Search NASA⌕ Search

SEARCH · Search NASA

Results for “Brittle failure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Precursors to failure in rocks while undergoing anelastic deformations

Specimens of pyrophyllite, which exhibits large anelastic deformation before brittle failure, were stressed to failure in a biaxial press to model stress accumulation prior to an earthquake. Optical holography, sound velocity measurements and photography through transparent pistons were used to study the specimens. A zone of preferential deformation around the incipient fault was monitored at 50% or more of ultimate failure strength; reversals of seismic velocities and formation of en echelon cracks near the coming macrocrack were also observed. The dependence of the seismic velocity reversals on moisture was noted.

Sobolev, G.↗

Characterization of runaway electron impact on instrumented sacrificial limiters on DIII-D

Instrumented sacrificial limiter heads, both domed (proud) and flat (flush) are used in DIII-D runaway electron (RE) wall strikes to study the wall impact dynamics with high spatial and time resolution. The approximate structure of the RE wetted area and heating depth on the domed limiter heads were predicted qualitatively using orbit-tracking simulations, although a strong left–right asymmetry (about the magnetic field direction) was not captured well by the simulations. It is hypothesized that this difference is perhaps due to the local 3D magnetic field perturbation of the dome limiter head. The average kinetic energy K and pitch angle θ of REs striking the limiter head were estimated from the spatial distribution of local HXR emission and were estimated to be roughly K ≈ 4 MeV and θ ≈ 0.2 rad. These values are roughly consistent with in-plasma values estimated before the loss event, indicating that RE kinetic energy and pitch angle are not drastically altered when transporting to the wall. Large shot–shot variations (1–10 kJ) in energy deposition into the limiter head were observed and were explained by shot–shot variations in locked magneto-hydrodynamics mode toroidal phase. For the largest deposited energies (10 kJ), graphite material failure and explosive dust release was observed, and the depth of material failure at higher energy deposition was successfully reproduced using modelling of volumetric energy deposition and brittle failure. The presence of energetic (keV) level ion impact during the RE wall strike was confirmed by three different surface analysis techniques. The ratio of energetic ion to RE flux appears to be larger on flat surfaces within the RE wetted area, although the energetic ion flux and total energy flux due to energetic ions have not yet been quantified.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Coupled diffusion-deformation-damage model for polymers used in hydrogen infrastructure

The soft materials used in the infrastructure of hydrogen storage and distribution systems are vulnerable because exposure to high-pressure hydrogen can lead to mechanical damage and property degradation. Some materials, such as polymers, can undergo mechanical failure due to a phenomenon wherein hydrogen gas diffuses through the polymer chains and occupies preexisting cavities or voids inside the polymer material. If the hydrogen gas pressure is reduced more quickly than hydrogen can diffuse back out of the polymer which is necessary for some applications, the trapped hydrogen gas instead escapes by rupturing the material, causing surface blistering or permanent damage. In this study, a continuum mechanics-based fully coupled diffusion-deformation model with damage is developed to predict the stress distribution and damage propagation while the polymer undergoes rapid decompression failure. The hyperelastic material model, along with the maximum principal strain failure theory, was chosen for this study as it represents the nonlinear material response with brittle failure observed in uniaxial tensile tests perfectly. EPDM polymer was chosen for this study because of its commercial availability and common use in hydrogen storage and distribution system. It has superior mechanical properties, high and low temperature resistance, and certain compounds work well in hydrogen gas. This work is useful for design engineers to alter the parameters while manufacturing polymer composites to increase their performance in a high-pressure hydrogen environment.

Kulkarni, Shank S.↗

Artificial neural network potentials for mechanics and fracture dynamics of two-dimensional crystals **

