Search NASA⌕ Search

SEARCH · Search NASA

Results for “FUEL CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Milestone 1.2.11: H 2 Production from Surrogate Non-Native Corrosion Plumes on Aluminum 6061-T6 Fuel Cladding Surrogates

Thick, localized, “non-native” corrosion plumes have been identified on Advanced Test Reactor fuel elements, raising concern on their impact on the radiolytic formation of molecular hydrogen gas (H 2 ) from aluminum-clad spent nuclear fuel (ASNF) under proposed extended (> 50 years) dry storage conditions. Here, we report our findings on H 2 generation from the gamma irradiation (up to 52 MGy) of surrogate “non-native” corrosion plume coupons: ambient-temperature-corroded (~350 days in water) aluminum alloy 6061 (AA6061) coupons in helium gas environments with ~0% added relative humidity. Additionally, we provide a comparison of proposed ASNF drying techniques— vacuum drying only, vacuum drying + 100 °C for 4 hr, and vacuum drying + 220 °C for 4 hr—on the yield of H 2 from these surrogate systems. The presented data indicates that similar amounts of H 2 (~2 × 10–3 µmol J–1) are formed from gamma irradiated AA6061 coupons corroded under different temperature regimes, i.e., ambient/350 days vs. 90 C/30 days. These findings validate current, complimentary modelling predictions based on high-temperature-corrosion irradiation data only. Further, the application of a heat treatment procedure (100 and 220 °C), in conjunction with vacuum drying, accelerated the rate at which a steady-state H 2 yield was attained, in comparison to vacuum only, due to the removal of H 2 precursors in the form of adsorbed waters. Interestingly, within the confidence limits of our measurements, negligible difference in total H 2 yield was found between the two investigated heat treatment procedures.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Cold Spray Deposition of 304L Stainless Steel to Mitigate Chloride-Induced Stress Corrosion Cracking in Canisters for Used Nuclear Fuel Storage

A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.

Dry Cask Storage Systems, cold spray, 304L stainle↗

Large Plate Experiment of Chloride-induced Stress Corrosion Cracking in Spent Nuclear Fuel Storage Canisters

This report is the comprehensive description of the completed experiment to evaluate the corrosion behavior of a large section of welded plate material harvested from the Sandia National Laboratories’ (SNL) full-size mockup of a spent nuclear fuel (SNF) dry storage canister. The plate was subjected to conditions aggressive to chloride-induced stress corrosion cracking for a total time of 2 years. The details of the establishment of this experiment, and the corrosion results are reported. This work is intended to inform aging management programs for SNF canisters under conditions of extended dry storage.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Large Plate Experiment of Chloride-induced Stress Corrosion Cracking in Spent Nuclear Fuel Storage Canisters

This report provides a description of the testing (in progress at the Savannah River National Laboratory) to evaluate the corrosion behavior of a large section of welded plate material harvested from the Sandia National Laboratories’ full-size mockup of a spent nuclear fuel (SNF) dry storage canister. The details of the establishment of this plate test, the interim corrosion results (from visual examination), and the general plan for examination of the plate in CY21 to evaluate crack growth behavior (if any) are provided. This work is intended to inform aging management programs for SNF canisters under conditions of extended dry storage. A “large plate” (approximately 51 x 46 cm with thickness 16 mm and weight about 30 kg) and containing a circumferential weldment from the mockup is the test specimen. The knowledge of the salt, temperature, humidity conditions for chloride-induced stress corrosion cracking (CISCC) including the threshold stress intensity factor, K iscc , were used to setup the large plate test in which a set of part-through-wall and through-wall electrical discharge machined (EDM) defects were positioned in the weld residual stress field of the welded plate material from the mockup canister. A marine salt solution was applied to this plate specimen with an air-brush spray, then dried, and then exposed to a sustained 71-73% RH condition at an ambient room temperature of 22 °C. The salt loading and environmental condition is expected to be aggressive to cause CISCC

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion of Ferrous Structural Alloys in Biomass Derived Fuels and Organic Acids

