations in situ.

Aveline, David C.↗

Experimental Design for the LATOR Mission

This paper discusses experimental design for the Laser Astrometric Test Of Relativity (LATOR) mission. LATOR is designed to reach unprecedented accuracy of 1 part in 10(exp 8) in measuring the curvature of the solar gravitational field as given by the value of the key Eddington post-Newtonian parameter gamma. This mission will demonstrate the accuracy needed to measure effects of the next post-Newtonian order (near infinity G2) of light deflection resulting from gravity s intrinsic non-linearity. LATOR will provide the first precise measurement of the solar quadrupole moment parameter, J(sub 2), and will improve determination of a variety of relativistic effects including Lense-Thirring precession. The mission will benefit from the recent progress in the optical communication technologies the immediate and natural step above the standard radio-metric techniques. The key element of LATOR is a geometric redundancy provided by the laser ranging and long-baseline optical interferometry. We discuss the mission and optical designs, as well as the expected performance of this proposed mission. LATOR will lead to very robust advances in the tests of Fundamental physics: this mission could discover a violation or extension of general relativity, or reveal the presence of an additional long range interaction in the physical law. There are no analogs to the LATOR experiment; it is unique and is a natural culmination of solar system gravity experiments.

Turyshev, Slava G.↗

Electron beam test of key elements of the laser-based calibration system for the muon g - 2 experiment

We report the test of many of the key elements of the laser-based calibration system for muon g - 2 experiment E989 at Fermilab. The test was performed at the Laboratori Nazionali di Frascati's Beam Test Facility using a 450 MeV electron beam impinging on a small subset of the final g - 2 lead-fluoride crystal calorimeter system. The calibration system was configured as planned for the E989 experiment and uses the same type of laser and most of the final optical elements. We show results regarding the calorimeter's response calibration, the maximum equivalent electron energy which can be provided by the laser and the stability of the calibration system components.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Laterally Coupled Quantum-Dot Distributed-Feedback Lasers

InAs quantum-dot lasers that feature distributed feedback and lateral evanescent- wave coupling have been demonstrated in operation at a wavelength of 1.3 m. These lasers are prototypes of optical-communication oscillators that are required to be capable of stable single-frequency, single-spatial-mode operation. A laser of this type (see figure) includes an active layer that comprises multiple stacks of InAs quantum dots embedded within InGaAs quantum wells. Distributed feedback is provided by gratings formed on both sides of a ridge by electron lithography and reactive-ion etching on the surfaces of an AlGaAs/GaAs waveguide. The lateral evanescent-wave coupling between the gratings and the wave propagating in the waveguide is strong enough to ensure operation at a single frequency, and the waveguide is thick enough to sustain a stable single spatial mode. In tests, the lasers were found to emit continuous-wave radiation at temperatures up to about 90 C. Side modes were found to be suppressed by more than 30 dB.

Qui, Yueming↗

Statistical Correlation of Heliostat Pointing Deviation With Wind

This work was carried out as part of the Heliostat Consortium (HelioCon) Field Deployment subtask with the aim to develop a reduced order model framework for correlating wind speed and pointing deviation of a heliostat facet. There are only sparse field measurements of heliostat pointing deviations and accompanying wind conditions published in the literature. Heliostat test standards, such as IEC 62862-4-3, propose a suite of tests including laser pointing repeatability at wind speeds below 4 m/s, and provide technical requirements for heliostat slope and tracking deviations in coarse average wind speed bins of 4 m/s, 6 m/s, and 8 m/s. In addressing the gap of the variation of heliostat pointing deviation with wind speed, field measurements of laser pointing on a grid target and wind conditions were analyzed in this study at the Third-Party Metrology Platform at the National Laboratory of the Rockies (NLR) Flatirons Campus. Horizontal pointing deviations were found to follow a logarithmic relationship with peak wind speed, whereas vertical pointing deviations follow an exponential relationship with peak wind speed. Both horizontal and vertical pointing deviations also follow a second order polynomial relationship, as expected from the proportionality of elastic loads and deformations with the square of wind speed. The results indicate that heliostat facet pointing deviations in the vertical direction increase at a faster rate than in the horizontal direction with increasing wind speed over the tested range, however these are dependent on the heliostat structural design. Next steps are recommended for additional field measurements to confirm a linear relationship of pointing deviation with applied moment on a heliostat facet, and to distinguish between gravity-induced and wind-induced pointing deviations at different elevation angles. The derived correlations in the preliminary analysis in this report serve as a case study for heliostat developers and plant operators to estimate the wind-induced pointing deviations and their variation with peak gust wind speed. Next steps in future work would recommend higher resolution and longer duration datasets for different elevation angles and wind directions to reduce uncertainties and variance of collected laser beam spot data and their correlations with bin-averaged wind speed.

