Search NASA⌕ Search

SEARCH · Search NASA

Results for “Interphase boundary”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Microstructural Changes to Thermally Sprayed Materials Subjected to Dynamic Compression

Dynamic compression of materials can induce a variety of microstructural changes. As thermally-sprayed materials have highly complex microstructures, the expected pressure at which changes occur cannot be predicted a priori. In addition, typical in-situ measurements such as velocimetry are unable to adequately diagnose microstructural changes such as failure or pore collapse. Quasi-isentropic compression experiments with sample recovery were conducted to examine microstructural changes in thermally sprayed tantalum and tantalum-niobium blends up to 8 GPa pressure. Spall fracture was observed in all tests, and post-shot pore volume decreased relative to the initial state. The blended material exhibited larger spall planes with fracture occurring at interphase boundaries. An estimate of the pressure at which pore collapse is complete was determined to be ~26 GPa for pure tantalum and ~19 GPa for the tantalumniobium blend under these loading conditions.

36 MATERIALS SCIENCE↗

Protective coatings with nanoscale multilayer architecture: current state and main trends

Binary systems (layers) and multicomponent layers with bilayer thicknesses varying from microns to a few nanometers are considered. A strong dependence of the microstructure formation on the deposition conditions (the magnitude of the bias potential, the flow of inert and reactive gases, the ion beam power (current density) supplied to the target) is found. General regularities in the change in the functional properties and structural state of the coatings are formulated. The conditions for the formation of a columnar structure and growth texture are noted; various mechanisms and their interpretation are proposed. Finally, the relationship among the size of nanograins, diffusion at the interphase boundary, and effects determining the physico-mechanical, tribological characteristics, as well as resistance to corrosion and oxidation, is shown.

36 MATERIALS SCIENCE↗

Enhanced Radiation Damage Tolerance of Amorphous Interphase and Grain Boundary Complexions in Cu-Ta

Amorphous interfacial complexions are particularly resistant to radiation damage and have been primarily studied in alloys with good glass-forming ability, yet recent reports suggest that these features can form even in immiscible alloys such as Cu-Ta under irradiation. In this work, the mechanisms of damage production and annihilation due to primary knock-on atom collisions are investigated for amorphous interphase and grain boundaries in a Cu-Ta alloy using atomistic simulations. Amorphous complexions, in particular amorphous interphase complexions that separate Cu and Ta grains, result in less residual defect damage than their ordered counterparts. Stemming from the nanophase chemical separation in this alloy, the amorphous complexions exhibit a highly heterogeneous distribution of atomic excess volume, as compared to a good glass former like Cu-Zr. Complexion thickness, a tunable structural descriptor, plays a vital role in damage resistance. Thicker interfacial films are more damage-tolerant because they alter the defect production rate due to differences in intrinsic displacement threshold energies during the collision cascade. Overall, the findings of this work highlight the importance of interfacial engineering in enhancing the properties of materials operating in radiation-prone environments and the promise of amorphous complexions as particularly radiation damage-tolerant microstructural features.

36 MATERIALS SCIENCE↗

Observation of [VCu1–Ini2+VCu1–] Defect Triplets in Cu-Deficient CuInS2

Copper indium disulfide (CuInS2) is a semiconductor with a direct energy band gap of 1.53 eV, an optimal value for highly efficient thin-film solar cells. But it has reached only ~ 11 % power conversion efficiency, far less than the theoretically achievable value of ~ 30 %. The cause of this low performance is not understood. A single crystal grown from 1 mol% Cu-deficient melt was studied, using atomic resolution high-angle annular dark-field (HAADF) scanning transmission electron microscopy (STEM) and electron dispersive spectroscopy (EDS). While the bulk crystal is exactly stoichiometric CuInS2, it contains nanometer-thick, structurally coherent, Cu-deficient interphases that form along rotational twin boundaries in the {112} plane. Transition zones from bulk crystal to interphase are observed, where In is seen to move from its normal site InIn in the chalcopyrite structure to a tetrahedral interstitial site Ini, while Cu remains in its normal CuCu position. Two InIn rows of the bulk crystal merge into one row of Ini, causing excess Ini in the interphase. The concentrations of CuCu and Ini reflect a ratio of Cu vacancies, VCu, to excess Ini of ~ 2. Their relative lattice positions, and the high electrical resistivity of the crystal, suggests that VCu and excess Ini ‘precipitate’ as self-compensating, electrically neutral, [VCu1- Ini2+ VCu1-] defect triplets. This is the first atomic-level observation of the ordered defect that has been invoked as the basic structural modifier in chalcopyrite compound homologs. The interphases introduce an optical gap of 1.47 eV. Electron trapping in band tail states, evident from a photoconductivity exponent of 0.54, is the likely cause of an unusually low electron mobility of 0.1 cm2V-1s-1. The overall result is that making CuInS2 slightly copper-poor inserts nanometer-thick layers of the interphase into the bulk crystal. This study shows that apparently conflicting results of the effect of Cu deficiency on CuInS2 thin-film solar cells may be resolved by analyzing structure and composition at nanometer spatial resolution.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanistic origins of corrosion protection of aluminum alloys by graphene/polyetherimide nanocomposite coatings

