Grain boundary zirconia-modified garnet solid-state electrolyte

Here, we report a method for promoting electrochemical stability in garnet Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 solid-state electrolyte based on a composite two-phase oxide–oxide microstructure. Grain boundary precipitation of the controlled distribution of amorphous zirconium oxide microparticles is achieved through the addition of reactive tantalum carbide. During ambient-atmosphere sintering, the carbide decomposes through an in situ reaction, the ‘extra’ Ta substituting for Zr within the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 lattice. Density functional theory (DFT) calculations identify a thermodynamically favourable reaction path and show how substituting Ta 5+ at Zr 4+ sites affects the crystal structure as well as bulk ionic and electronic conductivities. Quantitative stereology highlights that zirconia also acts as a sintering aid, reducing compact porosity. Cryogenic focused-ion-beam scanning electron microscopy and fractography analysis of cycled solid-state electrolytes illustrates that near-universally observed intergranular Li-metal dendrite propagation is suppressed by the two-phase microstructure, favouring transgranular dendrites instead. Importantly, DFT demonstrates that compared with the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 surface, the zirconium oxide surface per se is less electronically conductive and does not trap excess electrons to reduce Li ions. This is a key reason for the substantial improvement in the electrochemical properties over the single-phase baseline.

36 MATERIALS SCIENCE

Rapid scalable plasma processing of thin-film Li–La–Zr–O solid-state electrolytes

Solid-state electrolytes, such as lithium lanthanum zirconium oxide (LLZO), show promise as technologies for next-generation high-energy-density batteries, but commercial development has been hindered by a lack of scalable processing methods. Current fabrication methods are costly or require long annealing steps to create dense films. We report an atmospheric pressure blown-arc nitrogen plasma jet process to rapidly form sub-micrometer-thick, dense amorphous LLZO (a-LLZO) films from sol-gel precursors. Films are processed in less than 2 min, an order of magnitude faster than what has previously been reported. We demonstrate 500-nm-thick a-LLZO films processed at 350°C with an ionic conductivity of 2 × 10 −6 S/cm at 30°C and 2 × 10 −3 S/cm at 100°C and a conductance of 19 S at 100°C, the highest conductance of any LLZO phase to date. Here, the films exhibit outstanding smooth surface morphology with low defectivity, advancing atmospheric plasma processing as a scalable processing method for solid-state electrolytes.

25 ENERGY STORAGE

Digital light processing of porous LLZTO scaffolds for Li-garnet solid-state batteries

Li 7 La 3 Zr 2 O 12 (LLZO)-based solid-state electrolytes (SEs) are promising materials for next-generation solid-state batteries. In this work, digital light processing (DLP), an emerging additive manufacturing technology, is employed to produce porous Ta-doped LLZO (LLZTO) scaffolds. The self-standing scaffolds are 100 μm thick and have 40% porosity. The scaffolds demonstrate symmetric cell cycling stability exceeding 1,500 h at 0.1 mA/cm2 current density, with a capacity of 0.1 mAh/cm 2 (1 h for each half cycle). At higher current densities, reversible soft shorts frequently happen, while immediate hard shorts are prevented due to Li dendrite growth being hindered by the tortuous pore network. In addition to the cycling stability, the phase stability of LLZTO is investigated during the post-printing thermal process for printing resin removal. We discovered that the LLZTO partially decomposes into Li 2 Zr 2 O 7 and other impurity phases from 400°C to 800°C, but the pure LLZTO phase is restored upon the completion of resin removal beyond 800°C.