This work investigated the corrosivity of biomass-derived liquid fuels and organic acids associated with bio-oils and conducted a corrosion compatibility evaluation of several structural ferrous alloys in the fuels and acids. Here, the acidity parameters and solution conductivity values were higher in raw pyrolysis bio-oils than postprocessed oils with significant corrosion attack for carbon steel and Fe-2.25Cr-1Mo. However, higher-grade stainless steels, ferritic Fe-15Cr (15Cb) and austenitic types 304L and 316L, showed negligible corrosion loss, whereas lower-Cr ferritic grades 409, 410, and 416 were attacked. Metal leaching tests and electrochemical impedance spectroscopy measurements revealed superior corrosion resistance of 316 over 410 stainless steels in solutions of formic and oxalic acids that can be present in bio-oils. The corrosion evaluation methods utilized in this work provide effective screening tools to identify the compatible structural alloys for bio-oils.

09 BIOMASS FUELS↗

Preliminary Modeling of Chloride Deposition on Spent Nuclear Fuel Canisters in Dry Storage Relevant to Stress Corrosion Cracking

This study presents a method that can be used to gain information relevant to determining the corrosion risk for spent nuclear fuel (SNF) canisters during extended dry storage. Currently, it is known that stainless steel canisters are susceptible to chloride-induced stress corrosion cracking (CISCC). However, the rate of CISCC degradation and the likelihood that it could lead to a through-wall crack is unknown. This study uses well-developed computational fluid dynamics and particle-tracking tools and applies them to SNF storage to determine the rate of deposition on canisters. The deposition rate is determined for a vertical canister system and a horizontal canister system, at various decay heat rates with a uniform particle size distribution, ranging from 0.25 to 25 µm, used as an input. In all cases, most of the dust entering the overpack passed through without depositing. Most of what was retained in the overpack was deposited on overpack surfaces (e.g., inlet and outlet vents); only a small fraction was deposited on the canister itself. These results are provided for generalized canister systems with a generalized input; as such, this paper is intended to demonstrate the technique. This study is a part of an ongoing effort funded by the U.S. Department of Energy, Nuclear Energy Office of Spent Fuel Waste Science and Technology, which is tasked with doing research relevant to developing a sound technical basis for ensuring the safe extended storage and subsequent transport of SNF. This work is being presented to demonstrate a potentially useful technique for SNF canister vendors, utilities, regulators, and stakeholders to utilize and further develop for their own designs and site-specific studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

M4SF-20LL010302042: Process Model for Radionuclide Incorporation into Corrosion Products

This progress report (Level 4 Milestone Number M4SF-20LL010302042) summarizes research conducted at Lawrence Livermore National Laboratory (LLNL) within the Crystalline Activity Number SF-20LL010302041. The research is focused on actinide and radionuclide sequestration in steel corrosion products. Fuel matrix degradation models suggest that the near field is likely to be reducing at the time of canister breaching, steel corrosion, and radionuclide release, but more oxidizing conditions may prevail in the far field. The incorporation of radionuclides into corrosion phases may limit the rate of radionuclide release by sequestering a portion of the radionuclide source term. For these reasons there is a need to evaluate the incorporation of Pu and other radionuclides into various Fe-oxide phases, and to understand the behavior of coprecipitated phases during mineral recrystallization processes and during re-oxidation events. Radionuclide coprecipitation with Fe minerals may impact long-term repository performance and is an ongoing research focus at Lawrence Livermore National Laboratory.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Steel Corrosion Impacts on Radionuclide Immobilization

This progress report (Level 4 Milestone Number M4SF-21LL010302052) summarizes research conducted at Lawrence Livermore National Laboratory (LLNL) within the Crystalline Activity Number SF-21LL01030205. The research is focused on actinide and radionuclide sequestration in steel corrosion products. Fuel matrix degradation models suggest that the near field is likely to be reducing at the time of canister breaching, steel corrosion, and radionuclide release, but more oxidizing conditions may prevail in the far field. The incorporation of radionuclides into corrosion phases may limit the rate of radionuclide release by sequestering a portion of the radionuclide source term. For these reasons there is a need to evaluate the incorporation of Pu and other radionuclides into various Fe-oxide phases, and to understand the behavior of coprecipitated phases during mineral recrystallization processes and during re-oxidation events. Radionuclide coprecipitation with Fe minerals may impact long-term repository performance and is an ongoing research focus at Lawrence Livermore National Laboratory.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Review and Summary of Corrosion Behavior for Aluminum-Clad Spent Nuclear Fuel in Dry Storage

