Miniature Beryllium Split-Hopkinson Pressure Bars for Extending the Range of Achievable Strain-Rates

Conventional Split Hopkinson Pressure Bars (SHPB) or “Kolsky” bars are often used for determining the high-rate compressive yield and failure strength of materials. However, for experiments generating very high strain-rates (>10 3 /s) miniaturization of the setup is often required for minimizing the effects of elastic wave dispersion in order to enable the inference of decreasingly short loading events from the data. Miniature aluminum and steel bars are often sufficient for meeting these requirements. However, for high enough strain-rates, miniaturization of steel or aluminum Kolsky bars may require prohibitively small diameter bars and test specimens that could become inappropriate for inferring representative properties of materials with large grain size relative to the test specimen size. The use of a beryllium Kolsky bar setup is expected to enable high rates to be accessible with larger diameter bars/specimen combinations due to the inherent physical properties of beryllium, which are expected to minimize the effects of elastic wave dispersion. For this reason, a series of beryllium Kolsky bars have been developed, and, in this paper, the dispersion characteristics of these bars are measured and compare the data with those of similarly sized 7075-T6 aluminum and C350 maraging steel. The results, which agree well with the theory, show no appreciable frequency dependence of the elastic wavespeed in the data from the beryllium bars, demonstrating its advantage over aluminum and steel in application to Kolsky bars.

36 MATERIALS SCIENCE↗

Anisotropic thermal-conductivity degradation in the phase-field method accounting for crack directionality

Dynamic loads applied to metals may lead to brittle or ductile fracture depending on the imposed strain rates, material properties, and specimen geometry. With an increase in the applied velocity, brittle to ductile failure mode transition may also be observed. Furthermore, at high strain rates, ductile fracture may be preceded by shear bands, which are narrow bands of intense plastic deformation, typically accompanied by a significant rise in temperature. Reliable models are needed to predict the response of metals subject to dynamic loads. In particular, capturing the interplay between heat conduction and crack propagation using the phase-field fracture method is still an open research field. To accurately capture the heat transfer physics across crack surfaces, damage models degrading thermal-conductivity are necessary. While isotropic thermal-conductivity degradation models were proposed, they may lead to errors as they are indifferent to crack directionality. In our current work, a new anisotropic approach is proposed in which thermal-conductivity, which depends on the phase-field gradient, is degraded solely across the crack. Here, it is shown that this approach improves the near-field approximation of temperature and heat flux compared with isotropic degradation, when taking the discontinuous crack solutions as reference. Additionally, the anisotropic degradation approach is implemented in a unified dynamic fracture model and a couple of examples demonstrate the viability of this approach.

42 ENGINEERING↗

Hydrogen-enhanced compatibility constraint for intergranular failure in FCC FeNiCoCrMn high-entropy alloy

The fundamental mechanism of hydrogen embrittlement was investigated in the high-entropy alloy FeNiCoCrMn using slow strain rate tensile tests with and without internal hydrogen. Hydrogen induced intergranular failure and reduced the average grain elongation parallel to the tensile axis, but also increased the local plasticity within grains. Here, the influence of hydrogen on plasticity establishes a compatibility constraint across grain boundaries, which results in failure along the hydrogen-weakened grain boundaries. This study is the first to directly confirm the presence of the hydrogen-enhanced compatibility constraint in a high-entropy alloy and highlights the importance of developing a physical understanding of grain-scale interactions.

36 MATERIALS SCIENCE↗

Neutron Diffraction Analysis of Residual Strain in High-Pressure Die Cast A383 Engine Blocks

The residual strains in three high-pressure die cast A383 engine blocks were measured using neutron diffraction. Residual strains and stresses can be generated during high-pressure die casting process due to high thermal gradients and may cause fatigue failure or dimensional distortion. Neutron diffraction can measure the residual strain distributions deep inside castings with complex geometries, because neutrons can penetrate substantially more material than x-rays. In this paper, the residual strains (in the axial and hoop directions) along the whole cylinder bridge of high-pressure die cast A383 engine blocks in as-cast and heat-treated conditions were measured by neutron diffraction methods. The effect of heat treatment on the distribution and magnitude of residual strains was also investigated. The results indicate that the residual strain in the cylinder bridge is tensile in both the axial and hoop components for both the as-cast and the heat-treated engine blocks. The residual strain in the hoop direction is bigger in magnitude than the residual strain in the axial direction. Heat treatment significantly relaxes the residual strain in the axial direction but only slightly relaxes the residual strain in the hoop direction.

