Search NASA⌕ Search

SEARCH · Search NASA

Results for “Indentation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Lateral cracks during sliding indentation on various optical materials

A series of static and sliding indentation (ie, scratching) was performed and characterized on a wide range of optical workpiece materials [single crystals of Al 2 O 3 (sapphire), SiC, Y 3 Al 5 O 12 (YAG), CaF 2 , and LiB 3 O 5 (LBO); a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass ceramic (Zerodur); and glasses of SiO 2 :TiO 2 (ULE), SiO 2 (fused silica), and P 2 O 5 –Al 2 O 3 –K 2 O–BaO (Phosphate)] at various applied loads using various indenters (Vickers, 10 µm conical, and 200 µm conical). Despite having different load dependencies, the lateral crack depth formed during sliding indentation quantitatively scales with that formed during static indentation, explaining why static indentation has been historically effective in describing various grinding parameters. Depending on the indenter geometry, the amount of residual trench damage (plastic deformation and local fracturing) during sliding indentation was often enhanced by more than an order of magnitude compared with static indentation. A simple ploughing scratch model, which considers both tangential and normal stresses (where the tangential stress is amplified by relatively small tangential contact area), explains this enhancement and other observed trends. Accounting for the high correlation between residual trench depth and volumetric fracturing, the model is extended to estimate the amount of fracture damage as a function of the material properties of the workpiece, indenter geometry, and applied load. Such a model has utility in the design of optimized grinding processes, particularly the abrasive geometry. Finally, at higher loads (>1 N), lateral cracks were often observed to preferentially propagate in the forward scratching direction, as opposed to perpendicular to the scratch as typically observed. High-speed imaging of the scratch process confirms that these cracks propagate ahead of the sliding indenter during the scratching event. Finite element stress analysis suggests the ploughing frictional forces increase the mode I tensile stresses at the leading edge of the sliding indenter explaining the direction of crack propagation of such cracks.

36 MATERIALS SCIENCE↗

Decoupling indentation size and strain rate effects during nanoindentation: A case study in tungsten

Materials indented at small scales may simultaneously exhibit indentation size and strain rate effects which complicate the identification of the mechanisms that control deformation and strength. Here, in this work, we explore the possibility that indentation size and rate effects in some materials can be decoupled in a simple way. Nanoindentation tests with various load-time histories were carried out to measure the hardness of a tungsten single crystal over a wide range of indentation depths (~500–3600 nm) and indentation strain rates (~5 ×10 –5 –2 ×10 –1 s –1 ). Under these conditions, this material exhibits significant indentation size and rate effects, but the size effect is, to a good approximation, independent of strain rate. It is shown that this behavior can be understood by the Nix-Gao model for the indentation size effect modified to include the effects of a strain rate dependent friction stress. As a consequence, the size and rate dependencies of the hardness can be expressed as the sum of two independent terms: H($\dot{ε}$ i , h c )=H f ($\dot{ε}$ i ) + (H 0 – H f ) $\sqrt{1+ \frac{h^*}{h_c}}$, where H($\dot{ε}$ i , h c ) is the hardness at given indentation strain rate ($\dot{ε}$ i ) and contact depth (h c ), H f ($\dot{ε}$ i ) is the hardness contributed by the rate dependent friction stress, and (H 0 – H f ) and h* are size and rate independent constants that follow from the Nix-Gao analysis. This formula, together with an expression for the rate dependence of H f , was successfully applied to decouple the indentation size and rate effects observed in tungsten. In addition, the physics underlying the rate independence of indentation size effect is discussed, which provides guidance for application of the proposed approach to other materials.

42 ENGINEERING↗

Å-Indentation for non-destructive elastic moduli measurements of supported ultra-hard ultra-thin films and nanostructures

During conventional nanoindentation measurements, the indentation depths are usually larger than 1–10 nm, which hinders the ability to study ultra-thin films (<10 nm) and supported atomically thin two-dimensional (2D) materials. Here, we discuss the development of modulated Å-indentation to achieve sub-Å indentations depths during force-indentation measurements while also imaging materials with nanoscale resolution. Modulated nanoindentation (MoNI) was originally invented to measure the radial elasticity of multi-walled nanotubes. Now, by using extremely small amplitude oscillations (<<1 Å) at high frequency, and stiff cantilevers, we show how modulated nano/Å-indentation (MoNI/ÅI) enables non-destructive measurements of the contact stiffness and indentation modulus of ultra-thin ultra-stiff films, including CVD diamond films (~1000 GPa stiffness), as well as the transverse modulus of 2D materials. Our analysis demonstrates that in presence of a standard laboratory noise floor, the signal to noise ratio of MoNI/ÅI implemented with a commercial atomic force microscope (AFM) is such that a dynamic range of 80 dB –– achievable with commercial Lock-in amplifiers –– is sufficient to observe superior indentation curves, having indentation depths as small as 0.3 Å, resolution in indentation <0.05 Å, and in normal load <0.5 nN. Being implemented on a standard AFM, this method has the potential for a broad applicability.