A description of the corrosion behavior of aluminum alloys used for cladding on aluminum-based, aluminum-clad nuclear fuel used in research reactors under potential dry storage conditions has been compiled. An evaluation is made of potential additional corrosion with water postulated to not be removed during drying. The relative humidity (RH) produced by typical dryness criteria for industrial spent nuclear fuel drying is expected to be low, particularly at high temperatures (17% RH at 20°C and lower at higher temperatures). Existing corrosion data suggests that negligible vapor-phase corrosion of aluminum is expected at such low humidity, even for nominally bare aluminum surfaces. That is, the predicted relative humidity from free water (e.g., 17% RH) is below the “critical” relative humidity (~40% RH at room temperature), below which no significant corrosion is observed for bare aluminum. Furthermore, reported room-temperature corrosion rates are very low even under saturated (100% RH) water vapor. Existing results showing significant vapor-phase corrosion corresponded specifically to conditions of high temper ed with high relative humidity. A relatively large reservoir of (chemically bound) water exists in the aluminum (oxy)hydroxide films on the SNF cladding surface. The estimated total could saturate the gas even at relatively high temperature if fully released; however, its release as molecular water is expected to only be plausible if the temperature during storage exceeds both the drying temperature and the threshold for thermal decomposition of the trihydroxides (~220°C). Therefore, the combination of high temperature and high relative humidity that could drive significant corrosion is considered implausible during sealed dry storage following an appropriate drying process, to include >220°C drying for canisters that may approach or exceed this temperature during storage. Vapor-phase testing of aluminum samples with an adherent (oxy)hydroxide layer, prepared in liquid water to resemble those on actual aluminum-clad spent nuclear fuel (ASNF), did not observe evidence of additional corrosion even at combined high-temperature (up to 180°C) and high-humidity (up to 100% RH) conditions. Instead, small net mass losses were observed for most specimens and attributed to dehydration of the samples, which had been air-dried only prior to testing. ASNF being moved to dry storage is expected to have an existing (oxy)hydroxide film, suggesting that the cladding will be less prone to additional corrosion than bare aluminum metal. If significant corrosion did occur during sealed storage, the overall extent and impact is expected to be small. Corrosion post-closure of a canister would not alter the total amount of hydrogen in the canister, so it would have no effect on the maximum H 2 release already assessed in existing bounding calculations. In addition, the total amount of water in a 25-µm dense bayerite film would consume a only ~8 µm additional aluminum metal on average, if fully consumed by oxidizing aluminum metal to Al 2 O 3 . These conclusions are consistent with ASNF-in-canister simulations to date, which included a reaction pathway for corrosion using kinetics from previous literature and believed to be conservative and predicted very low rates of corrosion.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Determination of Molecular Structure and Dynamics of Molten Salts by Advanced Neutron and X-ray Scattering Measurements and Computer Modeling

