Low earth orbit environmental effects on osmium and related optical thin-film coatings

A number of samples of optical thin film materials were flown on Shuttle flight STS-8 as part of an experiment to evaluate their interaction with residual atomic oxygen in low earth orbit. Osmium was selected because of its usefulness as a reflective optical coating for far-UV instruments and for confirmation of results from previous Shuttle flights in which such coatings disappeared. Reflectance data and photographic evidence are presented to support the hypothesis that the osmium disappearance is due to reaction with oxygen to form a volatile oxide. Platinum and iridium, which were included for comparison, fared much better.

Gull, T. R.↗

Ellipsometric method for the measurement of temperature and optical constants of incandescent transition metals

The development of a unique noncontact temperature measurement device utilizing rotating analyzer ellipsometry is described. The technique circumvents the necessity of spectral emissivity estimation by direct measurement concomitant with radiance brightness. Simultaneous determinations of dielectric constants and refractive indices allow changes in the physical and chemical state of a heated surface to be monitored. The results of optical property measurements at 633 nm as functions of temperature between 1000 and 2500 K for eight transition metals including Hf, Ir, Mo, Nb, Pd, Pt, Ta, and V are presented together with preliminary results of oxidation studies on iridium.

Hansen, George P.↗

Advanced Small Rocket Chambers. Basic Program and Option 2: Fundamental Processes and Material Evaluation

Propellants, chamber materials, and processes for fabrication of small high performance radiation cooled liquid rocket engines were evaluated to determine candidates for eventual demonstration in flight-type thrusters. Both storable and cryogenic propellant systems were considered. The storable propellant systems chosen for further study were nitrogen tetroxide oxidizer with either hydrazine or monomethylhydrazine as fuel. The cryogenic propellants chosen were oxygen with either hydrogen or methane as fuel. Chamber material candidates were chemical vapor deposition (CVD) rhenium protected from oxidation by CVD iridium for the chamber hot section, and film cooled wrought platinum-rhodium or regeneratively cooled stainless steel for the front end section exposed to partially reacted propellants. Laser diagnostics of the combustion products near the hot chamber surface and measurements at the surface layer were performed in a collaborative program at Sandia National Laboratories, Livermore, CA. The Material Sample Test Apparatus, a laboratory system to simulate the combustion environment in terms of gas and material temperature, composition, and pressure up to 6 Atm, was developed for these studies. Rocket engine simulator studies were conducted to evaluate the materials under simulated combustor flow conditions, in the diagnostic test chamber. These tests used the exhaust species measurement system, a device developed to monitor optically species composition and concentration in the chamber and exhaust by emission and absorption measurements.

Jassowski, Donald M.↗

NASA Tech Briefs, September 2011

Topics covered include: Fused Reality for Enhanced Flight Test Capabilities; Thermography to Inspect Insulation of Large Cryogenic Tanks; Crush Test Abuse Stand; Test Generator for MATLAB Simulations; Dynamic Monitoring of Cleanroom Fallout Using an Air Particle Counter; Enhancement to Non-Contacting Stress Measurement of Blade Vibration Frequency; Positively Verifying Mating of Previously Unverifiable Flight Connectors; Radiation-Tolerant Intelligent Memory Stack - RTIMS; Ultra-Low-Dropout Linear Regulator; Excitation of a Parallel Plate Waveguide by an Array of Rectangular Waveguides; FPGA for Power Control of MSL Avionics; UAVSAR Active Electronically Scanned Array; Lockout/Tagout (LOTO) Simulator; Silicon Carbide Mounts for Fabry-Perot Interferometers; Measuring the In-Process Figure, Final Prescription, and System Alignment of Large; Optics and Segmented Mirrors Using Lidar Metrology; Fiber-Reinforced Reactive Nano-Epoxy Composites; Polymerization Initiated at the Sidewalls of Carbon Nanotubes; Metal-Matrix/Hollow-Ceramic-Sphere Composites; Piezoelectrically Enhanced Photocathodes; Iridium-Doped Ruthenium Oxide Catalyst for Oxygen Evolution; Improved Mo-Re VPS Alloys for High-Temperature Uses; Data Service Provider Cost Estimation Tool; Hybrid Power Management-Based Vehicle Architecture; Force Limit System; Levitated Duct Fan (LDF) Aircraft Auxiliary Generator; Compact, Two-Sided Structural Cold Plate Configuration; AN Fitting Reconditioning Tool; Active Response Gravity Offload System; Method and Apparatus for Forming Nanodroplets; Rapid Detection of the Varicella Zoster Virus in Saliva; Improved Devices for Collecting Sweat for Chemical Analysis; Phase-Controlled Magnetic Mirror for Wavefront Correction; and Frame-Transfer Gating Raman Spectroscopy for Time-Resolved Multiscalar Combustion Diagnostics.