17 WIND ENERGY↗

Diode pumped Nd:YAG laser development

A low power Nd:YAG laser was constructed which employs GaAs injection lasers as a pump source. Power outputs of 125 mW TEM CW with the rod at 250 K and the pump at 180 K were achieved for 45 W input power to the pump source. Operation of the laser, with array and laser at a common heat sink temperature of 250 K, was inhibited by difficulties in constructing long-life GaAs LOC laser arrays. Tests verified pumping with output power of 20 to 30 mW with rod and pump at 250 K. Although life tests with single LOC GaAs diodes were somewhat encouraging (with single diodes operating as long as 9000 hours without degradation), failures of single diodes in arrays continue to occur, and 50 percent power is lost in a few hundred hours at 1 percent duty factor. Because of the large recent advances in the state of the art of CW room temperature AlGaAs diodes, their demonstrated lifetimes of greater than 5,000 hours, and their inherent advantages for this task, it is recommended that these sources be used for further CW YAG injection laser pumping work.

Reno, C. W.↗

In situ calibration of the foil detector for an infrared imaging video bolometer using a carbon evaporation technique

The InfraRed imaging Video Bolometer (IRVB) is a useful diagnostic for the multi-dimensional measurement of plasma radiation profiles. For the application of IRVB measurement to the neutron environment in fusion plasma devices such as the Large Helical Device (LHD), in situ calibration of the thermal characteristics of the foil detector is required. Laser irradiation tests of sample foils show that the reproducibility and uniformity of the carbon coating for the foil were improved using a vacuum evaporation method. Also, the principle of the in situ calibration system was justified.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Understanding spectral dependance of laser-induced damage precursors in dielectric materials (Full report_23-ERD-006)

The performance of high-energy laser systems is constrained by laser-induced damage in dielectric coatings, particularly those containing hafnium oxide (HfO 2 ). While thresholds at fundamental Nd harmonics are well studied, the spectral dependence of damage initiation—especially under dual-wavelength irradiation—remains poorly characterized. This project provides the first systematic investigation of wavelength-dependent laser damage in hafnia coatings, focusing on nanoscale precursors such as craze lines, nanobubbles, stoichiometric variations, nodules, and controlled crystallization. Coatings were fabricated via ion beam sputtering and electron-beam deposition and characterized using spectrophotometry, ellipsometry, AFM, GI-XRD, RBS, PCI absorption, and fs/ns laser damage testing. Results show that craze lines, benign under infrared light, strongly initiate damage under UV due to wavelength-selective field intensification. Substituting xenon for argon suppresses nanobubbles and improves UV thresholds by up to 32%. Oxygen modulation reveals that fully oxidized films maximize UV resistance, though at the cost of porosity and stress in multilayers. HfO 2 –SiO 2 composites resist crystallization and defects while achieving ppm-level absorption and elevated thresholds, whereas full crystallization of HfO 2 enhances LIDT by reducing defects and improving thermal transport. Collectively, these findings link photon energy, defect states, and bandgap collapse, providing a predictive framework for wavelength-dependent laser damage. The outcomes directly inform the design of durable, multi-wavelength coatings for facilities such as NIF, MEC, HAPLS, and DPAL, advancing the readiness of next-generation optics.

36 MATERIALS SCIENCE↗

Wind Tunnel Testing of a One-Dimensional Laser Beam Scanning and Laser Sheet Approach to Shock Sensing

A 15- by 15-cm supersonic wind tunnel application of a one-dimensional laser beam scanning approach to shock sensing is presented. The measurement system design allowed easy switching between a focused beam and a laser sheet mode for comparison purposes. The scanning results were compared to images from the tunnel Schlieren imaging system. The tests revealed detectable changes in the laser beam in the presence of shocks. The results lend support to the use of the one-dimensional scanning beam approach for detecting and locating shocks in a flow, but some issues must be addressed in regards to noise and other limitations of the system.

Tokars, Roger↗

Laser damage study of nodules in electron-beam-evaporated HfO{sub 2}/SiO{sub 2} high reflectors

A reactive electron beam evaporation process was used to fabricate 1.064 {mu}mHfO{sub 2}/SiO{sub 2} high reflectors. The deposition process was optimized to reduce the nodular density. Cross-sectioning of nodular defects by a focused ion-beam milling instrument showed that the nodule seeds were the residual particles on the substrate and the particulates from the silica source ''splitting.'' After optimizing the substrate preparation procedure and the evaporation process, a low nodular density of 2.7/mm{sup 2} was achieved. The laser damage test revealed that the ejection fluences and damage growth behaviors of nodules created from deep or shallow seeds were totally different. A mechanism based on directional plasma scald was proposed to interpret observed damage growth phenomenon.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Characterization of energetic formulations optimized for optical initiation

