Search NASA⌕ Search

SEARCH · Search NASA

Results for “Creep Rate”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Interactions between creep, fatigue and strain aging in two refractory alloys

The application of low-amplitude, high-frequency fatigue vibrations during creep testing of two strain-aging refractory alloys (molybdenum-base TZC and tantalum-base T-111) significantly reduced the creep strength of these materials. This strength reduction caused dramatic increases in both the first stage creep strain and the second stage creep rate. The magnitude of the creep rate acceleration varied directly with both frequency and A ratio (ratio of alternating to mean stress), and also varied with temperature, being greatest in the range where the strain-aging phenomenon was most prominent. It was concluded that the creep rate acceleration resulted from a negative strain rate sensitivity which is associated with the strain aging phenomenon in these materials. (A negative rate sensitivity causes flow stress to decrease with increasing strain rate, instead of increasing as in normal materials). By combining two analytical expressions which are normally used to describe creep and strain aging behavior, an expression was developed which correctly described the influence of temperature, frequency, and A ratio on the TZC creep rate acceleration.

Sheffler, K. D.↗

Creep Testing of High-Temperature Cu-8 Cr-4 Nb Alloy Completed

A Cu-8 at.% Cr-4 at.% Nb (Cu-8 Cr-4 Nb) alloy is under development for high-temperature, high heatflux applications, such as actively cooled, hypersonic vehicle heat exchangers and rocket engine combustion chambers. Cu-8 Cr-4 Nb offers a superior combination of strength and conductivity. It has also shown exceptional low-cycle fatigue properties. Following preliminary testing to determine the best processing route, a more detailed testing program was initiated to determine the creep lives and creep rates of Cu-8 Cr-4 Nb alloy specimens produced by extrusion. Testing was conducted at the NASA Lewis Research Center with constant-load vacuum creep units. Considering expected operating temperatures and mission lives, we developed a test matrix to accurately determine the creep properties of Cu-8 Cr-4 Nb between 500 and 800 C. Six bars of Cu-8 Cr-4 Nb were extruded. From these bars, 54 creep samples were machined and tested. The figure on the left shows the steady-state, or second-stage, creep rates for the samples. Comparison data for NARloy-Z (Cu-3 wt % Ag-0.5 wt % Zr), the alloy currently used in combustion chamber liners, were not unavailable. Therefore the steady-state creep rates for Cu at similar temperatures are presented. As expected, in comparison to pure Cu, the creep rates for Cu-8 Cr-4 Nb are much lower. The lives of the samples are presented in the figure on the right. As shown, Cu-8 Cr-4 Nb at 800 C is comparable to NARloy-Z at 648 C. At equivalent temperatures, Cu-8 Cr-4 Nb enjoys a 20 to 50 percent advantage in stress for a given life and 1 to 3 orders of magnitude greater life at a given stress. The improved properties allow for design tradeoffs and improvements in new and existing heat exchangers such as the next generation of combustion chamber liners. Average creep rates for Cu-8 Cr-4 Nb and pure Cu are shown. Average creep lives for Cu-8 Cr- 4 Nb and NARloy-Z are also shown. Currently, two companies are interested in the commercial usage of the Cu-8 Cr-4 Nb alloy. The Rocketdyne Division of Rockwell International is conducting independent testing to analyze the properties for their projected needs in advanced rocket engine applications. Metallamics, a company based in Traverse City, Michigan, is entering into a Space Act Agreement to evaluate and test Cu-Cr-Nb alloys as materials for welding electrodes that are used in robotic welding operations. Creep rate is one of the alloy properties that determines the degree to which a welding electrode will mushroom or expand at the tip. A material with a low creep rate will resist mushrooming and give the electrode a longer life, minimizing downtime. This application holds the potential for large-scale usage of the alloy in the automotive and other industries. Success here would dramatically decrease the cost of the alloy and increase availability for aerospace applications.