Source record↗

Characterization of Iridium Coated Rhenium Used in High-Temperature, Radiation-Cooled Rocket Thrusters

Materials used for radiation-cooled rocket thrusters must be capable of surviving under extreme conditions of high-temperatures and oxidizing environments. While combustion efficiency is optimized at high temperatures, many refractory metals are unsuitable for thruster applications due to rapid material loss from the formation of volatile oxides. This process occurs during thruster operation by reaction of the combustion products with the material surface. Aerojet Technical Systems has developed a thruster cone chamber constructed of Re coated with Ir on the inside surface where exposure to the rocket exhaust occurs. Re maintains its structural integrity at high temperature and the Ir coating is applied as an oxidation barrier. Ir also forms volatile oxide species (IrO2 and IrO3) but at a considerably slower rate than Re. In order to understand the performance limits of Ir-coated Re thrusters, we are investigating the interdiffusion and oxidation kinetics of Ir/Re. The formation of iridium and rhenium oxides has been monitored in situ by Raman spectroscopy during high temperature exposure to oxygen. For pure Ir, the growth of oxide films as thin as approximately 200 A could be easily detected and the formation of IrO2 was observed at temperatures as low as 600 C. Ir/Re diffusion test specimens were prepared by magnetron sputtering of Ir on Re substrates. Concentration profiles were determined by sputter Auger depth profiles of the heat treated specimens. Significant interdiffusion was observed at temperatures as low as 1000 C. Measurements of the activation energy suggest that below 1350 C, the dominant diffusion path is along defects, most likely grain boundaries, rather than bulk diffusion through the grains. The phases that form during interdiffusion have been examined by x ray diffraction. Analysis of heated test specimens indicates that the Ir-Re reaction produces a solid solution phase of Ir dissolved in the HCP structure of Re.

Stulen, R. H.↗

Oxide Protective Coats for Ir/Re Rocket Combustion Chambers

An improved material system has been developed for rocket engine combustion chambers for burning oxygen/ hydrogen mixtures or novel monopropellants, which are highly oxidizing at operating temperatures. The baseline for developing the improved material system is a prior iridium/rhenium system for chambers burning nitrogen tetroxide/monomethyl hydrazine mixtures, which are less oxidizing. The baseline combustion chamber comprises an outer layer of rhenium that provides structural support, plus an inner layer of iridium that acts as a barrier to oxidation of the rhenium. In the improved material system, the layer of iridium is thin and is coated with a thermal fatigue-resistant refractory oxide (specifically, hafnium oxide) that serves partly as a thermal barrier to decrease the temperature and thus the rate of oxidation of the rhenium. The oxide layer also acts as a barrier against the transport of oxidizing species to the surface of the iridium. Tests in which various oxygen/hydrogen mixtures were burned in iridium/rhenium combustion chambers lined with hafnium oxide showed that the operational lifetimes of combustion chambers of the improved material system are an order of magnitude greater than those of the baseline combustion chambers.

