Search NASA⌕ Search

SEARCH · Search NASA

Results for “low viscosity”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 343 records · Page 19

Synthesis and Characterization of Modified Phenylethynyl Terminated Polyimides

As an ongoing effort to develop structural adhesives for high performance aerospace applications, recent work has focused on phenylethynyl terminated imide (PETI) oligomers. The work reported herein involves the synthesis and characterization of a series of phenylethynyl containing oligomers designated LARC (TM) MPEI (Modified Phenylethynyl Terminated Polyimide). These oligomers contain mixtures of linear, branched and star-shaped molecules. The fully imidized polymers exhibited minimum melt viscosity as low as 600 poise at 335 C. Ti/Ti lap shear specimens processed at 288 C under 15 psi showed tensile shear strength of approx. 6000 psi and 5200 psi at ambient and 350 F temperatures, respectively. The chemistry and properties of these new MPEIs are presented and compared to an optimized linear PETI, LaRC(Tm) -PETI-5.

Chang, Alice C.↗

Synthesis and Characterization of Modified Phenylethynyl Imides

As an ongoing effort to develop structural adhesives for high-performance aerospace applications, recent work has focused on phenylethynyl terminated imide (PETI) oligomers. The work reported herein involves the synthesis and characterization of a series of phenylethynyl containing oligomers designated LARC(TM) MPEI (modified phenylethynyl imide). These oligomers presumably contain mixtures of linear, branched and star-shaped molecules. The fully imidized polymers exhibited minimum melt viscosities as low as 600 poise at 335 C, significantly lower than equivalent molecular weight linear materials. Ti/Ti lap shear specimens processed at 288 C under 15 psi showed tensile shear strengths as high as approx. 6000 psi and 5200 psi at ambient temperature and 177 C respectively. The chemistry and properties of these new MPEIs are presented and compared with an optimized linear PETI, LARC(TM)PETI-5.

Jensen, B. J.↗

AC Calorimetry and Thermophysical Properties of Bulk Glass-Forming Metallic Liquids

Thermo-physical properties of two bulk metallic glass forming alloys, Ti34Zr11Cu47Ni8 (VIT 101) and Zr57Nb5Ni12.6Al10CU15.4 (VIT 106), were investigated in the stable and undercooled melt. Our investigation focused on measurements of the specific heat in the stable and undercooled liquid using the method of AC modulation calorimetry. The VIT 106 exhibited a maximum undercooling of 140 K in free radiative cooling. Specific heat measurements could be performed in stable melt down to an undercooling of 80 K. Analysis of the specific heat data indicate an anomaly near the equilibrium liquidus temperature. This anomaly is also observed in y the temperature dependencies of the external relaxation time, the specific volume, and the surface tension; it is tentatively attributed to a phase separation in the liquid state. The VIT 101 specimen exhibited a small undercooling of about 50 K. Specific heat measurements were performed in the stable and undercooled melt. These various results will be combined with ground based work such as the measurement of T-T-T curves in the electrostatic levitator and low temperature viscosity and specific heat measurements for modeling the nucleation kinetics of these alloys.

Johnson, William L.↗

High Temperature Transfer Molding Resins

High temperature resins containing phenylethynyl groups that are processable by transfer molding have been prepared. These phenylethynyl containing oligomers were prepared from aromatic diamines containing phenylethynyl groups and various ratios of phthalic anhydride and 4-phenylethynlphthalic anhydride in glacial acetic acid to form a mixture of imide compounds in one step. This synthetic approach is advantageous since the products are a mixture of compounds and consequently exhibit a relatively low melting temperature. In addition, these materials exhibit low melt viscosities which are stable for several hours at 210-275 C, and since the thermal reaction of the phenylethynyl group does not occur to any appreciable extent at temperatures below 300 C, these materials have a broad processing window. Upon thermal cure at approximately 300-350 C, the phenylethynyl groups react to provide a crosslinked resin system. These new materials exhibit excellent properties and are potentially useful as adhesives, coatings, films, moldings and composite matrices.