Many experimental systems ignite energetic materials using lasers or other optical means. The ignition criteria can be different for each material, and will be dependent, at least, on the wavelength, power, energy density, and coherence of the light used. many of the more common energetic materials, such as HMX, PETN or RDX, are very poor light absorbers and are difficult to ignite optically, therefore the addition of a small amount ({approx} 1% by weight) of activated carbon aids in light absorption and thus ignition. However, these materials still suffer in terms of relatively large energy requirements and slow ignition times. Other materials, such ad DAATO{sub 3.5} (mixed N-oxide of 3,3-azo-bis(6-amino-1,2,4,5-tetrazine)), will ignite just from the energy supplied by a common camera flash, have very fast low-pressure burning rates, and due to decomposition mechanisms dominated by condensed phase reactions, have fast ignition times. Furthermore, the required ignition energies could be further reduced by the addition of nano-particulate transition metals (e.g. nano silver). by combining materials that are more optically sensitive with materials that are more explosively functional, interesting energetic systems with unique initiation criteria can be formulated. The optical characteristics of these formulations are examined using a 1064 nm Big Sky Nd:YAG laser and fiber optic system focused through a GRIN lens and into the sample, which is encased in a lexan holder. The energy from the laser is varied, from {approx} 0.7 mJ to {approx} 17 mJ, using neutral density filters, and is delivered in an {approx} 27.5 ns pulse. The energetic material is mixed with ethanol and slurry cast into the assembly. There are two types of ignition criteria detectable in these experiments. The first is a simple go/no-go criterion, in which any observable reaction is considered ignition, regardless of its violence. The second type requires both ignition and propagation of the reaction. By characterizing the energy required to initiate several different materials, more effective formulations can be designed using the better performing materials. Presented here are the results of laser initiation tests on a variety of compositions, principally combinations of PETN, DAATO{sub 3.5}, HMX, Ag{sub 2}BTA (silver bistetrazolamine), CuBTA, BNCP (bis-5-nitrotetrazolato tetraamine cobalt perchloriate), nm Ag, and a variety of MICs (metastable intermolecular compounds). Also presented are the conclusions as to which formulations are most suitable for optically initiated systems.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

U 3 Si 2 and UO 2 composites densified by spark plasma sintering for accident-tolerant fuels

This work reports the synthesis and characterization of the U 3 Si 2 and UO 2 composites sintered by spark plasma sintering (SPS) with controlled microstructures for accident-tolerant fuel application. The U 3 Si 2 and UO 2 composites with different silicide and oxide ratios were synthesized by SPS at temperatures from 1000 to 1300 °C for 5 minutes. The microstructure and phase composition of the SPS densified composite fuels were characterized with scanning electron microscopy, X-ray diffraction (XRD), and energy dispersed spectroscopy (EDS). A systematic study of the thermal and mechanical properties was conducted using microhardness testing and laser flash apparatus, along with oxidation resistance measurements using thermogravimetric analysis (TGA). The results show that the synthesis of composite fuels can be achieved with a 90% theoretical density (TD) at 1000 °C and over 95% TD when sintered at 1300 °C. XRD and EDS results confirmed that the dominant phases in the composites are U 3 Si 2 and UO 2 . Improved physical density generally leads to improved hardness, fracture toughness, thermal diffusivity, and onset temperature during the oxidation process. U 3 Si 2 was found to play a dominant role in determining the mechanical and oxidation properties of the composite fuels, whereas UO 2 had a more important impact on controlling the thermal diffusivity of the composites. The composite with 50 wt% UO 2 sintered at 1300 °C displayed the onset oxidation temperature of 500 °C by dynamic oxidation testing using TGA at a ramp degree of 10 °C/min. The composite also achieved a high fracture toughness of ~3.5 MPa m ½ . Finally, these results highlight the potential of composite fuel forms densified by SPS with simultaneously enhanced fissile element density, fracture toughness, thermal transport properties, and oxidation resistance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Methodology for Volume Reduction of Radioactive Metallic Waste - 19491

