Search NASA⌕ Search

SEARCH · Search NASA

Results for “InN”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

The INNs and outs of antibody nonproprietary names

An important step in drug development is the assignment of an International Nonproprietary Name (INN) by the World Health Organization (WHO) that provides healthcare professionals with a unique and universally available designated name to identify each pharmaceutical substance. Monoclonal antibody INNs comprise a –mab suffix preceded by a substem indicating the antibody type, e.g., chimeric (-xi-), humanized (-zu-), or human (-u-). The WHO publishes INN definitions that specify how new monoclonal antibody therapeutics are categorized and adapts the definitions to new technologies. However, rapid progress in antibody technologies has blurred the boundaries between existing antibody categories and created a burgeoning array of new antibody formats. Thus, revising the INN system for antibodies is akin to aiming for a rapidly moving target. The WHO recently revised INN definitions for antibodies now to be based on amino acid sequence identity. These new definitions, however, are critically flawed as they are ambiguous and go against decades of scientific literature. A key concern is the imposition of an arbitrary threshold for identity against human germline antibody variable region sequences. This leads to inconsistent classification of somatically mutated human antibodies, humanized antibodies as well as antibodies derived from semi-synthetic/synthetic libraries and transgenic animals. Such sequence-based classification implies clear functional distinction between categories (e.g., immunogenicity). However, there is no scientific evidence to support this. Dialog between the WHO INN Expert Group and key stakeholders is needed to develop a new INN system for antibodies and to avoid confusion and miscommunication between researchers and clinicians prescribing antibodies.

59 BASIC BIOLOGICAL SCIENCES↗

Optical characterization of free electron concentration in heteroepitaxial InN layers using Fourier transform infrared spectroscopy and a 2 Multiplication-Sign 2 transfer-matrix algebra

Fourier Transform Infrared (FTIR) reflectance spectroscopy has been implemented as a non-destructive, non-invasive, tool for the optical characterization of a set of c-plane InN single heteroepitaxial layers spanning a wide range of thicknesses (30-2000 nm). The c-plane (0001) InN epilayers were grown by plasma-assisted molecular beam epitaxy (PAMBE) on GaN(0001) buffer layers which had been grown on Al{sub 2}O{sub 3}(0001) substrates. It is shown that for arbitrary multilayers with homogeneous anisotropic layers having their principal axes coincident with the laboratory coordinates, a 2 Multiplication-Sign 2 matrix algebra based on a general transfer-matrix method (GTMM) is adequate to interpret their optical response. Analysis of optical reflectance in the far and mid infrared spectral range has been found capable to discriminate between the bulk, the surface and interface contributions of free carriers in the InN epilayers revealing the existence of electron accumulation layers with carrier concentrations in mid 10{sup 19} cm{sup -3} at both the InN surface and the InN/GaN interface. The spectra could be fitted with a three-layer model, determining the different electron concentration and mobility values of the bulk and of the surface and the interface electron accumulation layers in the InN films. The variation of these values with increasing InN thickness could be also sensitively detected by the optical measurements. The comparison between the optically determined drift mobility and the Hall mobility of the thickest sample reveals a value of r{sub H} = 1.49 for the Hall factor of InN at a carrier concentration of 1.11 Multiplication-Sign 10{sup 19} cm{sup -3} at 300 Degree-Sign {Kappa}.

36 MATERIALS SCIENCE↗

Growth kinetics and structural perfection of (InN){sub 1}/(GaN){sub 1–20} short-period superlattices on +c-GaN template in dynamic atomic layer epitaxy