Light-weighting vehicular components through adoption of light-metal structural alloys holds promise for reducing the fuel consumption of internal combustion engine vehicles and increasing the range of battery electric vehicles. However, the alloyed microstructure and surface precipitates of aluminum alloys render these materials susceptible to corrosion under modest excursions from neutral pH. Traditional chromium-based anodic passivation layers are subject to increasingly stringent environmental regulations, whereas options for sacrificial cathodic films are sparse for electropositive metals. While hybrid nanocomposite coatings have shown initial promise, mechanistic underpinnings remain poorly understood. Here, a fully imidized polyetherimide (PEI) resin is utilized as the continuous phase with inclusion of unfunctionalized exfoliated graphite (UFG). A comprehensive investigation of the mechanisms of corrosion protection reveals key fundamental design principles underpinning corrosion inhibition. First, strong interfacial adhesion, which for PEI is facilitated by binding of imide carbonyl moieties to Lewis acidic sites on Al surfaces. Second, the miscibility of ion-impervious nanoscopic UFG fillers and stabilization of a substantial interphase region at UFG/PEI boundaries that result in minimizing the free volume at the filler/polymer interface. Finally, extended tortuosity of ion diffusion pathways imbued by the below-percolation-threshold 2D fillers. These three design principles help govern and modulate ion transport from electrolyte/coating interfaces to the coating/metal interface and are crucial for the extended preservation of barrier properties. The results suggest an approach to systematically activate multiple modes of corrosion inhibition through rational design of hybrid nanocomposite coatings across hard-to-abate sectors where light metal alloys are likely to play an increasingly prominent role.

36 MATERIALS SCIENCE↗

MST-8 Colloquium: The Effect of Microstructure on the Spall Strength and Damage of 1045 Steel [Slides]

Three different microstructures of the same steel alloy were investigated to study the influence of microstructure on spall strength and damage. Microstructure influences spall behavior within the explored dynamic regime. Second phase morphology, interphase interface characteristics, and grain boundary character shown to influence spall behavior. Continued understanding of microstructure’s influence on spall and damage needed for targeted material design.

36 MATERIALS SCIENCE↗

Morphological Evolution and Dealloying During Corrosion of Ni20Cr (wt.%) in Molten FLiNaK Salts

The dealloying corrosion behavior of the FCC Ni20Cr (wt%) in molten LiF-NaF-KF (FLiNaK) salts at 600 °C under varying applied potentials was investigated. Using in-operando electrochemical techniques and a multi-modal suite of characterization methods, we connect electrochemical potential, thermodynamic stability, and electro-dissolution kinetics to the corrosion morphologies. Notably, under certain potential regimes, a micron-scale bicontinuous structure, characterized by a network of interconnected pores and ligaments riched with the composition of the more noble (MN) element, becomes prominent. At other potentials both MN and less noble (LN) elements dealloy but at different rates. The dealloying process consists of lattice and grain boundary diffusion of Cr to the metal/salt interface, interphase Cr oxidation, accompanied by surface diffusion of Ni to form interconnected ligaments. At higher potentials, the bicontinuous porous structure undergoes further surface coarsening. Concurrently, Cr(II), Cr(III), and Ni(II) begin to dissolve, with the dissolution of Ni occurring at a significantly slower rate. When solid-state transport of Cr is exceeded by the interfacial rates, dealloying depths are limited.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Superior Piezo-/Ferro-Electricity in Antiferroelectric Ag x NbO 3-δ Thin Films by Nanopillar Local Structure Design

Antiferroelectrics are fundamental mother compounds critical in developing innovative lead-free piezoelectrics and ferroelectrics and hold great promise for wide-ranging applications in energy conversion and electronic devices. However, harnessing their superior properties presents a significant challenge due to the delicate balance required between their various states. Here, in this study, through the unique design of nanopillar structures to alleviate the local polar heterogeneity, we have achieved significantly improved piezo-/ferro-electricity in classic lead-free antiferroelectric Ag x NbO 3-δ (x = 1, 0.9, and 0.8) epitaxial thin films. The effective piezoelectric coefficient reaches 440 pm V –1 , 1 order of magnitude larger than the stoichiometric AgNbO 3 , rivaling classic lead zirconate titanate piezoelectrics. Atomic-scale electron microscopy investigations unravel the underlying mechanisms. The nanopillars, characterized by antisite occupancy of both Ag and Nb atoms and forming out-of-phase boundaries with the matrix, reduce the local crystal symmetry via interphase strain. This leads to the creation of flexible multinanodomain structures that significantly facilitate polarization rotation, thus substantially enhancing the piezoelectric performance. This study demonstrates the feasibility of engineering local heterogeneity through nanopillar design, offering a generally applicable method for property improvement of a wide range of antiferroelectrics.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tuning the Anode–Electrolyte Interface Chemistry for Garnet-Based Solid-State Li Metal Batteries