Source record↗

Tensile creep and creep-recovery behavior of a SiC-fiber-Si3N4-matrix composite

The tensile creep and creep-recovery behavior of a hot-pressed unidirectional SiC-fiber/Si3N4-matrix composite was investigated at 1200 C in air, in order to determine how various sustained and cyclic creep loading histories would influence the creep rate, accumulated creep strain, and the amount of strain recovered upon specimen unloading. The data accumulated indicate that the fundamental damage mode for sustained tensile creep at stresses of 200 and 250 MPa was periodic fiber fracture and that the creep life and the failure mode at 250 MPa were strongly influenced by the rate at which the initial creep stress was applied. Cyclic loading significantly lowered the duration of primary creep and the overall creep-strain accumulation. The implications of the results for microstructural and component design are discussed.

Holmes, John W.↗

Interactions between creep, fatigue, and strain-aging in two refractory metal alloys.

The application of low-amplitude, high-frequency fatigue vibrations during creep testing of two strain-aging refractory alloys (molybdenum-base TZC and tantalum-base T-111) significantly reduced the creep strength of these materials. This strength reduction caused dramatic increases in both the first-stage creep strain and the second-stage creep rate. The magnitude of the creep rate acceleration varied directly with both frequency and A ratio (ratio of alternating to mean stress), and also varied with temperature, being greatest in the range where the strain-aging phenomenon was most prominent. It was concluded that the creep rate acceleration resulted from a negative strain rate sensitivity which is associated with the strain-aging phenomenon in these materials. (A negative rate sensitivity causes flow stress to decrease with increasing strain rate, instead of increasing as in normal materials.)

Sheffler, K. D.↗

High-temperature creep of polycrystalline chromium

The creep properties of high-purity, polycrystalline chromium were determined over the temperature range 0.51 to 0.78 T sub m, where T sub m is the melting temperature. Creep rates determined from step-load creep tests can be represented by the general creep equation; epsilon/D = k((sigma/E) to the nth power) where epsilon is the minimum creep rate, D is the diffusivity, k is the creep rate constant, sigma is the applied stress, E is the modulus, and n is the stress exponent, equal to 4.3 for chromium. This correlation and metallographic observations suggest a dislocation climb mechanism is operative in the creep of chromium over the temperature range investigated.

Stephens, J. R.↗

Creep-rupture and fractographic analysis of Stirling engine superalloys tested in air and 15 MPa hydrogen

A brief comparative analytical and microstructural evaluation of creep-rupture performance of two iron-base superalloys in air and 15 MPa of hydrogen, is presented. Creep rupture data are presented for the sheet alloy 19-9DL and the cast alloy XF-818, including temperature, initial stress, rupture life, minimum creep rate, time to reach one percent creep strain, and total elongation. In 19-9DL, both rupture life and minimum creep rate are more sharply dependent on small stress changes than in XF-818 in the given environment, and 19-9DL appears to become a more creep-resistant material with increasing Q (apparent activation energy) while the opposite is noted for XF-818. There appears to be no environmental effect on minimum creep rate for 19-9DL, whereas Q becomes less negative for XF-818 for 15 MPa of H2. Multiple cracks leading to rupture are observed on the fracture surfaces, with sheet specimens showing many more cracks close to the fracture surface than cast specimens.

Bhattacharyya, S.↗

Creep behavior of tantalum alloy T-222 at 1365 to 1700 K

High vacuum creep tests on the tantalum T-222 alloy at 0.42 to 0.52 T sub m show that the major portion of the creep curves, up to at least 1 percent strain, can be best described by an increasing creep rate, with strain varying linearly with time. Correlation and extrapolation of the creep curves on the basis of increasing creep rates results in more accurate engineering design data than would use of approximated linear rates. Based on increasing creep rates, the stress for 1 percent strain in 10,000 hours for T-222 is about four times greater than for the Ta-10W alloy. Increasing the grain size results in increased creep strength. Thermal aging prior to testing caused precipitation of the hexagonal close packed (Hf,Ta) sub 2 C, which initially increased creep strength. However, this dimetal carbide was converted during creep testing to face-centered cubic (Hf,Ta)C.