36 MATERIALS SCIENCE↗

A Load-Based Multiple-Partial Unloading Micro-Indentation Technique for Mechanical Property Evaluation

A load-based multiple-partial unloading microindentation technique has been developed for evaluating mechanical properties of materials. Comparing to the current prevailing nano/micro-indentation methods, which require precise measurements of the indentation depth and load, the proposed technique only measures indentation load and the overall indentation displacement (i.e. including displacement of the loading apparatus). Coupled with a multiple-partial unloading procedure during the indentation process, this technique results in a load-depth sensing indentation system capable of determining Young’s modulus of metallic alloys with flat, tubular, or curved architectures. Test results show consistent and correct elastic modulus values when performing indentation tests on standard alloys such as steel, aluminum, bronze, and single crystal superalloys. The proposed micro-indentation technique has led to the development of a portable loaddepth sensing indentation system capable of on-site, in-situ material property measurement.

36 MATERIALS SCIENCE↗

In situ frustum indentation of nanoporous copper thin films

Mechanical properties of thin films are often obtained solely from nanoindentation. At the same time, such measurements are characterized by a substantial amount of uncertainty, especially when mean pressure or hardness are used to infer uniaxial yield stress. In this paper we demonstrate that indentation with a pyramidal flat tip (frustum) indenter near the free edge of a sample can provide a significantly better estimate of the uniaxial yield strength compared to frequently used Berkovich indenter. This is first demonstrated using a numerical model for a material with an isotropic pressure sensitive yield criterion. Numerical simulations confirm that the indenter geometry provides a clear distinction of the mean pressure at which a material transitions to inelastic behavior. The mean critical pressure is highly dependent on the plastic Poisson ratio ν p so that at the 1% offset of normalized indent depth, the critical pressure p m c normalized to the uniaxial yield strength σ 0 is 1 < p m c /σ 0 < 1.3 for materials with 0 < ν p < 0.5. Choice of a frustum over Berkovich indenter reduces uncertainty in hardness by a factor of 3. These results are used to interpret frustum indentation experiments on nanoporous (NP) Copper with struts of typical diameter of 45 nm. An estimate of the yield strength of NP Copper is obtained 230 MPa < σ 0 < 300 MPa. Edge indentation further allows one to obtain in-plane strain maps near the critical pressure. Finally, comparison of the experimentally obtained in-plane strain maps of NP Cu during deformation and the strain field for different plastic Poisson ratios suggest that this material has a plastic Poisson ratio of the order of 0.2–0.3. However, existing constitutive models may not adequately capture post-yield behavior of NP metals.

36 MATERIALS SCIENCE↗

Mechanical characterization of Ti-6Al-4V titanium alloy at multiple length scales using spherical indentation stress-strain measurements

Recent advances in spherical indentation stress-strain protocols and analyses have demonstrated the capability for measuring reliably the local mechanical responses in polycrystalline metal samples at different length scales, ranging from sub-micron (regions within individual grains) to several hundreds of microns (regions covering several grains). These recent advances have now made it possible to study systematically the mechanical behavior of a single material system at different length scales, with tremendous potential to obtain new insights into the role of individual phases, interfaces, and other microscale constituents on the macroscale mechanical response of the material. In this paper, we report spherical indentation stress-strain measurements with different indenter sizes (microns to millimeters) on Ti-6Al-4V (Ti-64) which capture the mechanical response of single phase alpha-Ti-64, single colony (alpha-beta), few colonies, and many colonies of Ti-64. The results show that the average mechanical response (indentation modulus and yield strength) from multiple indentations remains relatively unchanged from single phase alpha to many colonies of Ti-64, while the variance in the response decreases with indenter size. In conclusion, the work-hardening response in indentation tests follows a similar behavior up to indentation zones of many colonies, which shows significantly higher work hardening rates.

