Effect of variation in diameter and pitch of rivets on compressive strength of panels with Z-section stiffeners I : panels with close stiffener spacing that fail by local buckling
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Highlights: • All coarse aggregates and steel fibres were surrounded by the binder. • X-ray diffraction is useful for explaining the increase in compressive strength with increasing temperature. • Rosenhahnite and/or quartz Dauphiné-twinned phases improved the compressive strength. • Polypropylene fibres prevented spalling and preserved the compressive strength. • Concrete with steel and polypropylene fibres did not exhibit spalling at 300 °C. Concrete with two types of steel fibres and a polypropylene fibre prevented spalling and preserved the compressive strength at 300 °C, which makes these concretes suitable for long-term applications up to 300 °C, such as for steam collectors or thermal energy storage systems. The compressive strength behaviour of three types of ultra-high-performance fibre-reinforced concrete manufactured with the same matrix was investigated. For this purpose, a complete characterisation of all the raw materials and the three types of fibres used was performed. The morphology of all concrete mixtures at room temperature was analysed using scanning electron microscopy–energy-dispersive X-ray spectroscopy. From the results, it was ascertained that the steel fibres and coarse siliceous aggregates were not in contact (being separated by ≥3.41 μm) and were surrounded by the binder (of ≥1 μm in thickness) for all the mixtures studied. Rosenhahnite and/or quartz Dauphiné-twinned phases improved the compressive strength (as determined by X-ray diffraction).
K-Basin sludge will be stored in the Sludge Transport and Storage Containers (STSCs) at an interim storage location on Central Plateau before being treated and packaged for disposal. During the storage period, sludge in the STSCs may consolidate/agglomerate, potentially resulting in high-shear-strength material. The Sludge Treatment Project (STP) plans to use water jets to retrieve K-Basin sludge after the interim storage. STP has identified shear strength to be a key parameter that should be bounded to verify the operability and performance of sludge retrieval systems. Determining the range of sludge shear strength is important to gain high confidence that a water-jet retrieval system can mobilize stored K-Basin sludge from the STSCs. The shear strength measurements will provide a basis for bounding sludge properties for mobilization and erosion. Thus, it is also important to develop potential simulants to investigate these phenomena. Long-term sludge storage tests conducted by Pacific Northwest National Laboratory (PNNL) show that high-uranium-content K-Basin sludge can self-cement and form a strong sludge with a bulk shear strength of up to 65 kPa. Some of this sludge has 'paste' and 'chunks' with shear strengths of approximately 3-5 kPa and 380-770 kPa, respectively. High-uranium-content sludge samples subjected to hydrothermal testing (e.g., 185 C, 10 hours) have been observed to form agglomerates with a shear strength up to 170 kPa. These high values were estimated by measured unconfined compressive strength (UCS) obtained with a pocket penetrometer. Due to its ease of use, it is anticipated that a pocket penetrometer will be used to acquire additional shear strength data from archived K-Basin sludge samples stored at the PNNL Radiochemical Processing Laboratory (RPL) hot cells. It is uncertain whether the pocket penetrometer provides accurate shear strength measurements of the material. To assess the bounding material strength and potential for erosion, it is important to compare the measured shear strength to penetrometer measurements and to develop a correlation (or correlations) between UCS measured by a pocket penetrometer and direct shear strength measurements for various homogeneous and heterogeneous simulants. This study developed 11 homogeneous simulants, whose shear strengths vary from 4 to 170 kPa. With these simulants, we developed correlations between UCS measured by a Geotest E-280 pocket penetrometer and shear strength values measured by a Geonor H-60 hand-held vane tester and a more sophisticated bench-top unit, the Haake M5 rheometer. This was achieved with side-by-side measurements of the shear strength and UCS of the homogeneous simulants. The homogeneous simulants developed under this study consist of kaolin clay, plaster of Paris, and amorphous alumina CP-5 with water. The simulants also include modeling clay. The shear strength of most of these simulants is sensitive to various factors, including the simulant size, the intensity of mixing, and the curing time, even with given concentrations of simulant components. Table S.1 summarizes these 11 simulants and their shear strengths.