Titran, R. H.↗

Development of a creep model informed by lower-length scale simulations to simulate creep in doped UO 2

Using molecular dynamics, we predict information at the atomistic scale used to develop a mechanistic UO 2 creep model for use in higher length-scale fuel performance codes. The ultimate objective of the model is to better describe the grain size dependence and therefore impact of doping on creep rates in UO 2 . In a previous NEAMS milestone, we found that Nabarro-Herring (bulk diffusional) creep was too low to capture the experimentally observed creep rates in standard UO 2 . Moreover, in that milestone, other mechanisms were explored, such as Coble (grain boundary) creep and dislocation climb, with each mechanism exhibiting different grain size dependencies. Again, these were orders of magnitude too low to describe the experimental creep rates. In this work, we address the previous assumptions made for the Coble creep mechanism by investigating the diffusivity of various defects at grain boundaries in UO 2 and, critically, to determine if enhanced grain boundary diffusivity allows the model to better reproduce experimental results. The diffusivity as a function of temperature for different concentrations of uranium vacancies and interstitials for bulk UO 2 have also been examined using cluster dynamics. Furthermore, using a concentration dependent segregation model, the concentration of defects at the grain boundary were predicted. This atomistic data was then input into the various creep mechanisms and the creep rates compared to the empirical MATPRO correlation (used in BISON) and experiment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal loading effects on chalk hydromechanical behavior for nuclear waste disposal

Safe disposal of heat-generating nuclear waste depends on host rock stability under thermal, hydrological, and mechanical stresses. This study investigates the effect of thermal loading on mechanical behavior of the shallowly buried Ghareb formation chalk through triaxial and hydrostatic constant strain rate and creep tests at temperatures up to 100 ˚C and effective pressures up to 20.7 MPa. Experimental results show that thermal loading reduces the elastic moduli of chalk by 50–75%, and a transition occurs above 60 ˚C where creep rates increase rapidly. Water saturation nearly doubles the thermally induced strain compared to dry conditions and strongly decreases material rigidity. Thermal loading also leads to significant pore pressure increases under undrained conditions and leads to reductions in the apparent permeability during drained conditions. Laboratory experimental data were used to parameterize and develop a preliminary constitutive model for predicting future deformation during repository operations in the Ghareb. The strongly coupled effects – mechanical weakening, fluid pressure fluctuations, and permeability modification – demonstrate that elevated repository temperatures will have a pronounced effect on the near field Ghareb behavior during waste disposal operations. The findings indicate that the coupled interactions must be considered in predictive models and repository design to ensure long-term nuclear waste isolation and safety.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Environmental degradation of 316 stainless steel in high temperature low cycle fatigue

Procedures based on modification of the conventional Strainrange Partitioning method are proposed to characterize the time-dependent degradation of engineering alloys in high-temperature, low-cycle fatigue. Creep-fatigue experiments were conducted in air using different waveforms of loading on 316 stainless steel at 816 C (1500 F) to determine the effect of exposure time on cyclic life. Reductions in the partitioned cyclic lives were observed with an increase in the time of exposure (or with the corresponding decrease in the steady-state creep rate) for all the waveforms involving creep strain. Excellent correlations of the experimental data were obtained by modifying the Conventional Strainrange Partitioning life relationships involving creep strain using a power-law term of either: (1) time of exposure, or (2) steady-state creep rate of the creep-fatigue test. Environmental degradation due to oxidation, material degradation due to the precipitation of carbides along the grain boundaries and detrimental deformation modes associated with the prolonged periods of creep were observed to be the main mechanisms responsible for life reductions at long exposure times.

Kalluri, Sreeramesh↗

Creep of CoO single crystals.