The growth kinetics and structural perfection of (InN){sub 1}/(GaN){sub 1–20} short-period superlattices (SPSs) were investigated with their application to ordered alloys in mind. The SPSs were grown on +c-GaN template at 650 °C by dynamic atomic layer epitaxy in conventional plasma-assisted molecular beam epitaxy. It was found that coherent structured InN/GaN SPSs could be fabricated when the thickness of the GaN barrier was 4 ML or above. Below 3 ML, the formation of SPSs was quite difficult owing to the increased strain in the SPS structure caused by the use of GaN as a template. The effective or average In composition of the (InN){sub 1}/(GaN){sub 4} SPSs was around 10%, and the corresponding InN coverage in the ∼1 ML-thick InN wells was 50%. It was found that the effective InN coverage in ∼1 ML-thick InN wells could be varied with the growth conditions. In fact, the effective In composition could be increased up to 13.5%, i.e., the corresponding effective InN coverage was about 68%, by improving the capping/freezing speed by increasing the growth rate of the GaN barrier layer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Features of InN growth by nitrogen-plasma-assisted MBE at different ratios of fluxes of group-III and -V elements

The results of investigations of the effect of the ratios of fluxes of the Group-III and -V elements on the structural and optical properties of an InN film deposited by plasma-assisted molecular-beam epitaxy (MBE) are presented. It is shown that the InN layer consists of free-standing nanocolumns at a flux ratio of III/V < 0.6. InN growth becomes two-dimensional (2D) in the ratio range 0.6 < III/V < 0.9; however, the InN layer has a nanoporous structure. Upon passage to metal-rich conditions of growth (III/V ∼1.1), the InN layer becomes continuous. The passage from 3D to 2D growth is accompanied by an increase in the threading-dislocation density. It results in a decrease in the photoluminescence (PL) intensity of InN at room temperature. The electron concentration in the InN layers amounts to ∼5 × 10{sup 18} cm{sup –3}, which results in a shift of the PL-signal peak to the wavelength region of 1.73–1.8 μm and to a shift of the absorption edge to the region of ∼1.65 μm.

36 MATERIALS SCIENCE↗

Initial exploration of growth of InN by electrochemical solution growth.

This report summarizes a brief and unsuccessful attempt to grow indium nitride via the electrochemical solution growth method and a modification thereof. Described in this report is a brief effort using a $50,000 LDRD award to explore the possibilities of applying the Electrochemical Solution Growth (ESG) technique to the growth of indium nitride (InN). The ability to grow bulk InN would be exciting from a scientific perspective, and a commercial incentive lies in the potential of extending the ESG technique to grow homogeneous, bulk alloys of In{sub x}Ga{sub 1-x}N for light emitting diodes (LEDs) operating in the green region of the spectrum. Indium nitride is the most difficult of the III-nitrides to grow due to its very high equilibrium vapor pressure of nitrogen1. It is several orders of magnitude higher than for gallium nitride or aluminum nitride. InN has a bandgap energy of 0.7eV, and achieving its growth in bulk for large area, high quality substrates would permit the fabrication of LEDs operating in the infrared. By alloying with GaN and AlN, the bulk material used as substrates would enable high efficiency emission wavelengths that could be tailored all the way through the deep ultraviolet. In addition, InN has been shown to have very high electronic mobilities (2700 cm{sup 2}/V s), making it a promising material for transistors and even terahertz emitters. Several attempts at synthesizing InN have been made by several groups. It was shown that metallic indium does not interact with unactivated nitrogen even at very high temperatures. Thus sets up an incompatibility between the precursors in all growth methods: a tradeoff between thermally activating the nitrogen-containing precursor and the low decomposition temperature of solid InN. We have been working to develop a novel growth technique that circumvents the difficulties of other bulk growth techniques by precipitating the column III nitrides from a solvent, such as a molten chloride salt, that provides an excellent host environment for the gallium nitride and indium nitride precursors. In particular, we have found that molten halide salts can solubilize both gallium (Ga{sup 3+}) and nitride (N{sup 3-}) ions without reacting with them to the extent that they are no longer available for reaction with each other. Literature reports indicate measured nitride ion concentrations in LiCl at 650 C as high as 10 mol% - a sufficient concentration to yield growth rates on the order of 0.1 to {approx}1 mm/hr under diffusion-limited growth conditions. Also, molten salts are compatible with the 400-1200 C temperatures likely to be necessary for growth of high-quality single-crystal III-nitrides. Since they can be worked with at (or close to) atmospheric pressure, scalability is not a problem and manufacturability issues are thus minimized, including capital equipment costs. Although the III-nitrides cannot be float-zone refined to remove impurities due to their high melting temperatures and vapor pressures, the salts can be, thus reducing sources of impurities before growth begins. Finally, the molten salts offer a number of pathways to improve the solubility and control the growth of the III-nitrides by functioning as an electrolyte in electrochemical processes. We have already demonstrated growth of wurtzite GaN particles ranging from 0.2 to 0.9 mm in two hours in our laboratory using these techniques. It was the goal of this work to extend this ESG approach to the growth of indium nitride. The hope was that the abundance of the activated form of nitrogen, namely the triply-charged nitride ion (N{sup -3}) would enable the facile growth of InN in solution at low temperatures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Epitaxial growth of high purity cubic InN films on MgO substrates using HfN buffer layers by pulsed laser deposition