This paper deals with the correlation between the time evolution of the degree of hydration and the compressive strength of Recycled Aggregate Concrete (RAC) for different water to cement ratios and initial moisture conditions of the Recycled Concrete Aggregates (RCAs). Particularly, the influence of such moisture conditions is investigated by monitoring the hydration process and determining the compressive strength development of fully dry or fully saturated recycled aggregates in four RAC mixtures. Hydration processes are monitored via temperature measurements in hardening concrete samples and the time evolution of the degree of hydration is determined through a 1D hydration and heat flow model. The effect of the initial moisture condition of RCAs employed in the considered concrete mixtures clearly emerges from this study. In fact, a novel conceptual method is proposed to predict the compressive strength of RAC-systems, from the initial mixture parameters and the hardening conditions. -- Highlights: •The concrete industry is more and more concerned with sustainability issues. •The use of recycled aggregates is a promising solution to enhance sustainability. •Recycled aggregates affect both hydration processes and compressive strength. •A fundamental approach is proposed to unveil the influence of recycled aggregates. •Some experimental comparisons are presented to validate the proposed approach.
The main thrust of the work reported herein is to study the effect of chemical additives to make beneficial use of carbon dioxide in enhancing the compressive strength of dry-cast concrete. The additives used in this investigation were calcium and magnesium oxides and silicates, nickel oxide, sodium hydroxide, sodium bicarbonate and strontium chloride. The experimental results showed that both the carbonation reactions and the compressive strength of dry-cast concrete mixtures were improved when using chemical additives. Experimental investigations for optimisation were also undertaken with selected additives to further increase the carbon dioxide uptake and improve the compressive strength. The best results were obtained when using calcium silicate in combination with calcium oxide. The early-age compressive strength of specimens made from the optimised mixture increased from 9·82 MPa to 13·32 MPa, and the specimens’ carbon dioxide uptake increased from 8·76% to 10·62% of cement weight.
Matrix graphite (MG) with incompletely graphitized binder used in high-temperature gas-cooled reactors (HTGRs) is commonly suspected to exhibit lower oxidation resistance in air. In order to reveal the oxidation performance, the oxidation behavior of newly developed A3-3 MG at the temperature range from 500 to 950°C in air was studied and the effect of oxidation on the compressive strength of oxidized MG specimens was characterized. Results show that temperature has a significant influence on the oxidation behavior of MG. The transition temperature between Regimes I and II is ~700°C and the activation energy ( E a ) in Regime I is around 185 kJ/mol, a little lower than that of nuclear graphite, which indicates MG is more vulnerable to oxidation. Oxidation at 550°C causes more damage to compressive strength of MG than oxidation at 900°C. Comparing with the strength of pristine MG specimens, the rate of compressive strength loss is 77.3% after oxidation at 550°C and only 12.5% for oxidation at 900°C. Microstructure images of SEM and porosity measurement by Mercury Porosimetry indicate that the significant compressive strength loss of MG oxidized at 550°C may be attributed to both the uniform pore formation throughout the bulk and the preferential oxidation of the binder.
Compressive strength and failure modes of boron fiber-magnesium matrix composite
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The influences of fly ash and metakaolin added as substitutions (by up to 50 wt%) of magnesium potassium phosphate cement (MKPC) on the microstructures and compressive strengths of the MKPC pastes were investigated. The results indicate that the aluminosilicate fractions of both fly ash and metakaolin are involved in the acid-base reaction of MKPC system, leading to a preferential formation of irregular crystalline struvite-K incorporated with Al and Si elements and/or amorphous aluminosilicate phosphate products. Metakaolin is more reactive than fly ash in the MKPC system. For the same addition dosage, the MKPC pastes containing metakaolin exhibit higher compressive strengths than the pastes containing fly ash. This is attributed to the formation of more highly reinforced microstructures and denser interfaces between the metakaolin particle and hydration products (e.g. struvite-K) in the MKPC paste containing metakaolin. Addition of 30 wt% metakaolin increases the compressive strengths of MKPC pastes at all test ages.