Li-metal anode

Effects of Al concentration on the structure and conductivity of lithium lanthanum zirconium oxide

Cubic Li 7-3x Al x La 3 Zr 2 O 12 (LLZO) is a promising, next-generation solid electrolyte due to its stability with Li-metal and high bulk conductivity (~1 mS cm -1 ). However, the source of the high conductivity is not completely understood. In this work, we address this key knowledge gap through the integration of elemental analysis, neutron diffraction sensitive to Li and O atoms, and impedance spectroscopy to understand the structure–property correlations for LLZO. We show the metal–oxygen framework structure remains constant with variation in Al substitution, resulting in a constant activation energy of ~0.35 eV and little effect on the bulk conductivity. Instead, Li concentration, Al blocking and trapping of mobile defects, and Li–Li nearest neighbor interactions largely control the Al substituted LLZO bulk conductivity, resulting in decreases from 0.73 to 0.22 mS cm -1 as the Al concentration increases from 0.17 to 0.32 mol. These results differ from those of Ta substituted LLZO, where the framework structure and Li–Li site distances play large roles in controlling the conductivity. The increased understanding of the controlling factors of conductivity allows for greater ability to tailor the design of and substitution into the LLZO structure for improved conductivity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

The Key Role of Grain Boundary Dynamics in Revolutionizing the Potential of Solid Electrolytes

Solid electrolytes (SEs) have the potential to enhance the safety and performance of Li-metal batteries. However, the existence of grain boundaries in polycrystalline SEs presents a significant challenge for both ionic and electronic migration, promoting the propagation of detrimental lithium dendrites. This study compares the roles of grain boundaries in electrical properties of three distinct SEs including garnet-type Li 6.5 La 3 Zr 1.5 Ta 0.5 O 12 (LLZO), argyrodite-type Li 6 PS 5 Cl (LPSC), and NASICON-type Li 1+x+y Al x (Ti,Ge) 2-x Si y P 3-y O 12 (LATP). Results demonstrate that the electronic and ionic conductivities of solid-state electrolytes are affected differently by grain boundaries, depending on the specific type of electrolyte. For instance, LLZO and LATP experience dielectric breakdown at 3.7 and 5.3 V, respectively, while LPSC does not exhibit such behavior. Here, a new chemical modification is proposed that simultaneously alters the composition of both the surface and grain boundaries of SEs, ultimately reducing electronic conductivity for the LLZO SEs. Consequently, the proposed LLZO exhibits unprecedented dendrite-free cycling stability, achieving a remarkable 12 000-h lifetime at room temperature, surpassing conventional strategies such as surface coatings in dendrite mitigation. This study highlights the significance of modifying grain boundaries to design safe and durable Li-metal batteries. It provides new insights for developing SEs that are highly resistant to dendrite formation.

36 MATERIALS SCIENCE

Lithium Dendrite-Free Li 7 N 2 I-LiOH Solid Electrolytes for High Energy Lithium Batteries

All-solid-state lithium batteries (ASSLBs) hold great potential to improve the safety and energy density of today’s lithium-ion batteries by using non-flammable inorganic solid electrolytes. Solid electrolytes (SEs) are believed to prevent Li dendrite growth because of high mechanical strength and high Li+ transference numbers. Significant advances in SE have been achieved, among which, Li7La3Zr2O12 (LLZO) and Li2S–P2S5 (LPS) are the most promising SEs for bulk-type solid-state lithium batteries because of high ionic conductivities (>10-4 S/cm2). However, in contrast to our expectations, the growth of lithium dendrites is not suppressed but is facilitated in LLZOs and LPSs regardless of dopants, porosity, and crystallinity of the electrolytes. Despite the unity Li transference number and over two-times of shear modulus than that of Li metal, the critical current densities for Li plating and stripping in these SEs are less than 1.0 mA cm-2, which is one-fourth to one-tenth of that in liquid electrolytes at room temperature. The incompatibility between LLZO and LPS with Li metal seriously limits the energy density of all-solid-state batteries. The mechanism for lithium dendrite formation and growth in SEs are still disputable. Lack of understanding of the Li dendrite formation mechanism seriously impeded the development of solid-state lithium batteries. The development of the criterion for Li dendrite suppression is essential for the success of solid electrolyte lithium batteries. In this project, a criterion for Li dendrite suppression will be developed through thermodynamics and kinetics analysis of lithium dendrite nucleation/growth, which will guide the solid-state electrolyte design. Li7N2I-LiOH, Li5NI2-LiOH and Li3YCl6 solid electrolyte with high ionic conductivity and low electronic conductivity were used to validate the criterion for lithium dendrite suppression. Different surface modifications were also explored to enhance the dendrite suppression capability of SSEs.