Fortini, Arthur↗

Single Crystal Membranes

Single crystal a- and c-axis tubes and ribbons of sodium beta-alumina and sodium magnesium beta-alumina were grown from sodium oxide rich melts. Additional experiments grew ribbon crystals containing sodium magnesium beta, beta double prime, beta triple prime, and beta quadruple prime. A high pressure crystal growth chamber, sodium oxide rich melts, and iridium for all surfaces in contact with the melt were combined with the edge-defined, film-fed growth technique to grow the single crystal beta-alumina tubes and ribbons. The crystals were characterized using metallographic and X-ray diffraction techniques, and wet chemical analysis was used to determine the sodium, magnesium, and aluminum content of the grown crystals.

Stormont, R. W.↗

High-temperature oxidation and erosion-resistant refractory coatings

Various refractory coating systems were evaluated for rocket nozzle applications by actual rocket test firings. A reference is noted which identifies failure mechanisms and gives results of the firing tests for 18 coating systems. Iridium, iridium-rhenium, and hafnium oxide-zirconium oxide coatings show most promising results.

Peterson, D. A.↗

High-temperature oxidation of a rapidly solidified amorphous Ta-Ir alloy

The oxidation products formed at 500 and 700 C on an amorphous Ta-44.5 at. pct Ir alloy in an Ar-0.1 percent O2 gas mixture were characterized using SEM, XRD, EPMA, TEM, STEM, AES, and XPS. Initially, a thin (3-4 nm) layer of Ta2O5 formed at the surface of the alloy. Continued growth of the Ta2O5, which occurred very rapidly, involved diffusion of oxygen anions from the Ta2O5/gas interface to the alloy/Ta2O5 interface, where tantalum was selectively oxidized. Because the oxide grew more quickly than iridium could diffuse back into the alloy, the iridium coalesced into platelets of crystalline iridium-rich alloy that were oriented approximately parallel to the oxide/alloy interface, and which became embedded in a matrix of Ta2O5. The unoxidized core remained in the glassy state. The oxidation process and/or the dissolution of oxygen into the unoxidized alloy caused the alloy to become embrittled.

Cotell, Catherine M.↗

IR-doped ruthenium oxide catalyst for oxygen evolution

A method for preparing a metal-doped ruthenium oxide material by heating a mixture of a doping metal and a source of ruthenium under an inert atmosphere. In some embodiments, the doping metal is in the form of iridium black or lead powder, and the source of ruthenium is a powdered ruthenium oxide. An iridium-doped or lead-doped ruthenium oxide material can perform as an oxygen evolution catalyst and can be fabricated into electrodes for electrolysis cells.

Valdez, Thomas I.↗

The development of materials capable of operation in an oxidizing atmosphere for extended periods of time

An evaluation is presented of silicon carbide, zirconium diboride, and iridium-coated graphite as materials for construction of furnace cores which could operate under highly oxidizing conditions at temperatures of approximately 2,200 C in the presence of molten aluminum oxide. It was found that silicon carbide and zirconium diboride could not withstand oxidizing atmospheres in the presence of aluminum oxide at temperature 2,200 C. However, graphite furnace cores coated with iridium were found to be useful furnace cores at 2,200 C in an oxidizing atmosphere for reasonably extended periods of time.

Duhamel, A. P.↗

Partial analysis of experiment LDEF A-0114

Due to delays in manifesting the return of the Long Duration Exposure Facility from space, attention was concentrated on extracting the maximum information from the EIOM-2 (oxygen interaction with materials experiment) flown on STS-8 in September 1983. An analysis was made of the optical surfaces exposed during that flight and an assessment made of the effect of the 5 eV atomic oxygen upon their physical and chemical properties. The surfaces studied were of two types: high-purity thin films sputtered or evaporated onto 2.54-cm diam lambda/20 fused silica optical flats, and highly polished bulk samples. Rapid etching of carbon and carbonaceous surfaces was observed with polycarbonate CR-39 showing the largest etch of any substrate flown and measured. Of the metals tested, only osmium and silver showed large effects, the former being heavily etched and the later forming a very thick layer of oxide. The first measurable effects on iridium, aluminum, nickel, tungsten and niobium thin films are reported.

