Identification of a cast iron alloy containing nonstrategic elements

A program was performed to address the mechanical and environmental needs of Stirling engine heater head and regenerator housing components, while reducing the dependence on strategic materials. An alloy was developed which contained no strategic elemental additions per se. The base is iron with additions of manganese, molybdenum, carbon, silicon, niobium, and ferro-chromium. Such an alloy should be producible on a large scale at very low cost. The resulting alloy, designated as NASAUT 4G-Al, contained 15 Mn, 15 Cr, 2 Mo, 1.5 C, 1.0 Si, 1.0 Nb (in weight percent) with a balance of Fe. This alloy was optimized for chemistry, based upon tensile strength, creep-rupture strength, fracture behavior, and fatigue resistance up to 800 C. Alloys were also tested for environmental compatibility. The microstructure and mechanic properties (including hardness) were assessed in the as-cast condition and following several heat treatments, including one designed to simulate a required braze cycle. The alloy was fabricated and characterized in the form of both equiaxed and columnar-grained castings. The columnar grains were produced by directional solidification, and the properties were characterized in both the longitudinal and transverse orientations. The NASAUT 4G-Al alloy was found to be good in cyclic-oxidation resistance and excellent in both hydrogen and hot-corrosion resistance, especially in comparison to the baseline XF-818 alloy. The mechanical properties of yield strength, stress-rupture life, high-cycle-fatigue resistance, and low-cycle-fatigue resistance were good to excellent in comparison to the current alloy for this application, HS-31 (X-40), with precise results depending in a complex manner on grain orientation and temperature. If required, the ductility could be improved by lowering the carbon content.

Cooper, C. V.↗

Directional solidification of flake and nodular cast iron during KC-135 low-g maneuvers

Alloys solidified in a low-gravity environment can, due to the elimination of sedimentation and convection, form unique and often desirable microstructures. One method of studying the effects of low-gravity (low-g) on alloy solidification was the use of the NASA KC-135 aircraft flying repetitive low-g maneuvers. Each maneuver gives from 20 to 30 seconds of low-g which is between about 0.1 and 0.001 gravity. A directional solidification furnace was used to study the behavior of off eutectic composition case irons in a low-g environment. The solidification interface of hypereutectic flake and spheroidal graphite case irons was slowly advanced through a rod sample, 5 mm in diameter. Controlled solidification was continued through a number of aircraft parabolas. The known solidification rate of the sample was then correlated with accelerometer data to determine the gravity level during solidification for any location of the sample. The thermal gradient and solidification rate were controlled independently. Samples run on the KC-135 aircraft exhibited bands of coarser graphite or of larger nodules usually corresponding to the regions solidified under low-g. Samples containing high phosphorous (used in order to determine the eutectic cell) exhibited larger eutectic cells in the low-g zone, followed by a band of coarser graphite.

Curreri, P. A.↗

Cast iron freezing mechanisms

This task focused on liquid phase sintering and infiltration studies of refractory metals and metal composites. Particular emphases was placed on those powered metal compacts which produce liquid alloys in sintering. For this class of materials, heating to a two phase region causes the constituent components to react, forming an alloy liquid which must wet the solid phase. Densification is initially driven by the free energy effects which cause rapid rearrangement. Further densification occurs by evaporation and condensation, surface diffusion, bulk flow, and volume diffusion.

Lillybeck, N. P.↗

Investigation of Wear and Friction Properties Under Sliding Conditions of Some Materials Suitable for Cages of Rolling-Contact Bearings

An investigation of wear and friction properties of a number of materials sliding against SAE 52100 steel was conducted. These materials included brass, bronze, beryllium copper, monel, nichrome v, 24s-t aluminum, nodular iron, and gray cast iron. The metals investigated may be useful as possible cage (separator or retainer) materials for rolling-contact bearings of high-speed turbine engines. The ability of materials to form surface films that prevent welding is a most important factor in both dry friction and boundary lubrication. On the basis of wear and resistance to welding only, the cast irons were the most promising materials investigated; they showed the least wear and the least tendency to surface failure when run dry, and when boundary lubricated they showed the highest load capacity. On the basis of mechanical properties, nodular iron is superior to gray cast iron. Bronze had the lowest friction coefficient under dry sliding conditions. The results with brass, beryllium copper, and aluminum were poor and these materials do not appear, with regard to friction and wear, to be suitable for cages.

