At least 37 records · Page 2

OBSERVATIONS AND IMPLICATIONS OF INTERGRANULAR STRESS CORROSION CRACK GROWTH OF ALLOY 152 WELD METALS IN SIMULATED PWR PRIMARY WATER

Significant intergranular (IG) crack growth during stress corrosion cracking (SCC) tests has been documented during tests in simulated PWR primary water on two alloy 152 specimens cut from a weldment produced by ANL. The cracking morphology was observed to change from transgranular (TG) to mixed mode (up to ~60% IG) during gentle cycling and cycle + hold loading conditions. Measured crack growth rates under these conditions often suggested a moderate degree of environmental enhancement consistent with faster growth on grain boundaries. However, overall SCC propagation rates at constant stress intensity (K) or constant load were very low in all cases. Initial SCC rates up to 6x10-9 mm/s were occasionally measured, but constant K/load growth rates dropped below ~1x10-9 mm/s with time even when significant IG engagement existed. Direct comparisons were made among loading conditions, measured crack growth response and cracking morphology during each test to assess IGSCC susceptibility of the alloy 152 specimens. These results were analyzed with respect to our previous SCC crack growth rate measurements on alloy 152/52 welds.

alloy 152, SCC, stress corrosion cracking, intergr↗

Mechanical Properties and Corrosion Behavior of AA5754-AA6061 Dissimilar Aluminum Alloys Welded by Cold Metal Transfer

The trend of using lightweight materials in the automotive industry brings along the necessity of dissimilar welding of aluminum alloys such as AA5754 and AA6061. Hybrid structures in automobiles are subjected not only to mechanical forces but also corrosive effects of the environment. In this study, cold metal transfer welding, which is suitable for welding thin sheets and dissimilar materials, was applied to join AA5754 to AA6061. It was aimed to investigate the effect of weld heat input on mechanical properties and corrosion rate measured by the Tafel extrapolation method in 3.5 wt.% NaCl solution at room temperature. The tensile strength of AA5754-AA6061 joints tended to reduce with increasing heat input. Corrosion test results showed that the increased heat input decreased the corrosion resistance and caused intergranular corrosion besides pitting corrosion.

36 MATERIALS SCIENCE↗

AN ULTRASONIC PHASED ARRAY EVALUATION OF INTERGRANULAR STRESS CORROSION CRACK (IGSCC) DETECTION IN AUSTENITIC STAINLESS STEEL PIPING WELDS

Research is being conducted for the U.S. Nuclear Regulatory Commission at the Pacific Northwest National Laboratory to assess the effectiveness and reliability of advanced nondestructive examination (NDE) methods for the inspection of light water reactor (LWR) components and challenging material/component configurations. This study assessed the effectiveness of far-side inspections on wrought stainless steel piping with austenitic welds, as found in thin-walled, boiling water reactor (BWR) component configurations, for the detection and characterization of intergranular stress corrosion cracks (IGSCC).

36 MATERIALS SCIENCE↗

Decoupling the role of stress and corrosion in the intergranular cracking of noble-metal alloys

Intergranular stress-corrosion cracking (IGSCC) is a form of environmentally induced crack propagation causing premature failure of elemental metals and alloys. It is believed to require the simultaneous presence of tensile stress and corrosion; however, the exact nature of this synergy has eluded experimental identification. For noble metal alloys such as Ag–Au, IGSCC is a consequence of dealloying corrosion, forming a nanoporous gold layer that is believed to have the ability to transmit cracks into grain boundaries in un-dealloyed parent phase via a pure mechanical process. Here using atomic-scale techniques and statistical characterizations for this alloy system, we show that the separate roles of stress and anodic dissolution can be decoupled and that the apparent synergy exists owing to rapid time-dependent morphology changes at the dealloyed layer/parent phase interface. We discuss the applicability of our findings to the IGSCC of important engineering Fe- and Ni-based alloys in critical applications.