Understanding the mechanics and failure of materials at the nanoscale is critical for their engineering and applications. The accurate atomistic modeling of brittle failure with crack propagation in covalent crystals requires a quantum mechanics-based description of individual bond-breaking events. Artificial neural network potentials (NNPs) have emerged to overcome the traditional, physics-based modeling tradeoff between accuracy and accessible time and length scales. Previous studies have shown successful applications of NNPs for describing the structure and dynamics of molecular systems and amorphous or liquid phases of materials. However, their application to deformation and failure processes in materials is still uncommon. In this study, we discuss the apparent limitations of NNPs for the description of deformation and fracture under loadings and propose a way to generate and select training data for their employment in simulations of deformation and fracture simulations of crystals. We applied the proposed approach to 2D crystalline graphene, utilizing the density-functional tight-binding method for more efficient and extensive data generation in place of density functional theory. Then, we explored how the data selection affects the accuracy of the developed artificial NNPs. It revealed that NNP’s reliability should not only be measured based on the total energy and atomic force comparisons for reference structures but also utilize comparisons for physical properties, e.g. stress–strain curves and geometric deformation. In sharp contrast to popular reactive bond order potentials, our optimized NNP predicts straight crack propagation in graphene along both armchair and zigzag (ZZ) lattice directions, as well as higher fracture toughness of ZZ edge direction. Our study provides significant insight into crack propagation mechanisms on atomic scales and highlights strategies for NNP developments of broader materials.

2D materials↗

Multiscale fatigue crack initiation in hierarchical additively manufactured alloys

Bioinspired hierarchical microstructures offer a route toward engineered fatigue resistance in additively manufactured alloys. However, it remains unclear how discrete structural constituents independently govern damage accumulation, particularly during the critical fatigue initiation regime where short cracks strongly interact with local microstructure. Here, we investigate multiscale fatigue initiation in a dual-phase, nanolamellar AlCoCrFeNi 2.1 high-entropy alloy. By comparing microscale specimens that isolate the nanolamellar structure against macroscale specimens containing the full melt-pool architecture, we identify size-dependent fatigue initiation mechanisms. We find that failure is dictated by nanolamellar interfaces at the microscale, whereas mesoscale melt pool boundaries serve to initiate fatigue at the macroscale. This mechanistic shift is accompanied by a transition from macroscale quasi-brittle failure to microscale plasticity-driven crack extension. Our results provide a physical framework for understanding how structural hierarchy governs the transition from discrete microstructural deformation to continuum fatigue fracture behavior, informing the design of damage-tolerant, additively manufactured alloys.

36 MATERIALS SCIENCE↗

Creep/Rupture Behavior of Melt-Infiltrated SiC/SiC Composites Being Investigated

The failure behavior of melt-infiltrated SiC/SiC ceramic matrix composites is under investigation at the NASA Glenn Research Center as part of NASA's Ultra-Efficient Engine Technology Program. This material was originally developed under the High Speed Research Office's Enabling Propulsion Materials Program. Creep and rupture data provide accelerated testing information to predict material behavior under engine use situations (1500 to 2400 F). This information gives insights into various material development paths to improve composites as well as improve understanding of failure mechanisms. The left figure shows the fracture surface of a CMC material following over 200 hr of testing at 2400 F. This surface demonstrates the kind of fibrous pullout desirable for maximum crack deflection, hence non-brittle failure. Microscopy suggests that creep and rupture of these materials can best be considered as a probabilistic property, rather than a material property. Fiber failure occurs first in isolated regions, while stronger adjacent fibers remain intact. The right figure shows a region where oxide deposits blur and round the fiber images. Because the oxidation kinetics of SiC are well understood, this oxide scale can be used as a measure of the length of time various regions of the composites have been exposed to the environment, hence providing vital information regarding the sequence of failure. The oxide scale in the right figure indicates an early failure of this tow of fibers, whereas adjacent tows remain oxide free, suggesting failure much later in time. The path of various cracks can be followed throughout the composite in this manner, suggesting failure mechanisms.

Hurst, Janet B.↗

Influence of Finite Element Size in Residual Strength Prediction of Composite Structures

The sensitivity of failure load to the element size used in a progressive failure analysis (PFA) of carbon composite center notched laminates is evaluated. The sensitivity study employs a PFA methodology previously developed by the authors consisting of Hashin-Rotem intra-laminar fiber and matrix failure criteria and a complete stress degradation scheme for damage simulation. The approach is implemented with a user defined subroutine in the ABAQUS/Explicit finite element package. The effect of element size near the notch tips on residual strength predictions was assessed for a brittle failure mode with a parametric study that included three laminates of varying material system, thickness and stacking sequence. The study resulted in the selection of an element size of 0.09 in. X 0.09 in., which was later used for predicting crack paths and failure loads in sandwich panels and monolithic laminated panels. Comparison of predicted crack paths and failure loads for these panels agreed well with experimental observations. Additionally, the element size vs. normalized failure load relationship, determined in the parametric study, was used to evaluate strength-scaling factors for three different element sizes. The failure loads predicted with all three element sizes provided converged failure loads with respect to that corresponding with the 0.09 in. X 0.09 in. element size. Though preliminary in nature, the strength-scaling concept has the potential to greatly reduce the computational time required for PFA and can enable the analysis of large scale structural components where failure is dominated by fiber failure in tension.

