Search NASA⌕ Search

SEARCH · Search NASA

Results for “Layered oxide scale”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Oxidation instability of SiC and Si3N4 following thermal excursions

The effect of thermal excursion and thermal cycling on the oxidation stability of chemical vapor-deposited (CVD) SiC and Si3N4 was studied at 1350 C. Thermal cycling alone produced no noticeable change in oxidation kinetics. However, TEM showed that oxide scales grown in cycles consist of alternating layers of SiO2 and Si2N2O. When the oxidation of CVD SiC or Si3N4 at 1350 C was interrupted with a 1.5-h annealing in Ar at 1500 C, the kinetics of reoxidation at 1350 C were found to be drastically increased. The SiC and Si3N4 then oxidized essentially at the same rate, which is over 50 times the preannealing rate, and comparable to the expected oxidation rate of these materials at 1500 C.

Ogbuji, Linus U. J. T.↗

Morphological and chemical characteristics of oxide scales formed on δ-phase plutonium metal alloys II: 2.0 at% Ga

The focused ion-beam scanning electron microscopy (FIB-SEM) and three-dimensional (3D) microscopy were applied to characterize the subsurface morphological features of oxide scales formed on an ~2.0 at. % Ga plutonium (Pu) metal alloy. Using the FIB-SEM technique, a number of morphological features formed in the interior of the oxide scale from Pu metal’s environmental exposure were observed and identified. Auger electron spectroscopy (AES) was utilized to characterize the cross-sectional composition and chemistry of the oxide scale. The oxide scale formed during inert storage and operational environments was found to be highly variable in thickness and morphology, presenting some regions with a thin (<400 nm), dense oxide layer and others with a thick (>2 µm) scale with substantial lateral cracking. After subsequent exposure to dry air environment, the oxide scale became thicker (~4 µm) and slightly more porous. The changes following aging in a moist air environment were observed to be more severe, with the formation of a highly porous internal structure containing significant lateral and transverse cracking. In comparison to the scale formed on an ~3.5 at. % Ga-Pu metal alloy, the oxide morphology of the lower gallium alloy investigated here exhibited greater variation in thickness and a noteworthy dependence on the presence of water vapor, particularly in terms of the internal porosity formed during growth of the oxide.

36 MATERIALS SCIENCE↗

Suppressing Atmospheric Degradation of Sulfide-Based Solid Electrolytes via Ultrathin Metal Oxide Layers

Sulfide-based solid-state electrolytes (SSEs) are promising materials with superior Li-ion conductivity; however, their poor atmospheric stability limits commercial manufacturing at scale. Here, we investigate the impact of ultrathin metal oxide layers deposited via atomic layer deposition (ALD) on the stability of Li 6 PS 5 Cl (LPSCl). Al 2 O 3 layers grown directly on LPSCl particles significantly stabilize the surface chemistry and Li-ion transport properties relative to uncoated material upon exposure to both an ambient atmosphere (22% relative humidity, RH) and humidified O 2 (100% RH). Detailed investigations indicate that coatings impede the surface and bulk degradation kinetics of exposed materials, even for coatings as thin as ∼1 Å. Furthermore, this suggests that stabilization is due to more than just a physical barrier. Shifts in valence band edge positions of coated LPSCl indicate that ALD coatings alter the surface electronic structure and resulting oxidation tendency of underlying LPSCl, suggesting new avenues to improving the environmental stability of sulfide SSEs.