36 MATERIALS SCIENCE↗

Effect of Welding Parameters on the Corrosion Behavior of Dissimilar Alloy Welds of T6 AA6061 Al-Galvanized Mild Steel

Partial replacement of steel by Aluminium (Al) alloys is a promising approach adopted by automotive sector to improve fuel efficiency without compromising on the strength. However, this results in the generation of dissimilar welds of Al alloys and steel. Understanding the corrosion behavior of Al alloys–steel welds as a function of welding parameters is critical in the successful application of such alloys. The present study reports the intergranular corrosion behavior of T6 heat-treated AA6061 Al alloy-galvanized mild steel lap joints, welded by metal inert gas welding–brazing technique as a function of different welding parameters, viz. weld speed (4-6 m/min) and wire feed rate (0.8-0.9 m/min), following ASTM G 67-04. Weld characterization was performed by field emission scanning electron microscopy (FESEM), x-ray diffraction and nano-hardness measurement. Results indicate heavy dissolution and metal loss at the interface. A high volume fraction of Al-Fe intermetallics was precipitated at the weld interfaces, resulting in high hardness and higher localized corrosion. The thickness of Al-Fe intermetallic layer increased with increasing wire feed rate and lower weld speed which enhanced the severity of galvanic and intergranular corrosion.

36 MATERIALS SCIENCE↗

Influences of Quench Cooling Rate on Microstructure and Corrosion Resistance of Al-Cu-Mg Alloy Based on the End-Quenching Test

To investigate the effects of the quench cooling rate on corrosion resistance of Al-Cu-Mg alloy, an end-quenching test was conducted and the microstructures at different cooling rates were observed by SEM and TEM. Additionally, the corrosion resistance was characterized by an intergranular corrosion test and electrochemical test. Moreover, the finite element method was applied to simulate the end quenching process. The results indicate that the actual end quenching process can be approximated as one-dimensional heat transfer, and the cooling rate varies at different cooling distances. By affecting the microstructures, decreasing the cooling rate leads to a decline in the corrosion properties. Low cooling rates coarsen the constituent particles and grain boundary particles, resulting in a wide precipitation-free zone and an increase in the intensity of corrosion reactions. A high cooling rate concentrates on the intragranular precipitant, which can reduce the pitting depth and represents a conversion from localized corrosion to general corrosion.

36 MATERIALS SCIENCE↗

Effect of chloride content of molten nitrate salt on corrosion of A516 carbon steel.

The corrosion behavior of A516 carbon steel was evaluated to determine the effect of the dissolved chloride content in molten binary Solar Salt. Corrosion tests were conducted in a molten salt consisting of a 60-40 weight ratio of NaNO{sub 3} and KNO{sub 3} at 400{sup o}C and 450{sup o}C for up to 800 hours. Chloride concentrations of 0, 0.5 and 1.0 wt.% were investigated to determine the effect on corrosion of this impurity, which can be present in comparable amounts in commercial grades of the constituent salts. Corrosion rates were determined by descaled weight losses, corrosion morphology was examined by metallographic sectioning, and the types of corrosion products were determined by x-ray diffraction. Corrosion proceeded by uniform surface scaling and no pitting or intergranular corrosion was observed. Corrosion rates increased significantly as the concentration of dissolved chloride in the molten salt increased. The adherence of surface scales, and thus their protective properties, was degraded by dissolved chloride, fostering more rapid corrosion. Magnetite was the only corrosion product formed on the carbon steel specimens, regardless of chloride content or temperature.

36 MATERIALS SCIENCE↗

Effects of Variations in Salt-Spray Conditions on the Corrosion Mechanisms of an AE44 Magnesium Alloy

The understanding of how corrosion affects magnesium alloys is of utmost importance as the automotive and aerospace industries have become interested in the use of these lightweight alloys. However, the standardized salt-spray test does not produce adequate corrosion results when compared with field data, due to the lack of multiple exposure environments. This research explored four test combinations through three sets of cycles to determine how the corrosion mechanisms of pitting, intergranular corrosion, and general corrosion were affected by the environment. Of the four test combinations, Humidity-Drying was the least corrosive, while the most corrosive test condition was Salt Spray-Humidity-Drying. The differences in corrosivity of the test conditions are due to the various reactions needed to cause corrosion, including the presence of chloride ions to cause pit nucleation, the presence of humidity to cause galvanic corrosion, and the drying phase which trapped chloride ions beneath the corrosion by-products.