25 ENERGY STORAGE

Radiation Damage Mechanisms in Oxide-Based Solid Electrolytes

Ion implantation is a promising approach to mitigate dendrite formation in metal anode solid-state batteries by modifying the chemical and mechanical properties of oxide-based electrolyte surfaces such as Li 7 La 3 Zr 2 O 12 (LLZO). Yet, the detailed atomistic mechanisms and potentially adverse side effects of ion implantation remain poorly understood. In this study, we used molecular dynamics simulations to elucidate the evolution of radiation-induced damage in LLZO. The results reveal that radiation damage is primarily driven by recoils from heavy ions in the lattice, producing antisite defect clusters whose density decreases as recoil energy increases, a counterintuitive finding that highlights complex cascade fragmentation. Radiation-induced disruption to the crystal sublattice connectivity, especially in the La–O network critical for Li-ion transport, leads to degradation in ionic pathways at low energies, while higher energy cascades can form new conduction pathways via enhanced Zr–O network connectivity. These findings provide a mechanistic foundation for optimizing ion implantation strategies that balance disruption of the lattice for surface modification for dendrite resistance with preservation of essential ionic conductivity.

Defects

Particle‐Size‐Dependent Lithium‐Ion Transport in PEO/LLZO Composite Electrolytes

Lithium-metal batteries with solid electrolytes can deliver higher energy density and improved safety than conventional Li-ion batteries. Among solid electrolyte candidates, polymer/ceramic composite electrolytes are attractive because they combine polymer flexibility with the high ionic conductivity of ceramics. However, whether ceramic fillers synergistically reduce polarization losses in the polymer matrix remains unclear. A central unknown is the critical polymer/ceramic interfacial resistance (Rint,crit), below which adding ceramics lowers electrolyte overpotential. Here, we present the first macroscale model framework to quantify R int,crit for composite electrolytes based on polyethylene oxide (PEO) and Ta-doped Li 7 La 3 Zr 2 O 12 (LLZO). A 1D model for DC-polarization of tri-layer cells (PEO-LiTFSI/LLZO/PEO-LiTFSI) shows that LLZO surface functionalization reduces the PEO/LLZO interfacial resistance, consistent with electrochemical impedance measurements. Extending to a 2D composite model, we show notably that Rint,crit scales linearly with LLZO particle diameter and shifts toward experimentally accessible values (e.g., 28.8 Ωcm 2 ) as particle size increases. At fixed ceramic volume fraction, larger LLZO particles reduce the number of interfacial crossings, driving more current through the ceramic phase and lowering concentration polarization. In contrast, R int,crit is largely independent of ceramic volume fraction. These results demonstrate that ceramic filler-size engineering can enable synergistic, energy-efficient transport in polymer/ceramic composite electrolytes.

25 ENERGY STORAGE

Effect of H + Exchange and Surface Impurities on Bulk and Interfacial Electrochemistry of Garnet Solid Electrolytes

Contact loss and current constriction pose significant challenges at the Li metal interface of solid-state batteries. For garnet-structured Li 7 La 3 Zr 2 O 12 (LLZO), these effects are amplified by Li + /H + exchange and surface contamination reactions, which lead to conductivity losses and poor Li wetting. In this study, we utilize a variety of surface treatment processes across 37 cells to selectively induce proton exchange and contamination reactions in LLZO. The resulting bulk and surface chemistry is systematically characterized and correlated to changes in electrochemical properties. Additionally, we combine impedance analysis and finite element method modeling to deconvolute sources of impedance contributions at the Li metal interface. Specifically, we show that constriction impedance at the Li metal interface arises not solely from voids, but also from ionically-resistive surface contaminants. Further, these findings emphasize the connection between ionic conductivity and constriction, demonstrating that micron-scale ionically-resistive components increase constriction even with identical contact geometries. Finally, we leverage our comprehensive dataset to highlight unstable overpotential growth as a failure mechanism, additionally showing that the phase of a cell’s impedance is a sensitive indicator for the onset of interfacial instability. Overall, this study clarifies the impacts of proton exchange and surface contamination on electrochemical properties at the Li|solid electrolyte interface and elucidates insights that are generalizable to other solid-state battery systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Nanoscale Miscibility in In Situ Polymerized Hybrid Electrolytes Speeds Up Ion Dynamics and Enables Stable Cycling of Li Metal Batteries