Atmospheric chemistry↗

Morphological and chemical characteristics of oxide scales formed on δ-Phase plutonium metal alloys I: 3.5 at% ga

Focused ion-beam scanning electron microscopy (FIB-SEM) and three-dimensional (3D) microscopy were applied to characterize the subsurface morphological features of oxide scales formed on an ~3.5 at.% Ga plutonium (Pu) metal alloy. Using the FIB-SEM technique, a number of morphological features formed in the interior of the oxide scale from Pu metal's environmental exposure were observed and identified. Here, Auger electron spectroscopy (AES) was utilized to characterize the cross-sectional composition and chemistry of the oxide scale. The oxide scale formed during inert storage and operational environments has a characteristic internal scale structure that includes a relatively dense oxide layer with some lateral and transverse cracking. Generally, after subsequent exposure to dry air environment, the oxide scale retained most of the original structural and chemical characteristics. However, after aging in a moist air environment, while the oxide scale was found to maintain the chemical characteristics of the source oxide, the scale was found to be on average thinner and without the previously observed internal microcracking, likely the result of spallation of the source scale during exposure to the new environment.

36 MATERIALS SCIENCE↗

Some TEM observations of Al2O3 scales formed on NiCrAl alloys

The microstructural development of Al2O3 scales on NiCrAl alloys has been examined by transmission electron microscopy. Voids were observed within grains in scales formed on a pure NiCrAl alloy. Both voids and oxide grains grew measurably with oxidation time at 1100 C. The size and amount of porosity decreased towards the oxide-metal growth interface. The voids resulted from an excess number of oxygen vacancies near the oxidemetal interface. Short-circuit diffusion paths were discussed in reference to current growth stress models for oxide scales. Transient oxidation of pure, Y-doped, and Zr-doped NiCrAl was also examined. Oriented alpha-(Al, Cr)2O3 and Ni(Al, Cr)2O4 scales often coexisted in layered structures on all three alloys. Close-packed oxygen planes and directions in the corundum and spinel layers were parallel. The close relationship between oxide layers provided a gradual transition from initial transient scales to steady state Al2O3 growth.

Smialek, J.↗

Some TEM observations of Al2O3 scales formed on NiCrAl alloys

The microstructural development of Al2O3 scales on NiCrAl alloys has been examined by transmission electron microscopy. Voids have been observed within grains in scales formed on a pure NiCrAl alloy. Both voids and oxide grains grew measurably with oxidation time at 1100 C. The size and amount of porosity decreased towards the oxide-metal growth interface. It was postulated that the voids resulted from an excess number of oxygen vacancies near the oxide-metal interface. Short-circuit diffusion paths were discussed in reference to current growth stress models for oxide scales. Transient oxidations of pure, Y-doped, and Zr-doped NiCrAl was also examined. Oriented alpha-(Al,Cr)2O3 and Ni(Al,Cr)2O4 scales often coexisted in layered structures on all three alloys. Close-packed oxygen planes and directions in the corundum and spinel layers were parallel. The close relationships between oxide layers provided a gradual transition from initial transient scales to steady state Al2O3 growth.

Smialek, J.↗

Effect of water vapor on high-temperature oxidation of NiAl alloy

The high-temperature oxidation of NiAl is studied with dry oxygen and water vapor. The oxidation in H 2 O results in a thicker Al 2 O 3 oxide scale than that in O 2 . The oxide scale formed initially is a single layer of γ-Al 2 O 3 that subsequently transforms into a α-Al 2 O 3 /γ-Al 2 O 3 bilayer structure, in which the inner α-Al2O3 layer formed in H2O has a higher porosity than that in O 2 . Finally, further density functional theory calculations show that H protons derived from H 2 O molecules penetrate into the oxide lattice and boost the formation of lattice vacancies in both α-Al 2 O 3 and γ-Al 2 O 3 , thus enhancing the oxide scale growth.

36 MATERIALS SCIENCE↗

Impact of Residual Lithium on the Adoption of High-Nickel Layered Oxide Cathodes for Lithium-Ion Batteries

High-nickel layered oxide cathodes are becoming appealing for lithium-ion batteries employed in portable electronics and electric vehicles because of their higher energy density, low or no cobalt content, and ability to be manufactured with existing infrastructure. However, high-nickel layered oxides are plagued by the formation of residual lithium species, such as LiOH and Li 2 CO 3 , on the surface, which are detrimental to the manufacturing process and performance. Despite the problems residual lithium causes for the industry, academia mainly focuses on the safety risks and electrochemical impacts of residual lithium. In this Perspective, we examine the residual lithium problem through a lens of its impact on cathode slurry instability and large-scale manufacturing of high-nickel layered oxides. Additionally, methods of measuring residual lithium are discussed from the perspective of their accuracy as well as practicality in the manufacturing process. Furthermore, we hope that this Perspective would encourage the academic endeavor to consider the practical obstacles caused by residual lithium on the industrialization of high-nickel layered oxides and their mitigation, while attempting to improve their electrochemical performance and safety through doping, surface modifications, or other approaches.

