Search NASA⌕ Search

SEARCH · Search NASA

Results for “Diffusion Welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Understanding formation mechanisms of intermetallic compounds in dissimilar Al/steel joint processed by resistance spot welding

Here, this paper confirmed the formation mechanism of intermetallic compounds (IMCs) in Al/steel resistance spot welds with transmission electron microscopy, electron backscatter diffraction, nanoindentation and thermodynamic calculations. In particular, the formation of AlFe with BCC_B2 structure, which is not commonly seen in welds, was identified. The formation mechanism of IMCs at the high welding energy region is described as follows. Al 13 Fe 4 first nucleates from the Al side, followed by Al 5 Fe 2 growth with Fe atoms accumulating at the Al 13 Fe 4 grain boundaries. Then, Al 5 Fe 2 grains grow continuously to coarse columnar grains, and AlFe forms at the interface of Al 5 Fe 2 grains and the ferrite phase. Lastly, the needle-like Al 13 Fe 4 forms in the cooling process. At the middle welding energy region, only equiaxed Al 5 Fe 2 and small Al 13 Fe 4 grains are formed at the interface because of the lower diffusion rates of Al and Fe, hence postponing the growth of Al 5 Fe 2 and Al 13 Fe 4 . At the low welding energy region, only sporadic Al 5 Fe 2 and Al 13 Fe 4 grains are formed surrounded by the Al phase.

42 ENGINEERING↗

Validation of Manufacturing Process Designs for Stamped Microchannel Recuperators

Microchannel recuperators can achieve high-efficiency power cycles and chemical reactions by recovering waste heat from hot turbine exhaust and chemical reaction streams. However, the industrial application of microchannel recuperators are restricted by the high cost of patterning and bonding. The objective of this study was thus to investigate new methods for producing microchannel recuperators for emerging markets. Based on greenfield cost estimates, process designs based on stamping, laser welding and vacuum brazing of 316L stainless steel laminae were found to be more economical than conventional photochemical machining and diffusion bonding. Subsequently, validation experiments were conducted to produce stamped microchannel components using cost model parameters. At a mass flow rate of 0.99 g/s, the test article made with laser welding was found to provide higher effectiveness than the test article produced using vacuum brazing. Preliminary investigations showed that residual stresses during laser welding of the laminae led to significant warpage, collapsing channels and making lamina-to-lamina fit up challenging. In contrast, the test article produced by vacuum brazing of stamped laminae showed no clogging and 4.6% and 10.5% channel height standard deviation for the cold and hot channels, respectively. Channel variation in the vacuum brazing sample was determined to be caused by misregistration of laminae during brazing. In future work, efforts are needed to choose cheaper, more ductile brazing foils as well as design a brazing fixture to improve lamina-to-lamina registration.

42 ENGINEERING↗

Unveiling the Interplay: Cold Work, Recrystallization, and Flux Expulsion in SRF Cavities

The fabrication of SRF cavities from sheet materials includes deep-drawing, electron beam welding, chemical and mechanical polishing, high-temperature heat treatment, and material diffusion. The performance of these cavities is frequently limited by magnetic flux trapping giving rise to additional rf loss. In this presentation, we thoroughly examine how recrystallization influences flux expulsion in SRF cavities, using cold-worked niobium sheets from various suppliers. Our findings reveal that cold-worked sheets enhance flux expulsion, especially at lower heat treatment temperatures, by promoting improved recrystallization. In particular, a traditionally fabricated Nb cavity half-cell from an annealed poly-crystalline Nb sheet after an 800 C heat treatment leads to a bi-modal microstructure that ties in with flux trapping and inefficient flux expulsion. This non-uniform microstructure is related to varying strain profiles along the cavity shape. A novel approach to prevent this non-uniform microstructure is presented by fabricating a 1.3 GHz single cell Nb cavities with a cold-worked sheet and subsequent heat treatment leading to better flux expulsion after 800 C/3h

Dhakal, P. [Old Dominion Univ., Norfolk, VA (Unite↗

The roles of kinematic constraint and diffusion in non-equilibrium solid state phase transformations of Ti-6Al-4V

A solid state phase transformation of Ti-6Al-4V was studied using high speed in situ x-ray diffraction measurements made during rapid cooling of a cold metal transfer arc weld bead deposited onto a water cooled substrate. Analysis of body centered cubic (BCC) and hexagonal close packed (HCP) lattices revealed an abrupt, nonlinear shift in the lattice parameters of both phases just after the HCP phase had nucleated. Postmortem transmission electron microscopy confirmed that V diffusion was mostly suppressed during cooling. Together, these results indicate that at this cooling rate of approximately 10 4 K/s, which is representative of cooling rates of many additive manufacturing and welding processes, kinematic coherency of the BCC–HCP interfaces gives rise to the anomalous lattice expansion and contraction behaviors of both phases during the initial nucleation and growth stages of (mostly) martensitic transformation from BCC to HCP; the role of diffusion in such lattice anomalies is shown to be minimal.