While the potential use of copolymerized electrolytes in Li metal batteries is subject to intense investigation, the fundamental understanding of the nanoscale domain formation and its effect on Li + transport is still lacking. In this study, we investigated the correlation between the Li + transport mechanism and the miscibility of monomers in polymer blend electrolytes derived from the in situ copolymerization of methyl methacrylate (MMA) and vinylene carbonate (VC) in the presence of polyethylene glycol dimethyl ether (PEGDME) plasticizer and bis(trifluoromethanesulfonyl)imide (LiTFSI) salt. The addition of a polar short chain plasticizer reduced the dynamic and structural heterogeneities of the electrolyte. Small-angle X-ray scattering (SAXS) measurements and coarse-grained molecular dynamics (MD) simulations were used to investigate the nanoscale structure of the electrolytes. The distribution of relaxation times corresponding to the three distinct diffusion mechanisms of the free and interfacial Li + ions at the copolymer/plasticizer and electrolyte/SEI boundaries was analyzed in a broad temperature range to elucidate the Li + transport mechanism. Furthermore, the chemical composition of the SEI and the contribution of a ceramic lithium lanthanum zirconium oxide (LLZO, Li 7 La 3 Zr 2 O 12 ) phase on the interfacial resistance, salt degradation, and SEI stability were studied by X-ray photoelectron spectroscopy (XPS) depth profile analysis and electrochemical testing.

Li metal

Methods for Quantitative Thermal Analysis of Lithium Solid-State and Beyond Battery Safety

The use of differential scanning calorimetry (DSC) to measure the thermal behavior of individual components and electrolyte/electrode combinations is common. However, here we focus on DSC tests on an anode, cathode, and electrolyte (ACE) component combination over a temperature range that includes many of the phase transitions and key reactions (i.e., to 500 °C) that contribute to thermal runaway. This method can help quantify the complex reaction network in a full cell, thereby informing potential safety issues. Here, we used DSC heat flow data from a solid-state Li 0.43 CoO 2 +C+PVDF | LLZO | Li metal ACE sample and its components to quantify key factors affecting results. We focused on three areas: (1) ACE sample preparation and assembly in DSC pans, (2) DSC measurement parameters, and (3) heat flow analysis. Key points include the choice of component ratios (e.g., commercially relevant N:P capacity ratio), the importance of conductive carbon and binder, type of pan used, DSC ramp rate, and integration method used when dealing with broad and overlapping exothermic peaks. This work deepens the scientific basis and best practices for obtaining heat flow data from ACE samples for early-stage evaluation of solid-state and beyond battery safety.

25 ENERGY STORAGE

Ion Size Effects on the Thermodynamic, Kinetic, and Mechanical Properties during Ion Exchange in Solid-State Electrolytes

Ion exchange offers a pathway to impose residual compressive stresses to mitigate the electro-chemo-mechanical cracking of solid-state electrolytes such as lithium lanthanum zirconium oxide. This study uses a coupled multiscale framework (integrating density functional theory (DFT), molecular dynamics (MD), and continuum modeling) to examine how exchange ion size influences stress, diffusion, fracture toughness, and electronic properties. Larger isovalent ions (Na + , Ag + , K + ) were exchanged with Li + , with DFT confirming their preference for octahedral 96h sites and a linear relationship between ion size and chemical free expansion coefficient. MD simulations reveal stress and concentration effects on exchange ion diffusivity at elevated temperatures, with Na + and Ag + maintaining favorable mobility while K + showing concentration-dependent clustering. Continuum modeling predicts the range of fracture strength improvements and the required ion exchange concentration profile. It was shown that a 5% surface exchange concentration can induce ∼0.6 GPa of surface compressive stress using Na + and ∼1.0 GPa of surface compressive stress using Ag + . On the other hand, larger ion exchange species may penalize Li + diffusivity by increasing the activation volume and activation energy. Interestingly, Na + has a negligible penalty on Li-ion diffusivity. The room temperature Li + ion diffusivity is reduced by ∼40% with Ag + ion exchange. Electronic band structure analysis shows no size-dependent change in the bandgap, though Ag + introduces localized defect states near the valence band maximum. This study highlights ion size as a key factor in optimizing LLZO properties, offering a framework to improve the solid-state battery performance.