25 ENERGY STORAGE↗

Reaction inhomogeneity coupling with metal rearrangement triggers electrochemical degradation in lithium-rich layered cathode

High-energy density lithium-rich layered oxides are among the most promising candidates for next-generation energy storage. Unfortunately, these materials suffer from severe electrochemical degradation that includes capacity loss and voltage decay during long-term cycling. Present research efforts are primarily focused on understanding voltage decay phenomena while origins for capacity degradation have been largely ignored. Here, we thoroughly investigate causes for electrochemical performance decline with an emphasis on capacity loss in the lithium-rich layered oxides, as well as reaction pathways and kinetics. Advanced synchrotron-based X-ray two-dimensional and three-dimensional imaging techniques are combined with spectroscopic and scattering techniques to spatially visualize the reactivity at multiple length-scales on lithium- and manganese-rich layered oxides. These methods provide direct evidence for inhomogeneous manganese reactivity and ionic nickel rearrangement. Coupling deactivated manganese with nickel migration provides sluggish reaction kinetics and induces serious structural instability in the material. Our findings provide new insights and further understanding of electrochemical degradation, which serve to facilitate cathode material design improvements.

25 ENERGY STORAGE↗

Calcination Heterogeneity in Li-Rich Layered Oxides: A Systematic Study of Li 2 CO 3 Particle Size

Li- and Mn-rich (LMR) layered oxide positive-electrode materials exhibit high energy density and have earth-abundant compositions relative to conventional Ni-, Mn-, and Co-oxides (NMCs). The lithiation of coprecipitated precursors is a key part of the synthesis and offers opportunities for tuning the properties of LMR materials. Whereas the morphology of transition metal precursors has received substantial attention, that of Li sources has not. Using Li 1.14 Mn 0.57 Ni 0.29 O 2 as a model system, in this work, we establish a detailed understanding of LMR calcination pathways via in situ and ex situ diffraction, spectroscopy, microscopy, and thermogravimetry. Our work shows that a large Li 2 CO 3 particle size modulates a previously misunderstood thermogravimetric feature present at the Li 2 CO 3 melting point during layered oxide calcination and causes heterogeneity at larger length scales (inter-secondary particle) than previously reported (intra-secondary particle). We found that electrochemical performance is largely insensitive to this heterogeneity. Finally, this work highlights the sensitivity of layered oxide calcination pathways to synthesis conditions and suggests design rules to minimize calcination heterogeneity in layered oxides beyond LMR.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical deposition of amorphous aluminum oxides on lead pipes to prevent lead leaching into the drinking water

Over 5000 public drinking water systems in the US are out of compliance with the Lead and Copper Rule. Lead leaching from lead pipes is limited by the solubility of a naturally occurring scale. Changes in water quality may cause this scale to become more soluble, releasing lead into the drinking water. We propose a novel electrochemical method to prevent lead leaching from lead pipes. In this method, an aluminum wire and an alkaline phosphate electrolyte are inserted into the pipes. The pipes are then anodized for 2 h by using an external power supply, resulting in the electrodeposition of an insoluble aluminum oxide layer on top of the preexisting scale. This technology was tested on lead pipes from the EBMUD water distribution systems located in Berkeley, CA, using recirculating synthetic and actual tap water for 120 days. The untreated pipes leached an average of 23 ppb and 38 ppb of lead respectively, when using free chlorine and monochloramine as disinfection residuals. In contrast, the treated pipes leached 3 ppb and 5 ppb respectively. These results suggest that the proposed treatment has the potential to prevent lead leaching regardless of the disinfection residual and thus should be further explored in a field trial.