Delaminations in laminated composite materials can degrade the compressive strength of these materials. Delaminations can form as a result of impact damage or processing flaws. In order to better understand the effects of these delaminations on the compressive behavior of laminated composite plates, programs have been conducted to assess the criticality of prescribed delaminations of known size, shape, and location on the compression strength of laminated composites. A review of these programs is presented along with highlights of pertinent findings from each.
Low velocity impact damage on the compressive strength of graphite/epoxy hat stiffened panels is studied. Fourteen panels, representative of minimum-mass designs for two compression load levels were tested. Eight panels were damaged by impact and the effect on compressive strength was evaluated by comparing the results with data for undamaged panels. The impact tests consisted of firing 1.27 cm diameter aluminum projectiles normal to the plane of the panel at a velocity of approximately 55 m/sec to simulate impact from runway debris. The results of this investigation indicate that impact damage in the panels designed for 0.53 MN/m was contained locally and the damaged panels were capable of carrying the design load. The panels designed for 1.58 MN/m failed between 50 and 58 percent of the design load due to impact damage in the high axial stiffness region. The extent of damage in the high axial stiffness region of both panel designs increased with the magnitude of applied axial load. Damage in this region was the most significant factor in reducing panel strength. Limited damage that was not visually detectable reduced ultimate strength as much as extensive visible damage.
An experimental investigation has been conducted to determine the effect of low-velocity impact damage and unloaded circular holes on the compressive strength of a 48-ply orthotropic graphite/epoxy flat laminate. Specimens were impacted by a 1.27-cm-diameter aluminum sphere with speeds from 52 to 101 m/x to simulate momenta typical of low-velocity impact hazards that can occur in commercial aircraft service. It is shown that low-velocity impact damage can significantly degrade the static compressive strength of the laminate. Specimens that fail at axial strains above 0.008 in the undamaged condition can fail at strains as low as 0.0031 when impacted at 100 m/s. Circular holes also reduce the static compressive strength of the laminate. The failure strain decreases as the hole diameter increases.
Presented in this paper are the plan, equipment, procedures, and findings of an experimental investigation of the tolerance to low velocity impact of a graphite epoxy (AS4/3501-6) and graphite bismaleimide (M6/CYCOM3100) advanced composites. The applied impacts were governed by the Air Force Guide Specification 87221. Specimens of each material system having a common nominal layup (10% 0 deg; 80% +/-45 deg; 10% 90 deg), a common 7 inch (17.78 cm) by 10 inch (25.40 cm) size, five different thicknesses (9, 26, 48, 74, and 96 plies), and ambient moisture content were impacted and strength tested at room temperature. Damaged areas and post impact compression strengths (PICS) were among the most significant findings obtained. While the undamaged per ply compression strength of both materials is a strong function of laminate thickness, the per ply PICS is not. The average difference in per ply PICS between the two material systems is about seven percent. Although a smaller percentage of the applied kinetic energy was absorbed by the Gr/BMI than by the Gr/Epoxy composites, larger damaged areas were produced in the Gr/BMI than in Gr/Epoxy. Within the limitations of this investigation, the Gr/BMI system seems to offer no advantage in damage tolerance over the Gr/Epoxy system examined.
This report gives a comparison of the accuracy of the three methods for calculating the compressive strength of flat sheet and stiffener combinations such as occur in stressed-skin or monocoque structures for aircraft. Of the three methods based upon various assumptions with regard to the interaction of sheet and stiffener, the method based upon mutual action of the stiffener and an effective width as a column gave the best agreement with the results of the tests. An investigation of the effect of small curvature resulted in the conclusion that the compressive strength of the curved panels is, for all practical purposes, equal to the strength of flat panels except for thick sheet where non-uniform curvature throughout the length may cause the strength of the curved panel to be 10 to 15 percent less than that of a corresponding flat panel.