36 MATERIALS SCIENCE↗

Defect formation by pristine indenter at the initial stage of nanoindentation

Nano-indentation is a sophisticated method to characterize mechanical properties of materials. This method samples a very small amount of material during each indentation. Therefore, this method is extremely useful to measure mechanical properties of nano-materials. The measurements using nanoindentation is very sensitive to the surface topology of the indenter and the indenting surfaces. The mechanisms involved in the entire process of nanoindentation require an atomic level understanding of the interplay between the indenter and the substrate. In this paper, we have used atomistic simulation methods with empirical potentials to investigate the effect of various types of pristine indenter on the defect nucleation and growth. Using molecular dynamics simulations, we have predicted the load-depth curve for conical, vickers, and sperical tip. The results are analyzed based on the coherency between the indenter tip and substrate surface for a fixed depth of 20 Å. The depth of defect nucleation and growth is observed to be dependent on the tip geometry. A tip with larger apex angle nucleates defects at a shallower depth. However, the type of defect generated is dependent on the crystalline orientation of the tip and substrate. For coherent systems, prismatic loops were generated, which released into the substrate along the close-packed directions with continued indentation. For incoherent systems, pyramidal shaped dislocation junctions formed in the FCC systems and disordered atomic clusters formed in the BCC systems. These defect nucleation and growth process provide the atomistic mechanisms responsible for the observed load-depth response during nanoindentation.

36 MATERIALS SCIENCE↗

Effect of Indenter Elastic Modulus on Hertzian Ring Crack Initiation in Silicon Carbide

The effect of spherical indenter stiffness on Hertzian-contact-induced fracture initiation was examined in hot-pressed silicon carbides (SiCs). Hertzian ring crack initiation forces were measured using zirconia, steel, silicon nitride, alumina, or tungsten carbide spherical indenters (elastic moduli ranging between 213 and 630 GPa). The two (flat target) SiCs were fully dense, and had equivalent elastic moduli (~450 GPa) and fracture toughnesses; however, about 20% of the grains in one SiC were larger than the largest grains in the other. Decreasing the indenter elastic modulus consistently resulted in lower ring crack initiation forces and those differences were statistically significant. Such a decrease in Hertzian ring crack initiation force with decreased indenter elastic modulus indicates the presence of a non-zero friction coefficient. Additionally, independent of the indenter material, ring crack initiation occurred at lower Hertzian indentation forces in the SiC containing larger grains suggesting that the grains in that tail of the grain-size-distribution acted as Griffith-type flaws. Lastly, selecting a spherical indenter material that has the same or similar elastic modulus as the target material provides simpler interpretation, and estimates of ring crack initiation stresses with greater usefulness and fidelity. Such a "matched" condition serves to circumvent the complexities that a ubiquitously unknown coefficient of friction introduces in the estimation of Hertzian ring crack initiation stress.

36 MATERIALS SCIENCE↗

Ceramic wear in indentation and sliding

The various wear mechanisms involved with single-crystal ceramic materials in indentation and in sliding contacts. Experiments simulating interfacial events have been conducted with hemispherical, conical and pyramidal indenters (riders). With spherical riders, under either abrasive or adhesive conditions, two types of fracture pits have been observed. First, spherical-shaped fracture pits and wear particles are found as a result of either indenting or sliding. These are shown to be due to a spherical-shaped fracture along the circular or spherical stress trajectories. Second, polyhedral fracture pits and debris, produced by anisotropic fracture, and also found both during indenting and sliding. These are primarily controlled by surface and subsurface cracking along cleavage planes. Several quantitative results have also been obtained from this work. For example, using a pyramidal diamond, crack length of Mn-Zn ferrite in the indentation process grows linearly with increasing normal load. Moreover, the critical load to fracture both in indentation and sliding is essentially isotropic and is found to be directly proportional to the indenter radius.

Miyoshi, K.↗

Ceramic wear in indentation and sliding contact

The various wear mechanisms involved with single-crystal ceramic materials in indentation and in sliding contacts. Experiments simulating interfacial events have been conducted with hemispherical, conical and pyramidal indenters (riders). With spherical riders, under either abrasive or adhesive conditions, two types of fracture pits have been observed. First, spherical-shaped fracture pits and wear particles are found as a result of either indenting or sliding. These are shown to be due to a spherical-shaped fracture along the circular or spherical stress trajectories. Second, polyhedral fracture pits and debris, produced by anisotropic fracture, and also found both during indenting and sliding. These are primarily controlled by surface and subsurface cracking along cleavage planes. Several quantitative results have also been obtained from this work. For example, using a pyramidal diamond, crack length of Mn-Zn ferrite in the indentation process grows linearly with increasing normal load. Moreover, the critical load to fracture both in indentation and sliding is essentially isotropic and is found to be directly proportional to the indenter radius.