Cubic InN films have been grown on MgO substrates with HfN buffer layers by pulsed laser deposition (PLD). It has been found that the use of HfN (100) buffer layers allows us to grow cubic InN (100) films with an in-plane epitaxial relationship of [001]{sub InN}//[001]{sub HfN}//[001]{sub MgO}. X-ray diffraction and electron back-scattered diffraction measurements have revealed that the phase purity of the cubic InN films was as high as 99%, which can be attributed to the use of HfN buffer layers and the enhanced surface migration of the film precursors by the use of PLD. - Graphical abstract: Cubic InN films have been grown on MgO substrates with HfN buffer layers by pulsed laser deposition (PLD). It has been revealed that the phase purity of the cubic InN films was as high as 99 %, which can be attributed to the use of HfN buffer layers and the enhanced surface migration of the film precursors by the use of PLD.

36 MATERIALS SCIENCE↗

Crystallinity, Surface Morphology, and Photoelectrochemical Effects in Conical InP and InN Nanowires Grown on Silicon

The growth conditions of two types of indium-based III–V nanowires, InP and InN, are tailored such that instead of yielding conventional wire-type morphologies, single-crystal conical structures are formed with an enlarged diameter either near the base or near the tip. By using indium droplets as a growth catalyst, combined with an excess indium supply during growth, “ice cream cone” type structures are formed with a nanowire “cone” and an indium-based “ice cream” droplet on top for both InP and InN. Surface polycrystallinity and annihilation of the catalyst tip of the conical InP nanowires are observed when the indium supply is turned off during the growth process. This growth design technique is extended to create single-crystal InN nanowires with the same morphology. Conical InN nanowires with an enlarged base are obtained through the use of an excess combined Au–In growth catalyst. Electrochemical studies of the InP nanowires on silicon demonstrate a reduction photocurrent as a proof of photovolatic behavior and offer insight as to how the observed surface polycrystallinity and the resulting interface affect these device-level properties. Furthermore, a photovoltage is induced in both types of conical InN nanowires on silicon, which is not replicated in epitaxial InN thin films.

36 MATERIALS SCIENCE↗

Epitaxial growth, electrical and optical properties of a-plane InN on r-plane sapphire

The heteroepitaxy of a-plane (1120) InN films on r-plane (1102) sapphire substrates, by nitrogen radio frequency plasma-assisted molecular beam epitaxy, has been investigated and compared to that of c-plane (0001) InN. The epitaxial growth of a-plane InN proceeded through the nucleation, growth, and coalescence of three-dimensional islands, resulting in surface roughness that increased monotonically with epilayer thickness. The full width at half maximum of (1120) x-ray diffraction rocking curves decreased significantly with increasing InN thickness, characteristic of structural improvement, and it reached the value of 24 arcmin for a 1 {mu}m thick film. Hall-effect measurements exhibited a similar dependence of electron concentration and mobility on thickness for both the a- and c-plane InN films. The analysis of the Hall-effect measurements, by considering the contribution of two conducting layers, indicates a similar accumulation of low mobility electrons with N{sub s}>10{sup 14} cm{sup -2} at the films' surface/interfacial region for both the a- and c-plane InN films. From optical transmittance measurements, the absorption edge of 0.768 eV was determined for the 1 {mu}m a-plane film, consistent with the expected Burstein-Moss effect. Photoluminescence spectra exhibited a lower energy peak at 0.631 eV, suggesting defect-related transitions.

