Self-Lubricating Composite Containing Chromium Oxide

A self lubricating. friction and wear reducing composite material useful over a wide temperature range of from cryogenic temperature up to about 900 C. contains 60 80 wt. % of particulate Cr2O3, dispersed in a metal binder of a metal alloy containing Cr and at least 50 wt. % of Ni, Cr or a mature of Ni and Cr. It also contains 5-20 wt. % of a fluoride of at least one Group I, Group II or rare earth metal and. optionally, 5-20 wt. % of a low temperature lubricant metal, such as Ag. Au, Pt, Pd, Rh and Cu. This composite exhibits less oxidation instability and less abrasiveness than composites containing chromium carbide, is readily applied using plasma spray and can be ground and polished with a silicon carbide abrasive.

Dellacorte, Christopher↗

The x ray microprobe determination of chromium oxidation state in olivine from lunar basalt and kimberlitic diamonds

The synchrotron x-ray microprobe is being used to obtain oxidation state information on planetary materials with high spatial resolution. Initial results on chromium in olivine from various sources including laboratory experiments, lunar basalt, and kimberlitic diamonds are reported. The lunar olivine was dominated by Cr(2+) whereas the diamond inclusions had Cr(2+/Cr(3+) ratios up to about 0.3. The simpliest interpretation is that the terrestrial olivine crystallized in a more oxidizing environment than the lunar olivine.

Sutton, S. R.↗

Vibrational sum frequency generation spectroscopy reveals the inertness of chromium oxide (001) surfaces

Nanoengineered metal oxides such as Cr(III)-oxide (chromia) films have diverse potential applications in corrosion inhibition, remediation, energy generation, catalysis, data storage, and biological and environmental systems. Concerns about material degradation or oxidation to toxic chromate necessitate an understanding of chromia/aqueous interfaces, beginning with their hydroxylation and hydration behavior. Vibrational sum-frequency generation spectroscopy (vSFG) provides specific molecular-level information about water at the oxide/aqueous junction with high surface selectivity. To overcome the strong absorber problem typical of certain metal oxides in the UV–visible range during nonlinear optical studies, we employed molecular beam epitaxy to deposit transparent, epitaxial nanofilms of Cr 2 O 3 with (001) crystalline orientation on sapphire (Al 2 O 3 (001)) substrates, as confirmed by atomic force microscopy and X-ray diffraction. vSFG spectra of the air and water interfaces of the Cr 2 O 3 (001) films reveal hydroxyl features corresponding to both dissociated and molecular water on the surface. In contrast to the dangling hydroxyls found on the bare Al 2 O 3 (001) substrate, the hydroxyl groups on the deposited Cr 2 O 3 (001) nanofilm do not readily undergo isotopic H/D exchange when exposed to varying forms of D 2 O under ambient conditions. When considering the chemistries of the corresponding trivalent cations in aqueous solution, the finding is at variance with their similar acidities and proton exchange dynamics but consistent with markedly slower inner-sphere water ligand exchange of hexaquo Cr 3+ . This finding challenges the idea that proton and water exchange at the water/Cr₂O₃(001) interface are solely correlated, driven by the strength of metal-bridging oxygen bonds and surface hydroxyl distribution, without direct causation.

Boamah-Agyemang, Mavis D. [Pacific Northwest Natio↗

First-Principles Study of the Voltage Profile and Mobility of Mg Intercalation in a Chromium Oxide Spinel

The development of Mg batteries, which can potentially achieve higher energy densities than Li-ion systems, is in need of cathodes that can reversibly intercalate Mg 2+ and exhibit a higher energy density than the state-of-the-art Chevrel and thio-spinel cathodes. Recent theoretical and experimental studies indicate that the oxide spinel family presents a set of promising Mg cathodes. Here specifically, in this work, we investigate Mg intercalation into the spinel-MgxCr 2 O 4 system. Using first-principles calculations in combination with a cluster expansion model and the nudged elastic band theory, we calculate the voltage curve for Mg insertion at room temperature and the activation barriers for Mg diffusion, respectively, at different Mg concentrations in the Cr 2 O 4 structure. Our results identify a potential limitation to Mg intercalation in the form of stable Mg-vacancy orderings in the Cr 2 O 4 lattice, which exhibit high migration barriers for Mg diffusion in addition to a steep voltage change. Additionally, we propose cation substitution as a potential mechanism that can be used to suppress the formation of the stable Mg-vacancy ordering, which can eventually enable the practical usage of Cr 2 O 4 as a Mg-cathode.