36 MATERIALS SCIENCE↗

Effect of local structure and stoichiometry on the dynamic behavior of bi-metal interfaces

Molecular dynamics (MD) simulations are performed to investigate the failure behavior of Al/Al, Al/Fe, and Al/AlFe bi-layers under high strain-rate shock loading. Additional simulations are performed to invesigate solely the tensile response of these systems and to isolate the effects of loading history on damage and failure. Specifically, the compression stage of the shock is excluded from the tensile simulations. This study shows that local structure variation, including the introduction of serrations, plays different roles in controlling damage nucleation depending on the specific loading condition. Under shock loading, the stress for void nucleation and the resulting void distribution is insensitive to an interface structure, whereas under pure tensile loading, the opposite is true, even though the strain rate is comparable. The above difference can be explained based on the corresponding change in the total deformation prior to damage nucleation under shock loading, which is missing from the pure tensile loading. Therefore, it is concluded that whether local interface structure matters under high strain-rate loading depends on the specific loading history and the stress state: the local structure variation matters only when it alters the deformation behavior, and subsequently, damage nucleation and evolution.

36 MATERIALS SCIENCE↗

Identifying multiple synergistic factors on the susceptibility to stress relaxation cracking in variously heat-treated weldments

The 347H austenitic stainless steel has been widely used for pressure vessels and pipeline (PVP) applications due to its excellent creep and corrosion resistance, which fit ideally to the harsh conditions in petrochemical industries, fossil fuel or nuclear power plants, and modern energy storages. However, a failure mode has been commonly observed with cracks emerging at the heat affected zone (HAZ) of weldments during post-weld heat treatment (PWHT) or under intermediate to high temperature service conditions. This phenomenon is termed as Stress Relaxation Cracking (SRC) since the purpose of PWHT is to relieve the welding-induced residual stress fields, or as Stress Age Cracking (SAC) if failure happens during service. A leading literature explanation of this failure suggests that the residual stress relaxation and the precipitation dissolution and/or re-precipitation occur in the same temperature range, which can lead to locally high strains and thus to crack at the grain boundaries. Since in situ spatial measurements of residual stress fields, microstructural evolution, and failure processes are nearly infeasible, this work recourses to a micromechanical finite element framework that models the high temperature failure as the nucleation and growth of grain boundary cavities, whereas various parameters such as thermomechanical loading history and its evolution, the competition of grain-interior dislocation creep and grain-boundary diffusion in failure lifetime, and microstructural heterogeneities (such as the precipitate free zone near grain boundaries) can be quantitatively incorporated. It can be concluded from these microstructure-explicit simulations that an accurate knowledge of residual stress evolution and a carefully calibrated set of material constitutive parameters are the essential prerequisites for lifetime predictions. The understanding of individual governing factors also leads to a mechanistic interpretation of the observed SRC susceptibility C-curves. In conclusion, these results suggest that the criticality of residual stress evolution, but not the precipitation-induced local strains, be the leading factor for SRC.