Satyanarayana, Arunkumar↗

Shoemaker-Levy 9 and the tidal disruption of comets

The break-up of Periodic Comet Shoemaker-Levy 9 into multiple pieces following its grazing encounter with Jupiter in July 1992 can be used to study tidally-induced fracture in comets. This spectacular event allows us not only to set limits on the size, strength and density of Shoemaker-Levy 9 itself, but provides invaluable guidance to numerical modeling of such encounters. In an extensive treatment of tidal breakup which assumed self-gravitating, homogeneous, perfectly elastic bodies, Dobrovolskis derived simple analytical expressions for the tidally-induced surface and central stresses. Both can be cast in such a way that Poisson's ratio is the only material dependent constant entering these expressions. Whether both surface and central failure must be initiated as a criterion for breakup, or either one of them is sufficient, remains a subject of disagreement. To resolve this debate, we model the details of cometary breakup using a three-dimensional Smooth Particle Hydrodynamics (SPH) code modified to simulate fracture in small solid objects. At lower stresses associated with brittle failure, we use a rate-dependent strength based on the nucleation of incipient flaws whose number density is given by a Weibull distribution.

Benz, W.↗

Effects of Near Field Pyroshock on the Performance of a Nitramine Nitrocellulose Propellant

The overall purpose of this study is to investigate the effects of a pyroshock environment on the performance characteristics of a propellant used in pyrotechnic devices such as guillotine cutters. Near field pyroshock which is defined by acceleration amplitudes in excess of 10,000g at a frequency of greater than 10,000 Hz is a highly transient environment that has a known potential to cause failure in both structural and electronic components. A heritage pressure cartridge assembly which uses a nitramine nitrocellulose propellant with a known performance baseline will be exposed to a near field pyroshock event. The pressure cartridge will then be fired in an ambient closed bomb firing to collect pressure time history. The two performance characteristics that will be evaluated are the pressure amplitude and time to peak pressure. This data will be compared to the base-lined ambient closed bomb data to evaluate the effects of the shock on the performance of the propellant. It is expected that the pyroshock environment will cause brittle failures of the propellant increasing the surface area of said propellant. This increase of surface area should result in increased combustion rate which should show as an increased pressure peak and decreased time to peak pressure in the pressure time data.

Baca, Arcenio B.↗

Global Failure Modes in High Temperature Composite Structures

Composite materials have been considered for many years as the major advance in the construction of energy efficient aerospace structures. Notable advances have been made in understanding the special design considerations that set composites apart from the usual "isotropic" engineering materials such as the metals. As a result, a number of significant engineering designs have been accomplished. However, one shortcoming of the currently favored composites is their relatively unforgiving behavior with respect to failure (brittleness) under seemingly mild impact conditions and large efforts are underway to rectify that situation, much along the lines of introducing thermoplastic matrix materials. Because of their relatively more pronounced (thermo) viscoelastic behavior these materials respond with "toughness" in fracture situations. From the point of view of applications requiring material strength, this property is highly desirable. This feature impacts several important and distinct engineering problems which have been' considered under this grant and cover the 1) effect of impact damage on structural (buckling) stability of composite panels, the 2) effect of time dependence on the progression of buckling instabilities, and the 3) evolution of damage and fracture at generic thickness discontinuities in structures. The latter topic has serious implications for structural stability problems (buckling failure in reinforced shell structures) as well as failure progression in stringer-reinforced shell structures. This grant has dealt with these issues. Polymer "toughness" is usually associated with uncrosslinked or thermo-plastic polymers. But, by comparison with their thermoset counterparts they tend to exhibit more pronounced time dependent material behavior; also, that time dependence can occur at lower temperatures which places restriction in the high temperature use of these "newer and tougher" materials that are not quite so serious with the thermoset matrix materials. From a structural point of view the implications of this material behavior are potentially severe in that structural failure characteristics are no longer readily observed in short term qualification tests so characteristic for aerospace structures built from typical engineering metals.