Gregory, J. C.↗

Niobium matrix composites for high temperature turbine blades, phase 2

This program demonstrated the feasibility of fabricating fiber-reinforced MMC (niobium matrix) turbine blades to net shape by chemical vapor infiltration (CVI). A controllable, repeatable niobium infiltration process was developed, and the kinetics of both deposition and infiltration were studied. Several continuous refractory fibers (Nicalon, Nextel 440, FP-Al2O3, HPZ, and tungsten mesh) were investigated as potential reinforcements for strengthening niobium. Thermodynamic and experimental evaluation indicated FP-Al2O3 and tungsten to be the most chemically compatible with niobium, while Nicalon, FP-Al2O3, and tungsten were found to be best with regard to reinforcing capability. Finally, a protective coating for iridium was found to provide substantial oxidation protection to the niobium blade matrix.

Heng, Sangvavann↗

Long Life Testing of Oxide-Coated Iridium/Rhenium Rockets

22-N class rockets, composed of a rhenium (Re) substrate, an iridium (Ir) coating, and an additional composite coating consisting of Ir and a ceramic oxide, were tested on gaseous oxygen/gaseous hydrogen (GO2/GH2) propellants. Two rockets were tested, one for nearly 39 hours at a nominal mixture ratio (MR) of 4.6 and chamber pressure (Pc) of 469 kPa, and the other for over 13 hours at a nominal MR of 5.8 and 621 kPa Pc. Four additional Ir/Re rockets, with a composite Ir-oxide coating fabricated using a modified process, were also tested, including one for 1.3 hours at a nominal MR of 16.7 and Pc of 503 kPa. The long lifetimes demonstrated on low MR GO2/GH2 suggest greatly extended chamber lifetimes (tens of hours) in the relatively low oxidizing combustion environments of Earth storable propellants. The oxide coatings could also serve as a protective coating in the near injector region, where a still-mixing flowfield may cause degradation of the Ir layer. Operation at MR close to 17 suggests that oxide-coated Ir/Re rockets could be used in severely oxidizing combustion environments, such as high MR GO2/GH2, oxygen/hydrocarbon, and liquid gun propellants.

Reed, Brian D.↗

Advanced Materials and Manufacturing for Low-Cost, High-Performance Liquid Rocket Combustion Chambers

A document describes the low-cost manufacturing of C103 niobium alloy combustion chambers, and the use of a high-temperature, oxidation-resistant coating that is superior to the standard silicide coating. The manufacturing process involved low-temperature spray deposition of C103 on removable plastic mandrels produced by rapid prototyping. Thin, vapor-deposited platinum-indium coatings were shown to substantially improve oxidation resistance relative to the standard silicide coating. Development of different low-cost plastic thrust chamber mandrel materials and prototyping processes (selective laser sintering and stereolithography) yielded mandrels with good dimensional accuracy (within a couple of mils) for this stage of development. The feasibility of using the kinetic metallization cold-spray process for fabrication of free-standing C1O3 thrusters on removable plastic mandrels was also demonstrated. The ambient and elevated temperature mechanical properties of the material were shown to be reasonably good relative to conventionally processed C103, but the greatest potential benefit is that coldsprayed chambers require minimal post-process machining, resulting in substantially lower machining and material costs. The platinum-iridium coating was shown to provide greatly increased oxidation resistance over the silicide when evaluated through oxyacetylene torch testing to as high as 300 F (= 150 C). The iridium component minimizes reaction with the niobium alloy chamber at high temperatures, and provides the high-temperature oxidation resistance needed at the throat.