36 MATERIALS SCIENCE↗

A potential emerging issue concerning repair welding of out-of-core PWR components involving tritium exposure and 3 He retention

This paper identifies a potential but previously unrecognized risk of helium-induced embrittlement and cracking during repair welding of out-of-core pressurized water reactor (PWR) components exposed to tritium-contaminated coolant. While previous weldability concerns centered on 4 He accumulation in neutron-irradiated alloys located within the in-core or near-core regions, new measurements show that 3 He generated by tritium decay can accumulate in out-of-core components. Because hydrogen isotopes readily diffuse to grain boundaries and become trapped there, significant 3 He generation at grain boundaries may lead to cracking during weld repairs. Initial data from far-below-core PWR flux thimble tubes confirm the presence of 3 He levels above known cracking thresholds for repair welds. In conclusion, these findings indicate that out-of-core regions should be considered when defining safe weld repair windows in reactors operating for 60–100 years.

Extended PWR lifetimes↗

Enhanced Interfacial Bonding of Graft Copolymers

To understand how thermoplastic welding strength can be tuned through chemical modifications and macromolecular topology, we combined coarse-grained molecular dynamics (MD) simulations with experimental validation. Our simulations examined the diffusion dynamics of both linear and graft polymers across representative interfaces, revealing that diffusion-controlled interdigitation follows a power law, with the exponent decreasing from 0.34 to 0.11 as grafting density increases from 7.5 to 196% (with side chains grafted to both sides of a monomer unit). The addition of side chains enhances welding efficiency, as dense bottlebrush polymers with high grafting density reach maximum rupture strength faster than linear polymers. However, their saturated rupture strength is lower. This observation is subsequently corroborated by experimental lap-shear tests comparing linear polyethylene with octene grafted polyethylene elastomers. Our MD simulations show that unlike linear polymers, where backbone entanglements dominate, the grafted side chains introduce mechanisms in addition to entanglement dilution. The rapid interdigitation of side chains creates a dense mesh of entropic van der Waals contacts, which can also enhance the film welding. Furthermore, our MD simulations reveal a brittle rupture behavior in linear and comb-like (mildly grafted) polymers, while bottlebrush (densely grafted) polymers display elastomeric behavior with a pronounced stress plateau prior to fracture. Our simulations deconvolute the influence of polymer topology on deformation behavior. The rate of polymer deformation becomes lower than the applied strain rate prior to rupture, and the onset of this deviation is progressively delayed from linear to bottlebrush polymers. This trend highlights the critical role of molecular architecture in governing the mechanical response. In conclusion, these results provide deeper insight into the underlying welding mechanisms of topological polymers and present a potential approach for mitigating the interface anisotropy that is inherent in advanced manufacturing techniques such as fused filament fabrication.

graft copolymers↗

Investigations on the multiple-sector hard-copper X-band accelerating structures

The development of advanced, high gradient accelerating structures is one of the leading activity of the particle accelerator community. In the technological research of new construction methods for these devices, high-power testing is a critical step for the verification of their viability. Recent experiments showed that accelerating cavities made out of hard copper, fabricated without high-temperature processes, can achieve better performance as compared with soft copper ones. Recently, we have built cavities using Tungsten Inert Gas welding and the high-power experiments confirmed that this joining process is a robust and low-cost alternative to brazing or diffusion bonding. This is a good solution for high-gradient operation, with a gradient of about 150 MV/m in X-band, at a breakdown rate of 10 -3 /pulse/meter using a shaped RF pulse with a 150 ns flat part. We continue the design, construction and high power tests of three-cells standing-wave X-band accelerating cavities fabricated with a split-open geometry, made of hard copper and vacuum-sealed by welding. Our aim is the fabrication of accelerating structures made out of hard copper alloys by using innovative cost-effective technologies. Moreover, our method of multiple-sector structures opens the way to new technological approaches and design methods, for example providing the possibility of placing dampers of the parasitic higher-order modes. Such structures with dampers allow for acceleration of multi-bunch beams, both in standing and in travelling-wave accelerating modality. Here, this paper describes the design of two cavities made of multiple sectors that were fabricated at the Italian Institute for Nuclear Physics in Frascati, Italy (INFN-LNF), assembled by means of clamping and then joined with the Tungsten Inert Gas welding in order to preserve the hardness of the metal. These are three-cell standing-wave X-band accelerating cavities, to be operated in the π-mode. We report the low-power RF tests of the first one, made of two halves, and the RF design of the second one, made of four quadrants. Both structures were built for high-gradient tests at SLAC National Accelerator Laboratory.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Diffuser Braze Development

