Dopant Location, Local Structure, and Electronic Properties of Au[subscript 24]Pt(SR)[subscript 18] Nanoclusters
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
N/A
Abstract not provided
ZrC 1-x (sub-stoichiometric zirconium carbide), a group IV transition metal carbide, is being considered for various high temperature applications. Departure from stoichiometry changes the thermo-physical response of the material. Reported thermo-physical properties exhibit, in some cases, a degree of scatter with one likely contributor to this being the uncertainty in the C/Zr ratio of the samples produced. Conventional, methods for assigning C/Zr to samples are determined either by nominal stochiometric ratios or combustion carbon analysis. In this study, a range of stoichiometries of hot-pressed ZrC 1-x were examined by SEM, XRD, Raman spectroscopy and static 13 C NMR spectroscopy and used as a basis to correct the C/Zr. Graphite, amorphous, and ZrC 1-x carbon signatures are observed in the 13 C NMR spectra of samples and are determined to vary in intensity with sintering temperature and stoichiometry. In this study a method is outlined to quantify the stoichiometry of ZrC 1-x and free carbon phases, providing an improvement over the sole use and reliance of widely adopted bulk carbon combustion analysis. We report significantly lower C/Zr values determined by 13 C NMR analysis compared with carbon analyser and nominal methods. Furthermore, the location of carbon disassociated from the ZrC 1-x structure is analysed using SEM and Raman spectroscopy.
The short-range order (SRO) in Pd 78 Cu 6 Si 16 liquid was studied by high energy x-ray diffraction and ab initio molecular dynamics (MD) simulations. The calculated pair correlation functions at different temperatures agree well with the experimental results. The partial pair correlation functions from ab intio MD simulations indicate that Si atoms prefer to be uniformly distributed while Cu atoms tend to aggregate. By performing structure analysis using Honeycutt-Andersen index, Voronoi tessellation, and atomic cluster alignment method, we show that the icosahedron and face-centered cubic SRO increase upon cooling. The dominant SRO is the Pd-centered Pd 9 Si 2 motif, namely the structure of which motif is similar to the structure of Pd-centered clusters in the Pd 9 Si 2 crystal. The study further confirms the existence of trigonal prism capped with three half-octahedra that is reported as a structural unit in Pd-based amorphous alloys. The majority of Cu-centered clusters are icosahedra, suggesting that the presence of Cu is benefit to promote the glass forming ability.
Single crystalline, sub-15 nm BaZr{sub x}Ti{sub 1-x}O{sub 3} (0 {<=} x {<=} 1) nanocrystals were synthesized at room temperature via the vapor diffusion sol-gel method. As-prepared nanocrystals exhibit noncentrosymmetric regions whose volume fraction increases significantly upon substitution of small amounts of Zr{sup 4+} for Ti{sup 4+} and reaches a maximum for substitution levels ranging from 10 to 20 mol%.
Frustration in chain packing has been proposed to play an important role in thermodynamic and dynamic properties of polymeric melts and glasses. Based on a quantitative analysis using Voronoi tessellations and large scale molecular dynamics simulations of flexible and semi-flexible polymers, we demonstrate that the rigid polymer chains have higher averaged Voronoi polyhedral volumes and significantly wider distribution of the volume due to frustration in the chain packing. Using these results, we discuss the advantage of the rigid polymers for possible enhancement of transport properties, e.g. for enhancing ionic conductivity in solid polymer electrolytes.
Abstract not provided
Explore the source record for details and available documents.
It is an interesting but challenge issue to prepare isotropic controllable thermal expansion materials with a wide coefficient of thermal expansion (CTE) range. Herein we report controllable thermal expansion in the double ReO 3 -type (Mn 1-x Ni x )ZrF 6 solid solutions, whose CTE varies from -4.4 to +15.5 × 10 -6 K -1 (300–700 K). In particular, zero thermal expansion has been obtained in the composition of (Mn 0.6 Ni 0.4 )ZrF 6 . (Mn 1-x Ni x )ZrF 6 exhibits full solid solution character. The thermal expansion of (Mn 1-x Ni x )ZrF 6 is adjusted by the flexibility of the atomic linkages, which is confirmed by the technique of temperature-dependent high-energy synchrotron X-ray pair distribution function.
Two-body and three-body energies, modulated by higher-body terms and nuclear quantum effects, determine the structure of liquid water and require sub-chemical accuracy that is achieved by the MB-pol model but not by existing DFT functionals.
Aminophosphines are a class of inexpensive, environmentally benign phosphorus precursors that have provided routes to various metal phosphides. In this work, we use the aminophosphine tris(diethyl)aminophosphine to synthesize tin phosphide nanocrystals.
This work integrates experiments and computational methods to quantify how the cis/trans ratio of the OSDA used in SSZ-39 synthesis impacts the crystallization kinetics, material properties, and final product composition. The crystallization kinetics increase by 30% when increasing the trans isomer content from 14% to 80%. Per prior work, in all cases based on the synthesis gel composition and product yield aluminum is the limiting reagent, and the absence of any amorphous material detected in the time resolved PXRD studies leads us to conclude that FAU dissolution is the rate limiting step in the formation of SSZ-39 in this synthesis protocol. The TGA and NMR results suggest that the trans isomer of OSDA is selectively incorporated into the product. The NMR binding studies, and corresponding DFT-based results show that the trans isomer binds to FAU more strongly than the cis isomer, providing one possible explanation for this enhancement in kinetics and preferential uptake of the trans isomer. The EDS analysis indicates that the Si/Al ratios are between 7.7 and 8.6 at low and high trans OSDA content, indicating zeolite composition is mildly sensitive to the trans isomer content. EDS results show this decrease in aluminum content leads to a corresponding decrease in sodium uptake. DFT-based calculations confirm OSDA–sodium interactions cannot explain any decrease in sodium uptake, reinforcing lower aluminum content as the cause of lower sodium uptake. Preliminary cobalt titration experiments show a surprisingly low cobalt uptake but also show a clear dependence of the cobalt uptake on the solution pH.