The crystals were creep tested in compression over ranges of temperature, stress, and oxygen pressure. The creep curves were S-shaped, and only the inflection creep rate was analyzed. A formula is presented for the inflection creep rate in the range from 1000 to 1200 C, 850 to 1700 psi, and 0.001 to 1 atm oxygen. Slip was found to occur on two orthogonal slip systems. The presence of subboundaries was observed by optical and transmission electron microscopy. It is suggested that the creep rate is controlled by oxygen diffusion.

Clauer, A. H.↗

Creep-rupture behavior of 6 candidate stirling engine iron-base superalloys in high pressure hydrogen. Volume 1: Air creep-rupture behavior

Four wrought alloys (A-286, IN 800H, N-155, and 19-9DL) and two cast alloys (CRM-6D and XF-818) were tested to determine their creep-rupture behavior. The wrought alloys were used in the form of sheets of 0.89 mm (0.035 in.) average thickness. The cast alloy specimens were investment cast and machined to 6.35 mm (0.250 in.) gage diameter. All specimens were tested to rupture in air at different times up to 3000 h over the temperature range of 650 C to 925 C (1200 F to 1700 F). Rupture life, minimum creep rate, and time to 1% creep strain were statistically analyzed as a function of stress at different temperatures. Temperature-compensated analysis was also performed to obtain the activation energies for rupture life, time to 1% creep strain, and the minimum creep rate. Microstructural and fracture analyses were also performed. Based on statistical analyses, estimates were made for stress levels at different temperatures to obtain 3500 h rupture life and time to 1% creep strain. Test results are to be compared with similar data being obtained for these alloys under 15 MPa (2175 psi) hydrogen.

Bhattacharyya, S.↗

Quarterly Management Document – FY22, 1st Quarter, Multi-pass Hybrid Laser Arc Welding of Alloy 740H

This report summarizes the progress made on the project during the first quarter of FY22. The model for deep penetration laser welding continues to be developed to understand and mitigate cracking issues associated with laser welding Alloy 740H. The effects of laser wobble on laser welding of this alloy are also being developed. Additionally, the short-term creep behavior of welds made by various hybrid laser arc parameters has been obtained and the results indicate they are comparable to welds made by conventional gas tungsten arc welding which is a factor 2 slower than the hybrid welds. Additionally, the creep behavior of laser-only welds is also consistent with conventional gas tungsten arc welds as well as the hybrid laser arc welds made under this project. However, the creep rate of the laser-only welds is much higher than that observed in the hybrid laser arc welded specimens. This is most likely due to the narrower weld produced by laser-only welding compared to hybrid laser arc welding and, thus, the higher creep rate of laser-only welded creep specimens is likely a result of the increased fraction of base metal (which exhibits a higher creep rate than weld metal) contained within the gage section of the creep specimen. Creep rupture lifetimes were all about the same for both laser-only and hybrid laser arc welded specimens and consistent with the creep rupture lifetime of conventional gas tungsten arc welded creep specimens.

36 MATERIALS SCIENCE↗

Long-time creep behavior of the niobium alloy C-103

The creep behavior of C-103 was studied as a function of stress, temperature, and grain size for test times to 19000 hr. Over the temperature range 827 to 1204 C and the stress range 6.89 to 138 MPa, only tertiary (accelerating) creep was observed. The creep strain epsilon can be related to time t by an exponential relation epsilon = epsilon(0) + K e raised to power (st) - 1), where epsilon (0) is initial creep strain, K is the tertiary creep strain parameter, and s is the tertiary creep rate parameter. The observed stress exponent 2.87 is similar to the three power law generally observed for secondary (linear) creep of Class I solid solutions. The apparent activation energy 374 kj/g mol is close to that observed for self diffusion of pure niobium. The initial tertiary creep rate was slightly faster for fine grained than for coarse-grained material. The strain parameter K can be expressed as a combination of power functions of stress and grain size and an exponential function of temperature. Strain time curves generated by using calculated values for K and s showed reasonable agreement with observed curves to strains of at least 4 percent. The time to 1 percent strain was related to stress, temperature, and grain size in a similar manner as the initial tertiary creep rate.

