Capacity Fade of Graphite/NMC811: Influence of Particle Morphology, Electrolyte, and Charge Voltage

LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) is an important Li-ion battery cathode material; however, there is a tradeoff between delivered capacity and capacity retention. As the charge potential increases the capacity rises but at the expense of capacity retention. The decrease in capacity retention has been ascribed to several factors including particle cracking, surface reconstruction, transition metal dissolution, and electrolyte reactivity. The present study compares 4.1 and 4.3 V charging limits in commercially relevant graphite/NMC811 pouch cells for single crystal (SC) and polycrystalline (PC) NMC811 with ethylene carbonate (EC)-containing or EC-free electrolytes. The electrochemistry is rationalized through analysis of electrochemical impedance spectroscopy, positive electrode X-ray photoelectron spectroscopy, soft X-ray absorption spectroscopy, X-ray diffraction, and negative electrode mapping by X-ray fluorescence. Graphite/SC-NMC811 cells show high-capacity retention at 4.1 V but exhibit degradation at 4.3 V charging potentials. The EC-free electrolyte cells led to higher capacity fade, especially when charged to 4.3 V. Cathode dissolution and deposition on the negative electrode from PC-NMC811 cells was higher than for samples from SC-NMC811 cells. This study reveals the impact of material type, charge voltage, and electrolyte composition on the reactions at the positive electrode, their influence on the negative electrode, and evolution with cycle number.

36 MATERIALS SCIENCE↗

Dynamically Stable Active Sites from Surface Evolution of Perovskite Materials during the Oxygen Evolution Reaction

Perovskite oxides are an important class of oxygen evolution reaction (OER) catalysts in alkaline media, despite the elusive nature of their active sites. In this work, we demonstrate that the origin of the OER activity in a La 1-x SrxCoO 3 model perovskite arises from a thin surface layer of Co hydr(oxy)oxide (CoO x H y ) that interacts with trace-level Fe species present in the electrolyte, creating dynamically stable active sites. Generation of the hydr(oxy)oxide layer is a consequence of a surface evolution process driven by the A-site dissolution and O-vacancy creation. In turn, this imparts a 10-fold improvement in stability against Co dissolution and a 3-fold increase in the activity-stability factor for CoO x H y / LSCO when compared to nanoscale Co-hydr(oxy)oxides clusters. Our results suggest new design rules for active and stable perovskite oxide-based OER materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

NASNF Processing and Packaging Technical Study

The ABD program will require development of a strategy for the dispositioning the Non-Aluminum Spent Nuclear Fuel (NASNF), some of which will be very challenging to handle and dissolve as described in this report. Not all the NASNF is suitable for processing through the electrolytic dissolver. The strategy may involve dissolution of the majority of the NASNF inventory in the electrolytic dissolver combined with some other disposition alternative(s) for the fraction that is not suitable for electrolytic dissolution. This report highlights the risks and challenges associated with the baseline approach of using the electrolytic dissolver to process all of the NASNF. In addition, the characteristics of the NASNF and how those characteristics relate to the risks associated with electrolytically dissolving the specific fuel types.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nanoscale Compositional Mapping of Commercial LiNi 0.8 Co 0.15 Al 0.05 O 2 Cathodes Using Atom Probe Tomography

Nickel-rich cathodes provide improved specific capacity that lead to higher gravimetric energy density, critical for electric vehicles. However, poor long-term capacity retention at elevated temperatures/high C-rates (the rate of charge and discharge on a battery) stem from material issues: surface phase changes, corrosive side reactions with the electrolyte, ion dissolution and propagation of cracks. Introducing dopants, developing nanoscale surface coatings and graded core-shell structures have all improved the electrochemical performance of nickel-rich cathodes. However, a material level understanding on the effect of Li composition and distribution in Ni-rich cathodes is limited, due to a lack of characterization methods available that can directly image Li at the nanoscale. Hence, it is critical to establish methods such as atom probe tomography (APT), having both nanometer scale spatial resolution and high compositional sensitivity to quantitatively analyze battery cathodes. To fully realize its potential as a method for quantitative compositional analysis of commercial Li-ion batteries, we provide a comprehensive description of the challenges in sample preparation and analyze the dependency of the analysis parameters, specifically laser pulse energy on the measured stoichiometry of elements in a high Ni content cathode material; LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA). In this work, our findings show the stoichiometry variations cannot be explained by charge state ratios or Ga implantation damage alone during FIB preparation, indicating that additional factors such as crystallographic orientation may need to be considered to achieve quantitative nanoscale compositional analysis of such battery cathodes using APT.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Failure Modes of Platinized pn+-GaInP Photocathodes for Solar-Driven H2 Evolution