Connell, John W.↗

Phenylethynyl Terminated Arylene Ether Oxadiazole and Triazole Oligomers and Their Cured Polymers

Several novel phenylethynyl terminated arylene ether oligomers containing oxadiazole and triazole rings were prepared as part of an effort to develop high performance polymers with an attractive combination of properties (e.g. processability and mechanical performance) for future NASA applications. The oligomers displayed low melt viscosities and good solubilities. Thin films cast from solutions of the oligomers and cured for one hour at 350 C in air gave good tensile properties. Titanium to titanium (6Al-4V) tensile shear specimens were readily fabricated and provided moderate strengths. The chemistry and properties of these new materials are discussed.

Thompson, C. M.↗

Adhesive and Composite Properties of a New Phenylethynyl Terminated Imide

A relatively new phenylethynyl terminated imide oligomer (PETI) from the reaction of 2,3,',4'- biphenyltetracarboxylic dianhydride, 4,4'-oxydianiline and endcapped with 4- phenylethynylphthalic anhydride at a calculated number average molecular weight of 5000 g/mole was evaluated as an adhesive and composite matrix. The asymmetric dianhydride imparts a low melt viscosity to the oligomer and a high glass transition temperature to the cured resin. Preliminary adhesive work with titanium (6Al-4V) adherend gave good room temperature (RT) tensile shear strengths and excellent retention of RT strength at 260 C. Preliminary composite work using unsized IM7 carbon fiber provided moderate to high mechanical properties. The chemistry, mechanical, and physical properties of the new PETI in neat resin, adhesive and composite form are presented.

Thompson, C. M.↗

Research to Significantly Enhance Composites Survivability at 550 F in Oxidative Environments

Methylene dianiline (MDA) and its derivatives have been used in the synthesis of polyimides to yield polymers with characteristic low-density, high tensile strength, improved solubility in organic solvents, low-melt viscosities and high thermal stability (greater than 550 F) in air. Polyimides with such properties are desirable for use in aerospace systems, e.g., jet engines, airframe, missiles, and rockets where weight is critical. Recent research at Prairie View A&M University is focused on developing monomers to generate polyimides with enhanced performance over that of NASA s PMR-15. The objective of this work is to synthesize three ring aromatic diamines which are non-toxic and when reacted with the appropriate dianhydrides will yield polyimides with lower viscosity, improve processability, good retention of mechanical properties, and oxidative stability at high environmental temperatures. Modifications of the three ring aromatic diamines include replacing the methylene linkages with aromatic ethers by nucleophilic aromatic substitution reactions and incorporating mono- and di-substituents to the center aromatic ring. An update of current reactions involved in synthesis efforts to generate three ring aromatic monomers for polyimides with methylene, carbonyl, and ether linkages separating the aromatic moieties will be displayed.

Meador, Michael A.↗

Adhesive Properties of Cured Phenylethynyl Containing Imides

Considerable attention has been directed towards acetylene terminated oligomers over the last 20 years' and recent work has focused on phenylethynyl terminated imide (PETI) oligomers. These reactive oligomers possess several features which make them attractive candidates for use as composite matrices and adhesives. The phenylethynyl group can be readily incorporated into many different functionalized oligomers. The reactive oligomers possess relatively low melt viscosities and thermally cure without the evolution of volatile by-products. Once cured, they typically display high glass transition temperatures (Tgs), excellent solvent resistance and high mechanical properties. new modified phenylethynyl-terminated imide (LaRC MPEI) oligomers were synthesized at various molecular weights utilizing a small amount of trifunctional amine. As long as the amount of triamine is relatively small, this approach produces a mixture of linear, star-shaped and branched polymer chains that has lower melt and solution viscosity than an equivalent molecular weight linear phenylethynyl terminated imide oligomers. The work reported herein involves the synthesis and characterization of a copolymer using this approach and the preparation of blends utilizing a phenylethynyl containing reactive plasticizer of lower molecular weight called LaRC LV-121. The chemistry and properties of this new MPEI as well as some blends of MPEI with LV-121, are presented and compared to the linear version, LARC-PETI-5.