At the request of SRTE, through the PDRD project, SRNL is developing a vacuum brazing process to facilitate the fabrication of hydrogen purification systems. In particular, this effort is directed at tube-style hydrogen diffusers. The diffusers are comprised of numerous palladium-silver tubes that are brazed to a nickel fitting, which is subsequently welded to a stainless steel tube, fitting, or tube sheet. Historically, torch brazing has been used as a heat source; for this work vacuum furnace brazing was suggested to improve the uniformity of the process. This report describes the braze process development for braze selection and simple nickel fitting to tube brazing. Five braze alloys were selected and sessile drop testing was conducted over a range of temperatures from 25 to 75° C over the liquidus temperature. Samples were characterized for wetting angle, erosion, and brazability. The cup-to-tube braze joints were inspected using digital radiography, ultrasonic testing, and metallographic examination. Two of the five alloys exhibited excellent fabrication properties and are considered for further development.

36 MATERIALS SCIENCE↗

Forming mechanism of equilibrium and non-equilibrium metallurgical phases in dissimilar aluminum/steel (Al–Fe) joints

Abstract Forming metallurgical phases has a critical impact on the performance of dissimilar materials joints. Here, we shed light on the forming mechanism of equilibrium and non-equilibrium intermetallic compounds (IMCs) in dissimilar aluminum/steel joints with respect to processing history (e.g., the pressure and temperature profiles) and chemical composition, where the knowledge of free energy and atomic diffusion in the Al–Fe system was taken from first-principles phonon calculations and data available in the literature. We found that the metastable and ductile (judged by the presently predicted elastic constants) Al 6 Fe is a pressure ( P ) favored IMC observed in processes involving high pressures. The MoSi 2 -type Al 2 Fe is brittle and a strong P -favored IMC observed at high pressures. The stable, brittle η-Al 5 Fe 2 is the most observed IMC (followed by θ-Al 13 Fe 4 ) in almost all processes, such as fusion/solid-state welding and additive manufacturing (AM), since η-Al 5 Fe 2 is temperature-favored, possessing high thermodynamic driving force of formation and the fastest atomic diffusivity among all Al–Fe IMCs. Notably, the ductile AlFe 3 , the less ductile AlFe, and most of the other IMCs can be formed during AM, making AM a superior process to achieve desired IMCs in dissimilar materials. In addition, the unknown configurations of Al 2 Fe and Al 5 Fe 2 were also examined by machine learning based datamining together with first-principles verifications and structure predictions. All the IMCs that are not P- favored can be identified using the conventional equilibrium phase diagram and the Scheil-Gulliver non-equilibrium simulations.

36 MATERIALS SCIENCE↗

On the solid-state-bonding mechanism in friction stir welding

This study is a critical assessment of various solid-state-bonding mechanisms is established for friction stir welding (FSW) processes of engineering alloys. The commonly assumed sintering-like diffusional-bonding hypothesis is criticized in this work as not the dominant mechanism. For the wide spectrum of material constitutive laws and FSW processing conditions examined and employed in realistic applications, the thermomechanical history on the workpiece–workpiece interface traverses in the creep-dominated regime for the growth/shrinkage of interfacial cavities. The evolution of the bonding fraction relies mainly on the creep strain rate in the adjourning workpieces, weakly on stress triaxiality, and negligibly on interfacial diffusion.

36 MATERIALS SCIENCE↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Microstructure and mechanical behavior of laser remelted amorphous Al-Ni-La welds

To explore the feasibility of using laser powder bed fusion systems to print bulk amorphous Al alloys, a single autogenous weld produced by laser remelting on a cast Al-5La-9Ni (at.%) alloy was studied for its microstructure and mechanical behavior. The solidification rates experienced by material within the welds were high enough to produce entirely amorphous regions within the welds. Welds were characterized using SEM, STEM, and APT and were found to contain Ni-rich amorphous clusters. Micropillar compression tests were used to assess mechanical properties of the welds and found that all of the amorphous regions exhibited yield strengths around 1 GPa. In conclusion, these results are discussed in the context of diffusivity of Ni and rare earth elements in liquid, glass forming ability, thermodynamic driving force for phase formation during solidification, free volume concentrations in bulk metallic glasses, and cluster-related softening.