The long-term stability for the hydrogen-evolution reaction (HER) of homojunction pn+-Ga0.52In0.48P photocathodes (band gap = 1.8 eV) with an electrodeposited Pt catalyst (pn+-GaInP/Pt) has been systematically evaluated in both acidic and alkaline electrolytes. Electrode dissolution during chronoamperometry was correlated with changes over time in the current density-potential (J-E) behavior to reveal the underlying failure mechanism. Pristine pn+-GaInP/Pt photocathodes yielded an open-circuit photopotential (Eoc) as positive as >1.0 V vs the potential of the reversible hydrogen electrode (RHE) and a light-limited current density (Jph) of >12 mA cm-2 (1-sun illumination). However, Eoc and Jph gradually degraded at either pH 0 or pH 14. The performance degradation was attributed to three different failure modes: (1) gradual thinning of the n+-emitter layer due to GaInP dissolution in acid; (2) active corrosion of the underlying GaAs substrate at positive potentials causing delamination of the upper GaInP epilayers; and (3) direct GaAs/electrolyte contact compromising the operational stability of the device. This work reveals the importance of both substrate stability and structural integrity of integrated photoelectrodes toward stable solar fuel generation.

CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSICS,S↗

Reaction Mechanism of Electrodeposited ε-MnO 2 : A Proton-Centered Pathway in Aqueous Zn-Ion Systems

Aqueous Zn/MnO 2 batteries have garnered significant interests owing to their abundance, high theoretical specific capacity, safety, and low cost. However, large-scale application of these systems is limited by the incomplete understanding of the MnO 2 reaction chemistry. The different crystal lattice structures among MnO 2 polymorphs contribute to the variations in reported reaction mechanisms. Among them, ε-MnO 2 polymorph, the dominant phase in electrolytic manganese dioxide (EMD), is notably observed during the charge cycles of aqueous Zn/MnO 2 batteries. Here, in this work, we investigate the electrochemical behavior of an ε-MnO 2 cathode synthesized via electrodeposition from a ZnSO 4 and MnSO 4 electrolyte, onto a 3-dimensional carbon cloth substrate. Proton intercalation emerges as the dominant charge storage mechanism, critically enabling the reversibility of ε-MnO 2 during cycling, as revealed by operando synchrotron X-ray diffraction and X-ray absorption spectroscopy. Additionally, a proton-coupled dissolution/redeposition pathway operates alongside minor Zn 2+ intercalation, as quantified by Rietveld refinement. Morphological and chemical heterogeneities are studied by transmission X-ray microscopy further validates this reaction mechanism. These mechanistic insights provide the foundation for rationally designing Zn/MnO 2 batteries with optimized proton dynamics and charge transfer, advancing these systems as a viable solution for safe, cost-effective grid-scale energy storage.

36 MATERIALS SCIENCE↗

Multimodal In Situ Characterization Uncovers Unexpected Stability of a Cobalt Electrocatalyst for Acidic Sustainable Energy Technologies

An accelerated development of durable and affordable sustainable energy technologies is often hindered by a limited understanding of how non-precious materials within these systems degrade. In acidic proton exchange membrane fuel cells and water electrolyzers, metallic cobalt (Co) is considered an unstable component that is often combined with precious metals or other stabilizers. To understand the mechanisms behind Co instability, we employ an experimental platform that quantifies dissolution with on-line inductively coupled plasma mass spectrometry and product formation with electrochemical mass spectrometry during electrochemical testing, along with ex- situ characterization. Under varied conditions (electrocatalysis, time, gas-type saturation, and ion concentration), windows of Co stability are observed that are different than predicted with classical chemical thermodynamics, suggesting new stabilization and degradation mechanisms than previously understood. Notably, Co is active for the hydrogen evolution reaction (HER), with prolonged stability that is ~300 mV different than thermodynamically projected. Additionally, in an oxygenated environment, Co concurrently performs the HER and oxygen reduction reaction (ORR) yet undergoes different morphology changes and dissolution mechanisms. Interestingly, in the absence of electrocatalysis, there is a 22x decrease in dissolution in an oxygen-free environment, proposing a route to decrease Co losses during device shutdown protocols. Lastly, under more extreme operating conditions, Co becomes stable after a substantial amount of dissolution, suggesting that high concentrations of Co 2+ ions in the microenvironment induce the formation of a stable CoHO 2 surface. Altogether, these results can be leveraged to improve the design and development of more robust and cost-effective sustainable energy technologies, as well as promote strategic strategies for prolonged material utilization.