Miyoshi, K.↗

Evaluation of the Fracture Toughness of Nb-40Al-8Cr-1W-1Y-0.05B Intermetallic Material by Indentation Techniques

The fracture toughness of an Nb-40Al-8Cr - 1W-1Y-0.05B intermetallic material was evaluated by indentation techniques at room temperature. Two widely used indentation methods, crack size measurement and indent strength, yielded excellent agreement with a conventional fracture toughness technique using straight-through precracked specimens, despite the occasional formation of poorly configured cracks. However, the modified indentation technique, using dummy indent flaws, resulted in a low fracture toughness compared to that evaluated by the other methods. The material did not exhibit rising R-curve behavior, as evaluated from the indentation strength data. These results indicate that indentation fracture principles are applicable to this brittle intermetallic material without modification of the residual contact stress term originally calibrated for ceramic materials.

Choi, S. R.↗

Interaction of Cracks Between Two Adjacent Indents in Glass

Experimental observations of the interaction behavior of cracks between two adjacent indents were made using an indentation technique in soda-lime glass. It was specifically demonstrated how one indent crack initiates and propagates in the vicinity of another indent crack. Several types of crack interactions were examined by changing the orientation and distance of one indent relative to the other. It was found that the residual stress field produced by elastic/plastic indentation has a significant influence on controlling the mode of crack interaction. The interaction of an indent crack with a free surface was also investigated for glass and ceramic specimens.

Choi, S. R.↗

Fracture Toughness of PMMA as Measured with Indentation Cracks

Fracture toughness of polymethyl methacrylate (PMMA) was evaluated with indentation cracks. The cracks were developed by indenting in a liquid acetone environment, as suggested by previous researchers. Due to the inconsistency in crack configurations with varying indentation loads and to the negligible residual stress from indentation, the application of the indentation strength method was limited in evaluating fracture toughness of PMMA. The semi-elliptical crack approximation, however, particularly at a low indentation load of 9.8 N, resulted in reasonable agreement with the value determined by three conventional fracture toughness testings using the compact tension (CT), double cantilever beam (DCB), and single edge notched beam (SENB) specimens. Measurements at other indentation load typically were in poor agreement with conventional methods due to poorly developed crack configurations.

Choi, S. R.↗

Crack nucleation and growth during dynamic indentation of chemically-strengthened glass

Dynamic point impact loading is a primary cause of fracture of glass screens on mobile devices. An improved understanding of crack initiation and evolution under high-speed indentation could contribute to the development of materials with better performance, but experimental observations are challenging due to the short timescales and limited depth-of-field of optical microscopy. To address this need, we have observed fracture of a chemically-strengthened glass during dynamic indentation using in situ x-ray phase-contrast imaging (XPCI). Median cracks initiate below the surface of the glass, at a depth approximately corresponding to the depth at which the surface residual compressive stress diminishes to zero. These cracks initially propagate at ~10ms –1 , rapidly accelerating to > 100ms –1 . We also observe some evidence for rate-dependent behavior, in that indentation at the lowest rates studied here (below about ~0.15ms –1 ) fails to initiate cracks regardless of the depth of the indentation (up to 18μm), while indentation at higher rates produces median cracks that either arrest or cause complete fracture, depending on the depth of indentation.

36 MATERIALS SCIENCE↗

Use of indentation to study the degradation of photovoltaic backsheets

The ability of electrical insulating materials within a module to act as insulators is a key safety requirement for photovoltaic (PV) technology. Presently, however, the durability of backsheets may not be readily assessed. For example, the mechanical tensile test continues to be developed, and its use has not been validated such that a technically based pass/fail criteria may be established. This study examines the use of simple indentation methods, including durometer hardness and instrumented indentation, as a means to quantitively assess the degradation of PV backsheets. Characteristics including: hardness, modulus, load/displacement profile, creep hold response, and residual impression are explored in an empirical study. Glass/encapsulant/backsheet mini-modules constructed using backsheets including: polyamide (PA), poly(ethylene terephthalate) (PET), polyvinyl fluoride (PVF) laminate ('TPE'), and polyvinylidene fluoride (PVDF) were examined. An M-type durometer as well as Berkovich and cube-corner tips were used in the indentation experiments. Additional characterizations were performed to interpret the indentation measurements including: surface roughness measurements using atomic force microscopy (AFM), a chemical integrity study using Fourier-transform infrared spectroscopy (FTIR), and phase-transition measurements using differential scanning calorimetry (DSC). The results are analyzed in the context of the combined accelerated stress test (C-AST) also explored in this study. Instrumented indentation (i.e., using a Berkovich tip) was able to distinguish between backsheets and quantify the effects of accelerated testing (including up to 60%, 25%, and 20% change in hardness, modulus, and creep displacement, respectively). The embrittlement of the backsheets was not readily assessable using cube-corner indentation. Cracking of the known-bad polyamide backsheet was observed from the C-AST, which was not observed to result from steady state UV weathering.