Lithium (Li) metal anode is a promising candidate for high energy density solid-state batteries. However, the interface issues, including large interfacial resistance and Li dendrite generation, have always frustrated the attempt to commercialize solid-state Li metal batteries (SSLBs). Here, we report that infusing the garnet-type solid electrolytes (GSEs) with air-stable electrolyte Li 3 PO 4 (LPO) dramatically reduces the interfacial resistance to ~1 Ω cm 2 and achieves a high critical current density of 2.2 mA cm -2 under ambient condition due to enhanced interfacial stability to Li metal anode. The coated and infused LPO electrolytes not only improve the mechanical strength and Li-ion conductivity of grain boundaries, but also form a stable Li-ion conductive but electron-insulating LPO-derived solid-electrolyte interphase between Li metal and GSEs, and consequently eliminates the Li dendrites growth and prevents the direct reduction of GSEs by Li metal over a long cycle life. This interface engineering approach together with grain-boundary modification on GSEs represents a promising strategy to revolutionize the anode-electrolyte interface chemistry for SSLBs and provides new design strategy for other-types of solid-state batteries.

25 ENERGY STORAGE↗

The Importance of a Moving Boundary Approach for Modeling the SEI Layer Growth to Predict Capacity Fade

One of the contributing factors to the aging of lithium-ion batteries is the growth of the solid-electrolyte interphase (SEI) layer. The growth of the SEI layer leads to the irreversible loss of lithium available for cycling and increases the resistance of the battery. Physics-based models in literature model the kinetically limited or solvent diffusion-limited growth. In such models, the interface resistance is a constant, and the contribution to the overpotential of the intercalation reaction from the SEI layer is considered to be ohmic. In this study, we propose a model that describes the growth of the SEI layer on the electrode surface as a moving interface. The transport of lithium ions and the solvent in the electrolyte are affected by this moving interface. The equations that govern the species transport and the potential drop across the SEI layer are derived from dilute solution theory and solved by transforming the coordinates of the moving boundary. The ion transport induces changes in the conductivity across the SEI layer, which affects the potential drop that arises due to its growth. The effects of this potential on capacity fade are studied over cycling the battery.

25 ENERGY STORAGE↗

Single-phase local-high-concentration solid polymer electrolytes for lithium-metal batteries

Solid polymers are promising electrolytes for Li-metal batteries, but they have limitations: they cannot simultaneously achieve high ionic conductivity, good mechanical strength and compatibility with high-voltage cathodes while suppressing Li dendrites. Here, we design a class of locally high-concentration solid polymer electrolytes based on polymer blends, which are termed Li-polymer in F diluter (LPIFD). The Li-polymer (polymer-in-salt) ensures continuous Li-ion conduction channels and contributes to the solid electrolyte interphase (SEI), and the F diluter (inert fluorinated polymer) adds mechanical strength. Studies reveal that a single-phase LPIFD, which is based on a miscible polymer blend, lacks phase boundaries and forms an organic-less and LiF-rich SEI, effectively suppressing lithium dendrites. The single-phase LPIFD delivers ionic conductivity of 3.0 x 10 -4 S cm -1 and enables the Li anode to reach a high coulombic efficiency of 99.1% and a critical current density of 3.7 mA cm -2 . Furthermore, the ability to form an F-rich cathode electrolyte interphase allows LiNi 0.8 Co 0.1 Mn 0.1 O 2 ||Li cells to achieve a cycle life of 450 cycles at a high operating voltage of 4.5 V. In conclusion, this design will inspire efforts to commercialize polymer electrolytes for high-energy Li-metal batteries.

25 ENERGY STORAGE↗

Electron leakage through heterogeneous LiF on lithium–metal battery anodes

The solid–electrolyte interphase (SEI) that forms on lithium ion battery (LIB) anodes prevents degradation-causing transfer of electrons to the electrolyte. Grain boundaries (GBs) between different SEI components, like LiF, have been suggested to accelerate Li+ transport. However, using the non-equilibrium Green's function technique with density functional theory (NEGF-DFT), we find that GBs enhance electron tunneling in thin LiF films by 1–2 orders of magnitude, depending on the bias. Extrapolating to thicker films using the Wentzel–Kramers–Brillouin (WKB) method emphasizes that safer batteries require passivation of GBs in the SEI.