25 ENERGY STORAGE↗

Chromium Oxidation State in Planetary Basalts: Oxygen Fugacity Indicator and Critical Variable for Cr-Spinel Stability

Cr is a ubiquitous and relatively abundant minor element in basaltic, planetary magmas. At the reduced oxidation states (<FMQ) of many planetary basalts Cr is present in melts as both divalent and trivalent forms. The ratio of trivalent to divalent Cr present in the melt has many consequences for the stability and Cr concentration of magmatic phases such as spinel, clinopyroxene, and olivine. However, understanding the Cr valence in quenched melts has historically been plagued with analytical issues, and only recently has reliable methodology for quantifying Cr valence in quenched melts been developed. Despite this substantial difficulty, the pioneering works of Hanson and Jones and Berry and O'Neill provided important insights into the oxidation state of Cr in in silicate melts. Here we present a series of 1-bar gas mixing experiments performed with a Fe-rich basaltic melt in which have determined the Cr redox ratio of the melt at over a range of fO2 values by measuring this quantity in olivine with X-ray Absorption Near Edge Spectroscopy (XANES). The measured Cr redox ratio of the olivine phenocrysts can be readily converted to the ratio present in the conjugate melt via the ratio of crystal-liquid partition coefficients for Cr3+ and Cr2+. We have applied these results to modeling Cr spinel stability and Cr redox ratios in a primitive, iron-rich martian basalt.

Bell, A. S.↗

Enhancement of oxidative vaporization of chromium (III) oxide and chromium by oxygen atoms

Rates of oxidative vaporization of Cr2O3 were found to be markedly enhanced in the presence of O atoms. Investigations were conducted over the temperature range 470 to 1520 K. For Cr2O3 the enhancement was about 10 to the 9th power at 820 K in oxygen containing 2.5 percent atoms. Rapid oxidative vaporization of bare chromium was observed below 1070 K, the rate being about one-half that of Cr2O3. Results are interpreted in terms of thermochemical analysis.

Fryburg, G. C.↗

Selected fretting-wear-resistant coatings for titanium - 6-percent-aluminum - 4-percent-vanadium alloy

A titanium - 6-percent-aluminum - 4-percent-vanadium alloy (Ti-6Al-4V) was subjected to fretting-wear exposures against uncoated Ti-6Al-4V as a baseline and against various coatings and surface treatments applied to Ti-6Al-4V. The coatings evaluated included plasma-sprayed tungsten carbide with 12 percent cobalt, aluminum oxide with 13 percent titanium oxide, chromium oxide, and aluminum bronze with 10 percent aromatic polyester; polymer-bonded polyimide, polyimide with graphite fluoride, polyimide with molybdenum disulfide (MoS2), and methyl phenyl silicone bonded MoS2, preoxidation surface treatment, a nitride surface treatment, and a sputtered MoS2 coating. Results of wear measurements on both the coated and uncoated surfaces after 300,000 fretting cycles indicated that the polyimide coating was the most wear resistant and caused the least wear to the uncoated mating surface.

Bill, R. C.↗

Oxidative vaporization kinetics of chromium (III) oxide in oxygen from 1270 to 1570 K

Rates of oxidative vaporization of Cr2O3 on preoxidized resistively heated chromium were determined in flowing oxygen at 0.115 torr for temperatures from 1270 to 1570 K. Reaction controlled rates were obtained from experimental rates by a gold calibration technique. These rates were shown to agree with those predicted by thermochemical analysis. The activation energy obtained for the oxidative vaporation reaction corresponded numerically with the thermochemical enthalpy of the reaction. A theoretical equation is given for calculating the rate from thermodynamic data by using boundary layer theory.

Stearns, C. A.↗

Auger electron spectroscopy and depth profile study of oxidation of modified 440C steel

Auger electron spectroscopy (AES) and sputtering were used to study selective oxidation of modified 440C steel. The sample was polycrystalline. Oxidation was performed on initially clean surfaces for pressures ranging from 1 x 10 to the minus 7th power to 1 x 10 to the minus 5th power torr and temperatures ranging from room temperature to 800 C. AES traces were taken during oxidation. In situ sputtering depth profiles are also obtained. A transition temperature is observed in the range 600 to 700 C for which the composition of the outer surface oxide changed from iron oxide to chromium oxide. Heating in vacuum about 5 x 10 to the minus 10 power torr to 700 C causes conversion of the iron oxide surface to chromium oxide.