36 MATERIALS SCIENCE↗

High Cubic-Phase Purity InN on MgO (001) Using Cubic-Phase GaN as a Buffer Layer

High cubic-phase purity InN films were grown on MgO (001) substrates by molecular beam epitaxy with a cubic-phase GaN buffer layer. The cubic phase purity of the InN grown layers has been analyzed by high resolution X-ray diffraction, {mu}-Raman scattering and transmission electron microscopy. It is evidenced that the hexagonal-phase content in the InN overlayer much depends on hexagonal-phase content in the cubic-phase GaN buffer layer and increases with increasing the hexagonal-phase GaN content. From Raman scattering measurements, in addition, the InN layer with lowest hexagonal component (6%), only Raman characteristics of cubic TO{sub InN} and LO{sub InN} modes were observed, indicating a formation of a small amount of stacking faults, which does not affect on vibrational property.

36 MATERIALS SCIENCE↗

Growth of very large InN microcrystals by molecular beam epitaxy using epitaxial lateral overgrowth

Very thick InN (∼40 μm) was grown by molecular beam epitaxy using the epitaxial lateral overgrowth (ELO) technique. In some regions, the ELO of InN was observed as expected, indicating an important step toward fabricating quasi-bulk InN substrates. Interestingly, most parts of the sample consist of large flat-topped microcrystals and well-faceted microstructures. This is likely due to local growth condition variations during ELO, which is supported by an experiment where ELO of InN was performed on a substrate with various stripe mask patterns. TEM characterization of a flat top InN microcrystal revealed few stacking faults and only related threading dislocations. Defect-free small faceted microcrystals were also observed. The thick InN crystals show a narrow photoluminescence spectrum with a peak at 0.679 eV and linewidth of 16.8 meV at 4 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Real-Time Optical Monitoring and Simulations of Gas Phase Kinetics in InN Vapor Phase Epitaxy at High Pressure

Understanding the kinetics of nucleation and coalescence of heteroepitaxial thin films is a crucial step in controlling a chemical vapor deposition process, since it defines the perfection of the heteroepitaxial film both in terms of extended defect formation and chemical integrity of the interface. The initial nucleation process also defines the film quality during the later stages of film growth. The growth of emerging new materials heterostructures such as InN or In-rich Ga(x)In(1-x)N require deposition methods operating at higher vapor densities due to the high thermal decomposition pressure in these materials. High nitrogen pressure has been demonstrated to suppress thermal decomposition of InN, but has not been applied yet in chemical vapor deposition or etching experiments. Because of the difficulty with maintaining stochiometry at elevated temperature, current knowledge regarding thermodynamic data for InN, e.g., its melting point, temperature-dependent heat capacity, heat and entropy of formation are known with far less accuracy than for InP, InAs and InSb. Also, no information exists regarding the partial pressures of nitrogen and phosphorus along the liquidus surfaces of mixed-anion alloys of InN, of which the InN(x)P(1-x) system is the most interesting option. A miscibility gap is expected for InN(x)P(1-x) pseudobinary solidus compositions, but its extent is not established at this point by experimental studies under near equilibrium conditions. The extension of chemical vapor deposition to elevated pressure is also necessary for retaining stoichiometric single phase surface composition for materials that are characterized by large thermal decomposition pressures at optimum processing temperatures.