347H stainless steel weldments↗

DEM analysis of the effect of interface transition zone on dynamic splitting tensile behavior of high-strength concrete based on multi-phase model

Highlights: • Crushable aggregates with the real geometry shape are generated by using clump-cluster method. • Flat-Joint Model is adopted as the constitutive law. • The tensile strength is almost not affected by ITZ strength when its strength exceeds 0.8 times that of mortar. • A modified formula that can reflect the functional relationship between the ITZ strength and the TDIF is proposed. The tensile strength is one of the main parameters in the design of concrete structures and has an important influence on the cracking performance and durability of concrete materials. As the weak region in concrete, the strength of the interface transition zone (ITZ) directly affects the dynamic mechanical response of concrete. Meanwhile, considering that the tensile performance of concrete is far weaker than its compressive performance, the study of the strength of ITZ is of great significance to the dynamic tensile fracture characteristics and mechanical properties of concrete. In this paper, a method combining 3D scanning technology and Clump-Cluster was proposed to generate a real geometry shape model of crushable aggregate. On this basis, the 3D discrete element model (DEM) of high-strength concrete was constructed using the Flat-Joint Model (FJM). The effects of the ITZ strength on the failure mode, number of microcracks, tensile strength and strain rate effect of high-strength concrete under strain rates from 0.01/s to 100/s were studied by splitting tensile test. The simulation results indicate that the number of microcracks generated decreases with the increase of ITZ strength, and the proportion of ITZ cracks decreases obviously. When the ITZ strength exceeds the critical value of 0.8 times that of mortar, the tensile strength is almost not affected by ITZ strength. In addition, based on the numerical simulation results, a modified formula that can reflect the functional relationship between the ITZ strength and the dynamic increasing factor of the concrete tensile strength (TDIF) is proposed, and the rationality of the TDIF modified formula is verified.

36 MATERIALS SCIENCE↗

High strain-rate compression behavior of polymeric rod and plate Kelvin lattice structures

The compressive high strain-rate behavior of polymeric Kelvin lattice structures with rod-based or plate-based unit cells was investigated through experimental techniques and finite element simulations. Polymeric lattice structures with 5x5x5 unit cell geometries were manufactured on the millimeter scale using vat polymerization additive manufacturing and tested at low (0.001/s) and high (1000/s) strain-rates. High strain-rate experiments were performed and validated for a viscoelastic split-Hopkinson (Kolsky) pressure bar system (SHPB) coupled with high-speed imaging and digital image correlation (DIC). Experimental results at both low and high strain-rates show the formation of a localized deformation band which was more prevalent in low relative density specimens and low strain-rate experiments. Strain-rate effects of lattice specimens strongly correlate with effects of the base polymer material; both bulk polymer and lattice specimen demonstrated strain-rate hardening, strain-rate stiffening, and decreased fracture strain under dynamic loading. Results show mechanical failure properties and energy absorption depended strongly on the relative density of the lattice specimen and exhibited distinct scaling between relative density and geometry type (rod, plate) and loading rate. High relative density plate-lattices demonstrated inferior mechanical properties to rod-lattices; however, there exists a critical relative density for a given mechanical property (17%- 28%) below which plate-lattices outperform rod-lattices of similar mass. As a result, high strain-rate explicit finite element simulations were performed and showed good agreement with the mechanical failure trends and deformation modes observed in the experiments.

36 MATERIALS SCIENCE↗

Passive sensing of a microparticle modified hybrid, fiber-reinforced composite

The widespread commercial adoption of high-performance, fiber-reinforced composites has pushed research interests toward the next generation of composites. These new composites are tasked with integrating additional functionalities into the structures without causing a trade-off in mechanical performance. One such functionality that has received significant interest is sensing. This is especially important for composites using high-performance fibers (e.g., carbon fiber) because their strain-to-failure is relatively low, resulting in brittle fracture. Besides, fiber damage can be hidden within the composite, potentially leading to premature catastrophic failure if not detected. In prior research, we demonstrated continuous feed-through deposition of ceramic nanoparticles on carbon fiber’s surface that simultaneously enhanced both the piezoresistive response and interlaminar shear strength. In this work, a similar continuous feed-through deposition process was used to demonstrate passive sensing and energy harvesting by integrating ferroelectric microparticles on the surface of electrically nonconductive fibers. The sensing and energy harvesting capabilities were characterized by mechanically straining composite beams and measuring the power generated. The improvements in mechanical properties are shown through interlaminar shear strength tests. Therefore, this research aims to demonstrate a high throughput, commercially scalable approach to coat fibers with ferroelectric microparticles that enable passive sensing as well as improved mechanical performance when fabricated into a fiber-reinforced composite.