Martin, Holly J.↗

Intergranular Stress Corrosion Crack Initiation and Temperature Dependence of Alloy 600 in Pressurized Water Reactor Primary Water

Stress corrosion crack (SCC) initiation of a solution annealed, cold-worked (CW) UNS N06600 (Alloy 600) material was investigated in 360 and 325ºC simulated PWR primary water using constant load tensile instrumented for in-situ detection by the direct current potential drop technique. This CW material with high boron and low carbon bulk concentrations was found to be highly susceptible to SCC. Consistent SCC initiation times were obtained at both temperatures and the thermal activation energy for SCC initiation is estimated at ~116 kJ/mol.

Zhai, Ziqing↗

Corrosion mechanism of cold forged 316 stainless steel in molten FLiNaK salt

This study examined how cold forging (CF) affects the corrosion of 316 stainless steel (SS) in molten FLiNaK salt at 700 °C for 48 h. CF samples had two corrosion areas: one near the top and another displaying intergranular corrosion (IGC). Samples with lower CF (5–30 %) showed more IGC, while the 50 % CF sample had less IGC but the shallowest corrosion depth. This was due to the increased number of grain boundaries, which raised the potential corrosion initiation sites, and certain grain boundaries promoting chromium dissolution, thus enhancing IGC.

FLiNaK↗

Stainless steel corrosion by molten nitrates : analysis and lessons learned.

A secondary containment vessel, made of stainless 316, failed due to severe nitrate salt corrosion. Corrosion was in the form of pitting was observed during high temperature, chemical stability experiments. Optical microscopy, scanning electron microscopy and energy dispersive spectroscopy were all used to diagnose the cause of the failure. Failure was caused by potassium oxide that crept into the gap between the primary vessel (alumina) and the stainless steel vessel. Molten nitrate solar salt (89% KNO{sub 3}, 11% NaNO{sub 3} by weight) was used during chemical stability experiments, with an oxygen cover gas, at a salt temperature of 350-700 C. Nitrate salt was primarily contained in an alumina vessel; however salt crept into the gap between the alumina and 316 stainless steel. Corrosion occurred over a period of approximately 2000 hours, with the end result of full wall penetration through the stainless steel vessel; see Figures 1 and 2 for images of the corrosion damage to the vessel. Wall thickness was 0.0625 inches, which, based on previous data, should have been adequate to avoid corrosion-induced failure while in direct contact with salt temperature at 677 C (0.081-inch/year). Salt temperatures exceeding 650 C lasted for approximately 14 days. However, previous corrosion data was performed with air as the cover gas. High temperature combined with an oxygen cover gas obviously drove corrosion rates to a much higher value. Corrosion resulted in the form of uniform pitting. Based on SEM and EDS data, pits contained primarily potassium oxide and potassium chromate, reinforcing the link between oxides and severe corrosion. In addition to the pitting corrosion, a large blister formed on the side wall, which was mainly composed of potassium, chromium and oxygen. All data indicated that corrosion initiated internally and moved outward. There was no evidence of intergranular corrosion nor were there any indication of fast pathways along grain boundaries. Much of the pitting occurred near welds; however this was the hottest region in the chamber. Pitting was observed up to two inches above the weld, indicating independence from weld effects.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Wire Electrical Discharge Machined Surfaces of P91 Steel

The extensive usage of P91 steel in certain reactor components requires its precision fabrication by wire electrical discharge machining (WEDM). The WEDM cut surfaces consist of primarily re-melted and solidified layer (recast layer) of 2-8 µm. The recast layer is a result of fast removal of heat by unaffected metallic substrate and dielectric medium leading to rapid cooling. The WEDM surface is expected to affect the component performance in terms of its corrosion properties. The microstructural changes taking place due to EDM cutting of P91 steel bring about a drastic change in the electrochemical response of surface as compared to that for bulk P91 steel. The surface microstructure is shown to alter the passivation behavior and resistance to localized corrosion. Electrochemical polarization studies were done to evaluate passivation, pitting and intergranular corrosion (IGC) behavior and field emission gun—scanning electron microscopy was used for microstructural characterization of P91 steel surfaces. The passivation behavior for P91 steel WEDM cut surfaces was better than that for diamond polished surface. But pitting corrosion resistance decreased for the P91 steel WEDM surface which is a result of inhomogeneities in the microstructure of recast layer. The IGC resistance though increased due to the decreased grain size in the surface layer.