Johnson, Robert L↗

Analysis of the Erosion of Cubic Centered and Face Centered Metallic Materials [Analyse de L'erosion de Matereaux Metalliques de Structures Cubiques Centree et Face Centree]

A generalized law of erosion, in nondimensional form, is proposed. The aforementioned explicitly gives an account of the nature and the microstructure of the material impacted, the angle of impact of the particles, and their hardness. The erosion behavior of various steels, pig iron, and cast iron is examined as well as the behavior of new ordered intermetallic materials, Fe-25% Al-(Zr, Cr, B). The concern of such alloys in an erosion-corrosion environment is shown. --- Une loi généralisée d'usure par érosion, sous forme non dimensionnelle, est proposée. Celle-ci rend compte explicitement de la nature et de la microstructure du matériau impacté, de l'angle d'impact des particules, de leur acuité at de leur durete. Le comportement à l'érosion de divers aciers et fontes est examiné ainsi que la tenue de nouveaux matériaux intermétalliques ordonnés Fe-25% Al - (Zr, Cr, B). L'interet de tels alliages dans des environnements agressifs du type érosion-corrosion est montré. Mots clés: usure, érosion, modèle, matériaux métalliques, intermétalliques Fe-Al.

A Magnée↗

Lubricous Deposit Formed In Situ Between Wearing Surfaces at High Temperatures

Many components of future aircraft will be constructed from novel high-temperature materials, such as superalloys and ceramic composites, to meet expected operating temperatures in excess of 300 C. There are no known liquid lubricants that can lubricate above 300 C without significant decomposition. Solid lubricants could be considered, but problems caused by the higher friction coefficients and wear rates of the solid lubricant film make this an undesirable approach. An alternative method of lubrication is currently being investigated: vapor phase lubrication. In vapor phase lubrication, an organic liquid (in our studies a thioether was used) is vaporized into a flowing air stream that is directed to sliding surfaces where lubrication is needed. The organic vapor reacts at the concentrated contact sliding area generating a lubricous deposit. This deposit has been characterized as a thin polymeric film that can provide effective lubrication at temperatures greater than 400 C. Initial tribological studies were conducted at the NASA Lewis Research Center and Cleveland State University with a high-temperature friction and wear tribometer. A cast iron rod was loaded (a 4-kg mass was used to generate a contact pressure of 1.2 MPa) against a reciprocating, cast iron plate at 500 C. This system was then lubricated with the vapor phase of thioether.

Source record↗

Cast iron-base alloy for cylinder/regenerator housing

NASACC-1 is a castable iron-base alloy designed to replace the costly and strategic cobalt-base X-40 alloy used in the automotive Stirling engine cylinder/generator housing. Over 40 alloy compositions were evaluated using investment cast test bars for stress-rupture testing. Also, hydrogen compatibility and oxygen corrosion resistance tests were used to determine the optimal alloy. NASACC-1 alloy was characterized using elevated and room temperature tensile, creep-rupture, low cycle fatigue, heat capacity, specific heat, and thermal expansion testing. Furthermore, phase analysis was performed on samples with several heat treated conditions. The properties are very encouraging. NASACC-1 alloy shows stress-rupture and low cycle fatigue properties equivalent to X-40. The oxidation resistance surpassed the program goal while maintaining acceptable resistance to hydrogen exposure. The welding, brazing, and casting characteristics are excellent. Finally, the cost of NASACC-1 is significantly lower than that of X-40.

Witter, Stewart L.↗

Fully Deuterated Aliphatic Hydrocarbons Obtained From Iron Carbide Treated with DCl and D2O