Ferrante, J.↗

The Effects of Mixing Multi-Component HLW Glasses on Spinel Crystal Size

The Hanford Waste Treatment and Immobilization Plant will vitrify radioactive waste into borosilicate glass. The high-level waste (HLW) glass formulations are constrained by processing and property requirements, including restrictions aimed at avoiding detrimental impacts of spinel crystallization in the melter. To understand the impact of glass chemistry on crystallization, two HLW glasses precipitating small (?5 µm) spinel crystals were individually mixed with a glass that precipitated large (?45 µm) spinel crystals in ratios of 25, 50, and 75 wt%. The size of spinel crystals in the mixed glasses varied from 5 to 20 µm. Small crystal size was attributed to: (1) high concentrations of nuclei due to the presence of ruthenium oxide and (2) chromium oxide aiding high rates of nucleation. Results indicate that the spinel crystal size can be controlled using chromium oxide and/or noble metal concentrations in the melt, even in complex mixtures like HLW glasses. Small crystals tend to settle slowly, so they are acceptable in the melter without a risk of failure. Allowing higher concentrations of spinel-forming waste components in the waste glass enables glass compositions with higher waste loading, thus increasing plant operational flexibility. An additional benefit to the presence of chromium oxide in the glass composition is the potential for the oxide to protect melter walls against corrosion.

Lonergan, Charmayne E.↗

Carcinogenic Chromium(VI) Compounds Formed by Intracellular Oxidation of Chromium(III) Dietary Supplements by Adipocytes

Abstract Chromium(III) nutritional supplements are widely consumed for their purported antidiabetic activities. X‐ray fluorescence microscopy (XFM) and X‐ray absorption near‐edge structure (XANES) studies have now shown that non‐toxic doses of [Cr 3 O(OCOEt) 6 (OH 2 ) 3 ] + ( A ), a prospective antidiabetic drug that undergoes similar H 2 O 2 induced oxidation reactions in the blood as other Cr supplements, was also oxidized to carcinogenic Cr VI and Cr V in living cells. Single adipocytes treated with A had approximately 1 μm large Cr hotspots containing Cr III , Cr V , and Cr VI (primarily Cr VI thiolates) species. These results strongly support the hypothesis that the antidiabetic activity of Cr III and the carcinogenicity of Cr VI compounds arise from similar mechanisms involving highly reactive Cr VI and Cr V intermediates, and highlight concerns over the safety of Cr III nutritional supplements.

Wu, Lindsay E.↗

Microstructure Evolution of Gas Atomized Iron Based ODS Alloys

In a simplified process to produce precursor powders for oxide dispersion-strengthened (ODS) alloys, gas-atomization reaction synthesis (GARS) was used to induce a surface oxide layer on molten droplets of three differing erritic stainless steel alloys during break-up and rapid solidification. The chemistry of the surface oxide was identified using auger electron spectroscopy (AES) and scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). The precursor iron-base powders were consolidated at 850 C and 1,300 C using hot isostatic pressing (HIPing). Consolidation at the lower temperature resulted in a fully dense microstructure, while preventing substantial prior particle-boundary-oxide dissociation. Microstructural analysis of the alloys consolidated at the higher temperature confirmed a significant reduction in prior-particle-boundary-oxide volume fraction, in comparison with the lower-temperature-consolidated sample. This provided evidence that a high-temperature internal oxygen-exchange reaction occurred between the metastable prior particle-boundary-oxide phase (chromium oxide) and the yttrium contained within each prior particle. This internal oxygen-exchange reaction is shown to result in the formation of yttrium-enriched oxide dispersoids throughout the alloy microstructure. The evolving microstructure was characterized using transmission electron microscopy (TEM) and high-energy X-ray diffraction (HE-XRD).

36 MATERIALS SCIENCE↗

Process for the production of star-tracking reticles

Reticles designed with quartz bases are masked with desired pattern and then are coated with highly adherent layers of chromium, chromium silver alloy, silver, copper, and black chromium (mixture of chromium and chromium oxides). Black chromium final layer produces required nonreflective surface.