Dietz, Nikolaus↗

Periodic supply of indium as surfactant for N-polar InN growth by plasma-assisted molecular-beam epitaxy

We have investigated the self-surfactant effect of In for N-polar InN growth by plasma-assisted molecular-beam epitaxy. We found that InN quality was significantly improved if a thin In coverage (about 1.8 ML) was introduced before InN growth. However, this In coverage was slowly consumed during subsequent InN growth under N-rich condition. Periodically restoring In coverage for thick InN growth was proposed to solve this consumption problem. We suggest that the effect of In surfactant is to terminate the surface N dangling bonds and form an In adlayer, under which an efficient diffusion channel for lateral N adatom transport is created.

36 MATERIALS SCIENCE↗

Infrared study of the absorption edge of {beta}-InN films grown on GaN/MgO structures

Infrared optical studies were carried out in a group of cubic InN samples grown by gas source molecular beam epitaxy on MgO (001) substrates. Room temperature (RT) reflectance and low-temperature (LT) transmittance measurements were performed by using fast Fourier transform infrared spectrometry. Reflectance fittings allowed to establish that {beta}-InN films have large free-carrier concentrations present (>10{sup 19} cm{sup -3}), a result that is corroborated by Hall effect measurements. Each sample explored exhibited a different optical absorption edge. The Varshni parameters that describe adequately the optical absorption edge responses with temperature are obtained for the set of samples studied. The observed temperatures changes, from LT to RT, are the lowest reported for III-V semiconductor binary compounds. The temperature coefficient of the conduction band depends on the strength of the electron-phonon interaction (e-ph-i), as well as on the thermal expansion. It has been predicted that cubic InN has one of the smallest e-ph-i of all III-V compounds, which is corroborated by these results. The variation in values of absorption edges is clearly consistent with the Burstein-Moss and band renormalization effects, produced by high free electron concentrations. It is shown that the conduction band in {beta}-InN, analogous to wurtzite InN, follows a nonparabolic behavior.

36 MATERIALS SCIENCE↗

Epitaxial relationship of semipolar s-plane (1101) InN grown on r-plane sapphire

The heteroepitaxy of semipolar s-plane (1101) InN grown directly on r-plane sapphire by plasma-assisted molecular beam epitaxy is studied using transmission electron microscopy techniques. The epitaxial relationship is determined to be (1101){sub InN} Parallel-To (1102){sub Al{sub 2O{sub 3}}}, [1120]{sub InN} Parallel-To [2021]{sub Al{sub 2O{sub 3}}}, [1102]{sub InN}{approx} Parallel-To [0221]{sub Al{sub 2O{sub 3}}}, which ensures a 0.7% misfit along [1120]{sub InN}. Two orientation variants are identified. Proposed geometrical factors contributing to the high density of basal stacking faults, partial dislocations, and sphalerite cubic pockets include the misfit accommodation and reduction, as well as the accommodation of lattice twist.

36 MATERIALS SCIENCE↗

Study of structural properties of cubic InN films on GaAs(001) substrates by molecular beam epitaxy and migration enhanced epitaxy

InN epitaxial films with cubic phase were grown by rf-plasma-assisted molecular beam epitaxy (RF-MBE) on GaAs(001) substrates employing two methods: migration-enhanced epitaxy (MEE) and conventional MBE technique. The films were synthesized at different growth temperatures ranging from 490 to 550 Degree-Sign C, and different In beam fluxes (BEP{sub In}) ranging from 5.9 Multiplication-Sign 10{sup -7} to 9.7 Multiplication-Sign 10{sup -7} Torr. We found the optimum conditions for the nucleation of the cubic phase of the InN using a buffer composed of several thin layers, according to reflection high-energy electron diffraction (RHEED) patterns. Crystallographic analysis by high resolution X-ray diffraction (HR-XRD) and RHEED confirmed the growth of c-InN by the two methods. We achieved with the MEE method a higher crystal quality and higher cubic phase purity. The ratio of cubic to hexagonal components in InN films was estimated from the ratio of the integrated X-ray diffraction intensities of the cubic (002) and hexagonal (1011) planes measured by X-ray reciprocal space mapping (RSM). For MEE samples, the cubic phase of InN increases employing higher In beam fluxes and higher growth temperatures. We have obtained a cubic purity phase of 96.4% for a film grown at 510 Degree-Sign C by MEE.

