At least 37 records · Page 2

Interim results of long-term environmental exposures of advanced composites for aircraft applications

Interim results from a number of ongoing, long-term environmental effects programs for composite materials are reported. The flight service experience is evaluated for 142 composite aircraft components after more than five years and one million successful component flight hours. Ground-based outdoor exposures of composite material coupons after 3 years of exposure at five sites have reached equilibrium levels of moisture pickup which are predictable. Solar ultraviolet-induced material loss is discussed for these same exposures. No significant degradation has been observed in residual strength for either stressed or unstressed specimens, or for exposures to aviation fuels and fluids.

Pride, R. A.↗

Estimated Environmental Exposures for MISSE-3 and MISSE-4

Both modeling techniques and a variety of measurements and observations were used to characterize the environmental conditions experienced by the specimens flown on the MISSE-3 (Materials International Space Station Experiment) and MISSE-4 space flight experiments. On August 3, 2006, astronauts Jeff Williams and Thomas Reiter attached MISSE-3 and -4 to the Quest airlock on ISS, where these experiments were exposed to atomic oxygen (AO), ultraviolet (UV) radiation, particulate radiation, thermal cycling, meteoroid/space debris impact, and the induced environment of an active space station. They had been flown to ISS during the July 2006 STS-121 mission. The two suitcases were oriented so that one side faced the ram direction and one side remained shielded from the atomic oxygen. On August 18,2007, astronauts Clay Anderson and Dave Williams retrieved MISSE-3 and-4 and returned them to Earth at the end of the STS-118 mission. Quantitative values are provided when possible for selected environmental factors. A meteoroid/debris impact survey was performed prior to de-integration at Langley Research Center. AO fluences were calculated based on mass loss and thickness loss of thin polymeric films of known AO reactivity. Radiation was measured with thermoluminescent detectors. Visual inspections under ambient and "black-light" at NASA LaRC, together with optical measurements on selected specimens, were the basis for the initial contamination level assessment.

Pippin, Gary↗

Effect of Environmental Exposures on Fatigue Life of P/M Disk Superalloys

As the temperature capability of Ni-base superalloy powder metallurgy disks is steadily increased, environmental resistance and protection of advanced nickel-based turbine disk components are becoming increasingly important. Localized surface hot corrosion attack and damage from oxidation have been shown to impair disk fatigue life and may eventually limit disk operating temperatures. NASA Research Announcement (NRA) contracts have been awarded to GE Aviation and Honeywell Aerospace to separately develop fatigue resistant metallic and ceramic coatings for corrosion resistance and the corrosion/fatigue results of selected coatings will be presented. The microstructural response of a bare ME3 disk superalloy has been evaluated for moderate (704 C) and aggressive (760-816 C) oxidizing exposures up to 2,020 hours. Cross section analysis reveals sub-surface damage (significant for aggressive exposures) that consists of Al2O3 "fingers", interfacial voids, a recrystallized precipitate-free layer and GB carbide dissolution. The effects of a Nichrome corrosion coating on this microstructural response will also be presented.

Draper, Susan↗

Environmental exposure effects on composite materials for commercial aircraft

A study was conducted to determine the effects of long term flight and ground exposure on three commercially available graphite-epoxy material systems: T300/5208, T300/5209, and T300/934. Sets of specimens were exposed on commercial aircraft and ground racks for 1, 2, 3, 5, and 10 years. Inflight specimen sites included both the interior and exterior of aircraft based in Hawaii, Texas, and New Zealand. Ground racks were located at NASA-Dryden and the above mentioned states. Similar specimens were exposed to controlled lab conditions for up to 2 years. After each exposure, specimens were tested for residual strength and a dryout procedure was used to measure moisture content. Both room and high temperature residual strengths were measured and expressed as a pct. of the unexposed strength. Lab exposures included the effects of time alone, moisture, time on moist specimens, weatherometer, and simulated ground-air-ground cycling. Residual strengths of the long term specimens were compared with residual strengths of the lab specimens. Strength retention depended on the exposure condition and the material system. Results showed that composite materials can be successfully used on commercial aircraft if environmental effects are considered.