Dissolution↗

Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li + ) and operating temperature (25 °C and 60 °C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiO x formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiO x formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiO x phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiO x phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiO x phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.

electrochemical impedance spectroscopy↗

Effects of surface charge and cluster size on the electrochemical dissolution of platinum nanoparticles using COMB3 and continuum electrolyte models

We study the site-dependent dissolution of platinum nanoparticles under electrochemical conditions to assess their thermodynamic stability as a function of shape and size using empirical molecular dynamics and electronic-structure models. The third-generation charge optimized many-body potential is employed to determine the validity of uniform spherical representations of the nanoparticles in predicting dissolution potentials (the Kelvin model). To understand the early stages of catalyst dissolution, implicit solvation techniques based on the self-consistent continuum solvation method are applied. It is demonstrated that interfacial charge and polarization can shift the dissolution energies by amounts on the order of 0.74 eV depending on the surface site and nanoparticle shape, leading to the unexpected preferential removal of platinum cations from highly coordinated sites in some cases.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lithium oxidation and electrolyte decomposition at Li-metal/liquid electrolyte interfaces

In this work, we examine the evolution of events occurring when a Li metal surface is in contact with a 2 M solution of a Li salt in a solvent or mixture of solvents, via classical molecular dynamics simulations with a reactive force field allowing bond breaking and bond forming. The main events include Li oxidation and electrolyte reduction along with expansion of the Li surface layers forming a porous phase that is the basis for the formation of the solid-electrolyte interphase (SEI) components. Nucleation of the main SEI components (LiF, Li oxides, and some organics) is characterized. The analysis clearly reveals the details of these physical–chemical events as a function of time, during 20 nanoseconds. The effects of the chemistry of the electrolyte on Li oxidation and dissolution in the liquid electrolyte, and SEI nucleation and structure are identified by testing two salts: LiPF 6 and LiCF 3 SO 3 , and various solvents including ethers and carbonates and mixtures of them. The kinetics and thermodynamics of Li 6 F, the core nuclei in the LiF crystal, are studied by analysis of the MD trajectories, and via density functional theory calculations respectively. The SEI formed in this computational experiment is the “native” film that would form upon contact of the Li foil with the liquid electrolyte. As such, this work is the first in a series of computational experiments that will help elucidate the intricate interphase layer formed during battery cycling using metal anodes.

25 ENERGY STORAGE↗

Employing the Dynamics of the Electrochemical Interface in Aqueous Zinc-Ion Battery Cathodes

Intrinsically stable materials are desirable for constructing energy storage devices, which aim to demonstrate durability under the harsh electrochemical conditions that are detrimental to their lifespan. However, in this study it is demonstrated that the intrinsic instability of an electrochemical interface can be converted from an obstacle into an advantage. In aqueous zinc-ion batteries, manganese oxide (MnO 2 ) exhibits considerable dissolution even in electrolyte containing Mn 2+ salt. Balancing with redeposition alleviates the harmful impact of dissolution on performance and alters the trajectory of the active phase. Inclusion of Mn 2+ salt in the electrolyte induces MnO 2 deposition on all conductive surfaces, requiring that distracting side reactions be eliminated to isolate the dynamics of the active phase. Under conditions favoring dissolution, capacity decreases dramatically and a highly crystalline tetragonal ZnMn 2 O 4 phase forms, while redeposition helps maintain capacity and promotes a disordered cubic Zn-rich phase. Ultimately, this work aims to illuminate a path forward to unlock the potential of batteries made with materials that are fundamentally unstable in their operating environment.