Jensen, Brian J.↗

High T(sub g) Polymides for Resin Transfer Molding

A series of new polyimide resins with low melt viscosities and high glass transition temperatures (T(sub g)'s) of 340-350 C were developed for resin transfer molding (RTM) applications. The viscosities of these polyimide resins, based on 2,3,3'4'-Biphenyltetracarboxylic Dianhydride (a-BPDA), are in the range of 10-30 poise. The composites were fabricated successfully at 260-280 C with a pot life of 30-60 minutes by the RTM process. The viscosity profiles of the polyimide resins and the mechanical properties of the polyimide carbon fiber composites will be discussed.

Chuang, Kathy C.↗

Liquid Crystalline Thermosets from Ester, Ester-Imide, and Ester-Amide Oligomers

Main chain thermotropic liquid crystal esters, ester-imides, and ester-amides were prepared from AA, BB, and AB type monomeric materials and were end-capped with phenylacetylene, phenylmaleimide, or nadimide reactive end-groups. The resulting reactive end-capped liquid crystal oligomers exhibit a variety of improved and preferred physical properties. The end-capped liquid crystal oligomers are thermotropic and have, preferably, molecular weights in the range of approximately 1000-15,OOO grams per mole. The end-capped liquid crystal oligomers have broad liquid crystalline melting ranges and exhibit high melt stability and very low melt viscosities at accessible temperatures. The end-capped liquid crystal oligomers are stable for up to an hour in the melt phase. These properties make the end-capped liquid crystal oligomers highly processable by a variety of melt process shape forming and blending techniques including film extrusion, fiber spinning, reactive injection molding (RIM), resin transfer molding (RTM), resin film injection (RFI), powder molding, pultrusion, injection molding, blow molding, plasma spraying and thermo-forming. Once processed and shaped, the end- capped liquid crystal oligomers were heated to further polymerize and form liquid crystalline thermosets (LCT). The fully cured products are rubbers above their glass transition temperatures. The resulting thermosets display many properties that are superior to their non-end-capped high molecular weight analogs.

Theodornus J Dingemans↗

Liquid crystalline thermosets from ester, ester-imide, and ester-amide oligomers

Main chain thermotropic liquid crystal esters, ester-imides, and ester-amides were prepared from AA, BB, and AB type monomeric materials and were end-capped with phenylacetylene, phenylmaleimide, or nadimide reactive end-groups. The resulting reactive end-capped liquid crystal oligomers exhibit a variety of improved and preferred physical properties. The end-capped liquid crystal oligomers are thermotropic and have, preferably, molecular weights in the range of approximately 1000-15,000 grams per mole. The end-capped liquid crystal oligomers have broad liquid crystalline melting ranges and exhibit high melt stability and very low melt viscosities at accessible temperatures. The end-capped liquid crystal oligomers are stable for up to an hour in the melt phase. These properties make the end-capped liquid crystal oligomers highly processable by a variety of melt process shape forming and blending techniques including film extrusion, fiber spinning, reactive injection molding (RIM), resin transfer molding (RTM), resin film injection (RFI), powder molding, pultrusion, injection molding, blow molding, plasma spraying and thermo-forming. Once processed and shaped, the end-capped liquid crystal oligomers were heated to further polymerize and form liquid crystalline thermosets (LCT). The fully cured products are rubbers above their glass transition temperatures. The resulting thermosets display many properties that are superior to their non-end-capped high molecular weight analogs.