14 SOLAR ENERGY↗

Fictive temperature-independent density and minimum indentation size effect in calcium aluminosilicate glass

Using the calcium aluminosilicate system a glass was developed that exhibits fictive temperature-independent density by creating an intermediate glass between normal and anomalous glasses. Normal glass, such as soda-lime silicate glass, exhibits decreasing density with increasing fictive temperature while anomalous glass, such as silica glass, exhibits increasing density with increasing fictive temperature. This intermediate glass composition was found to exhibit the minimum indentation size effect during indentation hardness testing. It appears that the indentation size effect is correlated with a deformation-induced fictive temperature increase, which is accompanied by a density change and hardness change in the vicinity of the indentation. It is suggested from these observations that indentation size effect originates from the energy required to create interfaces and defects such as shear bands, subsurface cracks, and point defects near the indenter-specimen boundary, which accompany the volume change.

36 MATERIALS SCIENCE↗

The Effect of Indenter Ball Radius on the Static Load Capacity of the Superelastic 60NiTi for Rolling Element Bearings

Static load capacity is a critical design parameter for rolling element bearings used in space mechanisms because of the potential for Brinell (surface dent) damage due to shock and vibration loading events during rocket launch. Brinell damage to bearing raceways can lead to torque variations (noise) and reduced bearing life. The growing use of ceramic rolling elements with high stiffness in hybrid bearings exacerbates the situation. A new family of hard yet resilient materials based upon nickel-titanium is emerging to address such bearing challenges. 60NiTi is a superelastic material that simultaneously exhibits high hardness and a relatively low elastic modulus (approx. 100 GPa) and has been shown to endure higher indentation loads than conventional and high performance steel. Indentation load capacity has been reported for relatively large (12.7 mm diameter) ceramic (Si3N4) indenter balls pressed against flat plates of 60NiTi. In order to develop damage load threshold criteria applicable to a wide range of bearing designs and sizes, the effects of indenter ball radius and the accuracy of interpolation of the Hertz contact stress relations for 60NiTi must be ascertained. In this paper, results of indentation tests involving ceramic balls ranging from 6.4 to 12.7 mm in diameter and highly polished 60NiTi flat plates are presented. When the resulting dent depth data for all the indenter ball sizes are normalized using the Hertz equations, the data (dent depth versus stress) are comparable. Thus when designing bearings made from 60NiTi, the Hertz stress relations can be applied with relative confidence over a range of rolling element sizes and internal geometries.

bearings↗

The Effect of Indenter Ball Radius on the Static Load Capacity of the Superelastic 60NiTi for Rolling Element Bearings

Static load capacity is a critical design parameter for rolling element bearings used in space mechanisms because of the potential for Brinell (surface dent) damage due to shock and vibration loading events during rocket launch. Brinell damage to bearing raceways can lead to torque variations (noise) and reduced bearing life. The growing use of ceramic rolling elements with high stiffness in hybrid bearings exacerbates the situation. A new family of hard yet resilient materials based upon nickel-titanium is emerging to address such bearing challenges. 60NiTi is a superelastic material that simultaneously exhibits high hardness and a relatively low elastic modulus (~100GPa) and has been shown to endure higher indentation loads than conventional and high performance steel. Indentation load capacity has been reported for relatively large (12.7mm diameter) ceramic (Si3N4) indenter balls pressed against flat plates of 60NiTi. In order to develop damage load threshold criteria applicable to a wide range of bearing designs and sizes, the effects of indenter ball radius and the accuracy of interpolation of the Hertz contact stress relations for 60NiTi must be ascertained. In this paper, results of indentation tests involving ceramic balls ranging from 6.4 to 12.7mm in diameter and highly polished 60NiTi flat plates are presented. When the resulting dent depth data for all the indenter ball sizes are normalized using the Hertz equations, the data (dent depth vs. stress) are comparable. Thus when designing bearings made from 60NiTi, the Hertz stress relations can be applied with relative confidence over a range of rolling element sizes and internal geometries.

bearings↗