Hoffman, Daniel J.↗

Reproducible direct exposure environmental testing of metal-based magnetic media

A flow geometry and flow rate for mixed flowing gas testing is proposed. Use of an impinging jet of humid polluted air can provide a uniform and reproducible exposure of coupons of metal-based magnetic media. Numerical analysis of the fluid flow and mass transfer in such as system has shown that samples confined within a distance equal to the nozzle radius on the surface of impingement are uniformly accessible to pollutants in the impinging gas phase. The critical factor is the nozzle height above the surface of impingement. In particular, the uniformity of exposure is less than plus/minus 2% for a volumetric flow rate of 1600 cm(exp 3)/minute total flow with the following specifications: For a one inch nozzle, the height of the nozzle opening above the stage should be 0.177 inches; for a 2 inch nozzle - 0.390 inches. Not only is the distribution uniform, but one can calculate the maximum delivery rate of pollutants to the samples for comparison with the observed deterioration.

Sides, Paul J.↗

Retrospective dosimetry related to chronic environmental exposure

Radioactive contamination of the environment occurred in the early fifties as a result of the releases from the Mayak plutonium production complex (Southern Urals, Russia). The releases of liquid wastes into the Techa river resulted in chronic exposure of 30,000 residents of the riverside communities. Since 1951 90Sr body burdens have been measured for over half of this cohort. This paper presents the analysis of data on 90Sr in humans and describes the reconstruction of internal doses for these people.

NASA Discipline Radiation Health↗

Effects of environmental exposure on cryogenic thermal insulation materials

Investigation was made to optimize selection of insulation materials for reusable space vehicles which will be repeatedly operated over periods of up to ten years. Results of study are summarized in two reports. Volume I describes tests and significant findings. In Volume II, extensive test data obtained are organized in handbook form.

Parmley, R. T.↗

The effects of environmental exposure on reusable surface insulation for space shuttle

Coated specimens of reusable surface insulation (RSI) were exposed to alternate radiant heating and atmospheric exposure cycles to study the effects of surface contamination on the RSI coating. Different methods of heating were employed on clean and artificially contaminated specimens to determine the contributions of heating conditions to coating devitrification.

Ransone, P. O.↗

Environmental exposure effects on composite materials for commercial aircraft

Activities reported include completion of the program design tasks, resolution of a high fiber volume problem and resumption of specimen fabrication, fixture fabrication, and progress on the analysis methodology and definition of the typical aircraft environment. Program design activities including test specimens, specimen holding fixtures, flap-track fairing tailcones, and ground exposure racks were completed. The problem experienced in obtaining acceptable fiber volume fraction results on two of the selected graphite epoxy material systems was resolved with an alteration to the bagging procedure called out in BAC 5562. The revised bagging procedure, involving lower numbers of bleeder plies, produces acceptable results. All required laminates for the contract have now been laid up and cured. Progress in the area of analysis methodology has been centered about definition of the environment that a commercial transport aircraft undergoes. The selected methodology is analagous to fatigue life assessment.

Hoffman, D. J.↗

Environmental Exposure Effects on Composite Materials for Commercial Aircraft

This period's activities were highlighted by continued long term and accelerated lab exposure testing, and by completion of all fabrication tasks on the optional material systems, AS1/3501-6 and Kevlar 49/F161-188. Initial baseline testing was performed on the two optional material systems. Long term exposure specimens were returned from three of the four ground rack sites and from two of the three aircraft locations. Test data from specimens returned from Dryden after 2 years exposure do not indicate continuing trends of strength reduction from the 1 year data. Test data from specimens returned from the Wellington, new Zealand ground rack and on Air New Zealand aircraft after 1 year exposure show strength changes fairly typical of other locations.