Dingemans, Theodorous J.↗

High Temperature VARTM of Phenylethynyl Terminated Imides

Fabrication of composite structures using vacuum assisted resin transfer molding (VARTM) is generally more affordable than conventional autoclave techniques. Recent efforts have focused on adapting VARTM for the fabrication of high temperature composites. Due to their low melt viscosity and long melt stability, certain phenylethynyl terminated imides (PETI) can be processed into composites using high temperature VARTM (HT-VARTM). However, one of the disadvantages of the current HT-VARTM resin systems has been the high porosity of the resultant composites. For aerospace applications, the desired void fraction of less than 2% has not yet been achieved. In the current study, two PETI resins, LaRC PETI-330 and LaRC PETI-8 have been used to make test specimens using HT-VARTM. The resins were infused into ten layers of IM7-6K carbon fiber 5-harness satin fabric at 260 C or 280 C and cured at 371 C. Initial runs yielded composites with high void content, typically greater than 7% by weight. A thermogravimetric-mass spectroscopic study was conducted to determine the source of volatiles leading to high porosity. It was determined that under the thermal cycle used for laminate fabrication, the phenylethynyl endcap was undergoing degradation leading to volatile evolution. By modifying the thermal cycle used in laminate fabrication, the void content was reduced significantly (typically approximately 3%). Densities of the composites were determined using a density gradient column and the glass transition temperatures of the cured composites were measured by dynamic mechanical analysis. Photomicrographs of the panels were taken and void contents were determined by acid digestion. The results of this work are presented herein.

Cano, Roberto J.↗

Liquid Crystalline Thermosets from Ester, Ester-imide, and Ester-amide Oligomers

Main chain thermotropic liquid crystal esters, ester-imides, and ester-amides were prepared from AA, BB, and AB type monomeric materials and end-capped with phenylacetylene, phenylmaleimide, or nadimide reactive end-groups. The end-capped liquid crystal oligomers are thermotropic and have, preferably, molecular weights in the range of approximately 1000-15,000 grams per mole. The end-capped liquid crystaloligomers have broad liquid crystalline melting ranges and exhibit high melt stability and very low melt viscosities at accessible temperatures. The end-capped liquid crystal oli-gomers are stable forup to an hour in the melt phase. They are highly processable by a variety of melt process shape forming and blending techniques. Once processed and shaped, the end-capped liquid crystal oigomers were heated to further polymerize and form liquid crystalline thermosets (LCT). The fully cured products are rubbers above their glass transition temperatures.

Dingemans, Theodorus J.↗

High Temperature VARTM of Phenylethynyl Terminated Imides

Depending on the part type and quantity, fabrication of composite structures using vacuum assisted resin transfer molding (VARTM) can be more affordable than conventional autoclave techniques. Recent efforts have focused on adapting VARTM for the fabrication of high temperature composites. Due to their low melt viscosity and long melt stability, certain phenylethynyl terminated imides (PETI) can be processed into composites using high temperature VARTM (HT-VARTM). However, one of the disadvantages of the current HT-VARTM resin systems has been the high porosity of the resultant composites. For aerospace applications, the desired void fraction of less than 2% has not yet been achieved. In the current study, two PETI resins, LaRC PETI-330 and LaRC PETI-8 have been used to make test specimens using HT-VARTM. The resins were infused into ten layers of IM7-6K carbon fiber 5-harness satin fabric at 260 C or 280 C and cured at temperature up to 371 C. Initial runs yielded composites with high void content, typically greater than 7% by weight. A thermogravimetric-mass spectroscopic study was conducted to determine the source of volatiles leading to high porosity. It was determined that under the thermal cycle used for laminate fabrication, the phenylethynyl endcap was undergoing degradation leading to volatile evolution. This finding was unexpected as high quality composite laminates have been fabricated under higher pressures using these resin systems. The amount of weight loss experienced during the thermal cycle was only about 1% by weight, but this leads to a significant amount of volatiles in a closed system. By modifying the thermal cycle used in laminate fabrication, the void content was significantly reduced (typically ~ 3% or less). The results of this work are presented herein.