25 ENERGY STORAGE↗

Effect of Propagating Dopant Reactivity on Lattice Oxygen Loss in LLZO Solid Electrolyte Contacted with Lithium Metal

Lithium lanthanum zirconium oxide (LLZO) is widely known as the most stable solid electrolyte against lithium metal electrodes. This thermodynamic stability can be lost by the presence of dopants which are required to stabilize the cubic phase of LLZO and can be reduced by lithium metal. However, the role of oxygen in such reactions is taken for granted. In this work, the reduction of Nb-substituted LLZO (Nb-LLZO) is explored by Li metal and shows that interfacial reactions propagate and lead to the decomposition with substantial Nb 5+ reduction deep into the bulk electrolyte. Scanning Transmission Electron Microscopy with Energy Dispersive X-ray Spectroscopy and thermogravimetric analyses show much of the reduction is due to oxygen vacancies formed, leading to increased electronic conductivity mapped with conductive Atomic Force Microscopy. Density functional theory calculations indicate oxygen release is favored by increased excess lithiation of Nb-LLZO. Electrochemical impedance of polycrystalline Nb-LLZO shows the continuous evolution of ionically resistive interphases near the lithium metal interface with Nb-LLZO while single crystals show little reactivity at room temperature and self-limiting reduction at 60°C. This work underlines the role of grain boundaries in propagating destructive solid electrolyte reactions and highlights previously unseen mechanisms involving lattice oxygen in LLZO.

Li metal, solid-state electrolytes↗

Machine-Learning-Guided Insights into Solid-Electrolyte Interphase Conductivity: Are Amorphous Lithium Fluorophosphates the Key?

Despite decades of study, the identity of the dominant Li + -conducting phase within the inorganic SEI of Li-ion batteries remains unresolved. While the mosaic model describes LiF/Li 2 O/Li 2 CO 3 nanocrystallites within a disordered matrix, these crystalline phases inherently offer limited ionic conductivity. Growing evidence suggests that interfaces, grain boundaries, and amorphous phases may instead host the primary fast-ion pathways. Using diffusion-based generative structure prediction and machine-learning interatomic potentials (MLIPs), we investigate lithium difluorophosphate (LiPO 2 F 2 ), a key mixed-anion decomposition product of phosphorus- and fluorine-containing electrolytes. We identify a stable crystalline polymorph and demonstrate that the amorphous counterpart is conductive, with projected room-temperature σ ≈ 0.18 mS cm –1 and E a ≈ 0.40 eV. Here, this enhancement stems from structural disorder flattening the Li site-energy landscape and a low formation energy for Li-interstitial defects, which supplies additional mobile carriers. We propose amorphous mixed-anion Li-P-O-F phases as a promising conducting medium in the SEI, offering a specific target for engineering improved battery interfaces.

Zhong, Peichen [University of California, Berkeley↗

Non‐Linear Kinetics of The Lithium Metal Anode on Li 6 PS 5 Cl at High Current Density: Dendrite Growth and the Role of Lithium Microstructure on Creep

Abstract Interfacial instability, viz., pore formation in the lithium metal anode (LMA) during discharge leading to high impedance, current focusing induced solid–electrolyte (SE) fracture during charging, and formation/behaviour of the solid–electrolyte interphase (SEI), at the anode, is one of the major hurdles in the development of solid‐state batteries (SSBs). Also, understanding cell polarization behaviour at high current density is critical to achieving the goal of fast‐charging battery and electric vehicle. Herein, via in situ electrochemical scanning electron microscopy (SEM) measurements, performed with freshly deposited lithium microelectrodes on transgranularly fractured fresh Li6PS5Cl (LPSCl), the LiǀLPSCl interface kinetics are investigated beyond the linear regime. Even at relatively small overvoltages of a few mV, the LiǀLPSCl interface shows non‐linear kinetics. The interface kinetics possibly involve multiple rate‐limiting processes, i.e., ion transport across the SEI and SE|SEI interfaces, as well as charge transfer across the LiǀSEI interface. The total polarization resistance R P of the microelectrode interface is determined to be ≈ 0.8 Ω cm 2 . It is further shown that the nanocrystalline lithium microstructure can lead to a stable LiǀSE interface via Coble creep along with uniform stripping. Also, spatially resolved lithium deposition, i.e., at grain surface flaws, grain boundaries, and flaw‐free surfaces, indicates exceptionally high mechanical endurance of flaw‐free surfaces toward cathodic load (>150 mA cm −2 ). This highlights the prominent role of surface defects in dendrite growth.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