25 ENERGY STORAGE↗

Stabilizing Zinc Anode Reactions by Polyethylene Oxide Polymer in Mild Aqueous Electrolytes

Abstract Zn dendrites growth and poor cycling stability are significant challenges for rechargeable aqueous Zn batteries. Zn metal deposition‐dissolution in aqueous electrolytes is typically determined by Zn anode–electrolyte interfaces. In this work, the role of a long‐chain polyethylene oxide (PEO) polymer as a multifunctional electrolyte additive in stabilizing Zn metal anodes is reported. PEO molecules suppress Zn 2+ ion transfer kinetics and regulate Zn 2+ ion concentration in the vicinity of Zn anodes through interactions between ether groups of PEO and Zn 2+ ions. The suppressed Zn 2+ ion transfer kinetics and homogeneous Zn 2+ ion distribution at the interface promotes dendrite‐free homogeneous Zn deposition. In addition, electrochemically inert PEO molecules adsorbed onto Zn anodes can protect the anode surfaces from H 2 generation and, thereby, enhance their electrochemical stability. Stable cycling over 3000 h and high reversibility (Coulombic efficiency > 99.5%) of Zn anodes is demonstrated in 1 m ZnSO 4 electrolyte with 0.5 wt% PEO. This finding provides helpful insights into the mechanism of Zn metal anodes stabilization by low‐cost multifunctional polymer electrolyte additives that stabilize interfacial reactions.

Jin, Yan↗

Dissolution and initial hydration behavior of tricalcium aluminate in low activity sulfate solutions

Influences of alkali or alkaline earth sulfates on the hydration of cubic tricalcium aluminate (C 3 A) were evaluated by in situ dissolution rate measurements, by ex situ near-surface composition measurements with secondary ion mass spectrometry, and by in situ synchrotron X-ray diffraction to monitor precipitation of hydration products. Both slight reductions in dissolution rate and cation-specific interactions with the solid were observed. The near-surface Ca/Al ratio is significantly lower after some dissolution and the electrolyte cations are incorporated within the surface with different affinities (Mg 2+ > K + > Na + ). An interfacial dissolution-reprecipitation mechanism may explain the observations as well as, or better than, a simple cation exchange. The sulfate concentration in solution affects the rates of both C 3 A dissolution and precipitation of hydration products. Aditionally, sulfate ions likely adsorb at the hydrous Al-rich surface layer, thereby reducing the dissolution rate of aluminates and delaying the precipitation of aluminate hydration products.

36 MATERIALS SCIENCE↗

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE↗

Spectroscopic Insight on Neodymium Solvation in Lithium Borohydride-Supported Electrolyte

Borohydride-based electrolytes have recently emerged as promising media for the electrodeposition of electropositive metals, including rare earth (RE) elements. While the presence of supporting alkali metal cations and RE counteranions provides essential electrochemical conductivity for achieving fast metal electrodeposition, interactions between the host ligand and solvated neodymium (Nd) complexes remain unclear. This study provides insights into the coordination structure of a concentrated and directly solvated Nd salt in a lithium borohydride-supported electrolyte. Our spectroscopic results indicate that the RE coordination environment is significantly influenced by the solvation mechanism, which can vary between metathesis and complexation pathways, primarily dictated by stoichiometric factors. Under dilute conditions, nearly complete metathesis of anions leads to a high coordination number for the host ligand (borohydride), consistent with the previously reported solvated Nd speciation in chlorine-free electrolytes. In contrast, concentrated dissolution of the Nd salt in the supported electrolyte is dominated by a complexation pathway featuring a Li-ion-paired complex with a low coordination number of the host ligand. Density functional theory (DFT) calculations indicated that the observed blue shift in the borohydride vibration was the result of an increase in electron density drawn into the terminal B–H interbond region from the hydride as the coordination changed from Li to Nd. In conjunction with DFT results, vibrational analyses allowed correlation of the experimental shifts associated with changes in Nd ligation and coordination spheres, further consolidating the prevalence of highly chloride-coordinated species under concentrated conditions. In conclusion, the outcomes of this work illuminate the distinctive and heterogeneous coordination structures that the electroactive RE species can adopt at high concentrations in lithium borohydride-supported electrolytes, as a key step to comprehend the reported metal electrodeposition performance in these media.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