Ghose, Sayata↗

High Temperature VARTM of Phenylethynyl Terminated Imides (PETI) Resins

Fabrication of composite structures using vacuum assisted resin transfer molding (VARTM) is generally more affordable than conventional autoclave techniques. Recent efforts have focused on adapting VARTM for the fabrication of high temperature composites. Due to their low melt viscosity and long melt stability, certain phenylethynyl terminated imides (PETI) can be processed into composites using high temperature VARTM (HT-VARTM). However, one of the disadvantages of the current HT-VARTM resin systems has been the high porosity of the resultant composites. For aerospace applications a void fraction of less than 2% is desired. In the current study, two PETI resins, LARCTM PETI-330 and LARCTM PETI-8 have been used to fabricate test specimens using HT-VARTM. The resins were infused into carbon fiber preforms at 260 C and cured between 316 C and 371 C. Modifications to the thermal cycle used in the laminate fabrication have reduced the void content significantly (typically < 3%) for carbon fiber biaxially woven fabric. Photomicrographs of the panels were taken and void contents were determined by acid digestion. For carbon fiber uniaxial fabric, void contents of less than 2% have been obtained using both PETI-8 and PETI-330. Mechanical properties of the panels were determined at both room and elevated temperatures. These include short beam shear and flexure tests. The results of this work are presented herein.

Ghose, Sayata↗

Phenylethynyl Terminated Imide (PETI) Composites Made by High Temperature VARTM

Fabrication of composite structures using vacuum assisted resin transfer molding (VARTM) is generally more affordable than conventional autoclave techniques. Recent efforts have focused on adapting VARTM for the fabrication of high temperature composites. Due to their low melt viscosity and long melt stability, certain phenylethynyl terminated imides (PETI) can be processed into composites using high temperature VARTM (HT-VARTM). However, one of the disadvantages of the current HT-VARTM resin systems has been the high porosity of the resultant composites. For aerospace applications, a void fraction of <2% is desired. In the current study, two PETI resins, LARC. PETI-330 and LARC. PETI-8 have been used to fabricate test specimens using HT-VARTM. The resins were infused into carbon fiber preforms at 260 C and cured between 316 and 371 C. Photomicrographs of the panels were taken and void contents were determined by acid digestion. Modifications to the thermal cycle used in the laminate fabrication have reduced the void content significantly; typically .3% for carbon fiber biaxially woven fabric and less than 2% for carbon fiber uniaxial fabric. Mechanical properties (short beam shear and flexure) of the panels were determined at both room and elevated temperatures. The results of this work are presented herein. This paper is declared a work of the U.S. Government and is not subject to copyright protection in the United States.

Chose, Sayata↗

Polyimide Composites Properties of RTM370 Fabricated by Vacuum Assisted Resins Transfer Molding (VARTM)

RTM370 imide resin based on 2,3,3 ,4 -biphenyl dianhydride ( a-BPDA), 3,4 -oxydianinline (3,4 -ODA) with 4-phenylethynylphthalic (PEPA) endcap has shown to exhibit high Tg (370 C) and low melt viscosity (10-30 poise) at 280 C with a pot-life of 1-2 h. Previously, RTM370 resin has been fabricated into composites with T650-35 carbon fabrics by resin transfer molding (RTM) successfully. RTM370 composites exhibit excellent mechanical properties up to 327 C (620 F), and outstanding property retention after aging at 288 C (550 F) for 1000 hrs. In this presentation, RTM 370 composites will be fabricated by vacuum assisted resins transfer molding (VARTM), using vacuum bags without mold. The mechanical properties of RTM370 composites fabricated by VARTM will be compared to those of RTM370 made by RTM.

Chuang, Kathy C.↗

Composite Properties of RTM370 Polyimide Fabricated by Vacuum Assisted Resin Transfer Molding (VARTM)

RTM370 imide resin based on 2,3,3?,4?-biphenyl dianhydride (a-BPDA), 3,4'-oxydianinline (3,4'-ODA) with the 4-phenylethynylphthalic (PEPA) endcap has been shown to exhibit a high cured T(sub g) (370 C) and low melt viscosity (10-30 poise) at 280 C with a pot-life of 1-2 h. Previously, RTM370 resin has been successfully fabricated into composites reinforced with T650-35 carbon fabrics by resin transfer molding (RTM). RTM370 composites exhibit excellent mechanical properties up to 327?C (620?F), and outstanding property retention after aging at 288?C (550?F) for 1000 h. In this work, RTM370 composites were fabricated by vacuum assisted resin transfer molding (VARTM), using vacuum bags on a steel plate. The mechanical properties of RTM370 composites fabricated by VARTM are compared to those prepared by RTM.

Chuang, Kathy C.↗