APT↗

Room temperature corrosion behaviour of plastically deformed AISI 304 stainless steel by friction stir welding in neutral and acidified chloride solutions

Severe plastic deformation of 304L stainless steel plate was carried out by friction stirring under an isothermal tool temperature at 825°C. The friction stirred zone showed extensive grain refinement, high fraction of low angle grain boundaries due to dislocation rearrangement, Σ3 and Σ9 special grain boundaries and discrete Fe–Cr–Mn-rich particles. Electrochemical polarisation measurements were done on the base metal (BM) and friction stir welded (FSW) specimens in the neutral and acidified 3.5% NaCl solutions. The BM showed marginally better pitting resistance in the neutral chloride solution than the FSW because of a larger fraction of special grain boundaries, and larger grain size. Whereas in acidified 3.5% NaCl solution, the FSW showed better corrosion resistance than the BM. Furthermore, the surface film of the FSW had a lower impedance and a lower defect concentration than the BM indicating higher diffusivity of point defects in the FSW.

36 MATERIALS SCIENCE↗

Scientific Development of Core Block and Monolith Materials (FY2020 Progress)

This report presents the status of an effort to investigate welding and joining techniques for microreactor monolith structural materials. Previously reported results have demonstrated the potential to tier weld sub-scale components using electron beam welding. Tier welding has been investigated on larger scale test articles, and results indicate that tier welding is not feasible for larger components due to the penetration depth that is required. Additional techniques to produce full length parts have been examined, including diffusion bonding and gundrilling. Evaluations of these techniques are ongoing, and have shown early success on sub-scale components. These results indicate that while issues still exist for manufacturing microreactor structures, these challenges are better understood and solutions are in development.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Suppression of irradiation hardening in tungsten-coated ferritic steel for fusion reactor blanket applications

W-coated reduced activation ferritic steels have been developed for use as plasma facing components in fusion reactor blankets, offering excellent sputtering resistance and structural strength. Previous high-temperature coating methods, such as diffusion bonding and brazing, caused interfacial deterioration due to thermal stress from mismatched thermal expansion between W and reduced activation ferritic steel. To address this, underwater explosive welding was introduced as a high-velocity cold process that joins dissimilar materials while maintaining a strong, thin interface without the thermal issues associated with traditional methods. In this study, the effects of neutron irradiation on the hardness and microstructure in W-coated F82H reduced activation ferritic steel (W/F82H) joined by underwater explosive welding are investigated. Following neutron irradiation at 290 °C, irradiation hardening is suppressed in W, F82H, and their interface within the W/F82H material. Furthermore, microstructural observations indicate that the recovery of work hardening and relaxation of elastic strain introduced during coating significantly contribute to the suppression of irradiation hardening in W/F82H. In conclusion, W/F82H exhibits significantly suppressed irradiation hardening compared with those in stand-alone materials. This suppression is explained by residual stress from thermal expansion mismatch and the unique microstructure at the interface. These results provide valuable insights for the development of more durable materials in nuclear fusion applications.

36 MATERIALS SCIENCE↗

Materials and technological processes for High-Gradient accelerating structures: new results from mechanical tests of an innovative braze-free cavity.

Pure oxygen-free high-conductivity copper is a widely used material for manufacturing accelerating cavities working at room temperature. Several studies attempted to explain limitations associated with the maximum allowed field gradients and the behaviour of vacuum RF breakdown in copper accelerating structures through generation and movement of dislocations under stresses associated with RF electric and magnetic fields. Pure copper and also copper alloys undergo mechanical and thermal treatments to be hardened and strengthened during manufacturing, although their mechanical properties significantly change after heating above 590°C. High temperature brazing and diffusion bonding are assembly methods widely used to manufacture ultra-high vacuum accelerating devices. However, these processes, occurring at about 800–1000°C, significantly affect the mechanical properties of copper and copper alloys. We introduce here a novel Tungsten Inert Gas welding procedure, which is fast and keeps the high-gradient surfaces of the cavity and other components well below the copper annealing temperature. This process may be successfully used to manufacture copper-based accelerating components. This technology further preserves the hardness and cleanliness of copper in order to achieve the maximum accelerating gradient.

47 OTHER INSTRUMENTATION↗

2023 SRNL Aging and Lifetimes Report: Tritium Aging of Welded and Additively Manufactured Austenitic Stainless Steels

This report documents work performed in fiscal year 2023 at Savannah River National Laboratory (SRNL) collaborating with Sandia National Laboratories in support of the Aging and Lifetimes program. This work supports Gas Transfer Systems (GTS) design by measuring the mechanical behavior of structural materials used in GTS. Data on properties in relevant conditions are crucial for GTS lifetime assessments and predictions. To simulate relevant conditions, SRNL, in concert with the Savannah River Site, thermally pre-charges test specimens with tritium and stores them at -80°C to allow the tritium decay product, helium-3, to build up while limiting tritium diffusion. According to test plans based on how much helium-3 has accumulated, specimens are removed from storage and tested. Results from mechanical testing provide an empirical basis for GTS design as well as insight to how these structural materials degrade in a tritium environment.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