36 MATERIALS SCIENCE↗

Surface states and electronic structure of polar and nonpolar InN - An in situ photoelectron spectroscopy study

Valence band structure and surface states of InN with (0001), (000-1), (1-100), and (11-20) orientation were investigated in situ after growth using photoelectron spectroscopy. Depending on surface orientation, different occupied surface states are identified and differentiated from bulk contributions. For N-polar, m-plane, and a-plane InN, the surface states are located at the valence band maximum, while In-polar InN features surface states close to the Fermi level. The surface band alignment correlates with the position of surface states. For InN(0001), a much larger surface downward band bending is observed compared to N-polar, m-plane, and a-plane InN, where almost flat band conditions occur.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Nanostructural and electronic properties of polytypes in InN nanocolumns

Transmission electron microscopy techniques and density functional theory calculations were employed to investigate the nanostructural and electronic properties of InN polytypes observed in InN nanocolumns, grown on Si(111) by molecular beam epitaxy. Moiré fringes and alternating hexagonal and cubic lattice stacking sequences along the c-axis, observed among the wurtzite layers, implied the presence of different structures embedded in the basic 2H structure of the nanocolumns. Quantitative electron diffraction analysis and high-resolution image simulations verified the coexistence of the wurtzite structure with the 4H, 6H, and the 3C zinc-blende structural polytypes. Total energies calculations established the 2H wurtzite structure as the most stable polytype. The band gap of all polytypes was found direct with the energies and the band gaps of the 4H (E{sub g} = 0.64 eV) and 6H (E{sub g} = 0.60 eV) structures calculated between the corresponding values of the 2H (E{sub g} = 0.75 eV) and 3C (E{sub g} = 0.49 eV) basic structures. Theoretical and experimental analysis showed that at the initial stages of growth InN nanocolumns were under tensile strain along both the basal plane and growth direction. Structural polytypes were then introduced in the form of embedded inclusions to accommodate the excess tensile strain along the growth direction, allowing the entire process of polymorphism to be the dominant strain relaxation mechanism of InN nanocolumns. Moreover, the lattice and energetic properties and band gap values of InN polytypes showed a linear dependence on hexagonality, while the presence of polytypes led to a characteristic broadening of the photoluminescence emission peak toward lower emission energies.

36 MATERIALS SCIENCE↗

Effect of Mg doping on the structural and free-charge carrier properties of InN films

We present a comprehensive study of free-charge carrier and structural properties of two sets of InN films grown by molecular beam epitaxy and systematically doped with Mg from 1.0 × 10{sup 18} cm{sup −3} to 3.9 × 10{sup 21} cm{sup −3}. The free electron and hole concentration, mobility, and plasmon broadening parameters are determined by infrared spectroscopic ellipsometry. The lattice parameters, microstructure, and surface morphology are determined by high-resolution X-ray diffraction and atomic force microscopy. Consistent results on the free-charge carrier type are found in the two sets of InN films and it is inferred that p-type conductivity could be achieved for 1.0 × 10{sup 18} cm{sup −3} ≲ [Mg] ≲ 9.0 × 10{sup 19} cm{sup −3}. The systematic change of free-charge carrier properties with Mg concentration is discussed in relation to the evolution of extended defect density and growth mode. A comparison between the structural characteristics and free electron concentrations in the films provides insights in the role of extended and point defects for the n-type conductivity in InN. It further allows to suggest pathways for achieving compensated InN material with relatively high electron mobility and low defect densities. The critical values of Mg concentration for which polarity inversion and formation of zinc-blende InN occurred are determined. Finally, the effect of Mg doping on the lattice parameters is established and different contributions to the strain in the films are discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