36 MATERIALS SCIENCE↗

Role of Si2N2O in the passive oxidation of chemically-vapor-deposited Si3N4

The results of two-step oxidation experiments on chemically-vapor-deposited Si3N4 and SiC at 1350 C show that a correlation exists between the presence of a Si2N2O interphase and the strong oxidation resistance of Si3N4. During normal oxidation, k sub p for SiC was 15 times higher than that for Si3N4, and the oxide scale on Si3N4 was found by SEM and TEM to contain a prominent Si2N2O inner layer. However, when oxidized samples are annealed in Ar for 1.5 h at 1500 C and reoxidized at 1350 C as before, three things happen: the oxidation k sub p increases over 55-fold for Si3N4, and 3.5-fold for SiC; the Si3N4 and SiC oxidize with nearly equal k sub p's; and, most significantly, the oxide scale on Si3N4 is found to be lacking an inner Si2N2O layer. The implications of this correlation for the competing models of Si3N4 oxidation are discussed.

Ogbuji, Linus U. J. T.↗

Adherent Al2O3 scales formed on undoped NiCrAl alloys

Changes in the spalling behavior of Al2O3 scales formed on an undoped NiCrAl alloy are described. Two samples of Ni-15Cr-13Al (wt pct), one a control and the other sanded, were subjected to 25 oxidation cycles. It is observed that adherent scales formed on the sanded sample; however, the control sample had speckled, spalled scales. The data reveal that the adherent scales are caused by repeated removal of surface layers after each oxidation cycle. It is determined that interfacial segregation of sulfur influences spallation and sulfur removal increases bonding. The effect of moisture on scale adhesions is investigated.

Smialek, James L.↗

Understanding oxidation of Fe-Cr-Al alloys through explainable artificial intelligence

Abstract The oxidation resistance of FeCrAl based on alloying composition and oxidizing conditions is predicted using a combinatorial experimental and artificial intelligence approach. A neural network (NN) classification model was trained on the experimental FeCrAl dataset produced at GE Research. Furthermore, using the SHapley Additive exPlanations (SHAP) explainable artificial intelligence (XAI) tool, we explore how the NN can showcase further material insights that are unavailable directly from a black-box model. We report that high Al and Cr content forms protective oxide layer, while Mo in FeCrAl creates thick unprotective oxide scale that is vulnerable to spallation due to thermal expansion. Graphical abstract

Materials Science↗

Electrically Conductive and Protective Coating Compatibility with LSCF Cathodes

Ferritic stainless-steel interconnect materials are used in intermediate or high-temperature SOFCs because of their oxidation resistance, high formability, and low cost. Their corrosion resistance is due to the formation of a protective chromium oxide scale during operation. However, the protective oxide layer produces Cr-containing volatile species at SOFC operating temperatures and conditions, which can cause cathode poisoning. Spinel coatings have been developed to prevent cathode poisoning while maintaining an electrically conductive pathway through SOFC stacks. Generally, Mn-Co-O spinel has been the material of choice, but PNNL has developed an Mn-Cu-O spinel protective coating to remove the costly Co and enhance the electrical conductivity. This paper will focus on the electrically conductive coating’s compatibility with LSCF in high-temperature operating environments.