Bowland, Christopher↗

Understanding Strain and Failure of a Knot in Polyethylene Using Molecular Dynamics with Machine-Learned Potentials

A neural network potential (NNP) has been developed by fitting to ab initio electronic structure data on hydrocarbons and is used to study failure of linear and knotted polyethylene (PE) chains. A linear PE chain must be highly strained before breaking as the stress is equally distributed across the chain. In contrast, the stress in a PE chain with a 31 or overhand knot, accumulates at the knot’s entrance/exit. We find the strain energy is greatest when the bond length and angle are strained simultaneously, and that the knot weakens the chain by increasing the variance of the C–C–C angle, thereby allowing rupture at lower bond strains. Here, we extend our analysis to both 51 and 52 knots and find that both break at the entrance/exit of a loop. Notably, molecular scale PE knots exhibit many of the same characteristics as knots in a macroscopic rope, with stick–slip phenomena upon tightening and similar points of failure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-burnup Experiments in Reactivity Initiated Accidents (HERA)

HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.

(HERA)↗

High-burnup Experiments in Reactivity Initiated Accidents (HERA)

HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.

(HERA)↗

Dynamic Tensile Characterization of Thin-Sheet Brittle Metallic Materials

Refractory metals are favorable materials in applications where high strength and ductility are needed at elevated temperatures. In some cases, operating temperatures may be near the melting point of the material. However, as temperature drops, refractory metals typically undergo a significant mechanical response change - ductile-to-brittle transition. These materials may be subjected to high strain rate loading at an ambient temperature state, such as an impact or crash. Knowledge of the high rate material properties are essential for design as well as simulation of impact events. The high rate stress-strain behavior of brittle metallic materials at ambient temperature is rarely studied because of experimental challenges, particularly when failure is involved. Failure typically occurs within the non-gage section of the material, which invalidates any collected stress-strain information. Here, a method to determine a specimen geometry which will produce failures in the gage section is presented. Pure tungsten in thin-sheet form was used as a trial material to select a specimen geometry for high rate Kolsky tension bar experiments. A finite element simulation was conducted to derive a strain correction for more accurate results. The room temperature stress-strain behavior of pure tungsten at a strain rate of 24 s –1 is presented. The outcome of this experimental technique can be applied to other brittle materials for dynamic tensile characterization.

36 MATERIALS SCIENCE↗

Stress Relaxation Cracking in 347H Stainless Steel Arc Welds: Susceptibility Evaluation of Heat-Affected Zone

Stress relaxation cracking (SRC) is considered one of the major failure mechanisms for 347H stainless steel welds at elevated service temperatures or during post weld heat treatment (PWHT), especially within the heat-affected zone (HAZ). This work focuses on the characterization of SRC susceptibility within 347H physically simulated arc welded HAZ at elevated temperatures. A four-step SRC thermomechanical test in combination with finite element modeling (FEM) of the welding and testing processes is developed to establish a susceptibility map for HAZ. The test first runs a thermal cycle with three different peak temperatures (1335, 1275, and 1150 °C) to duplicate representative HAZ subzone microstructures, followed by time-to-failure examination under a variety of pre-stress (260–600 MPa) and pre-strain conditions (0.03–0.19) as a function of reheat temperatures between 750 and 1050 °C. With the aid of FEM, SRC susceptibility maps are generated to identify the threshold stress, plastic strain, and creep strain as a function of test temperature. It was found out that HAZ subzone with a lower peak temperature (1150 °C) appears to be slightly less susceptible to SRC than the other two subzones that experienced higher peak temperatures. Generally, time-to-fracture reduces with increasing initially applied stress and strain for all test temperatures. The pre-stress thresholds decrease from about 500 to 330 MPa as the testing temperature increases from 800 to 1050 °C, while the corresponding initial plastic strain thresholds reduces from 0.15 to 0.06. The SRC susceptibility was also evaluated through the Larson–Miller Parameter (LMP) analysis as a function of plastic strain, initial stress and starting stress upon reaching the testing temperature, respectively. The 1050 °C test with a high pre-applied strain (0.1) exhibits an extremely short time to failure (t = 3 s) that lies outside the general trend in LMP analysis. Additionally, it was identified that a plastic strain above 0.07 is identified to significantly reduce the bulk creep strain tolerance to fracture and therefore increases SRC susceptibility. Hardness measurement and fractography analysis indicated that the strain aging of niobium carbonitrides and other potential phases in conjunction with intergranular precipitates contributes to an increase in microhardness and increased intergranular cracking susceptibility.