36 MATERIALS SCIENCE↗

Oxidation kinetics of Nd-Fe-B permanent magnets with modified microstructure

Oxidation kinetics of Nd-Fe-B permanent magnets prepared by both spark plasma sintering (SPS) and conventional sintering techniques has been studied at elevated temperature in dry air environment. Compared with the conventional sintered magnet, the SPS magnet possesses much lower oxidation rate, which leads to less reduction of magnetic properties of the SPS magnet than that of the conventional sintered magnet. Microstructure observation shows that the SPS magnet possesses unique microstructure due to the special sintering mechanism of SPS technique. In detail, the grain size of the Nd{sub 2}Fe{sub 14}B main phase is fine and uniform, only a few Nd-rich phases form along the grain boundaries of Nd{sub 2}Fe{sub 14}B phase, while most of them agglomerate into triple junctions as small particles. Such microstructure modification restrains effectively the intergranular corrosion along Nd-rich phase in the SPS magnet. As a result, the SPS magnet possesses excellent corrosion resistance at elevated temperature.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Candidate Materials Used for Urea Hydrolysis Equipment in Coal-Fired Selective Catalytic Reduction Units

Corrosion tests were performed in the laboratory in order to assess the corrosion resistance of candidate materials used in urea hydrolysis equipment. The materials to be evaluated were exposed at 145 °C for 1000 h. Alloys 316L, 316L Mod., HR3C, Inconel 718, and TC4 were evaluated. Additionally, aluminide and chromate coatings applied to a 316L substrate were examined. After exposure, the mass changes in the test samples were measured by a discontinuous weighing method, and the morphologies, compositions, and phases of the corrosion products were analyzed using scanning electron microscopy, energy-dispersive spectroscopy, and x-ray diffraction. Results indicated that continuous pitting and dissolution corrosion were the main failure modes for 316L stainless steel. 316L Mod. and HR3C alloy showed better corrosion resistance than 316L due to their relatively high Cr contents, but HR3C exhibited a strong tendency toward intergranular corrosion. Inconel 718, TC4, and aluminide and chromate coating samples showed similar corrosion processes: only depositions formed by hydrothermal reactions were observed. Based on these results, a possible corrosion process in the urea hydrolysis environment was discussed for these candidate materials and questions to be clarified were proposed.

36 MATERIALS SCIENCE↗

Atomistic Mechanisms of Stress-Dependent Molten Salt Corrosion in NiCr Alloys

Ni-based structural alloys in molten salt environments often experience simultaneous mechanical loading and corrosive attack, yet the mechanisms governing stress-corrosion interactions remain unclear. Prior studies largely emphasize tensile stress, while the role of compressive stress has received limited attention. Here, reactive molecular dynamics simulations are used to investigate the coupled effects of applied strain and corrosion in Ni 0.75 Cr 0.25 exposed to molten FLiNaK at 800 °C. A Σ5(210) grain boundary model is subjected to tensile (+4%) to compressive (−4%) uniaxial strains, and corrosion behavior is evaluated through fluorine adsorption, charge redistribution, and grain boundary evolution. Tensile strain accelerates intergranular corrosion susceptibility by reducing local atomic packing through elastic dilation and increasing excess free volume at the grain boundary, which enhances atomic mobility and salt infiltration. In contrast, compressive strain can suppress corrosion by promoting the formation of a ridge-like surface layer along the grain boundary, limiting salt access to the underlying alloy. These results provide atomistic insight into how stress states influence grain boundary corrosion in molten salts.

36 - MATERIALS SCIENCE↗