Knauss, W. G.↗

Three-Dimensional High Fidelity Progressive Failure Damage Modeling of NCF Composites

Performance prediction of off-axis laminates is of significant interest in designing composite structures for energy absorption. Phenomenological models available in most of the commercial programs, where the fiber and resin properties are smeared, are very efficient for large scale structural analysis, but lack the ability to model the complex nonlinear behavior of the resin and fail to capture the complex load transfer mechanisms between the fiber and the resin matrix. On the other hand, high fidelity mesoscale models, where the fiber tows and matrix regions are explicitly modeled, have the ability to account for the complex behavior in each of the constituents of the composite. However, creating a finite element model of a larger scale composite component could be very time consuming and computationally very expensive. In the present study, a three-dimensional mesoscale model of non-crimp composite laminates was developed for various laminate schemes. The resin material was modeled as an elastic-plastic material with nonlinear hardening. The fiber tows were modeled with an orthotropic material model with brittle failure. In parallel, new stress based failure criteria combined with several damage evolution laws for matrix stresses were proposed for a phenomenological model. The results from both the mesoscale and phenomenological models were compared with the experiments for a variety of off-axis laminates.

Aitharaju, Venkat↗

The role of specimen size and grain boundary characteristics in the yield strength of tungsten in microtensile tests

To effectively use the measured properties from small-scale tensile tests for bulk material performance predictions, it is essential to understand the threshold of specimen size-effect strengthening and the interaction between dislocations and microstructures within miniaturized specimens. This study uses pure tungsten to investigate the size effect in terms of specimen size, grain size, and grain boundary characteristics relative to the yield strength of tungsten at room temperature. We evaluate the transition from miniaturized specimen properties to bulk properties and the deformation behavior through small-scale tensile tests of three specimen sizes (large: 80 × 100 × 233 µm³; medium: 7 × 7 × 18 µm³; and small: 2 × 2 × 5 µm³). The testing results reveal that the small and medium specimens exhibit high yield strength with ductile behavior, while the large specimens exhibit brittle failure, consistent with the room temperature strength of tungsten, indicating bulk behavior. We further explore the specimen size-effect sensitivity to yield stress and the scaling relationship between yield strength and the number of grains involved in the deformation. A power-law relationship with the exponent value of approximately -0.5 was found in the yield strength–grain number scaling, implying the Hall-Petch like behavior. A minimum of 7–17 effective grain boundaries across the tensile gauge dimension is required to accurately measure bulk properties.

36 - MATERIALS SCIENCE↗

Simulating the Formation of Lunar Floor-Fracture Craters Using Elastoviscoplastic Relaxation