14 SOLAR ENERGY↗

3D interface size effects on slip transfer in Ti/Nb nanolaminates

Two-phase nanolaminates are well-renowned for achieving extraordinarily high strengths but at the sacrifice of reduced toughness and strain to failure. Recently ”thick” interfaces, or so called 3D interfaces, in Cu/Nb nanolaminates were experimentally shown to improve both of these mechanical properties. Here, in this work, we study the effect of 3D interfaces in the hexagonal close packed (HCP)/body centered cubic (BCC) Ti/Nb nanolaminate system. Nanoindentation hardness testing suggests increased strength with the introduction of a 3D Ti–Nb interface and a positive size effect with increases in 3D interface thickness from 5 nm to 20 nm. To understand this effect from a single dislocation perspective, we present a phase-field dislocation dynamics (PFDD) model for multi-phase HCP/BCC systems. We employ the model to simulate stress-driven transfer of single dislocations across 3D Ti/Nb interfaces of various thicknesses. Our results show that the critical stress for slip transfer increases with the thickness of the interface. This positive size effect is stronger for transfer from basal or prismatic dislocations in the Ti layer to 110$\langle$111$\rangle$ dislocations in the Nb layer than the reverse. For this Ti/Nb system, a critical thickness of 2 nm is identified at which the asymmetry in slip transfer is minimized. This work showcases 3D interfaces as a beneficial microstructure modification to strengthen as well as reduce anisotropy in nanocrystalline materials containing HCP phases.

Dislocations↗

Validation of material models for puncture of 7075-T651 aluminum plate

Plate puncture simulations are challenging computational tasks that require advanced material models including high strain rate and thermal-mechanical effects on both deformation and failure, plus finite element techniques capable of representing large deformations and material failure. The focus of this work is on the material issues, which require large sets of experiments, flexible material models and challenging calibration procedures. In this study, we consider the puncture of 12.7 mm thick, 7075-T651 aluminum alloy plates by a cylindrical punch with a hemispherical nose and diameter of 12.7 mm. The plasticity and ductile failure models were isotropic with calibration data obtained from uniaxial tension tests at different temperatures and strain rates plus quasi-static notched tension tests and shear-dominated tests described here. Sixteen puncture experiments were conducted to identify the threshold penetration energy, mode of puncture and punch acceleration during impact, The punch was mounted on a 139 kg mass and dropped on the plates with different impact speeds. Since the mass was the same in all tests, the quantity of interest was the impact speed. The axis and velocity of the punch were perpendicular to the plate surface. The mean threshold punch speed was 3.05 m/s, and the mode of failure was plugging by thermal-mechanical shear banding accompanied by scabbing fragments. Application of the material models in simulations of the tests yielded accurate estimates of the threshold puncture speed and of the mode of failure. Time histories of the punch acceleration compared well between simulation and test. Remarkably, the success of the simulations occurred in spite of even the smallest element used being larger than the width of the shear bands.