According to Oparin, Mendeleev thought that the origin of petroleum was the result of the hydrolysis of iron carbides by superheated steam under pressure from the deep interior of the Earth through geological formations where the metal carbides exist. As early as 1877, Mendeleev described the reaction leading to the synthesis of hydrocarbons according to the general equation 3Fe(sub m)C(sub n) + mH2O yields mFe3O4 + C(sub 3n)H(sub 8m). Other experimental studies on the production of hydrocarbons from cast iron have been reported. Because of the possibility that hydrocarbons may have been trapped within the carbon matrix of the cast iron, which usually has a high content of carbon, we have studied the reaction of pure iron carbide with deuterium chloride and deuterated water. This was done in order to distinguish any newly formed deuterated hydrocarbons from any possible impurities of trapped hydrocarbons. The experiments were carried out by simply allowing iron carbide to react with concentrated deuterium chloride in D2O. The volatile hydrocarbon fraction examined by gas chromatography-mass spectrometry (GC/MS), using a Finnigan 1020/OWA instrument. contained low molecular weight hydrocarbons in a range C3 to C7. Lower molecular weight hydrocarbons were not detected by GC/MS because the MS scanning mode was preset above mass 40 to exclude components of air. The identified hydrocarbons are similar to those obtained under prebiotic conditions using high frequency discharge. The hydrocarbons found in common were propane, butane, pentane, 3-methylpentane, hexane, and heptane. The percent yields decline with increasing carbon number (propane 11%, n-heptane 1%). Similar results have been obtained by the direct treatment of metal carbides by pulse laser vaporization mass spectrometry. These results show that the hydrolysis of iron carbides may have been a significant source of hydrocarbons on the primitive Earth. There appears to be a predominance of straight chain isomers, which may have been important in the prebiotic synthesis of membrane-forming compounds.

Marquez, C.↗

The feasibility of low-G grey solidification of nodular iron in the F-104 experimental furnace package

The rationale for low-g experiments with cast iron and the need for solidification in the grey form during these experiments are reviewed. The factors which determine whether an iron melt will solidify grey or white are discussed. Cooling rate versus microstructure was studied for a nodular iron candidate material for F-104 low-g solidification. The study determined that low-g grey solidification, using the present F-104 furnace system, of the nodular iron composition studied is not feasible. Specimen microstructure strongly suggested that the F-104 furnace's gas cooling system was causing excessive localized chill resulting in the nucleation of the unwanted iron carbide phase. A change is suggested, in the quench system design, that could possibly overcome this problem.

Curreri, P. A.↗

Microstructural variations induced by gravity level during directional solidification of near-eutectic iron-carbon type alloys

The effects of gravity on the microstructure of directionally solidified near-eutectic cast irons are studied, using a Bridgman-type automatic directional solidification furnace aboard a NASA KC-135 aircraft which flies parabolic arcs and generates alternating periods of low-g (0.01 to 0.001 g, 30 seconds long) and high-g (1.8 g, 1.5 minutes long). Results show a refinement of the interlamellar spacing of the eutectic during low-g processing of metastable Fe-C eutectic alloys. Low-g processing of stable Fe-C-Si eutectic alloys (lamellar or spheroidal graphic) results in a coarsening of the eutectic grain structure. Secondary dendrite arm spacing of austenite increases in low-g and decreases in high-g. The effectiveness of low-gravity in the removal of buoyancy-driven graphite phase segregation is demonstrated.

Stefanescu, Doru M.↗

Modal Vibration Analysis of Large Castings

The art of experimental modal vibration analysis (MVA) has been extended to apply to large castings. This extension was made to enable the use of experimental MVA as a relatively inexpensive, simple means of assessing the internal structural integrity of tread shoes of crawler transporters used to move spacecraft to the launch pad at Kennedy Space Center. Each tread shoe is made from cast iron and weighs about a ton (has a mass .907 kg). The present extended version of experimental MVA could also be applied to other large castings. It could be especially useful to manufacturers as a means of rapidly discriminating against large castings that contain unacceptably large concentrations of internal defects. The use of experimental MVA to assess structural integrity is not new. What are new here are those aspects of the extension of experimental MVA that pertain to the application of MVA to objects so massive that it may not be practical or cost effective to mount them in special test fixtures that impose special test boundary conditions to test them in place under normal conditions of use.

Werlink, Rudolph J.↗

Ceramic port shields cast in an iron engine head

Silicon nitride exhaust and intake port shields have been successfully cast into a gray iron cylinder head of a heavy duty diesel single cylinder research engine. Careful design considerations, finite element, and probability of survival analyses indicated viability of the design. Foundry experience, NDE, and failure investigations are reported.

Hakim, Nabil S.↗

Acoustic determination of cracks in welded joints

The acoustic analysis method permits detection of any cracks that might take place and their manner of propagation. The study deals with the cracks produced in experiments to determine the welding technology for a welded gray cast iron workpiece by using piezoelectric transducers to determine vibration acceleration.

Baltanoiu, M.↗