A decontamination methodology for out-of-core nuclear reactor alloys is being developed to reduce the volume of low- and intermediate-level radioactive metallic wastes. For out-of-core reactor metals contamination is limited to surface oxides. For surface oxide removal a technology based on laser ablation is being explored. This paper presents work performed to identify the key parameters that affect the efficiency of removal of surface oxides from out-of-core reactor metals and alloys. This study examined carbon steel (used for coolant feeder pipes of CANDU{sup R} reactors) as a model reactor material. The morphology and thickness of oxides on a used feeder pipe vary considerably depending on its service life and the location along the pipe. Hence, oxides with different morphologies and thicknesses were first grown by corroding carbon steel coupons under different solution conditions. The oxides formed ranged from thin layers of uniformly distributed mixed Fe{sup II}/Fe{sup III} hydroxides/oxides to dual layers consisting of ferric oxide/oxyhydroxide islands with thickness up to 200 μm on top of the more uniformly distributed mixed Fe{sup II}/Fe{sup III} layer. Removal of these oxides was performed using a 1064 nm pulsed laser. Of the laser parameters tested, the pulse radiance was found to be the most important. Four radiances ranging from 5 to 200 MW/cm{sup 2} were used. At radiances higher than 100 MW/cm{sup 2}, single pulses were sufficient to remove both types of oxides, but also extensively melted the metal substrate. At lower radiances, multiple pulses were required to remove the oxides completely, but caused less damage to the metal substrate. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced Coating Removal Techniques

An important step in the repair and protection against corrosion damage is the safe removal of the oxidation and protective coatings without further damaging the integrity of the substrate. Two such methods that are proving to be safe and effective in this task are liquid nitrogen and laser removal operations. Laser technology used for the removal of protective coatings is currently being researched and implemented in various areas of the aerospace industry. Delivering thousands of focused energy pulses, the laser ablates the coating surface by heating and dissolving the material applied to the substrate. The metal substrate will reflect the laser and redirect the energy to any remaining protective coating, thus preventing any collateral damage the substrate may suffer throughout the process. Liquid nitrogen jets are comparable to blasting with an ultra high-pressure water jet but without the residual liquid that requires collection and removal .As the liquid nitrogen reaches the surface it is transformed into gaseous nitrogen and reenters the atmosphere without any contamination to surrounding hardware. These innovative technologies simplify corrosion repair by eliminating hazardous chemicals and repetitive manual labor from the coating removal process. One very significant advantage is the reduction of particulate contamination exposure to personnel. With the removal of coatings adjacent to sensitive flight hardware, a benefit of each technique for the space program is that no contamination such as beads, water, or sanding residue is left behind when the job is finished. One primary concern is the safe removal of coatings from thin aluminum honeycomb face sheet. NASA recently conducted thermal testing on liquid nitrogen systems and found that no damage occurred on 1/6", aluminum substrates. Wright Patterson Air Force Base in conjunction with Boeing and NASA is currently testing the laser remOval technique for process qualification. Other applications of liquid nitrogen operations include cutting of both soft and hard materials. While the laser will not cut materials, it can be used to roughen surfaces and to remove other materials from the substrate including oil, grease, and mold. The space program can benefit from several of these applications with the need for precise removal of coatings and other organic compounds in areas adjacent to sensitive space flight hardware. Significant advantages are evident when comparing liquid nitrogen and laser removal operations over current techniques of media blasting and sanding.

Seibert, Jon↗

Crystallization of fused silica surfaces by ultra-violet laser irradiation

In recent years, the increased use of high power lasers has created problems in optical elements due to laser damage. The International Organization for Standardization (ISO) describes in a publication ISO 11254 a laser-power resilience (LPR) test which we used to verify that by flattening the glass substrate of an optical element, we could improve the resistance to laser damage. We report on an evaluation of two types of samples of fused silica substrate whose surface roughness differed (R{sub a} = 0.20 nm and R{sub a} = 0.13 nm) using customized on-line laser damage testing. To induce laser damage to samples, we used the fifth harmonic generation from a Nd:YAG pulse laser (wavelength: 213 nm, pulse width: 4 ns, repetition frequency: 20 Hz). Results show that flattening reduced the progression of laser damage in the meta-phase laser damage phase by 1/3 of that without flattening. However, pro-phase laser damage which started at fluence 2.39 J/cm{sup 2} was unrelated to surface roughness. To analyze the pro-phase laser damage, we used x-ray diffraction (XRD), Raman spectroscopy, and variable pressure-type scanning electron microscopy (VP-SEM). From XRD data, we observed XRD patterns of cristobalite (111), cristobalite (102), {alpha}-quartz (111), and {beta}-quartz (102). Raman spectrum data showed an increase in the three-membered ring vibration (600 cm{sup -1}), four-membered ring vibration (490 cm{sup -1}), and many-membered ring vibration (450 cm{sup -1}, 390 cm{sup -1}, and 300 cm{sup -1}). We observed patchy crystallized areas on the sample surfaces in the VP-SEM images. Based on these experimental results, we believe that the dominant factors in pro-phase laser damage are their physical properties. Substrate and thin film material must be appropriately selected in producing an optical element with a high level of resilience to laser exposure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