Lunar floor-fracture craters formed during the height of mare basalt emplacement. Due to a general temporal and spatial relation with the maria, these craters, numbering some 200, may be diagnostic of the thermal structure of the crust during this time. As the name suggests, these craters exhibit brittle failure, generally limited to the central floor region. That, and a shallower depth than fresh lunar craters, has led to two main theories as to their formation: laccolith emplacement under the crater and viscous relaxation. The implications of each model for the state of the Moon's crust during this time are quite different, so the viability of each model must be checked. Laccolith emplacement has been treated elsewhere. However, previous attempts to study the relaxation of the craters have assumed only a uniform, Newtonian viscous response of the near surface to the topographic driving forces, and simply postulated that the fractures resulted from tensile stresses associated with floor uplift. Here, we use a more sophisticated rheological model that includes not only non-Newtonian viscous behavior (i.e., the viscosity is stress-dependent), but also incorporates elastic behavior and a plastic component to the rheology to directly simulate the formation of the floor fractures. The results of our simulations show that while elastoviscoplastic relaxation is potentially viable for larger floor-fracture craters, it is not viable for craters with diameters < or = 60 km, the size of the majority of floor-fracture craters. We employ the finite element method, a numerical technique well suited for boundary-value problems, via the commercially available MARC software package. To test the viability of topographic relaxation, our goal is to prepare the simulations as to maximize the amount of relaxation. We take advantage of the natural axisymmetry of craters, simulating one radial plane. Initial shapes are based on data for fresh craters from Pike. To simplify implementation, a fourth order polynomial is used for the basin, while a third order inverse function is used for the rim. This form closely approximates the long-wavelength behavior of complex craters, while ignoring higher-frequency topography, save the rim. This approximation is appropriate because crater relaxation is strongly controlled by long-wavelength topography. Loading is accomplished assuming a uniform gravity field (1.62 m/s-square) and a uniform density of 2900 kg/cubic m. The initial stress state is set to be hydrostatic, with an additional pressure term to account for any overlying topography. This additional pressure term is tapered exponentially with depth. While the simulations quickly settle on a preferred stress state, and while the final solution is fairly insensitive to the choice of the e-folding depth of the taper, selecting an e-folding depth close to the diameter of the crater sets the initial stress state near the preferred state. We assume a diuranally averaged surface temperature of -20 C, and allow temperature to increase with depth at a rate of 50 K//km. Assuming a thermal conductivity of 2 W/in/K, this gradient translates to a heat flow of 100mW/square m, an extremely high value for the Moon. Temperature, of course, will not increase without bound. To maximize relaxation, we allow our temperature profile to increase linearly until it reaches the solidus (assumed to be 1200C) at a depth of 24.4 km, at which point it is kept constant. The presence of melt will drop the bulk viscosity; however, we have no rheological control for partial melts. Therefore, we make no attempt to simulate this situation. Elastoviscoplastic rheological model. In general, geologic materials can behave in three main ways: elastically, viscously (via solid-state creep), and brittly (plasticity is a continuum approach to simulate this phenomenon). We combine these three deformation mechanisms in an extended Maxwell solid, where the total strain can be broken down into a simple summation of the elastic, creep, and plastic strains. In relaxation phenomena in general, the system takes advantage of any means possible to eliminate deviatoric stresses by relaxing away the topography. Previous analyses have only modeled the viscous response. Comparatively, the elastic response in our model can augment the relaxation, to a point. This effect decreases as the elastic response becomes stiffer; indeed, in the limit of infinite elastic Young's modulus (and with no plasticity), the solution converges on the purely viscous solution. Igneous rocks common to the lunar near-surface have Young's modulii in the range of 10-100 GPa. To maximize relaxation, we use a Young's modulus of 10 GPa. (There is negligible sensitivity to the other elastic modulus, the Poisson's ratio; we use 0.25.) For the viscous response, we use a flow law for steady-state creep in thoroughly dried Columbia diabase, because the high plagioclase (about 70 vol%) and orthopyroxene (about 17 vol%) content is similar to the composition of the lunar highland crust as described by remote sensing and sample studies: noritic anorthosite. This flow law is highly non-Newtonian, i.e., the viscosity is highly stress dependent. That, and the variability with temperature, stands in strong contrast to previous examinations of lunar floor-fracture crater relaxation. To model discrete, brittle faulting, we assume "Byerlee's rule," a standard geodynamical technique. We implement this "rule" with an-angle of internal friction of about 40 deg, and a higher-than-normal cohesion of about 3.2 MPa (to approximate the breaking of unfractured rock). The actual behavior of geologic materials is more complex than in our rheological model, so the uncertainties in the plasticity do not represent the state-of-the-art error. Additional information is contained in the original.

Dombard, A. J.↗

Unveiling the Fatigue Behavior of 2D Hybrid Organic–Inorganic Perovskites: Insights for Long-Term Durability

2D hybrid organic–inorganic perovskites (HOIPs) are commonly found under subcritical cyclic stresses and suffer from fatigue issues during device operation. However, their fatigue properties remain unknown. Here, the fatigue behavior of (C 4 H 9 -NH 3 ) 2 (CH 3 NH 3 ) 2 Pb 3 I 10 , the archetype 2D HOIP, is systematically investigated by atomic force microscopy (AFM). It is found that 2D HOIPs are much more fatigue resilient than polymers and can survive over 1 billion cycles. 2D HOIPs tend to exhibit brittle failure at high mean stress levels, but behave as ductile materials at low mean stress levels. These results suggest the presence of a plastic deformation mechanism in these ionic 2D HOIPs at low mean stress levels, which may contribute to the long fatigue lifetime, but is inhibited at higher mean stresses. The stiffness and strength of 2D HOIPs are gradually weakened under subcritical loading, potentially as a result of stress-induced defect nucleation and accumulation. The cyclic loading component can further accelerate this process. The fatigue lifetime of 2D HOIPs can be extended by reducing the mean stress, stress amplitude, or increasing the thickness. These results can provide indispensable insights into designing and engineering 2D HOIPs and other hybrid organic–inorganic materials for long-term mechanical durability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Residually Stressed Bimaterial Beam Specimen for Measuring Environmentally Assisted Crack Growth