36 MATERIALS SCIENCE↗

Surface smoothing for laser powder-bed Ti-6Al-4V by a transient liquid phase

Surface roughness is the primary driver of fatigue for additively manufactured metals. To address surface roughness, this work introduces a new method to smooth features beyond line-of-sight without material removal. The method applies a coating that triggers local surface remelting by activating a eutectic reaction during heat treatment. The associated liquid phase then wets and isothermally solidifies into a smoother surface. For Ti-6Al-4V fabricated with laser powder bed fusion, samples with and without TLP smoothing (using a Cu coating) were characterized with a suite of techniques, including mechanical testing, electron backscatter diffraction, synchrotron X-ray tomography, and fractography. TLP smoothing reduced surface roughness by 80% and amplified compressive residual stress at the surface by about 50%. With statistically equivalent virtual microstructures, crystal plasticity scrutinized the roles of phases, porosity, and surface roughness. Although the tensile strain-to-failure was reduced to 1% strain, the TLP smoothing process increased high-cycle fatigue strength by about 20% compared to control samples, pointing to future opportunities to optimize the new process through various coating compositions and heat treatment schedules. Overall, this work establishes a new paradigm for treating surfaces of materials for smoothness and compressive residual stress.

Additive manufacturing↗

Coal to Carbon Fiber (C2CF) Continuous Processing for High Value Composites (Final Report)

Coal tar is a condensed and recovered by-product of the coking of metallurgical coal for steel production. The heaviest fraction of distilled coal tar is an isotropic pitch largely used as a binder in the manufacturing of carbonaceous electrodes for primary aluminum smelting and in electric arc furnaces. Coal tar pitch offers high carbon yield upon carbonization. In this project, a process to convert the domestically sourced isotropic coal tar pitch, containing very low particulates (QI = 0.32 wt.%), to form flow-domain mesophase pitch amenable for melt spinning into precursor (green) fibers for carbon fiber, was developed and optimized. The final reproducible processing developed is reviewed in this report, along with several characterizations of the mesophase pitch. A final definition of the characteristics of a ‘spinnable’ mesophase pitch is presented. With this mesophase pitch, reproducible and stable multifilament melt spinning was developed, producing green fiber tows with filament diameters of approximately 20 m. The multifilament melt spinning was the most challenging aspect of the project and required the most effort. The best practices learned from this project for melt spinning are reviewed in this report. Once spun, the green fibers were oxidatively stabilized, carbonized and graphitized under inert gas atmosphere to form the final carbon fibers. Given the relatively high softening point of the mesophase pitch, no issues of interfilament fusion were observed during batch oxidation, and subsequent batch carbonization and graphitization went smoothly in all cases. An ~ 80 wt.% conversion of the green fiber mass to final carbon fiber was achieved. After graphitization, the carbon fibers showed high tensile moduli (most were ~ 600 GPa, or 87 Msi) consistent with commercially-available high-performance pitch-based carbon fiber. However, tensile strength and strain to failure were comparatively low. Further work to reduce defects in and on the fiber surfaces would increase these properties. SEM imaging of the graphitic fiber textures is presented herein. Rudimentary composites were fabricated from the carbon fibers and characterized showing similar modulus to baseline composites fabricated with commercial carbon fiber. Finally, a basic economic analysis was done showing the potential to increase the value of the isotropic coal tar pitch by up to 13.6 to 136 times based on a carbon fiber value of $\$$5/lb to $\$$50/lb, respectively. Moreover, the site case study suggests that the coal tar from the single integrated steel mill could supply production of up to 16 kt/yr of carbon fiber. Finally, a technological gap analysis was done which shed light on remaining technical challenges. These challenges included: recovery and utilization of condensates from the mesophase pitch processing, further advancing and increasing stability of the multifilament melt spinning processing, optimization of the oxidation processing, defect reduction for increased carbon fiber strength, and the development of a weaving process towards carbon fiber fabrics. To maximize the coal value chain, the primary objectives of this project were to (a) develop and scale efficient processing technology for producing melt-spinnable mesophase pitch from isotropic coal tar pitch, (b) clarify and simplify tedious continuous fiber processing technologies (particularly multifilament melt spinning of mesophase pitch) towards the efficient production of high performance carbon fiber, and (c) demonstrate and characterize representative composite parts derived from the final carbon fiber. Immense progress was made on all 3 objectives and is detailed in this report.