Titran, R. H.↗

Tensile and Compressive Constitutive Response of 316 Stainless Steel at Elevated Temperatures

Creep rate in compression is lower by factors of 2 to 10 than in tension if the microstructure of the two specimens is the same and are tested at equal temperatures and equal but opposite stresses. Such behavior is characteristic for monotonic creep and conditions involving cyclic creep. In the latter case creep rate in both tension and compression progressively increases from cycle to cycle, rendering questionable the possibility of expressing a time stabilized constitutive relationship. The difference in creep rates in tension and compression is considerably reduced if the tension specimen is first subjected to cycles of tensile creep (reversed by compressive plasticity), while the compression specimen is first subjected to cycles of compressive creep (reversed by tensile plasticity). In both cases, the test temperature is the same and the stresses are equal and opposite. Such reduction is a reflection of differences in microstructure of the specimens resulting from different prior mechanical history.

Manson, S. S.↗

Tensile and compressive constitutive response of 316 stainless steel at elevated temperatures

It is demonstrated that creep rate of 316 SS is lower by factors of 2 to 10 in compression than in tension if the microstructure is the same and tests are conducted at identical temperatures and equal but opposite stresses. Such behavior was observed for both monotonic creep and conditions involving cyclic creep. In the latter case creep rate in both tension and compression progressively increases from cycle to cycle, rendering questionable the possibility of expressing a time-stabilized constitutive relationship. The difference in creep rates in tension and compression is considerably reduced if the tension specimen is first subjected to cycles of tensile creep (reversed by compressive plasticity), while the compression specimen is first subjected to cycles of compressive creep (reversed by tensile plasticity). In both cases, the test temperature is the same and the stresses are equal and opposite. Such reduction is a reflection of differences in microstructure of the specimens resulting from different prior mechanical history.

Manson, S. S.↗

Microstructure-sensitive modeling of high temperature creep in grade-91 alloy

Predicting the effects of microstructure on high-temperature creep responses of steel components is critical to minimize the risks of failure and maximize economic viability in the energy sector. In this research, a recently developed advanced mechanistic constitutive model is employed to study the effect of microstructure on the creep responses and to rationalize experimentally reported variability in the performances of grade-91 alloy. Hundreds of experimental creep tests from the literature are used to assess the predictability of the model. The model proposed is shown to accurately predict the steady-state creep rates and also the less commonly considered, yet important, primary-to-secondary transients for a wide range of creep conditions. Further, the model is capable of extrapolating the creep response of grade 91 alloy even outside of the calibration regime. Using this model, the roles of initial microstructure described in terms of grain size, dislocation density, and precipitate content, on the creep responses are investigated. The effect of initial microstructure on the steady-state creep rates and creep-strain is found to vary with stress and temperature. Grain size plays a significant role in the low-stress creep, where the diffusional creep is dominant. On the other hand, the effects of dislocation densities and precipitate content are significant in the dislocation-plasticity-dominated high-stress and temperature regimes. Furthermore, by comparing model predictions against a large experimental creep database, it is found that variability in the creep responses can be rationalized on the basis of differences in the initial microstructure. Overall, this work provides a robust pathway for microstructure-aware engineering design, verification, and validation of metallic components for energy applications.

36 MATERIALS SCIENCE↗

Time dependency of strainrange partitioning life relationships

The effect of exposure time (or creep rate) on the CP life relationship is established by conducting isothermal CP tests at varying exposure times on 316 Ss at 1300 and 1500 F. A reduction in the CP cycle life is observed with an increase in the exposure time of the CP test at a given inelastic strain-range. This phenomenon is characterized by modifying the Manson-Coffin type of CP relationship. Two new life relationships: (1) the Steady State Creep Rate (SSRC) Modified CP life relationship, and (2) the Failure Time (FT) Modified CP life relationship, are developed in this report. They account for the effect of creep rate and exposure time within the CP type of waveform. The reduction in CP cyclic life in the long exposure time tests is attributed to oxidation and the precipitation of carbides along the grain boundaries.

Kalluri, S.↗