Hoffman, D. J.↗

Fixture for environmental exposure of structural materials under compression load

A device for stressing a deformable material specimen consists of top plate and a bottom plate sandwiching a guide cylinder. The specimen is positioned on the bottom plate and attached to a load piston. Force is applied through the top plate into the guide cylinder. Once the specimen is loaded, the stress is maintained by tightening tie bolt nuts.

Clark, R. K.↗

Crack growth behavior of AISI-4340 steel during environmental exposure

AISI-4340 is observed to undergo stress corrosion cracking when subjected to a constant load during exposure to a 3.5% NaCl solution. Crack initiation, nucleation, and growth has been monitored as a function of time. Stepped regions consisting of fast and slow crack growth periods are shown to correspond to microstructural changes observed in the fracture surface of the steel. These regions of fast and slow crack rate variations with time show that the crack growth rates do not increase continuously with an increase in the stress intensity.

Giannuzzi, Lucille A.↗

MISSE PEACE Polymers: An International Space Station Environmental Exposure Experiment Being Conducted

As part of the Materials International Space Station Experiment (MISSE), 41 different polymers are being exposed for approximately 1 1/2 years to the low-Earth-orbit (LEO) environment on the exterior of the International Space Station. MISSE is a materials flight experiment sponsored by the Air Force Research Lab/Materials Lab and NASA, and is the first external experiment on the space station. A similar set of 41 polymers will be flown as part of the Polymer Erosion and Contamination Experiment (PEACE) a shuttle flight experiment that is being developed at the NASA Glenn Research Center collaboratively with the Hathaway Brown School for girls. Therefore, these 41 polymers are collectively called the MISSE PEACE Polymers. The purpose of the MISSE PEACE Polymers experiment is to determine how durable polymers are in the LEO space environment where spacecraft, such as the space station, orbit. Polymers are commonly used as spacecraft materials because of their desirable properties such as good flexibility, low density, and certain electrical properties or optical properties (such as a low solar absorptance and high thermal emittance). Two examples of the use of polymers on the exterior of spacecraft exposed to the space environment include metalized Teflon FEP (fluorinated ethylene propylene, DuPont) thermal control materials on the Hubble Space Telescope, and polyimide Kapton (DuPont) solar array blankets.

deGroh, Kim K.↗

Coatings for Oxidation and Hot Corrosion Protection of Disk Alloys

Increasing temperatures in aero gas turbines is resulting in oxidation and hot corrosion attack of turbine disks. Since disks are sensitive to low cycle fatigue (LCF), any environmental attack, and especially hot corrosion pitting, can potentially seriously degrade the life of the disk. Application of metallic coatings are one means of protecting disk alloys from this environmental attack. However, simply the presence of a metallic coating, even without environmental exposure, can degrade the LCF life of a disk alloy. Therefore, coatings must be designed which are not only resistant to oxidation and corrosion attack, but must not significantly degrade the LCF life of the alloy. Three different Ni-Cr coating compositions (29, 35.5, 45wt. Cr) were applied at two thicknesses by Plasma Enhanced Magnetron Sputtering (PEMS) to two similar Ni-based disk alloys. One coating also received a thin ZrO2 overcoat. The coated samples were also given a short oxidation exposure in a low PO2 environment to encourage chromia scale formation. Without further environmental exposure, the LCF life of the coated samples, evaluated at 760C, was less than that of uncoated samples. Hence, application of the coating alone degraded the LCF life of the disk alloy. Since shot peening is commonly employed to improve LCF life, the effect of shot peening the coated and uncoated surface was also evaluated. For all cases, shot peening improved the LCF life of the coated samples. Coated and uncoated samples were shot peened and given environmental exposures consisting of 500 hrs of oxidation followed by 50 hrs of hot corrosion, both at 760C). The high-Cr coating showed the best LCF life after the environmental exposures. Results of the LCF testing and post-test characterization of the various coatings will be presented and future research directions discussed.

LCF life↗