Choi, Jung-Pyung↗

Ultrathin Magnesium-Based Coating as an Efficient Oxygen Barrier for Superconducting Circuit Materials

Scaling up superconducting quantum circuits based on transmon qubits necessitates substantial enhancements in qubit coherence time. Over recent years, tantalum (Ta) has emerged as a promising candidate for transmon qubits, surpassing conventional counterparts in terms of coherence time. However, amorphous surface Ta oxide layer may introduce dielectric loss, ultimately placing a limit on the coherence time. In this study, a novel approach for suppressing the formation of tantalum oxide using an ultrathin magnesium (Mg) capping layer is presented. Synchrotron-based X-ray photoelectron spectroscopy studies demonstrate that oxide is confined to an extremely thin region directly beneath the Mg/Ta interface. Additionally, it is demonstrated that the superconducting properties of thin Ta films are improved following the Mg capping, exhibiting sharper and higher-temperature transitions to superconductive and magnetically ordered states. Moreover, an atomic-scale mechanistic understanding of the role of the capping layer in protecting Ta from oxidation is established based on computational modeling. Further, this work provides valuable insights into the formation mechanism and functionality of surface tantalum oxide, as well as a new materials design principle with the potential to reduce dielectric loss in superconducting quantum materials. Ultimately, the findings pave the way for the realization of large-scale, high-performance quantum computing systems.

36 MATERIALS SCIENCE↗

The evolution and growth of Al2O3 scales on beta-NiAl

The formation and growth of Al2O3 scales on (beta)-NiAl were studied using electron microscopy and other analytical techniques to gain an understanding of the oxidation properties of (beta)-NiAl and of alumina-forming alloys, in general. The transient and mature stages of oxidation were studied as well as the transformation stage during which the oxide scale transforms from metastable Al2O3 phases to the thermodynamically stable alpha-Al2O3 phase. The transient oxidation stages were studied at 800 deg C and for short times at 1100C. At 800C, the scales consist predominantly of delta-Al2O3 which forms by cation vacancy ordering in the defective spinel lattice of gamma-Al2O3. At 1100C, a fast-growth morphology of theta-Al2O3 forms as a surface layer over delta-Al2O3. For both oxidation temperatures, the scales are often epitaxially oriented with respect to the metal. The transient scales grow by outward cation diffusion as evidenced by surface growth morphologies. The transformation to alpha-Al2O3 occurs within 1 hour at 1100C by a nucleation and radial growth process. The large volume decrease associated with the transformation results in a highly strained alpha-Al2O3 microstructure. A change in scale growth mechanism from outward cation to inward anion diffusion allows transient surface morphologies to be smoothed by surface diffusion. The mature stage of oxidation involves the growth of an alpha-Al2O3 scale having the lacey morphology formed as a result of the gamma yields alpha transformation. Growth of the scale occurs by counterdiffusion along grain boundaries resulting in ridges formed by impingement of alpha-Al2O3 nuclei during the transformation stage. Also scale growth occurs by inward oxygen diffusion through healed cracks; the cracks result from transformation stresses. The measured growth rates of scales having the lacey morphology are an order of magnitude less than fine-grained alpha-Al2O3 scales. Metal orientations were found to have a large effect on oxide morpholoies during all stages of oxidation.

Doychak, J. K.↗

High-Temperature Oxidation Behavior of FeCoCrNi+(Cu/Al)-Based High-Entropy Alloys in Humid Air

Previous studies showed some transition metal high-entropy alloy (HEA) compositions can have good oxidation resistance in air up to 800 °C. Four equiatomic HEAs have been developed based on FeCoCrNi with additions of Mn, Cu, Al or Al+Cu. The oxidation behavior of these HEAs was compared in humid (10 vol.% H2O) air at 800 °C for 100–500 h to investigate the influence of water vapor on the oxidation mechanisms. The Cu- and Al-containing alloys exhibited improved oxidation resistance over the Mn composition. For the Cu-containing alloy, a local attack of the Cu-rich phase was observed, which formed an Fe/Ni/Co/Cr spinel that was surrounded by Cr2O3. This oxide was thicker for the humid air atmosphere when compared to dry air, and the transition of the Cu oxide to the spinel was accelerated. The Al-containing HEA formed a thin Al2O3 scale with humidity suppressing AlN formation and forming a smoother oxide layer. The Al+Cu composition had the highest overall oxidation resistance (minimal local attack, no nitridation) and also showed a smooth oxide scale topography under humid air oxidation as opposed to a plate-like, rougher scale under dry air.

Crystallography↗