The design and development of fully functional Molten-Salt Reactors (MSR) require detailed knowledge of the molten salt properties in order to understand and predict the salt’s behavior. Fundamental properties of interest include molecular structure, speciation, and dynamics (such as diffusion coefficients) of salt components and dissolved corrosion and fission products. Computer modeling is necessary to predict changes in physical and chemical properties due to irradiation, burning of dissolved fuel, and corrosion. The modeling requires experimental data, and advanced neutron and x-ray scattering and spectroscopy provide the most reliable and direct determination of the structure (Pair-Distribution Functions, PDF), and dynamics of ions in the melt. This project dealt with both fluoride and chloride salts. The PDFs have been measured by a combination of neutron and x-ray diffraction. We utilized the techniques of isotope substitutions, a very powerful tool available for neutron-scattering, to extract the details of the liquid structure. Although similar measurements have been done before, modern advanced neutron and x-ray-scattering techniques allow collecting the data at much higher resolution and in a wider range of temperatures. Importantly, we were among the first to study fluoride salts by neutron scattering. The importance of impurities and their effects on salt properties have become apparent recently and so new methods of salt purification were developed. We took advantage of these developments to produce reliable data, which have been used for computer simulations of both clean salts and those with added fission and corrosion products most relevant for MSRs. Ab initio molecular dynamics simulations have been performed to understand the multi-component liquid solution, in particular solubility of impurities and thermodynamic interactions in relation to the ionic-cluster structure of the fluid. We applied machine learning to regress from the simulation and experimental data in order to develop a fast-acting model that can handle molten salt with an arbitrary (≥ 10) number of chemical elements and be able to predict chemical potential as a function of composition and temperature. This project resulted in a number of experimental and computer-simulation publications, a patent application, and numerous conference presentations (American Physical Society, American Chemical Society, and The Electrochemical Society among others). Multiple students and postdocs participated and collaborated on aspects of this project. This project seeded new collaborations between MIT and other institutions, such as the University of Massachusetts Lowell, the University of Illinois Urbana-Champaign, the University of California Berkeley, and Oak Ridge and Los Alamos National Labs. As such, this project has had a broad and lasting impact beyond its original scientific scope.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

L-Basin microbial monitoring program - evaluation of 20 years of monitoring

This report summarizes the results from over 20-years’ of activities for microbial monitoring of the bulk water, floc analysis, and test coupon surfaces for the Savannah River Site L Basin. The Microbial Monitoring Program provides important information for the characterization of overall water quality as it impacts the continued safe storage of spent nuclear fuel in L Basin. The potential impacts to fuel storage are: 1) microbial-influenced corrosion of the fuel; and 2) biofouling of the fuel storage systems.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Role of microstructure on CO corrosion of SiC layer in UO₂-TRISO fuel

The Advanced Gas Reactor Fuel Qualification and Development (AGR) program has focused on qualification of UCO kernel tristructural-isotropic (TRISO) particle fuel relative to UO₂ kernel TRISO particle fuel. However, a UO₂ kernel variant was included in the second AGR irradiation experiment (AGR-2) for comparison and to connect to historic fuel irradiation data. The development of a multiscale, post-irradiation examination (PIE) analysis approach through the AGR Program has allowed for a comprehensive understanding of individual particle failure. This approach has been applied to gain an understanding of SiC layer failure in UO₂ kernel TRISO fuel from AGR-2 after safety testing at 1600–1700 °C. Particle failure by intergranular CO corrosion, facilitated by a compromised inner pyrolytic carbon layer, has been confirmed through the combined application of modern x-ray computed tomography and electron microscopy techniques. In addition, a relationship between grain boundary character and CO corrosion has been identified. This finding provides an opportunity to develop mitigating strategies to improve the resilience of the SiC layer to CO corrosion in UO₂ TRISO fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

(Project 18-15531) Repair and Mitigation of Chloride-Induced Pitting and Chloride-Induced Stress Corrosion Cracking in Used Spent Nuclear Fuel Dry Cask Canister Materials (Final Technical Report)

Several experimental techniques were utilized to understand the corrosion and SCC performance of possible techniques for repairing cracks and pits in SS304 utilized for dry cask storage of spent nuclear fuel. The repairs examined included cold spray, FSW, soldering, and VFAW. The corrosion and SCC assessment techniques utilized for comparing repairs against the base material were 4-pt bending SCC testing in boiling MgCl 2 at stress levels between 0 MPa and 350 MPa, immersion testing in 40% RH brine solution meant to mimic a service-like environment, SSRT SCC testing in 40% RH brine solution. For FSW alone, scanning electrochemical cell microscopy and microelectrochemical syringe cell were utilized to understand the corrosion performance across the weld, in the retreating/advancing sides, and base material. Based on the results of this study, the FSW and cold spray repair techniques proved most viable for SCC repair in SS304 dry cask storage applications and continuing research is highly recommended to understand and quantify in further detail their SCC performance compared to unrepaired SS304. Additionally, solder and VFAW (patch or incline) would not be recommended based on the corrosion and SCC findings in this study.

42 ENGINEERING↗