Background: Subcritical crack growth can occur in a brittle material when the stress intensity factor is smaller than the fracture toughness if an oxidizing agent (such as water) is present at the crack tip. Objective: Here we present a novel bi-material beam specimen which can measure environmentally assisted crack growth rates. The specimen is “self-loaded” by residual stress and requires no external loading. Methods: Two materials with different coefficient of thermal expansion are diffusion bonded at high temperature. After cooling to room temperature a subcritical crack is driven by thermal residual stresses. A finite element model is used to design the specimen geometry in terms of material properties in order to achieve the desired crack tip driving force. Results: The specimen is designed so that the crack driving force decreases as the crack extends, thus enabling the measurement of the crack velocity versus driving force relationship with a single test. The method is demonstrated by measuring slow crack growth data in soda lime silicate glass and validated by comparison to previously published data. Conclusions: The self-loaded nature of the specimen makes it ideal for measuring the very low crack velocities needed to predict brittle failure at long lifetimes.

36 MATERIALS SCIENCE↗

Multi-scale characterization of supersolidus liquid phase sintered H13 tool steel manufactured via binder jet additive manufacturing

Additive manufacturing (AM) of H13 tool steel by binder jet 3D printing (BJ3DP) followed by pressureless supersolidus liquid phase sintering (SLPS) provides a low-cost alternative manufacturing method for components with intricate geometric features. However, the microstructure-mechanical property relationships for BJ3DP-SLPS produced H13 tool steel are not well understood, which makes it challenging to develop printing and post-processing methods that maximize part performance. In this work, we leverage atom probe tomography and transmission electron microscopy along with thermodynamic calculations to rationalize the microstructure-mechanical property relationships in as-sintered BJ3DP H13 tool steel. Here, we report for the first time, the presence of a continuous eutectic film-like carbide in H13 along with the more commonly observed cuboidal MX carbides in the prior liquid channels of the microstructure. Further, atom probe tomography revealed the interconnected nature of the MX carbides that appear to be discrete in two-dimensional micrographs. These continuous eutectic carbides and interconnected MX carbides result in brittle failure of the material. Characterization of these microstructural features will be critical in developing appropriate post-processing heat treatments for the improved mechanical performance of BJ3DP H13.

36 MATERIALS SCIENCE↗

Effect of thickness on degradation of austenitic 347H steel by direct-fired supercritical CO 2 power cycle environment

Austenitic 347H steel of two thicknesses (2.54 and 0.6 mm) was exposed to a simulated direct-fired supercritical CO 2 (sCO 2 ) power cycle environment at 650°C and 1 atm for 1000 h then tensile stressed at room temperature to study the deformation behavior. The thicker 347H formed a protective chromia scale over most of the surface, which minimized carburization of the underlying steel and resulted in no change in mechanical performance. In stark contrast, the thinner 347H formed non-protective Fe-rich oxides over the entire surface, resulting in extensive carburization of the underlying steel. Finally, this led to increased strength but significantly reduced ductility, resulting in partially brittle failure

36 MATERIALS SCIENCE↗

Post-irradiation examination of commercial tantalum alloys following neutron irradiation

Post irradiation examination of two commercial tantalum alloys (based on Ta-8 %W) revealed significant irradiation hardening following neutron irradiation in the High Flux Isotope Reactor at Oak Ridge National Laboratory. Tensile samples of commercial Ta alloys T-111 and ASTAR-811C were irradiated to a total neutron fluence (E > 0.1 MeV) in the range (2–4)x10 21 n/cm 2 (0.39–0.75 dpa) at an irradiation temperature near 900 °C. Tensile testing conducted at room temperature and at 800 °C revealed significant irradiation hardening under all test conditions. Samples that were tensile tested at room temperature exhibited brittle failure, whereas ductility was maintained for elevated temperature testing. The irradiation hardening and embrittlement noted for both alloys was attributed to irradiation-induced dislocation loop formation as confirmed through scanning transmission electron microscopy analysis. Corresponding energy dispersive x-ray spectroscopy revealed radiation-induced segregation of Hf in these loop populations. This Hf enrichment is shown to result in eventual co-precipitation of elongated (Hf,O)-rich precipitates along the dislocation loops. Further, these results show that irradiation hardening is enhanced via irradiation-enhanced precipitation at elevated irradiation temperatures. Consequently, the minimum recommended operating temperature window for Ta alloys should be increased to account for observed hardening/embrittlement at irradiation temperatures as high as 900 °C (1,173 K).

36 MATERIALS SCIENCE↗