Jagad, Harsh D. [Brown Univ., Providence, RI (Unit

Pristine Interface between Lithium Lanthanum Zirconate and Lithium Manganese Oxide by Pulsed Laser Deposition

Solid state lithium-ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid-electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO), with the high voltage cathode, spinel Li x Mn 2 O 4 (LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x-ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer-by-layer deposition of LLZTO and Li 3 N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li 2 MnO 3 , which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn 2 O 4 has a voltage of ≈3.7 V versus Li+/Li, the observation of a well-defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.

Garnet LLZO

A multiscale model to understand the interface chemistry, contacts, and dynamics during lithium stripping

A reversible Li-metal electrode, paired with a solid electrolyte, is critical for attaining higher energy density and safer batteries beyond the current lithium-ion cells. A stable stripping process may be even harder to attain as the stripping process will remove Li-atoms from the surface, and naturally reduce surface contact area, if not self-corrected by other mechanisms, such as diffusion and plastic deformation under an applied external stack pressure. Here, we capture these mechanisms occurring at multiple length- and time- scales, i.e., interface interactions, vacancy hopping, and plastic deformation, by integrating density functional theory (DFT) simulations, kinetic Monte Carlo (KMC), and continuum finite element method (FEM). By assuming the self-affine nature of multiscale contacts, we predict the steady-state contact area as a function of stripping current density, interface wettability, and stack pressure. We further estimate the exponential increase of overpotential due to contact area loss to maintain the same stripping current density. We demonstrate that a lithiophilic interface requires less stack pressure to reach the same steady-state contact area fraction than a lithiophobic interface. A “tolerable steady-state” contact area loss for maintaining stable stripping is estimated at 20 %, corresponding to a 10 % increase in overpotential. To constrain contact loss within the tolerance, the required stack pressure is 0.1, 0.5, and 2 times the yield strength of lithium metal for three distinct interfaces, lithiophilic Li/lithium oxide(Li2O), Li/lithium lanthanum zirconium oxide(LLZO), and lithiophoblic Li/lithium fluoride(LiF), respectively. The modeling results agree with experiments on the impact of the stack pressure quantitatively, while the discrepancy in stripping rate sensitivity is attributed to the simplifying interface interaction in our simulations. Overall, this multiscale simulation framework demonstrates the importance of electrochemical-mechanical coupling in understanding the dynamics of the Li/SE interface during stripping.

Feng, Min

Demonstration of the Reproducibility Challenges in the Sintering Behavior of Lithium‐Stuffed Garnets in Scaling up Synthesis

Lithium-stuffed garnets, such as Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for next-generation solid-state batteries because of their high room-temperature ionic conductivity and chemical stability against lithium metal anodes, which are crucial for achieving higher energy density. However, realizing LLZO's potential in practical devices requires synthesis methods that can be scaled reliably to large batch sizes for manufacturing. Herein, we investigate the sintering reproducibility of LLZO synthesized at larger scales using ultrasonic spray pyrolysis, a cost-effective and scalable synthesis route. Two 100 g batches of Al-doped LLZO are prepared and their sintering behavior is examined in detail. Both Al-LLZO batches contain over 90 wt.% cubic-phase LLZO, and both batches exhibit room temperature conductivities greater than 1 × 10 −4 S cm −1 at a relative density above 0.8. However, variations in secondary phases and subtle differences in Al content lead to significant differences in densification and microstructure. These results demonstrate that LLZO's sintering behavior is highly sensitive to small changes in secondary phases and Al content, creating reproducibility challenges when moving from laboratory- to manufacturing-scale synthesis.

36 MATERIALS SCIENCE